40 resultados para LIME
em Indian Institute of Science - Bangalore - Índia
Resumo:
Abstract is not available.
Resumo:
Rice husk ash (about 95% silica) with known physical and chemical characteristics has been reacted with lime and water. The setting process for a lime-excess and a lime-deficient mixture has been investigated. The product of the reaction has been shown to be a calcium silicate hydrate, C-S-H(I)+ by a combination of thermal analysis, XRD and electron microscopy. Formation of C-S-H(I) accounts for the strength of lime-rice husk ash cement.
Resumo:
Fly ash is a waste by-product obtained from the burning of coal by thermal power plants for generating electricity. When bulk quantities are involved, in order to arrest the fugitive dust, it is stored wet rather than dry. Fly ash contains trace concentrations of heavy metals and other substances in sufficient quantities to be able to leach out over a period of time. In this study an attempt was made to study the leachabilities of a few selected trace metals: Cd, Cu, Cr, Mn, Pb and Zn from two different types of class F fly ashes. Emphasis is also laid on developing an alternative in order to arrest the relative leachabilities of heavy metals after amending them with suitable additives. A standard laboratory leaching test for combustion residues has been employed to study the leachabilities of these trace elements as a function of liquid to solid ratio and pH. The leachability tests were conducted on powdered fly ash samples before and after amending them suitably with the matrices lime and gypsum; they were compacted to their respective proctor densities and cured for periods of 28 and 180 days. A marked reduction in the relative leachabilities of the trace elements was observed to be present at the end of 28 days. These relative leachability values further reduced marginally when tests were performed at the end of 180 days.
Resumo:
The strength of fly ash mixture often needs to be enhanced for its better utilization in geotechnical and environmental applications. Many fly ashes often improve their strength with lime but may not meet the requirements. Gypsum, which reduces the lime leachability, further improves the strength. An attempt is made in this paper to study the effect of gypsum on the strength development of two Class F fly ashes with different lime contents after curing them for different periods. The sustainability of improved strength has been examined after soaking the cured specimens in water and with different leachates containing heavy-metal ions. The strength of both the fly ashes investigated improved markedly up to a particular amount of the lime content, which can be taken as optimum lime content, and thereafter the improvement is gradual. The improvement in strength at higher lime contents continues for a longer period (even up to 180 days). Gypsum accelerates the gain in strength for lime-stabilized fly ashes, particularly in the initial curing periods at about optimum lime content. At high lime contents gypsum attributes very high strength after curing for long periods mainly due to the alteration of fly ash lime reaction compounds. Gypsum not only improves the reduction in the loss of strength due to soaking even at low curing periods but also improves the durability of stabilized fly ashes due to repeated cycles of wetting and drying.
Resumo:
The paper correlates the reactivity of rice husk ash with its physicochemical properties such as crystallinity, surface area, microstructure, particle size distribution, porosity and solubility. These properties, in tum, are dependent on the time-temperature conditions under which the ash is prepared. It is found that the reactivity of the ash cannot be quantified by any one of these parameters alone, though they all indicate it qualitatively. Therefore, a method for quantifying this property was developed, by which the Reactivity Index is obtained. There is only a gradual change in the reactivity index of RHA with ashing temperature, as in many other properties, like surface area, porosity and total volume of gas absorbed by unit mass of the silica ash. This reactive index is found to be useful in determining the optimum ash/lime ratios required to give the best performance for RHA-lime composites.
Resumo:
Abundant quantities of fly ash have been produced by thermal power plants situated ail over the world. Many applications of fly ash depend upon its pozzolanic reactivity. This reactivity depends upon many factors, including lime content. Many fly ashes show marked improvement with the addition of lime. However, for every fly ash, there is an optimum lime content for its maximum reactivity. There is no well-established simple test to determine the optimum lime content. In this paper an attempt is made to use a simple physical and physico chemical test to determine the optimum lime content. The principle behind the use of a pH test, liquid limit test, and free swell index test to determine the optimum lime content has been explained. All the methods predict nearly the same optimum lime content and correlate well with that determined by the strength test.
Resumo:
The paper addresses certain issues pertaining to the technology of lime-stabilised steam-cured blocks used for masonry construction. Properties of lime-stabilised steam-cured blocks using expansive soils and tank bed soils have been examined. Influence of parameters like steam curing period, lime content and fly ash content on wet strength of blocks is studied. Steam curing of lime stabilised blocks at 80degreesC for about 20 hours at atmospheric pressure leads to considerably higher strengths when compared with curing under wet cloth at ambient temperatures. Clay-fly ash fractions of the mix control the optimum lime content yielding maximum strength. Long-term strength behaviour of steam-cured blocks has been monitored. The results indicate a favourable lime-clay ratio for stable long-term strength. A small-scale steam cured block production system has been designed and implemented to construct a load bearing masonry structure, thus demonstrating the potential of steam-cured block as a material for masonry construction.
Resumo:
Disposal of large quantities of fly ash poses a major environmental problem. To enhance its utilization, fly ash is considered for stabilizing of expansive soft soils. Improving the strength of soil, which is of major importance, depends on the pozzolanic nature of fly ash. Fly ashes with high pozzolanic reactivity are widely used but those with less pozzolanic reactivity are greatly inhibited. As the strength development in natural expansive soil considered in this investigation is very less with different percentages of fly ash, an attempt is made to increase the same by addition of lime along with fly ash. Based on several tests conducted, the optimum lime contents for fly ash and soils are 5% and 8% respectively. The strength of compacted soil with different fly ash contents of 10 to 40% with lime contents of 5% and 8% are determined after curing for different periods. The strength improvement for any soil-fly ash mixture, which is substantial with 5% of lime, is further improved with 8% of lime. The strength of soil-fly ash mixtures with any lime content increases with curing period.
