Aqueous phase oxidation of sulphur dioxide at low concentrations catalysed by a PVP-Cu complex in the solid phase and dissolved Cu(II) in the liquid phase is studied in a rotating catalyst basket reactor (RCBR). The equilibrium adsorption of Cu(II) and S(VI) on PVP particles is found to be of the Langmuir-type. The diffusional effects of S(IV) species in PVP-Cu resin are found to be insignificant whereas that of product S(VI) are found to be significant. The intraparticle diffusivity of S(VI) is obtained from independent tracer experiments. In the oxidation reaction HSO3- is the reactive species. Both the S(IV) species in the solution, namely SO2(aq) and HSO3- get adsorbed onto the active PVP-Cu sites of the catalyst, but only HSO3- undergoes oxidation. A kinetic mechanism is proposed based on this feature which shows that SO2(aq) has a deactivating effect on the catalyst. A rate model is developed for the three-phase reaction system incorporating these factors along with the effect of concentration of H2SO4 on the solubility of SO2 in the dilute aqueous solutions of Cu(II). Transient oxidation experiments are conducted at different conditions of concentration of SO2 and O-2 in the gas phase and catalyst concentration, and the rate parameters are estimated from the data. The observed and calculated profiles are in very good agreement. This confirms the deactivating effect of nonreactive SO2(aq) on the heterogeneous catalysis.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The thermal degradation of poly(methyl methacrylate) (PMMA) in the presence of polysulfide polymers, namely, poly( styrene disulfide) (PSD) and poly(styrene tetrasulfide) (PST) was studied using thermogravimetry (TG) and direct pyrolysis-mass spectrometric (DP-MS) analysis. Both PSD and PST were found to stabilizethe PMMA degradation, which was explained by both radical recombination and a chain-transfer mechanism. (C) 1997 John Wiley & Sons, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Poly(alpha-methylstyrene peroxide) has been synthesized and characterized spectroscopically. The H-1 and C-13 NMR spectra are shown to reveal the stereochemical features and the endgroups in the peroxide chain. The preliminary studies on the chain dynamics of the polyperoxide chain has been done by measuring the spin-lattice relaxation times (T-1) of the main chain as well as the side chain carbons. It has been shown from the dependence of the spin-lattice relaxation times that the polyperoxide chain is more flexible compared to the corresponding hydrocarbon-backbone analog.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Poly(ethyleneoxide)-poly(vinylalcohol) blends were prepared and characterized using thermal, spectroscopic and structural methods, By all indications the blends appear to be microscopically inhomogeneous with no strong interpolymer bonding. The high degree of crystallinity in PEO regions induces a significant degree of ordering in neighbouring PVA regions, as evident from thermal properties. PVA obtained from solvent evaporation exhibits an irreversible endothermic transition which could be order-disorder type. Both IR and NMR spectroscopies also suggest the presence of subtle structural ordering influence of PEO on PVA. It is found to be possible to prepare self supporting films of the blends which consists of fine dispersion of PEO and PVA in each other. (C) 1999 Elsevier Science Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Poly(o-toluidine) (POT) and poly(m-toluidine) (PMT) blends with polyvinylchloride (PVC) of five different compositions have been prepared by solution blending. The POT-PVC and PMT-PVC blends were prepared using THF as a solvent in which POT-HNO3, PMT-HNO3 bases and PVC are soluble. The blends have been characterized by spectral, thermal and electrical measurements. The results indicate the formation of blends at all the compositions presently studied. The thermal stability of the POT-PVC and PMT-PVC blends is higher than that of POT-HNO3 and PMT-HNO3 salts, respectively. Using the present method, POT/PMT can conveniently be blended with 30% wt/wt of PVC without significant loss in its conductivity. (C) 1998 Elsevier Science Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The adsorption of poly(acrylic acid) (PAA) and poly(vinyl alcohol) (PVA) onto alumina has been studied as a function of pH, both individually and in the presence of each other. The adsorption density of PAA is found to decrease with an increase of pH while that of PVA shows the opposite trend. In a binary system containing PAA and PVA, the presence of PVA does not affect the adsorption of PAA onto alumina, but the addition of PAA diminishes the adsorption of PVA in the pH range investigated. The adsorption isotherm of PAA at acidic pH exhibits high-affinity Langmuirian behavior. The isotherms for PVA appear rounded and are of the low-affinity type, Once again the adsorption isotherms of PAA remain unaltered in the presence of PVA whereas those of PVA are significantly affected resulting in a lowering of the adsorption density consequent to PAA addition. A variation in the sequence of addition of PAA and PVA does not affect the adsorption behavior of either of the polymers, The electrokinetic behavior of alumina with PAA is hardly influenced by the addition of PVA, On the other hand, the electrophoretic mobility of alumina in the presence of PVA is significantly altered in the presence of PAA and closely resembles the trend observed with PAA alone. Desorption studies reveal that over 80% of PVA could be desorbed in the pH range 3-9 whereas in the case of PAA, the percent desorption increases from 20 to about 70% as the pH is increased from about 3 to 8. Solution conductivity tests confirm interaction of aluminum species and PAA in the bulk solution. FTIR spectroscopic data provide evidence in support of hydrogen bonding and chemical interaction in the case of the PAA-alumina system and hydrogen bonding with respect to the PVA-alumina interaction. (C) 1999 Academic Press.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nanoclusters of bimetallic Pt-Ru are electrochemically deposited on conductive polymer, poly(3,4-ethylenedioxythiophene)(PEDOT), which is also electrochemically deposited on a carbon paper substrate. The bimetallic deposition is carried out in an acidic electrolyte consisting of chloroplatinic acid and ruthenium chloride at 0.0 V versus saturated calomel electrode (SCE) on PEDOT coated carbon paper. A thin layer PEDOT on a carbon paper substrate facilitates the formation of uniform, well-dispersed, nano clusters of Pt-Ru of mean diameter of 123 nm, which consist of nanosize particles. In the absence of PEDOT, the size of the clusters is about 251 nm, which are unevenly distributed on carbon paper substrate. Cyclic voltammetry studies suggest that peak currents of methanol oxidation are several times greater on PtRu-PEDOT electrode than on Pt-Ru electrode in the absence of PEDOT. (C) 2011 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The kinetics of thermal degradation of poly(vinyl chloride) (PVC) in solution was investigated at various temperatures (210-250degreesC). The degradation rate coefficients were determined from the time evolution of the molecular weight distribution (MWD). The energy of activation, determined from the temperature dependence of the rate coefficient, was 26.6 kcal/mol. The degradation of PVC was also studied in the presence of a catalyst (HZSM-5 zeolite). The results indicated that increase of the degradation rate of PVC is first order with the HZSM-5 concentration up to 50 g/L and zero order at higher concentrations. The thermal degradation kinetics of PVC in the presence of 50 g/L of the catalyst was studied at various temperatures. The temperature dependency of the rate coefficient was used to calculate the activation energy (21.5 kcal/mol). This is consistent with the observation that the presence of a catalyst generally decreases the activation energy and promotes degradation. (C) 2002 John Wiley Sons, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, we report the results pretaining to the study of the structural, microstructural and the dielectric properties of poly(I-lithocholic acid) (PL), and the composite of PL dispersed in PMMA. The density of the composites was measured using Archimedes principle. The microstructural properties of the composities were studied using XRD and SEM techniques, which give an idea about the dispersion of the polymer PL in the PMMA matrix. The dielectric constants er of the composites were measured with a HP 4194A Impedance/Gain-Phase Analyzer in the frequency range 100 Hz-40 MHz at room temperature. The dielectric constants of the composites at different frequencies were predicted using Clasius-Mossotti and Maxwell's models.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Poly(alkyl aryl ether) dendrimers of up to four generations composed of a phloroglucinol core, branching components, and pentamethylene spacers are synthesized by a divergent growth methodology. A repetitive synthetic sequence of phenolic O-alkylation and O-benzyl deprotection reactions are adopted for the synthesis of these dendrimers. The peripheries of the dendrimers contain 6, 12, 24, and 48 phenolic hydroxyl groups, either in the protected or unprotected form, for the first, second, third, and fourth generations, respectively. Because of the presence of hydrophilic exterior and relatively hydrophobic interior regions, alkaline aqueous solutions of these dendrimers are able to solubilize an otherwise insoluble pyrene