173 resultados para Iron-glycine chelate
Resumo:
An experimental programme based on statistical analysis was used for optimizing the reverse Rotation of silica from non-magnetic spiral preconcentrate of Kudremukh iron ore. Flotation of silica with amine and starch as the Rotation reagents was studied to estimate the optimum reagent levels at various mesh of grind. The experiments were first carried out using a two level three factor design. Analysis of the results showed that two parameters namely, the concentration level of the amine collector and the mesh of grind, were significant. Experiments based on an orthogonal design of the hexagonal type were then carried out to determine the effects of these two variables, on recovery and grade of the concentrate. Regression equations have been developed as models. Response contours have been plotted using the 'path of steepest ascent', maximum response has been optimized at 0.27 kg/ton of amine collector, 0.5 kg/ton of starch and mesh of grind of 48.7% passing 300 mesh to give a recovery of 83.43% of Fe in the concentrate containing 66.6% Fe and 2.17% SiO2.
Resumo:
The results of the structural and conformational studies carried out using C-13 CPMAS NMR technique on several glycine and alanine containing peptides in the solid state are reported. The study demonstrates the effects of variations in C-13 chemical shifts due to conformation and hydrogen bonding. The possibility of applying this technique to obtain insight into the conformational characteristics of peptides of unknown structures is discussed.
Resumo:
A new iron fluorophosphate of the composition, [C6N4H21] [Fe2F2(HPO4)(3)][H2PO4](.)2H(2)O, I has been prepared by the hydrothermal route. This compound contains iron fluorophosphate layers and the H2PO4- anions are present in the interlayer space along with the protonated amine and water molecules. The compound crystallizes in the monoclinic space group P2(1)/c. (a = 13-4422(10) Angstrom, b = 9 7320(10) Angstrom, c = 18-3123(3) Angstrom, beta = 92-1480degrees, V = 2393-92(5) Angstrom 3, Z = 4, M = 719-92, d(calc). = 1.997 g cm(-3), R-1 = 0.03 and wR(2) = 0,09).
Resumo:
A layered iron sulfate of the composition [H3N(CH2)(2)NH2(CH2)(2)NH2(CH2)(2)NH3][(Fe3F6)-F-II(SO4)(2)], possessing a distorted Kagome lattice, prepared hydrothermally, is found to exhibit magnetic hysteresis like a ferrimagnet besides the characteristics of a frustrated system, like those of a spin glass.
Resumo:
Iron nanowires encapsulated in aligned carbon nanotube bundles show interesting magnetic properties. Besides the increased coercivity, Barkhausen jumps with 5 emu/g steps in magnetization are observed due to magnetization reversal or depinning of domains. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
Two new open-framework iron fluorophosphates, [C(4)N(2)H(12)](0.5) [FeF(HPO(4))(H(2)PO(4))] (I) and [C(4)N(2)H(12)][Fe(4)F(2)(H(2)O)(4)(PO(4))(4)]. 0.5H(2)O (II), were synthesized hydrothermally using piperazine as a templating agent. The structures were determined by single-crystal X-ray diffraction. Compound I crystallizes in the orthorhombic space group Pbca, a = 7.2126(2) Angstrom, b = 14.2071(4) Angstrom, c = 17.1338(2) Angstrom, Z = 8. The structure is composed of infinite anionic chains of [FeF(HPO(4))(H(2)PO(4))](n)(-) built by trans-fluorine sharing FeF(2)O(4) octahedra. These chains are similar to those found in tancoite-type minerals. Compound II crystallizes in the monoclinic space group P2(1)/n, a = 9.9045(3) Angstrom, b = 12.3011(3) Angstrom, c = 17.3220(4) Angstrom, beta = 103.7010(10)degrees, Z = 4. The structure of compound II has a three-dimensional (3D) architecture with an eight-membered channel along the b axis, in which protonoted piperazine molecules reside. The complex framework is built from two types of secondary building unit (SBU): one hexamer [Fe(3)F(2)(H(2)O)(2)(PO(4))(3)] (SBU6), and one dimer [FeO(4)(H(2)O)(2)PO(4)] (SBU2). The vertex sharing between these SBUs create the 3D structure.
Resumo:
Glycine Phosphite [NH3CH2COOH3PO3], abbreviated as GPI, undergoes a para-ferroelectric phase transition from the monoclinic symmetry P2(1)/a to P2(1) at 224.7 K. We report here a systematic study of the polarization switching process in this crystal. Growth of these crystals from aqueous solution has been undertaken employing both solvent evaporation and slow cooling methods. Hysteresis loop measurements along the polar b-axis yielded a spontaneous polarization value of 0.5 muC/cm(2) and a coercive field of 2.5 kV/cm. Conventional Merz technique was employed for polarization switching studies, wherein bipolar square pulses were applied to the sample to induce domain reversal. The transient switching pulse that flows through the sample on application of the field was recorded. The maximum switching time required for domain switching was measured both as a function of electric field and temperature. The experimentally observed switching curves were fitted with the model based on the Pulvari-Kuebler theory of nucleation and growth of domains. From the experimental data, the values of mobility and activation field were obtained. It was observed that switching process in this crystal is predominantly governed by the forward growth of domain walls in the high field region. However, switching process in GPI crystal was found to be slower than that found in other glycine based ferroelectric crystals.
