183 resultados para NEGATIVE THERMAL-EXPANSION
em Indian Institute of Science - Bangalore - Índia
Resumo:
We use a combination of classical model and first-principles density functional theory calculations to study lattice dynamics of Y2W3O12 and identify phonons responsible for its negative thermal expansion (NTE). Born dynamical charges of various atoms are found to deviate anomalously from their nominal values. We find that the phonons with energy from 4 to 10 meV are the primary contributors to its NTE. These phonons involve rotations of the YO6 octahedra and WO4 tetrahedra in mutually opposite sense and collective translational atomic displacements, reflecting a strong mixing between acoustic and optic modes.
Synthesis, Structure, Negative Thermal Expansion, and Photocatalytic Property of Mo Doped ZrV(2)O(7)
Resumo:
A new series of compounds identified in the phase diagram of ZrO(2)-V(2)O(8)-MoO(3) have been synthesized via the solution combustion method. Single crystals of one of the compounds in the series, ZrV(1.50)Mo(0.50)O(7.25), were grown by the melt-cool technique from the starting materials with double the MoO(3) quantity. The room temperature average crystal structure of the grown crystals was solved using the single crystal X-ray diffraction technique. The crystals belong to the cubic crystal system, space group Pa (3) over bar (No. 205) with a = 8.8969 (4) angstrom, V = 704.24 (6) angstrom(3), and Z = 4. The final R(1) value of 0.0213 was achieved for 288 independent reflections during the structure refinement. The Zr(4+) occupies the special position (4a) whereas V(5+) and Mo(6+) occupy two unique (8c) Wyckoff positions. Two fully occupied O atoms, (24d) and (4b), one partially occupied 0 atom (8c) have been identified for this molybdovanadate, which is a unique feature for these crystals. The structure is related to both ZrV(2)O(7) and cubic ZrMo(2)O(8). The temperature dependent single crystal studies show negative thermal expansion above 370 K. The compounds have been characterized by powder X-ray diffraction, solid-state UV-vis diffuse reflectance spectra, scanning electron microscopy (SEM), and transmission electron microscopy (TEM). The photocatalytic activity of these compounds has been investigated for the degradation of various dyes, and these compounds show specificity toward the degradation of non-azoic dyes.
Resumo:
We report on the synthesis, microstructure and thermal expansion studies on Ca0 center dot 5 + x/2Sr0 center dot 5 + x/2Zr4P6 -aEuro parts per thousand 2x Si-2x O-24 (x = 0 center dot 00 to 1 center dot 00) system which belongs to NZP family of low thermal expansion ceramics. The ceramics synthesized by co-precipitation method at lower calcination and the sintering temperatures were in pure NZP phase up to x = 0 center dot 37. For x a parts per thousand yen 0 center dot 5, in addition to NZP phase, ZrSiO4 and Ca2P2O7 form as secondary phases after sintering. The bulk thermal expansion behaviour of the members of this system was studied from 30 to 850 A degrees C. The thermal expansion coefficient increases from a negative value to a positive value with the silicon substitution in place of phosphorous and a near zero thermal expansion was observed at x = 0 center dot 75. The amount of hysteresis between heating and cooling curves increases progressively from x = 0 center dot 00 to 0 center dot 37 and then decreases for x > 0 center dot 37. The results were analysed on the basis of formation of the silicon based glassy phase and increase in thermal expansion anisotropy with silicon substitution.
Resumo:
Precise measurements of the ultrasonic velocities and thermal expansivities of amorphous Se80Te20 and Se90Te10 alloys are reported near the glass transition. The samples are produced by liquid quenching. The longitudinal and transverse velocities are measured at 10 MHz frequency using the McSkimin pulse superposition technique. The thermal expansivities,agr, are measured using a three-terminal capacitance bridge. Theagr-values show a sharp maximum near the glass transition temperature,T g. The ultrasonic velocities also show a large temperature derivative, dV/dT nearT g. The data are discussed in terms of existing theories of the glass transition. The continuous change inagr shows that the glass transition is not a first-order transition, as suggested by some theories. The samples are found to be deformed by small loads nearT g. The ultrasonic velocities and dV/dT have contributions arising from this deformation.
Resumo:
Precise measurements of the ultrasonic velocities and thermal expansivities of amorphous Se80Te20 and Se90Te10 alloys are reported near the glass transition. The samples are produced by liquid quenching. The longitudinal and transverse velocities are measured at 10 MHz frequency using the McSkimin pulse superposition technique. The thermal expansivities,agr, are measured using a three-terminal capacitance bridge. Theagr-values show a sharp maximum near the glass transition temperature,T g. The ultrasonic velocities also show a large temperature derivative, dV/dT nearT g. The data are discussed in terms of existing theories of the glass transition. The continuous change inagr shows that the glass transition is not a first-order transition, as suggested by some theories. The samples are found to be deformed by small loads nearT g. The ultrasonic velocities and dV/dT have contributions arising from this deformation.
