84 resultados para ELECTROLUMINESCENT POLYMERS

em Indian Institute of Science - Bangalore - Índia


Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper reports a new class of photo-cross-linkable side chain liquid crystalline polymers (PSCLCPs) based on the bis(benzylidene)cyclohexanone unit, which functions as both a mesogen and a photoactive center. Polymers with the bis(benzylidene)cyclohexanone unit and varying spacer length have been synthesized. Copolymers of bis(benzylidene)cyclohexanone containing monomer and cholesterol benzoate containing monomer with different compositions have also been prepared. All these polymers have been structurally characterized by spectroscopic techniques. Thermal transitions were studied by DSC, and mesophases were identified by polarized light optical microscopy (POM). The intermediate compounds OH-x, the monomers SCLCM-x, and the corresponding polymers PSCLCP-x, which are essentially based on bis(benzylidene)cyclohexanone, all show a nematic mesophase. Transition temperatures were observed to decrease with increasing spacer length. The copolymers with varying compositions exhibit a cholesteric mesophase, and the transition temperatures increase with the cholesteric benzoate units in the copolymer. Photolysis of the low molecular weight liquid crystalline bis(benzylidene)-cyclohexanone compound reveals that there are two kinds of photoreactions in these systems: the EZ photoisomerization and 2 pi + 2 pi addition. The EZ photoisomerization in the LC phase disrupts the parallel stacking of the mesogens, resulting in the transition from the LC phase to the isotropic phase. The photoreaction involving the 2 pi + 2 pi addition of the bis(benzylidene)cyclohexanone units in the polymer results in the cross-linking of the chains. The liquid crystalline induced circular dichroism (LCICD) studies of the cholesterol benzoate copolymers revealed that the cholesteric supramolecular order remains even after the photo-cross-linking.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The hydrothermal reaction of Ln(NO3)(3), Ni(NO3)(2), NaN3, and isonicotinic acid (L) yielded two novel 3-D coordination frameworks (1 and 2) of general formula [Ni(2)Ln(L)(5)(N-3)(2)(H2O)(3)] center dot 2H(2)O (Ln = Pr(III) for 1 and Nd(III) for 2), containing Ni-Pr or Ni-Nd hybrid extended three-dimensional networks containing both azido and carboxylate as co-ligands. Both the compounds are found to be isostructural and crystallize in monoclinic system having P2(1)/n space group. Here the lanthanide ions are found to be nonacoordinated. Both bidentate and monodentate modes of binding of the carboxylate with the lanthanides have been observed in the above complexes. Variable temperature magnetic studies of the above two complexes have been investigated in the temperature range 2-300 K which showed dominant antiferromagnetic interaction in both the cases and these experimental results are analyzed with the theoretical models. (c) 2008 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Different strategies for functionalization of the core region and periphery of core-shell type hyperbranched polymers (HBP) using the ``click'' reaction have been explored. For achieving periphera functionalization, an AB(2) + A-R-1 + A-R-2 type copolymerization approach was used, where A-R-1 is heptaethylene glycol monomethyl ether (HPEG-M) and A-R-2 is tetraethylene glycol monopropargyl ether (TEG-P). A very small mole fraction of the propargyl containing monomer, TEG-P, was used to ensure that the water-solubility of the hyperbranched polymer is minimally affected. Similarly, to incorporate propargyl groups in the core region, a new propargyl group bearing B-2-typ monomer was designed and utilized in an AB(2) + A(2) + B-2 + A-R-1 type copolymerization, such that the total mole fraction of B-2 + A(2) is small and their mole-ratio is 1: 1. Further, using a combination of both the above approaches, namely AB(2) + A(2) + B-2 + A-R-1 + A-R-2, hyperbranched structures that incorporate propargyl groups both at theperiphery and within the core were synthesized. Since the AB(2) monomer carries a hexamethylene spacer (C-6) and the periphery is PEGylated all the derivatized polymers form core-shell type structures in aqueous solutions. Attempts were made to ascertain and probe the location of the propargyl groups in these HBP's, by ``clicking'' azidomethylpyrene, onto them. However, the fluorescence spectra of aqueous solutions of the pyrene derivatized polymers were unable to discriminate between the various locations, possibly because the relatively hydrophobic pyrene units insert themselves into the core region to minimize exposure to water.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We present results of mechanical stress relaxation measurements on polymers confined at the air-water interface in the form of a monolayer. Systematic measurements allow, to our knowledge, for the first time, observation of the scaling of the stress relaxation time of the highly confined polymers as a function of both surface concentration and molecular weight. The observed scaling is found to be very close to that expected for motion of unentangled polymer solutions with hydrodynamic interactions. Our experimental observations thus clearly rule out the possibility of entanglement and hence reptation as a mode of relaxation in such highly confined polymeric systems.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conducting and semiconducting polymers are important materials in the development of printed, flexible, large-area electronics such as flat-panel displays and photovoltaic cells. There has been rapid progress in developing conjugated polymers with high transport mobility required for high-performance field-effect transistors (FETs), beginning(1) with mobilities around 10(-4) cm(2) V-1 s(-1) to a recent report(2) of 1 cm(2) V-1 s(-1) for poly(2,5-bis(3-tetradecylthiophen-2-yl) thieno[3,2-b] thiophene) (PBTTT). Here, the electrical properties of PBTTT are studied at high charge densities both as the semiconductor layer in FETs and in electrochemically doped films to determine the transport mechanism. We show that data obtained using a wide range of parameters (temperature, gate-induced carrier density, source-drain voltage and doping level) scale onto the universal curve predicted for transport in the Luttinger liquid description of the one-dimensional `metal'.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

