A decade ago, Budakian and Putterman [Phys. Rev. Lett. 85, 1000 (2000)] ascribed friction to the formation of bonds arising from contact charging when a gold tip of a surface force apparatus was dragged on polymethylmethacrylate surface. We propose a stick-slip model that captures the observed correlation between stick-slip events and charge transfer, and the lack of dependence of the scale factor connecting the force jumps and charge transfer on normal load. Here, stick-slip dynamics arises as a competition between the viscoelastic and plastic deformation time scales and that due to the pull speed with contact charging playing a minor role. Our model provides an alternate basis for explaining most experimental results without ascribing friction to contact charging.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Introduction of agriculture three millennia ago in Peninsular India’s Western Ghats altered substantially ancient tropical forests. Early agricultural communities, nevertheless, strived to attain symbiotic harmony with nature as evident from prevalence of numerous sacred groves, patches of primeval forests sheltering biodiversity and hydrology. Groves enhanced heterogeneity of landscapes involving elements of successional forests and savannas favouring rich wildlife. A 2.25 km2 area of relic forest was studied at Kathalekan in Central Western Ghats. Interspersed with streams studded with Myristica swamps and blended sparingly with shifting cultivation fallows, Kathalekan is a prominent northernmost relic of southern Western Ghat vegetation. Trees like Syzygium travancoricum (Critically Endangered), Myristica magnifica (Endangered) and Gymnacranthera canarica (Vulnerable) and recently reported Semecarpus kathalekanensis, are exclusive to stream/swamp forest (SSF). SSF and non-stream/swamp forest (NSSF) were studied using 18 transects covering 3.6 ha. Dipterocarpaceae, its members seldom transgressing tropical rain forests, dominate SSF (21% of trees) and NSSF (27%). The ancient Myristicaceae ranks high in tree population (19% in SSF and 8% in NSSF). Shannon-Weiner diversity for trees is higher (>3) in six NSSF transects compared to SSF (<3). Higher tree endemism (45%), total endemic tree population (71%) and significantly higher above ground biomass (349 t/ha) cum carbon sequestration potential (131 t/ha) characterizes SSF. Faunal richness is evident from amphibians (35 species - 26 endemics, 11 in IUCN Red List). This study emphasizes the need for bringing to light more of relic forests for their biodiversity, carbon sequestration and hydrology. The lives of marginal farmers and forest tribes can be uplifted through partnership in carbon credits, by involving them in mitigating global climatic change through conservation and restoration of high biomass watershed forests.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A substituted phosphoramidate has been used as a ligand to lanthanides for the first time. New complexes of lanthanide nitrates with O,O′,N-triisopropyl phosphoramidate (TIP) of the general formula Ln(TIP)3(NO3)3 where Ln=La-Yb and Y have been synthesised and characterised by chemical analysis, infrared and visible electronic spectra and electrical conductance.Infrared spectra indicate the coordination of the ligand to the metal ions through the oxygen of the P=O group. IR and conductance show that the nitrate groups are all coordinated. Electronic spectral shapes have been interpreted in terms of an eight coordinate geometry around the metal ions.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A literal Liapunov stability analysis of a spacecraft with flexible appendages often requires a division of the associated dynamic potential into as many dependent parts as the number of appendages. First part of this paper exposes the stringency in the stability criteria introduced by such a division and shows it to be removable by a “reunion policy.” The policy enjoins the analyst to piece together the sets of criteria for each part. Employing reunion the paper then compares four methods of the Liapunov stability analysis of hybrid dynamical systems illustrated by an inertially coupled, damped, gravity stabilized, elastic spacecraft with four gravity booms having tip masses and a damper rod, all skewed to the orbital plane. The four methods are the method of test density function, assumed modes, and two and one-integral coordinates. Superiority of one-integral coordinate approach is established here. The design plots demonstrate how elastic effects delimit the satellite boom length.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A crack mouth opening displacement (CMOD) gauge has been designed to estimate the crack length as well as the crack opening stress level in an automated fatigue crack propagation test programme. The CMOD gauge accurately predicts crack tip opening levels in K-controlled tests with constant K, K increasing or K decreasing. In all three K-controlled tests with a single 100% overload cycle, the CMOD gauge does not measure the crack tip opening stress level over a large range of crack lengths after the application of the overload. The CMOD gauge measures the stress level at which the overload plastic zone site opens. Caution should thus be exercised in using the crack opening stress level, estimated by the CMOD gauge, to explain fatigue crack propagation under arbitrary load sequences from the viewpoint of crack closure phenomena.