molecule and these supramolecular complexes precipitate upon neutralization of the aqueous solutions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The thermal degradation of a series of para-substituted poly(styrene peroxide)s with electron-donating [CH3, C(CH3)(3)] and electron-attracting (Br) substitutents are investigated by thermogravimetric analysis (TGA). The results indicate that the Hammett relationship can describe quantitatively the trends in maximum rate of polymer decomposition (T-max) observed in TGA and thus thermostability of substituted poly(styrene peroxide)s depends only on the electronic nature of substituents and their ability to stabilize macroradicals formed during chain scission. The experimental results are also substantiated by thermochemical calculations. (C) 2002 Elsevier Science Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Ultrasonic degradation of poly(methyl methacrylate) (PMMA) was carried out in several solvents and some mixtures of solvents. The time evolution of molecular weight distribution (MWD), determined by gel permeation chromatography, is analysed by continuous distribution kinetics. The rate coefficients for polymer degradation are determined for each solvent. The variation of rate coefficients is correlated with the vapour pressure of the solvent, kinematic viscosity of the solution and solvent-polymer interaction parameters. The vapour pressure and the kinematic viscosity of the solution are found to be more critical than other parameters (such as the Huggins and Flory-Huggins constants) in determining the degradation rates. (C) 2001 Society of Chemical Industry.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The ultrasonic degradation of poly(vinyl acetate) was carried out in six different solvents and two mixtures of solvents. The evolution of molecular weight distribution (MWD) with time was determined with gel permeation chromatography. The observed MWDs were analyzed by continuous distribution kinetics. A stoichiometric kernel that accounts for preferential mid-point breakage of the polymer chains was used. The degradation rate coefficient of the polymer in each solvent was determined from the model. The variations of rate coefficients were correlated with vapor pressure of the solvent, the Flory–Huggins polymer–solvent interaction parameter and the kinematic viscosity of the solution. A lower saturation vapor pressure resulted in higher degradation rates of the polymer. The degradation rate increased with increasing kinematic viscosity.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Poly(methacrylonitrile peroxide) (PMNP) has been synthesized from methacrylonitrile by free radical initiated oxidative polymerization and characterized by different spectroscopic methods. NMR spectroscopy confirmed the alternating copolymer structure with labile peroxy bonds in the main chain. The extreme instability of PMNP was noted from FTIR spectroscopy. Thermal degradation studies by using differential scanning calorimetry and thermogravimetry have revealed that PMNP degrades highly exothermically and the heat of degradation, 42.5 kcal mol−1, is of the same order as that reported for other vinyl polyperoxides. Mass spectral fragmentation pattern under electron impact (EI) condition has also been investigated. The mechanism of the primary exothermic degradation has been substantiated by thermochemical calculations. The chain dynamics of the polyperoxide chain has been studied by means of 13C spin–lattice relaxation times (T1) of the main chain as well as the side chain carbons. The temperature dependence of the spin–lattice relaxation times shows that the PMNP is more flexible compared to the analogous poly(styrene peroxide).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Current-voltage (I-V) and impedance measurements were carried out in doped poly(3-methylthiophene) devices by varying the carrier density. As the carrier concentration reduces the I-V characteristics indicate that the conduction mechanism is limited by metal-polymer interface, as also observed in impedance data. The temperature dependence of I-V in moderately doped samples shows a trap-controlled space-charge-limited conduction (SCLC); whereas in lightly doped devices injection-limited conduction is observed at lower bias and SCLC at higher voltages. The carrier density-dependent quasi-Fermi level adjustment and trap-limited transport could explain this variation in conduction mechanism. Capacitance measurements at lower frequencies and higher bias voltages show a sign change in values due to the significant variations in the relaxation behaviour for lightly and moderately doped samples. The electrical hysteresis increases as carrier density is reduced due to the time scales involved in the de-trapping of carriers.