246 resultados para OXIDATION CATALYSIS
em Indian Institute of Science - Bangalore - Índia
Resumo:
Late-transition-metal-doped Pt clusters are prevalent in CO oxidation catalysis, as they exhibit better catalytic activity than pure Pt, while reducing the effective cost and poisoning However, completely eliminating the critical problem of Pt poisoning still poses a big challenge. Here, we report for the first time that, among the bimetallic clusters ((Pt3M where M = Co, Ni, and Cu)/MgO(100)), the CO adsorption site inverts for Pt3Co/MgO(100) from Pt to Co, due to the complete uptake of Pt d-states by lattice oxygen. While this resolves the problem of Pt poisoning, good reaction kinetics are predicted through low barriers for Langmuir-Hinshelwood and Mars van Krevelen (MvK) mechanisms of CO oxidation for Pt3Co/MgO(100) and Li-doped MgO(100), respectively. Li doping in MgO(100) compensates for the charge imbalance caused by a spontaneous oxygen vacancy formation. Pt-3 Co/Li-doped MgO(100) stands out as an exceptional CO oxidation catalyst, giving an MvK reaction barrier as low as 0.11 eV. We thereby propose a novel design strategy of d-band center inversion for CO oxidation catalysts with no Pt poisoning and excellent reaction kinetics.
Resumo:
In recent times, (thio)urea derivatives have become synonymous with hydrogen bonding owing to their extensive applicability as small molecule organocatalysts. In this paper, another activation mode by thiourea derivatives, namely via Lewis base catalysis, is disclosed for the NBS-mediated oxidation of alcohols. The mild reaction conditions employed here is suitable for chemoselective oxidation of secondary alcohol in the presence of primary alcohol.
Resumo:
Thiosulfate (S2O32−) and tetrathionate (S4O62−)are oxidized to sulfate by air at atmospheric pressure and 50–70°C in the presence of cuprous oxide (Cu2O) as catalyst. Sulfate is produced from S2O32− by series-parallel reaction paths involving S4O62− as an intermediate. The rate data obtained for air oxidation of S2O32− on Cu2O agree well with a pseudo-homogeneous first order kinetic scheme, yielding values of rate constants for series parallel reaction paths which have been used in modelling the catalyzed air oxidation of S2O32−. Air oxidation of S4O62− on Cu2O proceeds at a higher rate in the presence of S2O32− than in its absence. Cu2O is less active than Cu2S for the air oxidation of S2O32−, as shown by the rate constant values which for Cu2O catalyzed oxidation are an order of magnitude smaller than those for the Cu2S catalyzed oxidation.
Resumo:
Copper(II) complexes of quaternised poly(4-vinylpyridine) (PVP) of different degrees of quaternisation and copper content have been prepared by crosslinking the polymer with 1,2-dibromoethane in the presence of Cu2+ ion as template. The stability constant of the PVP---Cu(II) complexes is found to increase with the degree of crosslinking quaternisation of the resin, but the rate at which Cu2+ is adsorbed by the resin decreases. An optimum combination of both stability and rate can be achieved with a moderate degree (31%) of crosslinking. A kinetic study reveals that quaternisation increases significantly the catalytic activity of the complex for the oxidation of S2O2−3 by O2 compared with PVP----Cu(II) without quaternisation, but it deactivates the complex for the oxidation of both S3O2−6 and S4O2−6. The batch reactor oxidation kinetics at pH 2.16, where the rate is observed to be maximum, is well explained by the Langmuir—Hinshelwood model assuming the coordination of both O2 and thioanion to Cu(II) as a precursor to the oxidation reaction.
Resumo:
Calcined samples of chromia supported on Al2O3, ZnO, or SnO2 show both Cr(VI) and Cr(III) on the surface, Cr(VI) being preponderant in the case of Al2O3-supported catalysts. The proportion of Cr(VI) decreases with increase in Cr content of the calcined catalysts. Reduction of the supported chromia catalysts in H2 at 720 K for 1 hr gives rise to Cr(III) and Cr(V). On carrying out the dehydrogenation of cyclohexane on the chromia catalysts a higher proportion of Cr(V) is found than after treatment with hydrogen. Vanadia supported on Al2O3 or MoO3 shows significant proportion of V(IV) on carrying out the oxidation of toluene on the catalysts. Calcined MoO3 (10%)/Al2O3 shows only Mo(VI) on the surface at 300 K, but on heating to 670 K in vacuum shows the presence of a considerable proportion of Mo(V) which on cooling disproportionates to Mo(IV) and Mo(VI). Mo(V) is noticed on surfaces of this catalyst on reduction with hydrogen as also on carrying out dehydrogenation of cyclohexane. While Bi2MoO6 shows only Mo(VI) on the surface at 300 K, heating it to 670 K in vacuum changes it entirely to Mo(V) which then gives rise to Mo(IV) and Mo(VI) on cooling.
