179 resultados para REACTOR KINETICS
Resumo:
The reactivation kinetics of passivated Mg acceptors in hydrogenated InP during unbiased annealing of a Schottky diode is reported. The reactivation is found to slow down gradually with annealing time and this phenomenon is attributed to substantial retrapping of H at the acceptor sites. It is found from the concentration profiles and the kinetics data that the reactivation is most likely limited by H2 molecule formation processes for longer annealing times; for shorter annealing times, contributions from in-diffusion of H also become significant. The diffusion of H during the initial period follows an Arrhenius relation with an activation energy for the effective diffusion coefficient of 1.13±0.10 eV. In the H2 formation regime, the reactivation is thermally activated with an activation energy for the annealing parameter of 1.71±0.10 eV. The H2 formation-limited regime of reactivation occurs sooner as the annealing temperature is increased.
Resumo:
Gas-phase controlled absorption of ammonia in foams made of solutions of sulphuric acid has been studied experimentally. Effects of gas-phase concentration of ammonia and type of surfactant on the performance of the foam-bed reactor are investigated. Gas-phase controlled absorption from a spherical bubble is anaylzed using the asymptotic value of Sherwood number (Sh = 6.58), for both negligible as well as significant changes in the volume of the bubble. The experimental data are shown to be in good agreement with the single-stage model of the foam-bed reactor using these asymptotic sub-models, as well as the diffusion-in-sphere analysis available in literature. Influence of effective diffusivity on the time dependence of fractional gas absorption has been found to be unimportant for foam columns with large times of contact. The asymptotic sub-models have been compared and use of the rigid-sphere asymptotic sub-model is recommended for foam columns of practical relevence.
Resumo:
Cure kinetics for the formation of copolyurethane networks of various compositions based on hydroxy-terminated polybutadiene(HTPB), poly(12-hydroxy stearic acid-co-TMP) ester polyol(PEP), and different isocyanates has been studied through viscosity build up during the cure reaction. The viscosity (N)-time (t) plots conform to the equation N = ae(bt), where a and b are empirical constants, dependent on the composition and the nature of the polyols and the isocyanates. The rate constants (b) for viscosity build up, evaluated from the slopes of dN/dt versus N plots at different temperatures, were found to vary significantly from 0.0073 to 0.25 min(-1); and the activation energies for gelation were found to be in the range 20 to 40 kJ mol(-1). The results have been interpreted in terms of the dependence of the rate constants on structural characteristics of the prepolymers. (C) 1997 John Wiley & Sons, Inc.
Resumo:
Non-exponential electron transfer kinetics in complex systems are often analyzed in terms of a quenched, static disorder model. In this work we present an alternative analysis in terms of a simple dynamic disorder model where the solvent is characterized by highly non-exponential dynamics. We consider both low and high barrier reactions. For the former, the main result is a simple analytical expression for the survival probability of the reactant. In this case, electron transfer, in the long time, is controlled by the solvent polarization relaxation-in agreement with the analyses of Rips and Jortner and of Nadler and Marcus. The short time dynamics is also non-exponential, but for different reasons. The high barrier reactions, on the other hand, show an interesting dynamic dependence on the electronic coupling element, V-el.
Resumo:
The reactivation kinetics of passivated boron accepters in hydrogenated silicon during zero bias annealing in the temperature range of 65-130 degrees C are reported, For large annealing times and high annealing temperatures, the reactivation process follows second-order kinetics and is rate limited by a thermally activated <(H)over tilde (2)> complex formation process, For short annealing times and low annealing temperatures, the reactivation rate is found to be larger than that due to <(H)over tilde (2)> complex formation alone. We conclude that the faster reactivation is caused by the diffusion of the liberated hydrogen atoms into the bulk as well as <(H)over tilde (2)> complex formation. The effective diffusion coefficient of hydrogen is measured and found to obey the Arrhenius relation with an activation energy (1.41 +/- 0.1) eV. (C) 1997 American Institute of Physics.
Resumo:
The kinetics of the processes in facing targets sputtering of multicomponent oxide films is presented. The novel configuration of the process exhibits an enhanced ionization efficiency. Discharge diagnostics performed using optical emission spectroscopy revealed strong dependence of plasma parameters on process conditions. Numerical simulation based on thermalization and diffusion of sputtered atoms has been performed to estimate the transport efficiency in off-axis mode. Composition, structure and epitaxial quality of YBa2Cu3O7-x films prepared was found to be strongly dependent on atomic flux ratios (of Cu/Y and Ba/Y) arriving at the substrate, resputtering effect and phase stability of YBa2Cu3O7-x These studies have been shown to be useful in understanding the complex processes that occur in sputtering of multicomponent films. (C) 1999 Elsevier Science S.A. All rights reserved.
Resumo:
Polymer degradation in solution has several advantages over melt pyrolysis, The degradation of low-density polyethylene (LDPE) occurs at much lower temperatures in solution (280-360degreesC) than in conventional melt pyrolysis (400-450degreesC). The thermal degradation kinetics of LDPE in solution was investigated in this work. LDPE was dissolved in liquid paraffin and degraded for 3 h at various temperatures (280-360degreesC). Samples were taken at specific times and analyzed with high-pressure liquid chromatography/gel permeation chromatography for the molecular weight distribution (MWD), The time evolution of the MWD was modeled with continuous distribution kinetics. Data indicated that LDPE followed random-chain-scission degradation. The rapid initial drop in molecular weight, observed up to 45 min, was attributed to the presence of weak links in the polymer. The rate coefficients for the breakage of weak and strong links were determined, and the corresponding average activation energies were calculated to be 88 and 24 kJ/mol, respectively. (C) 2002 John Wiley Sons, Inc.