Resumo:
Lime-fly ash mixtures are exploited for the manufacture of fly ash bricks finding applications in load bearing masonry. Lime-pozzolana reactions take place at a slow pace under ambient temperature conditions and hence very long curing durations are required to achieve meaningful strength values. The present investigation examines the improvements in strength development in lime-fly ash compacts through low temperature steam curing and use of additives like gypsum. Results of density-strength-moulding water content relationships, influence of lime-fly ash ratio, steam curing and role of gypsum on strength development, and characteristics of compacted lime-fly ash-gypsum bricks have been discussed. The test results reveal that (a) strength increases with increase in density irrespective of lime content, type of curing and moulding water content, (b) optimum lime-fly ash ratio yielding maximum strength is about 0.75 in the normal curing conditions, (c) 24 h of steam curing (at 80A degrees C) is sufficient to achieve nearly possible maximum strength, (d) optimum gypsum content yielding maximum compressive strength is at 2%, (e) with gypsum additive it is possible to obtain lime-fly ash bricks or blocks having sufficient strength (> 10 MPa) at 28 days of normal wet burlap curing.
Resumo:
The technical feasibility of utilization of fly ash as a low-cost adsorbent for the removal of metals from water has been studied. For two types of fly ashes, the retention capacities of copper, lead, and zinc metal ions have been studied. Contact time, initial concentration, and pH have been varied and their effect on retention mechanism has been studied. The dominant mechanisms responsible for retention are found to be precipitation due to the presence of calcium hydroxide, and adsorption due to the presence of silica and alumina oxide surfaces in the fly ash. First-order kinetic plots have revealed that the rate constant increases with increase in the initial concentration and pH. Langmuir adsorption isotherms have been plotted to study the maximum adsorption capacities for metal ions considered under different conditions. X-ray diffraction studies revealed the formation of new peaks corresponding to respective metal ions precipitates under alkaline conditions.
Comparison of ZnO films deposited on indium tin oxide and soda lime glass under identical conditions
Resumo:
ZnO films have been grown via a vapour phase transport (VPT) on soda lime glass (SLG) and indium-tin oxide (ITO) coated glass. ZnO film on ITO had traces of Zn and C which gives them a dark appearance while that appears yellowish-white on SLG. X-ray photoelectron spectroscopy studies confirm the traces of C in the form of C-O. The photoluminescence studies reveal a prominent green luminescence band for ZnO film on ITO. (C) 2013 Author(s).
Resumo:
Lime stabilization prevails to be the most widely adopted in situ stabilization method for controlling the swell-shrink potentials of expansive soils despite construction difficulties and its ineffectiveness in certain conditions. In addition to the in situ stabilization methods presently practiced, it is theoretically possible to facilitate in situ precipitation of lime in soil by successive permeation of calcium chloride (CaCl2 ) and sodium hydroxide (NaOH) solutions into the expansive soil. In this laboratory investigation, an attempt is made to study the precipitation of lime in soil by successive mixing of CaCl2 and NaOH solutions with the expansive soil in two different sequences.Experimental results indicated that in situ precipitation of lime in soil by sequential mixing of CaCl2 and NaOH solutions with expansive soil developed strong lime-modification and soil-lime pozzolanic reactions. The lime-modification reactions together with the poorly de- veloped cementation products controlled the swelling potential, reduced the plasticity index, and increased the unconfined compressive strength of the expansive clay cured for 24 h. Comparatively, both lime-modification reactions and well-developed crystalline cementation products (formed by lime-soil pozzolanic reactions) contributed to the marked increase in the unconfined compressive strength of the ex-pansive soil that was cured for 7–21 days. Results also show that the sequential mixing of expansive soil with CaCl2 solution followed by NaOH solution is more effective than mixing expansive soil with NaOH solution followed by CaCl2 solution. DOI: 10.1061/(ASCE)MT .1943-5533.0000483. © 2012 American Society of Civil Engineers.
Resumo:
We report a direct correlation between dissimilar ion pair formation and alkali ion transport in soda-lime silicate glasses established via broad band conductivity spectroscopy and local structural probe techniques. The combined Raman and Nuclear Magnetic Resonance (NMR) spectroscopy techniques on these glasses reveal the coexistence of different anionic species and the prevalence of Na+-Ca2+ dissimilar pairs as well as their distributions. The spectroscopic results further confirm the formation of dissimilar pairs atomistically, where it increases with increasing alkaline-earth oxide content These results, are the manifestation of local structural changes in the silicate network with composition which give rise to different environments into which the alkali ions hop. The Na+ ion mobility varies inversely with dissimilar pair formation, i.e. it decreases with increase of non-random formation of dissimilar pairs. Remarkably, we found that increased degree of non-randomness leads to temperature dependent variation in number density of sodium ions. Furthermore, the present study provides the strong link between the dynamics of the alkali ions and different sites associated with it in soda-lime silicate glasses. (C) 2014 Elsevier B.V. All rights reserved.