X-ray and He(II) ultraviolet photoelectron spectroscopy studies of the interaction of CO with oxygen on potassium-, caesium- and barium-covered Ag surfaces have shown the formation of carbonate at 300 K. While on a caesium-covered surface only carbonate formation takes place, on the potassium- and barium-covered surfaces molecularly chemisorbed CO is also formed. The variation of the surface concentrations of carbon and oxygen with temperature has been examined and a reaction sequence for the interaction of CO with adsorbed oxygen on potassium-, caesium- and barium-covered Ag surfaces is suggested.
Resumo:
XPS studies of the interaction of carbon monoxide with surfaces of Fe, Co and Ni indicate that at 300 K, the disproportionation reaction is prominent up to exposures of 103 L giving rise to high surface concentrations of carbon. At higher exposures and higher temperatures, dissociation of carbon monoxide accompanied by the formation of surface oxide layers becomes more prominent. In the case of copper, disproportionation is prominent up to 104 L even at 500 K followed by dissociation at higher exposures. These results are also supported by Auger spectroscopic studies.
Resumo:
Measurement of alveolar carbon monoxide (CO) presents a facile technique to estimate the lifespan, L, of red blood cells (RBCs) in vivo. Several recent studies employ this technique and calculate L (in days) using the expression, L = 13.8 (Hb)/P-CO(end), where (Hb) is the concentration (in g/dL) of hemoglobin in blood, and P-CO(end) is the endogenous production of CO (in ppm). Implicit in this calculation is the assumption that the fraction, f, of endogenous CO production due to RBC turnover is a constant equal to 0.7, which yields the expected RBC lifespan, L approximate to 120 days, in normal controls. In anemic patients, however, enhanced RBC turnover may increase f substantially above 0.7. The above expression then overestimates L. Here, we deriv an alternative tive expression, L = 3390[Hb]/322P(CO (end)-110, that accounts explicitly for the dependence of f on the rate of RBC turnover and thereby provides more accurate estimates of L without requiring additional measurements. Using the latter expression, we recalculate L from recent measurements on hepatitis C virus infected patients undergoing treatment with ribavirin. We find that our estimates of L in these patients (39 +/- 13 days) are significantly lower than current estimates (46 +/- 14 days), indicating that ribavirin affects RBC survival more severely than expected from current studies. Our expression for L is simple to employ in a clinical setting and would render the broadly applicable technique of alveolar CO measurement for the estimation of RBC lifespan more accurate.
Resumo:
Adsorption of CO has been investigated on the surfaces of polycrystalline transition metals as well as alloys by employing electron energy loss spectroscopy (eels) and ultraviolet photoelectron spectroscopy (ups). CO adsorbs on polycrystalline transition metal surfaces with a multiplicity of sites, each being associated with a characteristic CO stretching frequency; the relative intensities vary with temperature as well as coverage. Whilst at low temperatures (80- 120 K), low coordination sites are stabilized, the higher coordination sites are stabilized at higher temperatures (270-300 K). Adsorption on surfaces of polycrystalline alloys gives characteristic stretching frequencies due to the constituent metal sites. Alloying, however, causes a shift in the stretching frequencies, indicating the effect of the band structure on the nature of adsorption. The up spectra provide confirmatory evidence for the existence of separate metal sites in the alloys as well as for the high-temperature and low-temperature phases of adsorbed CO.
Resumo:
UPS and XPS studies indicate that carbon monoxide preferentially adsorbs dissociatively on the surfaces of the metallic glasses, Ni76B12Si12 and Fe40Ni38Mo4B18, suggesting that such metglasses could be potential catalysts for some of the reactions involving CO.
Resumo:
When the products of reaction between elemental sulphur and copper oxide at elevated temperature in vacuum are bubbled through chilled inert organic solvents like carbontetrachloride, orange-yellow solutions were obtained indicating the presence of lower oxide of sulphur. This lower oxide has been found to be disulphur monoxide as shown by three different types of reactions; (1) Mercury decomposition, (2) Reaction with hydrogen iodide and hydrolytic reaction in an alkaline homogeneous medium.
Resumo:
The interaction of CO with Cu, Pd, and Ni at different coverages of the metals on solid substrates has been investigated by He II and core-level spectroscopies, after the nature of variation of the metal core-level binding energies with the coverage or the cluster size is established. The separation between the (1 pi + 5 sigma) and 4 sigma levels of CO increases with a decrease in the size of the metal clusters, accompanied by an increase in the desorption temperature. In the case of Cu, the intramolecular shakeup satellite of CO disappears on small clusters. More importantly, CO dissociates on small Ni clusters, clearly confirming that metal-CO interaction strength increases with a decrease in the cluster size.