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Experiments are performed to determine the mass and stiffness variations along the wing of the blowfly Calliphora. The results are obtained for a pairs of wings of 10 male flies and fresh wings are used. The wing is divided into nine locations along the span and seven locations along the chord based on venation patterns. The length and mass of the sections is measured and the mass per unit length is calculated. The bending stiffness measurements are taken at three locations, basal (near root), medial and distal (near tip) of the fly wing. Torsional stiffness measurements are also made and the elastic axis of the wing is approximately located. The experimental data is then used for structural modeling of the wing as a stepped cantilever beam with nine spanwise sections of varying mass per unit lengths, flexural rigidity (EI) and torsional rigidity (GJ) values. Inertial values of nine sections are found to approximately vary according to an exponentially decreasing law over the nine sections from root to tip and it is used to calculate an approximate value of Young's modulus of the wing biomaterial. Shear modulus is obtained assuming the wing biomaterial to be isotropic. Natural frequencies, both in bending and torsion, are obtained by solving the homogeneous part of the respective governing differential equations using the finite element method. The results provide a complete analysis of Calliphora wing structure and also provide guidelines for the biomimetic structural design of insect-scale flapping wings.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The fracture properties of different concrete-concrete interfaces are determined using the Bazant's size effect model. The size effect on fracture properties are analyzed using the boundary effect model proposed by Wittmann and his co-workers. The interface properties at micro-level are analyzed through depth sensing micro-indentation and scanning electron microscopy. Geometrically similar beam specimens of different sizes having a transverse interface between two different strengths of concrete are tested under three-point bending in a closed loop servo-controlled machine with crack mouth opening displacement control. The fracture properties such as, fracture energy (G(f)), length of process zone (c(f)), brittleness number (beta), critical mode I stress intensity factor (K-ic), critical crack tip opening displacement CTODc (delta(c)), transitional ligament length to free boundary (a(j)), crack growth resistance curve and micro-hardness are determined. It is seen that the above fracture properties decrease as the difference between the compressive strength of concrete on either side of the interface increases. (C) 2010 Elsevier Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

An attempt to systematically investigate the effects of microstructural parameters in influencing the resistance to fatigue crack growth (FCG) in the near-threshold region under three different temper levels has been made for a high strength low alloy steel to observe in general, widely different trends in the dependence of both the total threshold stress intensity range, DELTA-K(th) and the intrinsic or effective threshold stress intensity range, DELTA-K(eff-th) on the prior austenitic grain size (PAGS). While a low strain hardening microstructure obtained by tempering at high temperatures exhibited strong dependence of DELTA-K(th) on the PAGS by virtue of strong interactions of crack tip slip with the grain boundary, a high strength, high strain hardening microstructure as a result of tempering at low temperature exhibited a weak dependence. The lack of a systematic variation of the near-threshold parameters with respect to grain size in temper embrittled structures appears to be related to the wide variations in the amount of intergranular fracture near threshold. Crack closure, to some extent provides a basis on which the increases in DELTA-K(th) at larger grain sizes can be rationalised. This study, in addition, provides a wide perspective on the relative roles of slip behaviour embrittlement and environment that result in the different trends observed in the grain size dependence of near-threshold fatigue parameters, based on which the inconsistency in the results reported in the literature can be clearly understood. Assessment of fracture modes through extensive fractography revealed that prior austenitic grain boundaries are effective barriers to cyclic crack growth compared to martensitic packet boundaries, especially at low stress intensities. Fracture morphologies comprising of low energy flat transgranular fracture can occur close to threshold depending on the combinations of strain hardening behaviour, yield strength and embrittlement effects. A detailed consideration is given to the discussion of cyclic stress strain behaviour, embrittlement and environmental effects and the implications of these phenomena on the crack growth behaviour near threshold.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Callus cultures of sandalwood (Santalum album L.) were established from shoot segments and shoot tips of trees over 20 years old. Shoots were induced directly from shoot tip callus, while in shoot segments embryoids developed from the callus within 4 weeks after subculturing on to a medium supplemented with gibberellic acid (GA). Embryoids of 4–5 mm were transferred to basal medium or basal medium supplemented with low concentrations of auxin showed plantlet development.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A detailed experimental and simulation study has been carried out in the present work to understand drop breakup in regions around the edge of the Rushton turbine in agitated vessels. The effect of impeller speed, impeller size, interfacial tension, and the viscosities of the two phases is studied on drop breakup through their effect on dmax, the size of the largest drop in the system, and the whole size distribution. The measurements were carried out using Galai particle size analyser and optical microscope. Experimental analysis shows that the dmax, maximum stable drop diameter varies with impeller tip velocity to the power -1. The variation of dmax with interfacial tension is studied using different surfactants. The effect of viscosity ratio, achieved by changing the dispersed phase viscosity, on dmax is captured. For the same dmax values obtained from two different dispersed phases show that the wider drop size distribution is observed for higher dispersed phase viscosity.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In some recent dropweight impact experiments [5] with pre-notched bend specimens of 4340 steel, it was observed that considerable crack tunneling occurred in the interior of the specimen prior to gross fracture initiation on the free surfaces. The final failure of the side ligaments happened because of shear lip formation. The tunneled region is characterized by a flat, fibrous fracture surface. In this paper, the experiments of [5] (corresponding to 5 m/s impact speed) are analyzed using a plane strain, dynamic finite element procedure. The Gurson constitutive model that accounts for the ductile failure mechanisms of micro-void nucleation, growth and coalescence is employed. The time at which incipient failure was observed near the notch tip in this computation, and the value of the dynamic J-integral, J d, at this time, compare reasonably well with experiments. This investigation shows that J-controlled stress and deformation fields are established near the notch tip whenever J d , increases with time. Also, it is found that the evolution of micro-mechanical quantities near the notch root can be correlated with the time variation of J d .The strain rate and the adiabatic temperature rise experienced at the notch root are examined. Finally, spatial variations of stresses and deformations are analyzed in detail.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Fracture behaviour of notched and un-notched plain concrete slender beams subjected to three-point or four-point bending is analyzed through a one-dimensional model, also called Softening Beam Model. Fundamental equations of equilibrium are used to develop the model. The influence of structural size in altering the fracture mode from brittle fracture to plastic collapse is explained through the stress distribution across the uncracked ligament obtained by varying the strain softening modulus. It is found that at the onset of fracture instability, stress at the crack tip is equal to zero. The maximum load and fracture load are found to be different and a unique value for the fracture load is obtained. It is shown that the length of the fracture process zone depends on the value of the strain softening modulus. Theoretical limits for fracture process zone length are also calculated. Several nonlinear fracture parameters, such as, crack tip opening displacement, crack mouth opening displacement and fracture energy are computed for a wide variety of beam specimens reported in the literature and are found to compare very well with experimental and theoretical results. It is demonstrated that by following a simple procedure, both pre-peak and post-peak portions of load versus crack mouth opening displacement curve can be obtained quite accurately. Further, a simple procedure to calculate the maximum load is also developed. The predicted values of maximum load are found to agree well with the experimental values. The Softening Beam Model (SBM), proposed in this investigation is very simple and is based on rational considerations. It can completely describe the fracture process from the beginning of formation of the fracture process zone till the onset of fracture instability.A l'aide d'un modèle unidimensionnel dit ldquoSoftening Beam Modelrdquo (SBM), on analyse le comportement à rupture de poutres élancées pleines entaillées ou non, soumises en flexion en trois ou quatre points. Des équations fondamentales d'équilibre sont utilisées pour développer le modèle. On explique l'influence de la taille du composant sur l'altération du mode de rupture en rupture fragile et en effondrement plastique par la distribution par la distribution des contraintes sur le ligament non fissuré lorsque varie le module d'adoucissement. On trouve que la contrainte à l'extrémité de la fissure est nulle est nulle au début de l'instabilité de la rupture. La charge maximum et la charge à la rupture sont trouvées différentes, et on obtient une valeur unique de la charge à la rupture. On montre que la longueur de la zone concernée par le processus de rupture d'pend de la valeur du module d'adoucissement. On calcule également les limites théoriques