Resumo:
Coarse (BOn/2)-O-n+/xH(2)O (10
Resumo:
Synthesis of calcium hydroxyapatite Ca-10(PO4)(6)(OH)(2) ceramic powders by a solid state reaction between commercially available tricalcium phosphate and calcium hydroxide powders has been attempted in the range 700-1000 degrees C. Reaction of tricalcium phosphate and calcium hydroxide in 3:2 molar ratio at 1000 degrees C leads to the formation of pure calcium hydroxyapatite phase. The sample has been characterised by XRD and IR spectral studies. The compacted powder is sintered to 93% of theoretical density when fired in air at 1300 degrees C for 2 hours.
Resumo:
Gadolinium oxide, cerium oxide, and 10 mol% gadolinia doped ceria ceramic powders have been synthesized using combustion technique. Though the cubic gadolinia phase is stable at room temperature, single phase monoclinic gadolinia was obtained as a result of combustion synthesis using fuel lean and stoichiometric precursor compositions. This powder was subjected to calcination treatment and ceria doping to study the stability of phases and the rate of phase transformation from monoclinic to cubic gadolinia. It was found that monoclinic gadolinia transforms to cubic gadolinia upon calcination at temperatures less than 1200 degrees C. It was also found that rate of phase transformation is more for powder produced using fuel lean compositions; and the rate is enhanced upon ceria doping. (C) 2015 Elsevier Ltd. All rights reserved.
Resumo:
Fine-particle metal chromites (MCr2O4, where M = Mg, Ca, Mn, Fe, Co, Ni, Cu, and Zn) have been prepared by the combustion of aqueous solutions containing the respective metal nitrate, chromium(III) nitrate, and urea in stoichiometric amounts. The mixtures, when rapidly heated to 350°C, ignite and yield voluminous chromites with surface areas ranging from 5 to 25 m2/g. MgCr2O4, sintered in air at 1500°C for 5 h, has a density of 4.0 g/cm3.
Resumo:
In situ formations of Al2O3 + ZrO2 + SiCW ternary composite powders have been obtained by carbothermal reduction of a mixture of Sillimanite. Kaolin and Zircon using two different carbon sources. Products formed were mixtures of alumina and zirconia along with silicon carbide in the form of whiskers. The effects of composition of the reactants, the role of fineness of the starting precursors and the nature of the carbon Source on the final product powder obtained are presented. XRD and SEM analyses indicate complete reaction of the precursors to yield Al2O3 + ZrO2 + SiCW as product powders, with the SiC having whisker morphology. It is also seen that zirconia could be stabilised to some extent in the tetragonal form without any stabilising agent by tailoring the starting materials and their composition. (C) 2002 Published by Elsevier Science B.V.
Resumo:
Nano ceramic alumina powders are synthesized by solution combustion synthesis using aluminium nitrate as oxidizer and urea as fuel with different fuel to oxidizer ratio. The variation of adiabatic flame temperatures are calculated theoretically for different fuel/oxidizer ratio according to thermodynamic concept and correlated with the observed flame (reaction) temperatures. A ``multi channel thermocouple setup connected to computer interfaced Keithley multi meter 2700'' is used to monitor the thermal events occurring during the process. The combustion products, characterized by XRD, show that the powders are composed of polycrystalline oxides with crystallite size of 32 to 52 nm. An interpretation based on maximum combustion temperature and the amount of gases produced during reaction for various fuel to oxide ratio has been proposed for the nature of combustion and its correlation with the characteristics of as-synthesized powder.
Resumo:
Fine powders comprising nanocrystallites of Ba0.85Ca0.15Zr0.1Ti0.9O3 (BCZT) were synthesized via oxalate precursor method, which facilitated to obtain homogenous and large grain sized ceramics at a lower sintering temperature. The compacted powders were sintered at various temperatures in the range of 1200 degrees C-1500 degrees C for an optimized duration of 10 h. Interestingly the one that was sintered at 1450 degrees C/10 h exhibited well resolved Morphotrophic Phase Boundary. The average grain size associated with this sample was 30 mu m accompanied by higher domain density mostly with 90 degrees twinning. These were believed to have significant contribution towards obtaining large strain of about 0.2% and piezoelectric coefficient as high as 563 pC/N. The maximum force that was generated by BCZT ceramic (having 30 mu m grain size) was found to be 161 MPa, which is much higher than that of known actuator materials such as PZT (40MPa) and NKN-5-LT (7 MPa). (C) 2014 AIP Publishing LLC.
Resumo:
Plasma sprayable powders were prepared from ZrO2-CaO-CeO2 system using an organic binder and coated onto stainless steel substrates previously coated by a bond coat (Ni 22Cr 20Al 1.0Y) using plasma spraying. The coatings exhibited good thermal barrier characteristics and excellent resistance to thermal shock at 1000 degrees C under simulated laboratory conditions (90 half hour cycles without failure) and at 1200 degrees C under accelerated burner rig test conditions (500 2 min cycles without failure). No destabilization of cubic/tetragonal ZrO2 phase fraction occured either during the long hours (45 h cumulative) or the large number of thermal shock tests. Growth of a distinct SiO2 rich region within the ceramic was observed in the specimens thermal shock cycled at 1000 degrees C apart from mild oxidation of the bond coat. The specimens tested at 1200 degrees C had a glassy appearance on the top surface and exhibited severe oxidation of the bond coat at the ceramic-bond coat interface. The glassy appearance of the surface is due to the formation of a liquid silicate layer attributable to the impurity phase present in commercial grade ZrO2 powder. These observations are supported by SEM analysis and quantitative EDAX data.