Resumo:
Interaction of carbon monoxide with a few chosen bimetallic overlayers has been investigated along with the core-level binding energies of the deposited metals by employing X-rays as well as UV photoelectron spectroscopies. Core-level binding energies of the deposited metals around monolayer coverages (0 similar to 1) are significantly different than those at high coverages or of the pure metals. Bimetallic overlayers such as Ni/Au and Cu/Pt showing large negative shifts in the surface core-level binding energy of the deposited metal interact strongly with carbon monoxide. In the case of Ni/Au (0(Ni) similar to 0.85), CO dissociates around 280 K. In contrast to this behavior, the interaction of CO with Pd/Mo or W, showing large positive shifts in the surface core-level binding energy, is very weak, and the CO desorption temperature is much lower than that from the clean Pd metal surface. The CO desorption temperature generally increases as the surface core-level shift of the deposited metal becomes more negative; the separation between the (5 sigma + 1 pi) and 4 sigma levels of CO also increases in this direction. These results suggest that the variation in the strength of interaction of CO with bimetallic overlayers is a chemical manifestation of the shift in the surface core-level binding energies of the deposited metals at monolayer coverages.
Resumo:
Oxygen reactivity and catalytic activity of the cobalt-containing layered defect perovskites, YBa2Cu2CoO7+delta and LaBa2Cu2CoO7+delta, in comparison with LaBa2Cu3O7-delta have been investigated employing temperature-programmed desorption (TPD) and temperature-programmed surface reactions (TPSR) in the stoichiometric and catalytic mode using carbon monoxide as a probe molecule. TPD studies showed evidence for the presence of two distinct labile oxygen species, one at (0 0 1/2) sites and the other at (0 1/2 0) sites in LaBa2Cu2CoO7+delta against a single labile species at (0 1/2 0) in the case of two other oxides. The activation energies for the catalytic oxidation of carbon monoxide by oxygen over LaBa2Cu3O7-delta, YBa2Cu2CoO7+delta, and LaBa2Cu2CoO7+delta have been estimated to be 24.2, 15.9, and 13.6 kcal/mol, respectively. The reactivity and catalytic activity of the oxide systems have been interpreted in terms of the structural changes brought about by substituents, guided by a directing effect of the larger rare earth cation. TPSR profiles, structural analysis, and infrared spectroscopic investigations suggest that the oxygen present at (0 0 1/2) sites in the case of LaBa2Cu2CoO7+delta is accessible to catalytic oxidation of CO through a Mars-Van Krevelen pathway. Catalytic conversion of CO to CO2 over LaBa2Cu2CoO7+delta occurs at 200 degrees C. The enhanced reactivity is explained in terms of changes brought about in the coordination polyhedra around transition metals, enhanced basal plane oxygen diffusivity, and redox potentials of the different transition metal cations.
Resumo:
Copper(l) complexes of bis(phosphine) monoxide ligands, bis(diphenylphosphino)ethane monoxide (dppeo) and bis(diphenylphosphino)methane monoxide (dppmo) have been prepared and characterized. One of the complexes with dppeo was characterized by X-ray crystal structure analysis confirming Cu(I) coordination to hard and soft donors. The stability of these complexes in solution was probed via spectroscopic and electrochemical studies. Copper(I) is more readily oxidized in the presence of the hard 0 donor ligands. In solution, they readily exchange the hard donor O, for soft ligands. Although copper(l) prefers soft ligands and is more stable towards oxidation in their presence, it coordinates to hard donors when there is electrostatic or an entropy driven advantage. (C) 2002 Elsevier Science Ltd. All rights reserved.
Lead Stereochemistry in Incommensurate Ferroelectric Perovskites and in Incommensurate Lead Monoxide
Resumo:
We have performed Rietveld refinements on neutron and synchrotron diffraction patterns and density functional calculations on various ferroelectric lead perovskites and on α lead monoxide (litharge). These structural data have allowed to shed some light on lead stereochemistry in these compounds. In particular, we discuss the changing in the lead behaviour between the paraelectric cubic phases and the low temperature anti or ferroelectric phases in Pb2CoWO6 and Pb2MgTeO6 (both incommensurate), in Pb2MgWO6 (antiferroelectric) and in PbMg1/3Nb2/3O3 (relaxor). The possible phase transition mechanisms are reviewed and the bonds are compared to those in the aperiodic structure of α-lead monoxide.
Resumo:
Base metal substituted Sn(0.95)M(0.05)O(2-delta) (M = Cu, Fe, Mn, Co) catalysts were synthesized by the solution combustion method and characterized by XRD, XPS, TEM and BET surface area analysis. The catalytic activities of these materials were investigated by performing CO oxidation. The rates and the apparent activation energies of the reaction for CO oxidation were determined for each catalyst. All the substituted catalysts showed high rates and lower activation energies for the oxidation of CO as compared to unsubstituted SnO(2). The rate was found to be much higher over copper substituted SnO(2) as compared to other studied catalysts. 100% CO conversion was obtained below 225 degrees C over this catalyst. A bifunctional reaction mechanism was developed that accounts for CO adsorption on base metal and support ions and O(2) dissociation on the oxide ion vacancy. The kinetic parameters were determined by fitting the model to the experimental data. The high rates of the CO oxidation reactions at low temperatures were rationalized by the high dissociative chemisorption of adsorbed O(2) over these catalysts.