Resumo:
This is the first report on the study carried out on high-pressure free-radical initiated oxidated copolymerization of styrene (STY) with alpha-methylstyrene (AMS) at various temperatures (45-65degreesC) at constant pressure (100 psi) and then at various pressures (50-300 psi) keeping the temperature (50degreesC) constant. The compositions of the copolyperoxides obtained from the H-1 NMT spectra were utilized to determine the reactivity ratios of the monomers. The reactivity ratios indicate that STY forms an ideal copolyperoxide with AMS and the copolyperoxide is richer in AMS. The effect of temperature and oxygen pressure in the reactivity ratios of the monomers was studied. The rates of copolymerization (R-p) were used to determine the overall activation energies (E-a) and activation volume (DeltaV(#)) of copolymerization. The unusually higher values of the DeltaV(#) may be due to the pressurizing fluid oxygen which itself is a reactant in the copolymerization, the side reactions, and the chain-transfer reactions occuring during copolymerizations.
Resumo:
Submicron size Co, Ni and Co-Ni alloy powders have been synthesized by the polyol method using the corresponding metal malonates and Pd powder by reduction of PdOx in methanol. The kinetics of the hydrogen evolution reaction ( HER) in 6 M KOH electrolyte have been studied on electrodes made from the pressed powders. The d.c. polarization measurements have resulted in a value close to 120 mV decade(-1) for the Tafel slope, suggesting that the HER follows the Volmer-Heyrovsky mechanism. The values of exchange current density (i(o)) are in the range 1-10 mA cm(-2) for electrodes fabricated in the study. The a.c. impedance spectra measured at several potentials in the HER region showed a single semicircle in the Nyquist plots. Exchange current density (i(o)) and energy transfer coefficient (alpha) have been calculated by employing a nonlinear least square-fitting program.
Resumo:
The thermal degradation of vinyl polyperoxides, poly(styrene peroxide, (PSP), poly(alpha-methylstyrene peroxide) (PAMSP) and poly(alpha-phenylstyrene pet-oxide) (PAPSP), was carried out at different temperatures in toluene. The time evolution of molecular weight distributions (MWDs) was determined by gel permeation chromatography (GPC). A continuous distribution model was used to evaluate the random chain degradation rate coefficients. The activation energies, determined from the temperature dependence of the rate coefficients, suggest that thermal degradation of polyperoxides is controlled by the dissociation of the O-O bonds in the backbone of the polymer chain. Among the three polyperoxides investigated, the thermal stability is the highest for PAPSP and the lowest for PAMSP. (C) 2002 Elsevier Science Ltd. All rights reserved.
Resumo:
Ultrasonic degradation of poly(methyl methacrylate) (PMMA) was carried out in several solvents and some mixtures of solvents. The time evolution of molecular weight distribution (MWD), determined by gel permeation chromatography, is analysed by continuous distribution kinetics. The rate coefficients for polymer degradation are determined for each solvent. The variation of rate coefficients is correlated with the vapour pressure of the solvent, kinematic viscosity of the solution and solvent-polymer interaction parameters. The vapour pressure and the kinematic viscosity of the solution are found to be more critical than other parameters (such as the Huggins and Flory-Huggins constants) in determining the degradation rates. (C) 2001 Society of Chemical Industry.
Resumo:
The degradation kinetics of polycarbonate [poly(bisphenol A carbonate)] in benzene catalyzed by commercial (rutile) TiO2 (BET surface area = 11 m(2)/g), anatase TiO2 (156 m(2)/g), and 1 atom % Pt/TiO2 (111 m2/g), prepared by the solution combustion technique, was investigated at various temperatures (230-280 degreesC) and 50 atm. The time evolution of the molecular weight distribution (MWD) was determined by gel permeation chromatography (GPC) and modeled with continuous distribution kinetics to obtain the degradation rate coefficients. The rate coefficients for the catalytic degradation of polycarbonate increased by factors of 20, 3.5, and 1.3 compared to the rate coefficients for thermal degradation when catalyzed by nanosized TiO2 anatase, Pt/TiO2 anatase, and commercial TiO2, respectively, at 280 degreesC. The increased catalytic activity of combustion for synthesized TiO2 and 1% Pt/TiO2 might be due to the increased acidity and BET surface area. The activation energies, determined from the temperature dependencies of the rate coefficients, were 16.3, 21.5, and 39.1 kcal/mol for commercial TiO2, combustion-synthesized Pt/TiO2, and anatase TiO2, respectively.
Resumo:
Experimental investigations into the effect of temperature on conversion of NO in the presence of hydrocarbons (ethylene, acetylene and n-hexane) are presented. An AC energized dielectric barrier discharge reactor was used as the plasma reactor. The experiments were carried out at different temperatures up to 200 degreesC. The discharge powers were measured at all the temperatures. The discharge power was found to increase with temperature. NO conversion in the presence of ethylene and n-hexane was better than that of acetylene at all temperatures. The addition of acetylene at room temperature showed no better conversion of NO compared to no additive case. While at higher temperatures, it could enhance the conversion of NO. A slight enhancement in NO and NOx removal was observed in the presence of water vapor. (C) 2003 Elsevier Science B.V. All rights reserved.
Resumo:
We present insightful results on the kinetics of photodarkening (PD) in Ge(x)As(45-x)Se(55) glasses at the ambient and liquid helium temperatures when the network rigidity is increased by varying x from 0 to 16. We observe a many fold change in PD and its kinetics with decreasing network flexibility and temperature. Moreover, temporal evolution of PD shows a dramatic change with increasing x. (C)2011 Optical Society of America