24 resultados para automotive steels

em Indian Institute of Science - Bangalore - Índia


Relevância:

70.00% 70.00%

Publicador:

Resumo:

Density reduction of automotive steels is needed to reduce fuel consumption, thereby reducing greenhouse gas emissions. Aluminum addition has been found to be effective in making steels lighter. Such an addition does not change the crystal structure of the material. Steels modified with aluminum possess higher strength with very little compromise in ductility. In this work, different compositions of Fe-Al systems have been studied so that the desired properties of the material remain within the limit. A density reduction of approximately 10% has been achieved. The specific strength of optimal Fe-Al alloys is higher than conventional steels such as ultra-low-carbon steels.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A series of dual-phase (DP) steels containing finely dispersed martensite with different volume fractions of martensite (V-m) were produced by intermediate quenching of a boron- and vanadium-containing microalloyed steel. The volume fraction of martensite was varied from 0.3 to 0.8 by changing the intercritical annealing temperature. The tensile and impact properties of these steels were studied and compared to those of step-quenched steels, which showed banded microstructures. The experimental results show that DP steels with finely dispersed microstructures have excellent mechanical properties, including high impact toughness values, with an optimum in properties obtained at similar to 0.55 V-m. A further increase in V-m was found to decrease the yield and tensile strengths as well as the impact properties. It was shown that models developed on the basis of a rule of mixtures are inadequate in capturing the tensile properties of DP steels with V-m > 0.55. Jaoul-Crussard analyses of the work-hardening behavior of the high-martensite volume fraction DP steels show three distinct stages of plastic deformation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The occurrence of a maximum in the percentage of intergranular fracture on the fracture surface during the transition from intermediate to low fatigue crack growth rates has been observed for a high strength steel. It is suggested that transgranular planar slip leading to slip localization is essential in promoting intergranular fracture when the cyclic plastic zone size becomes equal to the prior austenite grain size.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Dimensional analysis using π-theorem is applied to the variables associated with plastic deformation. The dimensionless groups thus obtained are then related and rewritten to obtain the constitutive equation. The constants in the constitutive equation are obtained using published flow stress data for carbon steels. The validity of the constitutive equation is tested for steels with up to 1.54 wt%C at temperatures: 850–1200 °C and strain rates: 6 × 10−6–2 × 10−2 s−1. The calculated flow stress agrees favorably with experimental data.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Severe plastic deformation techniques are known to produce grain sizes up to submicron level. This leads to conventional Hall-Petch strengthening of the as-processed materials. In addition, the microstructures of severe plastic deformation processed materials are characterized by relatively lower dislocation density compared to the conventionally processed materials subjected to the same amount of strain. These two aspects taken together lead to many important attributes. Some examples are ultra-high yield and fracture strengths, superplastic formability at lower temperatures and higher strain rates, superior wear resistance, improved high cycle fatigue life. Since these processes are associated with large amount of strain, depending on the strain path, characteristic crystallographic textures develop. In the present paper, a detailed account of underlying mechanisms during SPD has been discussed and processing-microstructure-texture-property relationship has been presented with reference to a few varieties of steels that have been investigated till date.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

From a detailed re-examination of results in the literature, the effects of microstructure sizes, namely interlamellar spacing, pearlitic colony size and the prior austentitic grain size on the thresholds for fatigue crack growth (ΔKth) and crack closure (Kcl, th) have been illustrated. It is shown that while interlamellar spacing explicitly controls yield strength, a similar effect on ΔKth cannot be expected. On the other hand, the pearlitic colony size is shown to strongly influence ΔKth and Kcl, th through the deflection and retardation of cracks at colony boundaries. Consequently, an increase in ΔKth and Kcl, th with colony size has been found. The development of a theoretical model to illustrate the effects of colony size, shear flow stress in the slip band and macroscopic yield strength on Kcl, th and ΔKth is presented. the model assumes colony boundaries as potential sites for slip band pile-up formation and subsequent crack deflection finally leading to zig-zag crack growth. Using the concepts of roughness induced crack closure, the magnitude of Kcl, th is quantified as a function of colony size. In deriving the model, the flow stress in the slip band has been considered to represent the work hardened state in pearlite. Comparison of the theoretically predicted trend with the experimental data demonstrates very good agreement. Further, the intrinsic or closure free component of the fatigue threshold, ΔKeff, th is found to be insensitive to colony size and interlamellar spacing. Using a criterion for intrinsic fatigue threshold which considers the attainment of a critical fracture stress over a characteristic distance corresponding to interlamellar spacing, ΔKth values at high R values can be estimated with reasonable accuracy. The magnitude of ΔKth as a function of colony size is then obtained by summing up the average value of experimentally obtained ΔKeff, th values and the predicted Kcl, th values as a function of colony size. Again, very good agreement of the theoretically predicted ΔKth values with those experimentally obtained has been demonstrated.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A series of high-martensite dual-phase (HMDP) steels exhibiting a 0.3 to 0.8 volume fraction of martensite (V m ), produced by intermediate quenching (IQ) of a vanadium and boron-containing microalloyed steel, have been studied for toughness and fatigue behavior to supplement the contents of a recent report by the present authors on the unusual tensile behavior of these steels. The studies included assessment of the quasi-static and dynamic fracture toughness and fatigue-crack growth (FCG) behavior of the developed steels. The experimental results show that the quasi-static fracturetoughness (K ICV ) increases with increasing V m in the range between V m =0.3 and 0.6 and then decreases, whereas the dynamic fracture-toughness parameters (K ID , K D , and J ID ) exhibit a significant increase in their magnitudes for steels containing 0.45 to 0.60 V m before achieving a saturation plateau. Both the quasi-static and dynamic fracture-toughness values exhibit the best range of toughnesses for specimens containing approximately equal amounts of precipitate-free ferrite and martensite in a refined microstructural state. The magnitudes of the fatigue threshold in HMDP steels, for V m between 0.55 and 0.60, appear to be superior to those of structural steels of a similar strength level. The Paris-law exponents (m) for the developed HMDP steels increase with increasing V m , with an attendant decrease in the pre-exponential factor (C).

Relevância:

20.00% 20.00%

Publicador: