183 resultados para ZIRCONIUM OXIDES


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Laser sintering was carried out using a high power continuous-wave CO2 laser to prepare pellets of zirconia (ZrO2), hafnia (HfO2) and yttria (Y2O3) mixed oxides as starting materials in the deposition of optical coatings. Hardened recrystallized pellets appeared to have been formed during laser treatment. X-ray diffraction analysis revealed a monoclinic-to-tetragonal phase transformation in the binary system while the ternary system was found to have a mixture of two crystalline phases. Cross-sectional scanning electron microscopy showed two isothermal crystalline regions in the ternary system. The optical inhomogeneity was low in the films deposited from the laser-fused pellets, but the absorption at a wavelength of 351 nm increased with increasing HfO2 content. The films deposited from laser-fused pellets were analysed by electron spectroscopy for chemical analysis and found to be stoichiometric and homogeneous.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The hot deformation characteristics of alpha-zirconium in the temperature range of 650 °C to 850 °C and in the strain-rate range of 10-3 to 102 s-1 are studied with the help of a power dissipation map developed on the basis of the Dynamic Materials Model.[7,8,9] The processing map describes the variation of the efficiency of power dissipation (η =2m/m + 1) calculated on the basis of the strain-rate sensitivity parameter (m), which partitions power dissipation between thermal and microstructural means. The processing map reveals a domain of dynamic recrystallization in the range of 730 °C to 850 °C and 10−2 to 1−1 with its peak efficiency of 40 pct at 800 °C and 0.1 s-1 which may be considered as optimum hot-working parameters. The characteristics of dynamic recrystallization are similar to those of static recrystallization regarding the sigmoidal variation of grain size (or hardness) with temperature, although the dynamic recrystallization temperature is much higher. When deformed at 650 °C and 10-3 s-1 texture-induced dynamic recovery occurred, while at strain rates higher than 1 s-1, alpha-zirconium exhibits microstructural instabilities in the form of localized shear bands which are to be avoided in processing.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Using dynamic TG in H2, X-ray powder diffraction and Mössbauer Spectroscopy the reactivities fot hydrogen reduction of Fe2O3 prepared at different temperatures, Fe2O3 doped with oxides of Mn, Co, Ni and Cu prepared at 300DaggerC from nitrate precursors and intermediate spinels derived from above samples during reduction have been explored. The reactivity is higher for finely divided Fe2O3 prepared at 250DaggerC. The reduction is retarded by Mn, marginally affected by Co and accelerated by Ni and Cu, especially at higher (5 at.%) dopant concentration. These reactivities confirmed also by isothermal experiments, are ascribed to the nature of disorder in the metastable intermediate spinels and to hydrogen rsquospill overrsquo effects.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Transition metal oxides like Fe2O3, Ni2O3, Co2O3 and MnO2 suppress the combustion of polystyrene. The effect has been explained on the basis of condensed-phase and gas-phase reactions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Transitions from the low-to the high-spin state in Fe2+ and Co3+ compounds have been examined by X-ray and UV photoelectron spectroscopy. It has been shown that the core-level bands in XPES, in particular the metal 3s band, as well as the valence bands, are diagnosis in the study of spin-state transitions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Description of gel-to-crystallite conversion process is made towards the synthesis of nanocrystalline titanates and aluminates. Thermodynamic and kinetic factors governing the conversion of a gel to meta-stable and stable nanocrystalline products(s) are discussed. Correlations between these factors and the preparative conditions employed for the syntheses of titanates and aluminates are arrived at.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Thermodynamic properties of three oxides of niobium have been measured using solid state electrochemical cells incorporating yttria-doped thoria (YDT) as the electrolyte in the temperature range T = (1000 to 1300) K. The standard Gibbs energies of formation of NbO, NbO2, and NbO2.422 from the elements can be expressed as: Delta(f)G(NbO)(o) +/- 547/J . mol(-1) = -414 986 + 86.861(T/K) Delta(f)G(NbO2)(o) +/- 548/J . mol(-1) = -779 864 + 164.438(T/K) Delta(f)G(NbO2.422)(o) +/- 775/J . mol(-1) = -911 045 + 197.932(T/K) The results are discussed in comparison with thermodynamic data reported in the literature. The new results refine data for NbO and NbO2 presented in standard data compilations. There are no data in thermodynamic compilations for NbO2.422 (Nb12O29). In the absence of the heat capacity and enthalpy of formation measurements, only the Gibbs energy of formation of NbO2.422 can be assessed. The free energy of formation of stoichiometric Nb2O5 is evaluated on the basis of measurements on NbO2.422 and information available in the literature on phase boundary compositions and isothermal variation of nonstoichiometric parameter with oxygen potential for Nb2O5-x. The results suggest a minor revision of data for Nb2O5. A minimum in the Gibbs energy of mixing for the system Nb-O occurs in the nonstoichiometric domain of Nb2O5-x with x = 0.036.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

X-Ray and uv photoelectron spectra of FeO, Fe2O3, and Fe3O4 have been studied along with those of a few model compounds. It has been possible to assign distinct bands due to Fe2+ and Fe3+ in the 3d, 3p, 3s, and 2p bands of Fe3O4. The spectra of Fe3O4 do not show major changes through the Verwey transition.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Attempts have been made to evaluate the thermal stability of rare earth oxide face coats against liquid titanium. Determination of microhardness profiles and concentration profiles of oxygen and metallic constituents of oxide in investment cast titanium rods has allowed grActation of relative stability of rare earth oxides. The relative stability of evaluated oxides in the order of increasing stability follows the sequence CeO2 — ZrO2 — Gd2O3 — didymium oxide — Sm2O3 —Nd2O3 — Y2O3. The grading does not follow the free energy data of the formation of these oxides. A better correlation with the experimental observations is obtained when the solubility of the metallic species in titanium is also taken into consideration.