Resumo:
Single crystal macroscopic thermal expansion coefficient measurements have been made on uniaxial lithium potassium sulphate crystal both along and normal to the six fold axis, employing Fizeau’s interferometer method. Measurements were made in the range of −120°C to 500°C. The results show that lithium potassium sulphate exhibits two major anomalies in its expansion coefficients around −95°C and 422°C respectively, the one at −95°C has been observed for the first time. The nature of dimensional changes of the crystal at the upper and lower transition points are opposite in nature. The crystal shows considerable lattice anisotropy. Megaw’s tilt concept has been invoked to explain the relative magnitudes of expansion coefficients alonga andc directions. Structural features responsible for the absence of ferroelectricity in this crystal have been pointed out.
Resumo:
The temperature variation of the coefficient of thermal expansion of caesium bromide has been computed in quasiharmonic approximation and compared with the experimental results.
Resumo:
Matthias, Miller and Remeika1 were the first to observe that triglycine sulphate becomes ferroelectric below 47°C. The dielectric properties and the specific heat of this crystal have been studied through the transition temperature by Hoshino, Mitsui, Jona and Pepinsky2. The observed variation of the dielectric properties as a function of temperature in this crystal shows that the transition is of second order. Hoshino et al. concluded that the anomaly is not of the λ-type, since their specific heat - temperature curve showed only a hump. It was decided to investigate the thermal expansion of this crystal as it might throw some light on the nature of the transition.
Resumo:
The linear compressibility and the thermal expansion of Al-Fe and Al-Mn quasicrystals have been reported to be anisotropic. The authors suggest that the observed anisotropy in these properties could be due to the presence of decagonal quasicrystals rather than icosahedral quasicrystals.
Resumo:
The present x-ray study has been undertook in order to correlate the phase transition in sodium metavanadate NaVO3 crystal with its structural aspects. The thermal expansion behaviour of NaVO3 was studied from room temperature up to 500 C, well beyond the transition temperature.
Resumo:
Thermal expansion of several compositions of Sr and Mg-doped LaGaO3 including an A-site deficient composition (La0.9Sr0.1)(0.98)(Ga0.8Mg0.2)O-2.821 were measured in the temperature range from 298 to 1273 K. The effect of doping on thermal expansion was studied by varying the composition at one site of the perovskite structure (either A or B), while keeping the composition at the other site invariant. Thermal expansion varied nonlinearly with temperature and exhibited an inflexion between 550 and 620 K, probably related to the change in crystal structure from orthorhombic to rhombohedral. The dependence of average thermal expansion coefficient (alpha (av)) on the dopant concentration on either A or B site of the perovskite structure was found to be linear, when the composition at the other site was kept constant. Mg doping on the B-site had a greater effect on the average thermal expansion coefficient than Sr doping on the A-site. Cation deficiency at the A-site decreases thermal expansion when compositions at both sites are held constant.
Resumo:
The effect of substitution of calcium on the anisotropic axial thermal expansion of cordierite was investigated by using a high-temperature X-ray diffraction technique. The compositions were prepared by the sol–gel route. In the Mg2-xCax-Al4Si5O18 system, single-phase cordierite can be prepared for x up to 0.5. Thermal expansion anisotropy (αa–αc) of cordierites reduces progressively by the substitution of increasing amounts of Ca for Mg.
Resumo:
The structures of Ca0.5Ti2P3O12 and Sr0.5Ti2P3O12, low-thermal-expansion materials, have been refined by the Rietveld method using high-resolution powder X-ray diffraction (XRD) data. The assignment of space group R[3 with combining macron] to NASICON-type compounds containing divalent cations is confirmed. 31P magic-angle spinning nuclear magnetic resonance (MASNMR) data are presented as supporting data. A comparison of changes in the polyhedral network resulting from the cation distribution, is made with NaTi2P3O12 and Nb2P3O12. Factors that may govern thermal expansion in this family of compounds are discussed.
Resumo:
The paper is based on a study to develop carbon-glass epoxy hybrid composites with desirable thermal properties for applications at cryogenic temperatures. It analyzes the coefficient of thermal expansion of carbon-epoxy and glass-epoxy composite materials and compares it with the properties of carbon-glass epoxy hybrid composites in the temperature range 300 K to 125K. Urethane modified epoxy matrix system is used to make the composite specimens suitable for use even for temperatures as low as 20K. It is noted that the lay-up with 80% of carbon fibers in the total volume fraction of fibers oriented at 30 degrees and 20% of glass fibers oriented at 0 degrees yields near to zero coefficient of thermal expansion as the temperature is lowered from ambient to 125 K. (c) 2010 Elsevier Ltd. All rights reserved.