3 resultados para TiAl

em Indian Institute of Science - Bangalore - Índia


Relevância:

10.00% 10.00%

Publicador:

Resumo:

A microstructural and X-ray investigation of Ti-AI-Mo alloys Ti-31 Al-15 Mo, Ti-31 Al-13 Mo, Ti-31Al-9Mo and Ti-35Al-9Mo (containing the Ti3Al, TiAl and β phases) indicates that the existing phase diagram of the ternary system for this composition range published by Ge Dhzhi-Min and Pylaeva is in error above 1473 K. An analysis of phase relations reveals that the error has arisen from their use of the Ti-AI diagram due to Bumps, Kessler and Hansen as a basis for generating the ternary. It is shown that a phase diagram of the ternary, consistent with the experimental results, can be generated using a version of the Ti-AI system due to Margolin. Simple geometric arguments are used to build up a new semi-quantitative description of the Ti-AI-Mo system which can be used as a basis for a detailed investigation of phase equilibria in this system.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Hydrogen plasma can be used for deoxidation of functional materials containing reactive metals in both bulk and thin film forms. Since the different species in the plasma are not in thermodynamic equilibrium, application of classical thermodynamics to the analysis of such a system is associated with some difficulties. While global equilibrium approaches have been tried, with and without additional approximations or constraints, there is some ambiguity in the results obtained. Presented in this article is the application of a local equilibrium concept to assess the thermodynamic limit of the reaction of each species present in the gas with oxides or oxygen dissolved in metals. Each reaction results in a different pal tial pressure of H2O. Because of the higher reactivity of the dissociated and ionized species and the larger thermodynamic driving force for reactions involving these species, they act as powerful reducing agents. It is necessary to remove the products of reaction from the plasma to prevent back reaction and gradual approach to global equilibrium. A quantitative description using the framework of the Ellingham-Richardson-Jeffes diagrams is presented.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In the present study, solidification microstructure and texture evolution in grain-refined Ti-6Al-4V and γ-TiAl alloys via trace boron addition are compared with their baseline counterparts. Boron addition resulted in dramatic grain refinement by almost an order of magnitude. The texture developed in these alloys is also markedly different from the baseline alloys.