de longueur de cette zone. Divers paramètres de rupture non linéaire sont calculés pour une large gamme d'éprouvettes en poutres reprises dans la littérature; on trouve qu'il existe une bonne concordance avec les résultats expérimentaux et théoriques. On démontre qu'en suivant une procédure simple on peut obtenir avec une bonne précision la courbe reliant les portions avant et après le pic de sollicitation en fonction du COD de la fissure. En outre, on développe une procédure simple pour calculer la charge maximum. Les valeurs prédites sont en bon accord avec les valeurs expérimentales. Le modèle SBM proposé est très simple et est basé sur des considérations rationnelles. Il est susceptible de décrire complètement le processus de rupture depuis le début de la formation de la zone intéressée jusqu'à l'amorçage de la rupture instable.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

An attempt has been made to systematically investigate the effects of microstructural parameters, such as the prior austenite grain size (PAGS), in influencing the resistance to fatigue crack growth (FCG) in the near-threshold region under three different temper levels in a quenched and tempered high-strength steel. By austenitizing at various temperatures, the PAGS was varied from about 0.7 to 96 μm. The microstructures with these grain sizes were tempered at 200 °C, 400 °C, and 530 °C and tested for fatigue thresholds and crack closure. It has been found that, in general, three different trends in the dependence of both the total threshold stress intensity range, ΔK th , and the intrinsic threshold stress intensity range, ΔK eff, th , on the PAGS are observable. By considering in detail the factors such as cyclic stress-strain behavior, environmental effects on FCG, and embrittlement during tempering, the present observations could be rationalized. The strong dependence of ΔK th and ΔK eff, th on PAGS in microstructures tempered at 530 °C has been primarily attributed to cyclic softening and thereby the strong interaction of the crack tip deformation field with the grain boundary. On the other hand, a less strong dependence of ΔK th and ΔK eff, th on PAGS is suggested to be caused by the cyclic hardening behavior of lightly tempered microstructures occurring in 200 °C temper. In both microstructures, crack closure influenced near-threshold FCG (NTFCG) to a significant extent, and its magnitude was large at large grain sizes. Microstructures tempered at the intermediate temperatures failed to show a systematic variation of ΔKth and ΔKeff, th with PAGS. The mechanisms of intergranular fracture vary between grain sizes in this temper. A transition from “microstructure-sensitive” to “microstructure-insensitive” crack growth has been found to occur when the zone of cyclic deformation at the crack tip becomes more or less equal to PAGS. Detailed observations on fracture morphology and crack paths corroborate the grain size effects on fatigue thresholds and crack closure.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A model for coalescence efficiency of two drops embedded in an eddy has been developed. Unlike the other models which consider only head-on collisions, the model considers the droplets to approach at an arbitrary angle. The drop pair is permitted to undergo rotation while they approach each other. For coalescence to occur, the drops are assumed to approach each other under a squeezing force acting over the life time of eddy but which can vary with time depending upon the angle of approach. The model accounts for the deformation of tip regions of the approaching drops and, describes the rupture of the intervening film, based on stability considerations while film drainage is continuing under the combined influence of the hydrodynamic and van der Waals forces. The coalescence efficiency is defined as the ratio of the range of angles resulting in coalescence to the total range of all possible approach angles. The model not only reconciles the contradictory predictions made by the earlier models based on similar framework but also brings out the important role of dispersed-phase viscosity. It further predicts that the dispersions involving pure phases can be stabilized at high rps values. Apart from explaining the hitherto unexplained experimental data of Konno et al. qualitatively, the model also offers an alternate explanation for the interesting observations of Shinnar.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The mode I and mode II fracture toughness and the critical strain energy release rate for different concrete-concrete jointed interfaces are experimentally determined using the Digital Image Correlation technique. Concrete beams having different compressive strength materials on either side of a centrally placed vertical interface are prepared and tested under three-point bending in a closed loop servo-controlled testing machine under crack mouth opening displacement control. Digital images are captured before loading (undeformed state) and at different instances of loading. These images are analyzed using correlation techniques to compute the surface displacements, strain components, crack opening and sliding displacements, load-point displacement, crack length and crack tip location. It is seen that the CMOD and vertical load-point displacement computed using DIC analysis matches well with those measured experimentally.