Resumo:
Continuous slurry reactor runs of two to four weeks duration were carried out for catalyzed air oxidation of thiosalts under a variety of conditions using poly (4-vinylpyridine) - Cu (II) and quaternized poly (4-vinylpyridine) - Cu (II) catalysts. Results obtained indicate that these catalysts have high activity and relatively long-term catalyst stability for thiosalt waste streams of < 1000 ppm thiosalt level. Using 2% (w/w) slurries of the poly (4-vinylpyridine) Cu (II) catalyst, effective oxidation of 700 ppm S2O32− influent to an effluent of < 100 ppm total thio-salts can be carried out continuously for at least one month when operating at 20 to 30°C with solution flow rates of$˜1l/h and aeration of 1300 XXX/h using a two-stage reactor system comprised of 12 l reactors. At higher thiosalt influent levels (i.e. > 1600 ppm) increased reaction temperatures enable depletion to < 100 ppm thiosalt effluent levels for up to one week of continuous operation. The catalysts deactivate much more readily at these higher influent levels as a result of greater copper losses and appreciable adsorption of S2O32− and S4O62−. The behaviour of continuous slurry reactors employed in the experimental studies, by use of batch reaction data for the poly (4-vinylpyridine) Cu (II) catalyzed oxidation of thiosalts, can be modelled successfully. Quaternized poly (4-vinylpyridine) Cu (II) catalyst has good long-term stability and copper losses are very low. The poly (4-vinylpyridine) Cu (II) catalyst, however, is susceptible to appreciable oxidation of the polymer matrix on long-term usage. This oxidation of the polymer matrix results in a substantial loss in the activity of the regenerated catalyst.
Resumo:
Ethanol oxidation in the vapor phase was studied in an isothermal flow reactor using thorium molybdate catalyst in the temperature range 220–280 °C. Under these conditions the catalyst was highly selective to acetaldehyde formation. The rate data were well represented by a steady state two-stage redox model given by the equation: View the MathML source The parameters of the above model were estimated by linear and nonlinear least squares methods. In the case of nonlinear estimation the sum of the squares of residuals decreased. The activation energies and preexponential factors for the reduction and oxidation steps of the model, estimated by nonlinear least squares technique are: 9.47 kcal/mole, 9.31 g mole/ (sec) (g cat) (atm) and 9.85 kcal/mole, 0.17 g mole/(sec) (g cat) (atm)0.5, respectively. Oxidations of ethanol and methanol over thorium molybdate catalyst were compared under similar conditions.
Resumo:
Rates of oxidation of p-xylene were measured in the temperature range 320 to 420 °C using tin vanadate as catalyst in an isothermal differential flow reactor. The amounts of p-xylene converted were determined by analyzing the main products (p-tolualdehyde, maleic anhydride, p-toluic acid and traces of terephthalic acid). Negligible amounts of products of complete combustion were formed. The reaction rates obtained for p-xylene followed the relation, Image based on the redox model. The mechanism of the reaction was determined by conducting different sets of experiments and it was found that the reaction followed the parallel-consecutive mechanism, in which p-tolualdehyde and maleic anhydride were formed from the parallel route whereas p-toluic acid was formed from the consecutive route.
Resumo:
Catalytic activity of cordierite honeycomb by a completely new coating method for the oxidation of major hydrocarbons in exhaust gas is reported here. The new coating process consists of (a) dipping and growing γ-Al2O3 on cordierite by combustion of monolith dipped in the aqueous solution of Al(NO3)3 and oxalyldihydrazide (ODH) (or glycine) at 600 °C and active catalyst phase Ce0.98Pd0.02O2−δ on γ-Al2O3-coated cordierite again by combustion of monolith dipped in the aqueous solution of ceric ammonium nitrate, ODH and 1.2 × 10−3 M PdCl2 solution at 500 °C. Weight of active catalyst can be varied from 0.02 wt% to 2 wt% which is sufficient but can be loaded even up to 12 wt% by repeating dip dry combustion. Adhesion of catalyst to cordierite surface is via oxide growth, which is very strong. ‘HC’ oxidation over the monolith catalyst is carried out with a mixture having the composition, 470 ppm of both propene and propane and 870 ppm of both ethylene and acetylene with the varying amount of O2. Three-way catalytic test is done by putting hydrocarbon mixture along with CO (10 000 ppm), NO (2000 ppm) and O2 (15 000 ppm). Below 350 °C full conversion is achieved. In this method, handling of nano-material powder is avoided.