Resumo:
The effect of Fe content (0.2 to 0.6 pct) on the microstructure and mechanical properties of a cast Al-7Si-0.3Mg (LM 25/356) alloy has been investigated. Further, 1 pct mischmetal (MM) additions (a mixture of rare-earth (RE) elements) were made to these alloys, and their mechanical properties at room and at elevated temperatures (up to 200 degreesC) were evaluated. A structure-property correlation on this alloy was attempted using optical microstructure analysis, fractographs, X-ray diffraction, energy-dispersive analysis of X-rays (EDX), and quantitative metallography by image analysis. An increase in Fe content increased the volume percentage of Fe-bearing intermetallic compounds (beta and pi phases), contributing to the lower yield strength (YS), ultimate tensile strength (UTS), percentage elongation, and higher hardness. An addition of 1 pct MM to the alloys containing 0.2 and 0.6 pct Fe was found to refine the microstructure; modify the eutectic silicon and La, Ce, and Nd present in the MM; form different intermetallic compounds with Al, Si, Fe, and Mg; and improve the mechanical properties of the alloys both at room and elevated temperatures.
Resumo:
Single crystals of a recent ferroelectric material, glycine phosphite were grown from aqueous solution employing the techniques of slow cooling and controlled evaporation. Powder X-ray diffraction studies as well as thermal analysis were carried out on the grown crystals. The morphology of the crystal has been determined using contact and optical goniometry. The mechanical hardness of the crystal was evaluated by Vickers indentation method. Thickness dependence of the dielectric properties has been investigated and the results can be interpreted in terms of a surface layer of lower dielectric constant.
Resumo:
In the present work, the reaction between a molten iron drop and dense alumina was studied using the X-ray sessile-drop method under different oxygen partial pressures in the gas atmosphere. The changes in contact angles between the iron drop and the alumina substrate were followed as functions of temperature and varying partial pressures of oxygen in the temperature range 1823 to 1873 K both in static and dynamic modes. The results of the contact angle measurements with pure iron in contact with dense alumina in extremely well-purified argon as well as under different oxygen partial pressures in the gas atmosphere showed good agreement with earlier measurements reported in the literature. In the dynamic mode, when argon was replaced by a CO-CO2-Ar mixture with a well-defined PO, in the gas, the contact angle showed an initial decrease followed by a period of nearly constant contact angle. At the end of this period, the length of which was a function of the P-O2 imposed, a further steep decrease in the contact angle was noticed. An intermediate layer of FeAl2O4 was detected in the scanning electron microscope (SEM) analysis of the reacted substrates. An interesting observation in the present experiments is that the iron drop moved away from the site of the reaction once the product layer covered the interface. The results are analyzed on the basis of the various forces acting on the drop.
Resumo:
To establish itself within the host system, Mycobacterium tuberculosis (Mtb) has formulated various means of attacking the host system. One such crucial strategy is the exploitation of the iron resources of the host system. Obtaining and maintaining the required concentration of iron becomes a matter of contest between the host and the pathogen, both trying to achieve this through complex molecular networks. The extent of complexity makes it important to obtain a systems perspective of the interplay between the host and the pathogen with respect to iron homeostasis. We have reconstructed a systems model comprising 92 components and 85 protein-protein or protein-metabolite interactions, which have been captured as a set of 194 rules. Apart from the interactions, these rules also account for protein synthesis and decay, RBC circulation and bacterial production and death rates. We have used a rule-based modelling approach, Kappa, to simulate the system separately under infection and non-infection conditions. Various perturbations including knock-outs and dual perturbation were also carried out to monitor the behavioral change of important proteins and metabolites. From this, key components as well as the required controlling factors in the model that are critical for maintaining iron homeostasis were identified. The model is able to re-establish the importance of iron-dependent regulator (ideR) in Mtb and transferrin (Tf) in the host. Perturbations, where iron storage is increased, appear to enhance nutritional immunity and the analysis indicates how they can be harmful for the host. Instead, decreasing the rate of iron uptake by Tf may prove to be helpful. Simulation and perturbation studies help in identifying Tf as a possible drug target. Regulating the mycobactin (myB) concentration was also identified as a possible strategy to control bacterial growth. The simulations thus provide significant insight into iron homeostasis and also for identifying possible drug targets for tuberculosis.
Resumo:
Monodisperse iron oxide nanocrystals with spherical and cubic morphologies, of comparable dimensions, have been prepared by the thermal decomposition of FeOOH. The lattice spacings of both forms agree with that of magnetite, Fe(3)O(4). The two, however, exhibit very different blocking temperatures. Nanocrystals of cubic morphology are superparamagnetic above 190 K while the spherical nanocrystals at a lower temperature, 142 K. The higher blocking temperatures in particles of cubic morphology are shown to be a consequence of exchange bias fields. We show that in the present iron oxide nanocrystals the exchange bias fields originate from the presence of trace amounts of wustite, FeO. A Reitveld refinement analysis of the X-ray diffraction patterns shows that nanocrystals of cubic morphology have a higher FeO content. The higher FeO content is responsible for the larger exchange bias fields that in turn lead to a higher blocking temperature for nanocrystals with cubic morphology.
Resumo:
The magnetic properties of iron-filled multi-walled carbon nanotubes dispersed in polystyrene (Fe-MWNT/PS) have been investigated as a function of Fe-MWNT concentration (0.1-15 wt%) from 300 to 10 K. Electron microscopy studies indicate that Fe nanorods (aspect ratio similar to 5) remain trapped at various lengths of MWNT and are thus, prevented from oxidation as well as aggregation. The magnetization versus applied field (M-H loop) data of 0.1 wt% of Fe-MWNTs in PS show an anomalous narrowing at low temperatures which is due to the significant contribution from shape anisotropy of Fe nanorods. The remanence shows a threshold feature at 1 wt%. The enhanced coercivity shows a maximum at 1 wt% due to the dominant dipolar interactions among Fe nanorods. Also the squareness ratio shows a maximum at 1 wt%.