ZnS:Cu, Br powder EL phosphors showed 6-line EPR signal at 25°C whose intensity increases with Cu content and on annealing in Zn-vapour. The signal arises from native Mn impurity. The starting material does not show any EPR signal since Mn2+ acts as an affinity potential well for a hole in ZnS, forming Mn3+ - a chemically uncommon situation in sulfides. In doped ZnS, holes are trapped at Cu such that Mn2+ persists. Deterioration of EL brightness is accompanied by the decrease in EPR signal intensity due to field assisted hole transference to Mn2+. Intentional addition of Mn in ZnS:Cu, Br decreases the brightness and shortens life time. Stable phosphors require ZnS with Mn content less than 1014 cm−3.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Combustion is a complex phenomena involving a multiplicity of variables. Some important variables measured in flame tests follow [1]. In order to characterize ignition, such related parameters as ignition time, ease of ignition, flash ignition temperature, and self-ignition temperature are measured. For studying the propagation of the flame, parameters such as distance burned or charred, area of flame spread, time of flame spread, burning rate, charred or melted area, and fire endurance are measured. Smoke characteristics are studied by determining such parameters as specific optical density, maximum specific optical density, time of occurrence of the densities, maximum rate of density increase, visual obscuration time, and smoke obscuration index. In addition to the above variables, there are a number of specific properties of the combustible system which could be measured. These are soot formation, toxicity of combustion gases, heat of combustion, dripping phenomena during the burning of thermoplastics, afterglow, flame intensity, fuel contribution, visual characteristics, limiting oxygen concentration (OI), products of pyrolysis and combustion, and so forth. A multitude of flammability tests measuring one or more of these properties have been developed [2]. Admittedly, no one small scale test is adequate to mimic or assess the performance of a plastic in a real fire situation. The conditions are much too complicated [3, 4]. Some conceptual problems associated with flammability testing of polymers have been reviewed [5, 6].

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A simple and inexpensive technique is described for the study of flammability of polymers, wherein the samples can be weighed continuously during their combustion in controlled atmosphere. The mass versus time curves for burning and quenching process in polystyrene samples are discussed. The experimental data indicates the efficiency of Monoammonium phosphate and ammonium halides in quenching of polystyrene.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Abstract is not available.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Synthesis, spectroscopic and thermal characterization of two new classes of polysulfide polymers: poly[1(phenoxymethyl) ethylene polysulfide] (PPMEP), and poly [1-(phenoxy) ethylene polysulfide] (PPEP) is presented. The direct pyrolysis mass spectrometry (DP-MS) technique, used to study the thermal degradation behavior of these polysulfide polymers, indicated that the polymers underwent degradation through the weak-links scission. The thermal stability of the polysulfide polymers decreased as the ``rank'' (number of sulfur atoms in the polysulfide linkage; n=1, 2, 4) increased. The main-chain flexibility of these polysulfide polymers in terms of their C-13 NMR spinlattice relaxation time (T-1) measurements on the backbone methine (-CH-) and methylene (-CH2-) carbons are reported here for the first time. A comparative study of the solution chain dynamics indicated that it increased as ``rank'' of the polysulfide linkages decreased as well as by introducing side chain spacers such as, ether (-O-) or methyleneoxy (-CH2O-) groups.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Two new neutral copper-azido polymers [Cu-3(N-3)(6)(tmen)(2)](n)(1)and [Cu-6(N-3)(12)(deen)(2)](n) (2) [tmen = N,N,N, N-tetramethylethylenediamine and deen = N,N-diethylethylenediamine] have been synthesized by using lower molar equivalents of the chelating diamine ligands with Cu(NO3)(2)center dot 3H(2)O and an excess of NaN3. The single crystal X-ray structure shows that in the basic unit of the 1D complex 1, the three Cu-II ions are linked by double end-on azido bridges with Cu-N-EO-Cu angles on both sides of the magnetic exchange critical angle of 108 degrees. Complex 2 is a 3D framework of a basic u-6 cluster. Cryomagnetic susceptibility measurements over a wide range of temperature exhibit dominant ferromagnetic behavior in both the complexes. Density functional theory calculations (B3LYP functional) have been performed on the trinuclear unit to provide a qualitative theoretical interpretation of the overall ferromagnetic behavior shown by the complex 1.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Two new coordination polymers [Cu(L-1)(2)](n)(ClO4)(n)center dot 2nH(2)O (1), [Cu(L-2)(2)](n)(ClO4)(n)center dot 2nH(2)O (2) of polydentate imine/pyridyl ligands, L-1 and L-2 with Cu(I) ion have been synthesized and characterized by single crystal X-ray diffraction studies, elemental analyses, IR' UV-vis and NMR spectroscopy. They represent 3-dimensional, sixfold interpenetrating diamondoid network structures having large pores of dimension, 35 x 21 angstrom(2) in 1 and 38 x 19 angstrom(2) in 2, respectively.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Hyperbranched polyethers having poly(ethylene glycol) (PEG) segments at their molecular periphery were prepared by a simple procedure wherein an AB2 type monomer was melt-polycondensed with an A-type monomer, namely, heptaethylene glycol monomethyl ether. The presence of a large number of PEG units at the termini rendered a lower critical solution temperature (LCST) to these copolymers, above which they precipitated out of an aqueous solution. In an effort to understand the effect of various molecular structural parameters on their LCST, the length of the hydrophobic spacer segment within the hyperbranched core and the extent of PEGylation were varied. Additionally, linear analogues that incorporates pendant PEG segments were also prepared and comparison of their LCST with that of the hyperbranched analogue clearly revealed that hyperbranched topology leads to a substantial increase in the LCST, highlighting the importance of the peripheral placement of the PEG units.