Resumo:
In-situ EXAFS studies of sulphided Mo/TiO2 catalysts have shown that at low Mo loadings (2–4 wt%), an active species with a short Mo-S distance of 2.25 Å is formed, while on Mo/TiO2 with high Mo loadings as well as on Mo/gamma-Al2O3, bulk MoS2 (Mo-S, 2.42 Å) is formed. The species with the short Mo-S distance has Mo in an oxidation state close to 6 + and is likely to result from the sulphidation of the tetrahedral molybdate species present in the oxidic precursor at low Mo loadings. The calcination temperature of the oxidic precursor appears crucial, a high calcination temperature of 973 K favouring the formation of MoS3 on sulphidation, and a low calcination temperature of 623 K favouring MoS2.
Resumo:
Aqueous phase oxidation of sulphur dioxide at low concentrations catalysed by a PVP-Cu complex in the solid phase and dissolved Cu(II) in the liquid phase is studied in a rotating catalyst basket reactor (RCBR). The equilibrium adsorption of Cu(II) and S(VI) on PVP particles is found to be of the Langmuir-type. The diffusional effects of S(IV) species in PVP-Cu resin are found to be insignificant whereas that of product S(VI) are found to be significant. The intraparticle diffusivity of S(VI) is obtained from independent tracer experiments. In the oxidation reaction HSO3- is the reactive species. Both the S(IV) species in the solution, namely SO2(aq) and HSO3- get adsorbed onto the active PVP-Cu sites of the catalyst, but only HSO3- undergoes oxidation. A kinetic mechanism is proposed based on this feature which shows that SO2(aq) has a deactivating effect on the catalyst. A rate model is developed for the three-phase reaction system incorporating these factors along with the effect of concentration of H2SO4 on the solubility of SO2 in the dilute aqueous solutions of Cu(II). Transient oxidation experiments are conducted at different conditions of concentration of SO2 and O-2 in the gas phase and catalyst concentration, and the rate parameters are estimated from the data. The observed and calculated profiles are in very good agreement. This confirms the deactivating effect of nonreactive SO2(aq) on the heterogeneous catalysis.
Resumo:
Interaction of CH3OH with Cu clusters deposited on ZnO films grown on a Zn foil as well as on a ZnO(0001)Zn crystal, has been examined by X-ray photoelectron spectroscopy. On clean Cu clusters, reversible molecular adsorption or formation of CH3O is observed. However if the Cu clusters are pretreated with oxygen, both CH3O and HCOO- species are produced. Model Cu/ZnO catalyst surfaces, containing both Cu1+ and Cu-0 species, show interesting oxidation properties. On a Cu-0-rich catalyst surface, only CH3O species is formed on interaction with CH3OH. On a Cu1+-rich surface, however, HCOO- ion is the predominant species.
Resumo:
In the framework of a project aimed at developing a reliable hydrogen generator for mobile polymer electrolyte fuel cells (PEFCs), particular emphasis has been addressed to the analysis of catalysts able to assure high activity and stability in transient operations (frequent start-up and shut-down cycles). In this paper, the catalytic performance of 1 at.% Pt/ceria samples prepared by coprecipitation, impregnation and combustion, has been evaluated in the partial oxidation of methane. Methane conversion and hydrogen selectivity of 96 and 99%, respectively, associated with high stability during 100h of reaction under operative conditions (start-up and shut-down cycles), have been obtained. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
A modified solution combustion technique was successfully used to synthesize sub-10 nm crystallites of hybrid CeO(2)-Al(2)O(3)-CeAlO(3). The fuel in the solution combustion was tuned to obtain mixed oxides and solid solutions of the compound. The compounds were characterized by X-ray diffraction, transmission electron microscopy and X-ray photoelectron spectroscopy. XRD and TEM analysis showed the substitution of Al(3+) ions in the CeO(2) matrix when a combination of glycine, urea, hexamine and oxalyl dihydrazide was used as fuel for the synthesis. The compounds showed high activity for CO oxidation and the activity of the compounds was dependent upon the composition of the oxide.