Resumo:
Attempts to prepare BaSnO3 by the hydrothermal method starting from SnO2·xH2O gel and Ba (OH)2 solution in teflonlined autoclaves at 150–260°C invariably lead to the formation of a hydrated phase, BaSn(OH)6·3H2O. On heating in air or on releasing the pressure Image at ≈260°C, BaSN (OH)6·3H2O converts to BaSnO3 fine powder which involves the formation of an intermediate oxyhydroxide, BaSnO(OH)4. TEM studies show that particle size of the resulting BaSnO3 ranges from 0.2–0.6 μm. Solid solutions of Ba(Ti, Sn) O3 were prepared from (TiO2+SnO2)·xH2O mixed gel and Ba(OH)2 solutions. Single-phase perovskite Ba(Ti, Sn)O3 was obtained up to 35 atom % Sn. Above this composition, the hydrothermal products are mixtures of BaTiO3 (cubic) and BaSn(OH)6·3H2O which on heating at ≈260°C give rise to BaTiO3+BaSnO3. Annealing at 1000°C results in monophasic Ba(Ti, Sn)O3, in the complete range of Sn/Ti. Formation of the hydrated phase is attributed to the amphoteric nature of SnO2·xH2O gel which stabilises Sn(OH)62− anions under higher H2O-pressures and elevated temperatures. The sintering characteristics and dielectric properties of ceramics prepared from these fine powders are presented.
Resumo:
We demonstrate ordered array formation of Au nanoparticles by controlled solid-state dewetting of a metal film on stepped alumina substrates. In situ transmission electron microscopy studies reveal that the dewetting process starts with nucleation of ordered dry regions on the substrate. The chemical potential difference between concave and convex surface regions induces anisotropic metal diffusion leading to the formation of nanowires in the valleys. The nanowires fragment due to Rayleigh instability forming arrays of metal nanoparticles on the substrate. The length scale of reconstruction relative to the starting film thickness is an important parameter in controlling the spatial order of the nanoparticles.
Resumo:
Ultrafine powders of SrTiO3 are prepared at 100–150°C by the hydrothermal method, starting from TiO2·xH2O gel and Sr(OH)2 and H2O-isopropanol mixed solvent as the medium, The X-ray diffractograms of the powder show line broadening. The minimum crystallite size obtained ranges from 5 to 20nm with 20% H2O-80% C3H7OH as the reaction medium, as estimated from X-ray half-peak widths and TEM studies. The electron diffraction results indicate high concentration of lattice defects in these crystallites. The optical spectra of the particle suspensions in water show that the absorption around the band gap is considerably broadened, together with the appearance of maxima in the far ultraviolet. Aqueous suspensions of SrTiO3 powders, as such, do not produce H2 or O2 on UV irradiation. After coating with rhodium, H2 and O2 are evolved on illumination. However, the turn over number of O2 is lower than the stoichiometrically expected values from the corresponding values of H2. No correlation of the photocatalytic activity with surface area is observed. The activity of Rh-SrTiO3 slowly deteriorates with extended period of irradiation.
Resumo:
The spherical indentation strength of a lead zirconate titanate (PZT) piezoelectric ceramic was investigated under poled and unpoled conditions and with different electrical boundary conditions (arising through the use of insulating or conducting indenters). Experimental results show that the indentation strength of the poled PZT is higher than that of the unpoled PZT. The strength of a poled PZT under a conducting indenter is higher than that under an insulating indenter. Poling direction (with respect to the direction of indentation loading) did not significantly affect the strength of material. Complementary finite element analysis (FEA) of spherical indentation of an elastic, linearly coupled piezoelectric half-space is conducted for rationalizing the experimental observations. Simulations show marked dependency of the contact stress on the boundary conditions. In particular, contact stress redistribution in the Coupled problem leads to a change in the fracture initiation, from Hertzian cracking in the unpoled material to Subsurface damage initiation in poled PZT. These observations help explain the experimental ranking of strength the PZT in different material conditions or under different boundary conditions.
Resumo:
Fine powders consisting of 0.1–0.5 μm size crystallites of CaTiO3 are prepared at 150–200°C by the hydrothermal method starting from hydrated titania gel and reactive calcium oxide suspended as an aqueous slurry in an autoclave. The resulting high-purity CaTiO3 is characterised by TEM, X-ray powder diffraction, chemical analyses and sintering characteristics. The hydrothermally prepared CaTiO3 powders are sinterable to high-density ceramics below 1400°C. The dc conductivity behaviour of the chemically reduced ceramics is presented.
Resumo:
Magnetic measurements have been used in combination with transmission electron microscopy to investigate small nickel metal particles in metal-ceramic composites. Estimates of the average number of atoms in the particles are given for nonmagnetic samples with low Ni content.