Al-Zn-Mg/SiCP composites processed by a liquid metal processing (stir casting) technique have been microstructurally characterised in the as-cast and extruded conditions. Uniform distribution of SiCP is observed with few defects, such as particle clusters, which are due to partial wetting and associated gas porosity. The constituent particles are associated with SiCP although their composition remains unaffected compared with the control alloy. Hot extrusion of the composite using a shear type die showed banding of particles in the extruded direction with 9 vol.% composite. Such defects however, are not predominant in 18% SiCP extruded composites. The presence Of Mg2Si is detected at the particle matrix interface as well as in the matrix.
Resumo:
Liquid phase co-spray forming (LPCSF) was employed to produce two Al-Si-Pb alloys. The preforms thus obtained were then subjected to hot extrusion at different extrusion ratios. Following extrusion, the materials were tensile tested at room temperature. The distribution of Pb particles and the microstructural characterization in as-formed preforms and in the extruded rods were studied on the basis of SEM observation. The influence of the Pb content on the mechanical properties was investigated. (C) 2002 Published by Elsevier Science B.V.
Transient analysis in Al-doped barium strontium titanate thin films grown by pulsed laser deposition
Resumo:
Thin films of (Ba0.5Sr0.5)TiO3 (BST) with different concentrations of Al doping were grown using a pulsed laser deposition technique. dc leakage properties were studied as a function of Al doping level and compared to that of undoped BST films. With an initial Al doping level of 0.1 at. % which substitutes Ti in the lattice site, the films showed a decrease in the leakage current, however, for 1 at. % Al doping level the leakage current was found to be relatively higher. Current time measurements at elevated temperatures on 1 at. % Al doped BST films revealed space-charge transient type characteristics. A complete analysis of the transient characteristics was carried out to identify the charge transport process through variation of applied electric field and ambient temperature. The result revealed a very low mobility process comparable to ionic motion, and was found responsible for the observed feature. Calculation from ionic diffusivity and charge transport revealed a conduction process associated with an activation energy of around 1 eV. The low mobility charge carriers were identified as oxygen vacancies in motion under the application of electric field. Thus a comprehensive understanding of the charge transport process in highly acceptor doped BST was developed and it was conclusive that the excess of oxygen vacancies created by intentional Al doping give rise to space-charge transient type characteristics. © 2001 American Institute of Physics.
Studies on Transport Phenomena in Rheocasting of Al-Si alloy in Presence of Electromagnetic Stirring
Resumo:
In the present investigation, various kinds of textures, namely, unidirectional, 8-ground, and random were attained on the die surfaces. Roughness of the textures was varied using different grits of emery papers or polishing powders. Then pins made of Al-4Mg alloys were slid against steel plates at various numbers of cycles, namely, 1, 3, 5, 10 and 20 using pin-on-plate reciprocating sliding tester. Tests were conducted at a sliding velocity of 2 minis in ambient conditions under both dry and lubricated conditions. A constant normal load of 35 N was applied in the tests. The morphologies of the worn surfaces of the pins and the formation of transfer layer on the counter surfaces were observed using a scanning electron microscope. Surface roughness parameters of the plates were measured using an optical profilometer. In the experiments, it was observed that the coefficient of friction and formation of the transfer layer depend on the die surface textures under both dry and lubricated conditions. More specifically, the coefficient of friction decreases for unidirectional and 8-ground surfaces while for random surfaces it increases with number of cycles. However, the coefficient of friction is highest for the sliding perpendicular to the unidirectional textures and least for the random textures under both dry and lubricated conditions. The difference in friction values between these two surfaces decreases with increasing number of cycles. The variation in the coefficient of friction under both dry and lubrication conditions is attributed to the change in texture of the surfaces during sliding. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
The dry sliding wear and friction behaviour of A356 Al alloy and its composites containing 10 and 20 vol.% SiC(P) have been studied using pin-on-disc set up. In these tests, A356 Al alloy and its composites are used as disc whereas brake pad was used in the form of pins. Wear tests were carried out at a load of 192 N and the sliding speed was varied from 1 to 5 m/s. Tests were done for a sliding distance of 15 km. The effects of sliding velocity on the wear rate, coefficient of friction and nature of tribolayers formed on discs have been studied. Wear rates of composites as calculated by weight loss method, found to be negative at sliding speed of more than 2 m/s. Worn surfaces of pins and discs have been analyzed using scanning electron microscope. SEM and EDAX analysis of worn surfaces of composite discs showed formation of tribolayers, consisting of mixture of oxides of Al, Si, Cu, Ca, Ba, Mg, and Fe. In these layers, copper and barium content found to be increase with sliding speed in the case of composites. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
The microscopic electron theory based on the pseudopotential formalism has been applied to the calculation of the heats of mixing and of activities in liquid Al·Sn alloys. The calculated values for both quantities were found to be in reasonable agreement with ,the experimental data.
Resumo:
The tie lines delineating ion-exchange equilibria between FeCr2O4FeAl2O4 spinel solid solution and Cr2O3Al2O3 solid solution with corundum structure have been determined at 1373 K by electron microprobe and EDAX point count analysis of oxide phases equilibrated with metallic iron. Activities in the spinel solid solution are derived from the tie lines and the thermodynamic data on Cr2O3Al2O3 solid solution available in the literature. The oxygen potentials corresponding to the tie-line composition of oxide phases in equilibrium with metallic iron were measured using solid oxide galvanic cells with CaOZrO2 and Y2O3ThO2 electrolytes. These electrochemical measurements also yield activities in the spinel solid solution, in good agreement with those obtained from tie lines. The activity-composition relationship in the spinel solid solution is analysed in terms of the intra-crystalline ion exchange between the tetrahedral and octahedral sites of the spinel structures. The ion exchange is governed by site-preference energies of the cations and the entropy of cations mixing on each site.
Resumo:
The concentration and chemical potential of oxygen in liquid Fe--Mn alloys equilibrated with the spinel solution, (Fe, Mn)Al sub 2+2x O sub 4+3x , and alpha -Al sub 2 O sub 3 have been determined at 1873K as a function of manganese concentration. The composition of the spinel phase has been determined using electron probe microanalysis. The results are compared with data reported in the literature. The deoxidation equilibrium has been computed using data on free energy of solution of oxygen in liquid iron, free energies of formation of hercynite and galaxite, and interaction parameters reported in the literature. The activity--composition relationship in spinel solution was derived from a cation distribution model. The model is in excellent agreement with the experimental data on oxygen concentration and potential and the composition of the spinel phase. 23 ref.--AA
Resumo:
A modified solution combustion technique was successfully used to synthesize sub-10 nm crystallites of hybrid CeO(2)-Al(2)O(3)-CeAlO(3). The fuel in the solution combustion was tuned to obtain mixed oxides and solid solutions of the compound. The compounds were characterized by X-ray diffraction, transmission electron microscopy and X-ray photoelectron spectroscopy. XRD and TEM analysis showed the substitution of Al(3+) ions in the CeO(2) matrix when a combination of glycine, urea, hexamine and oxalyl dihydrazide was used as fuel for the synthesis. The compounds showed high activity for CO oxidation and the activity of the compounds was dependent upon the composition of the oxide.