The constitutive flow behaviour in hot working of as cast magnesium has been studied with the help of a processing map developed in the temperature range 300-550°C and strain rate range 0·001-100 s−1. The map, interpreted using the dynamic materials model, revealed that the material undergoes dynamic recrystallisation at 425°C and 0·3 s−1, which are the optimum parameters for hot working. Ai temperatures higher than 450°C and strain rates lower than about 0·1 s−1, wedge cracking occurs in as cast magnesium. The wedge cracking domain has a high efficiency of power dissipation (60%), whereas the dynamic recrystallisation domain has a value of 34%. At temperatures below 450°C and strain rates above 10 s−1, the material exhibits flow instability in the form of mechanical twinning. At higher temperatures and strain rates, instability is manifested by flow localisation.