266 resultados para quasi-full band gap
Resumo:
We propose a compact model which predicts the channel charge density and the drain current which match quite closely with the numerical solution obtained from the Full-Band structure approach. We show that, with this compact model, the channel charge density can be predicted by taking the capacitance based on the physical oxide thickness, as opposed to C-eff, which needs to be taken when using the classical solution.
Resumo:
This study focuses on the temperature dependent optical band gap changes in the amorphous Ge2Sb2Te5 (GST) films. The behavior of the amorphous GST thin films at low temperatures has been studied. The band gap increment of around 0.2 eV is observed at low temperature (4.2 K) compared to room temperature (300 K). The band gap changes associated with the temperature are completely reversible. The other optical parameters like Urbach energy and Tauc parameter (B-1/2) are studied for different temperatures and discussed. The observed changes in optical band gap (E-g) are fitting to Fan's one phonon approximation. Phonon energy ((h) over bar omega) corresponding to a frequency of 3.59 THz is derived from Fan's approximation, which is close to the reported value of 3.66 THz. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Eulytite compounds, A(3)Bi(XO4)(3) (X = P, A = Ca, Cd, Sr, Pb), belong to the noncentrosymmetric space group l (4) over bar 3d (No. 220) as determined by single-crystal X-ray diffraction studies. The crystals were grown from the melt-cool technique with considerable difficulty as the compounds melt incongruently at their melting temperature, except for the compound Pb3Bi(PO4)(3). The unit cell parameter a is 9.984(5), 9.8611(3), 10.2035(3), and 10.3722(2) angstrom for Ca3Bi(PO4)(3), Cd3Bi(PO4)(3), Sr3Bi(PO4)(3), and Pb3Bi(PO4)(3) respectively, and there are four formula units in the unit cell. The structure of Pb3Bi(VO4)(3), a unique eulytite with vanadium substitution, is compared with all these phosphorus substituted eulytites. The A(2+) and Bi3+ cations occupy the special position (16c) while the O anions occupy the general Wyckoff position (48e) in the crystal structure. Only one O position has been identified for Pb3Bi(PO4)(3) and Pb3Bi(VO4)(3), whereas two O atom sites were identified for Ca3Bi(PO4)(3), Cd3Bi(PO4)(3), and Sr3Bi(PO4)(3). The UV-vis diffuse reflectance spectra indicate large band gaps for all the phosphate eulytites while a lower band gap is observed for the vanadate eulytite. The feasibility of the use of these compounds in optoelectronic devices has been tested by measuring the second-harmonic generation (SHG) values which have been found to be of a magnitude equivalent to the commercially used KDP (KH2PO4).
Resumo:
We discuss the results of an extensive mean-field investigation of the half-filled Hubbard model on a triangular lattice at zero temperature. At intermediate U we find a first-order metal-insulator transition from an incommensurate spiral magnetic metal to a semiconducting state with a commensurate linear spin density wave ordering stabilized by the competition between the kinetic energy and the frustrated nature of the magnetic interaction. At large U the ground state is that of a classical triangular antiferromagnet within our approximation. In the incommensurate spiral metallic phase the Fermi surface has parts in which the wave function renormalization Z is extremely small. The evolution of the Fermi surface and the broadening of the quasi-particle band along with the variation of the plasma frequency and a charge stiffness constant with U/t are discussed.
Resumo:
The recombination and the faradaic fluxes are shown to be sensitive to the location of a single level recombination center, when it is located near the band edges. As the surface level is shifted deeper into the band gap from either of the band edges, the back emission terms are dominated by electron capture and hole capture terms, and the occupancy of the surface level is no longer determined by its location in the band gap. However, when one of the back emission terms determines the surface state occupancy, it is shown that there exists a simple relation between the value of the surface level and the recombination and the faradaic fluxes respectively. Expressions to this effect are derived and verified in the case of the recombination flux, which characterized by the potential at which it attains its maximum value. For the faradaic flux the results are qualitative.
Resumo:
Excitation spectra and transient and steady-state photoconductivity have been studied in undoped and 0.8-mole% Cu-doped single-crystal β-AgI between 150 and 260°K. A single peak in the spectral response was found to occur in each case, at 2.88 eV for undoped and at 2.81 eV for copper-doped specimens at 260 K, the difference being due to a decrease in band gap. The anisotropy due to polarization of incident radiation parallel or perpendicular to the c direction, which is a measure of the energy difference between the Γ9 and Γ7 levels in the valence band, was found to be 0.010 eV. Transient-photoconductivity experiments showed that the hole lifetime was 6 μ sec at 300°K, an order of magnitude larger than the electron lifetime. The hole drift mobility was found to be 12±2 cm2/ V sec at 300°K and limited by traps at a depth of 0.51±0.01 eV with concentration (3-5)×109/cm3 and capture cross section 10-11 cm2. The study of photoconductivity decay versus temperature revealed the presence of shallow hole traps at 0.14±0.02 eV with concentration greater than 1016/cm3 and capture cross section 10-19 cm2. The steady-state photoconductivity was determined by the deep hole traps at 0.51 eV, and showed the presence of shallow electron traps at a depth of 0.28 eV. The trap distribution was found to be substantially the same in pure and copper-doped specimens, indicating the monovalent substitutional role of copper. The effects of iodine annealing, cadmium doping, and heating above the transition temperature were also studied. The possible nature of the traps is discussed.
Resumo:
Transparent glasses in the system 0.5Li(2)O-0.5K(2)O-2B(2)O(3) (LKBO) were fabricated via the conventional melt quenching technique. Amorphous and glassy nature of the samples was confirmed by X-ray diffraction and differential scanning calorimetry (DSC) respectively. Complex dielectric and impedance studies were conducted on the samples at different temperatures in the 100 Hz-10 MHz frequency range. ac conductivity was calculated from the dielectric data and the conductivity relaxation was found to obey the Jonscher's law. The Nyquist's plots (Z `'(omega) vs. Z'(omega)) showed single suppressed semicircles at all the temperatures under study indicating the non ideal Debye type relaxation process to be active. Activation energies for conduction and relaxation process were calculated using the Arrhenius relation. The UV-visible optical transmission spectra was shown a wide transmission window and calculated optical band gap was found to be 5.67 eV.
Resumo:
The paper analyses electromagnetic wave propagation through nonlinear photonic crystal beam-splitters. Different lattice configurations of Y-junction beam-splitters are simulated and propagation properties are investigated with introducing nonlinearity with varying the rod size in crystal lattice. It is seen that nonlinear photonic crystal shows a considerable band-gap even at low refractive contrast. The division of power in both arms of beam-splitters can be controlled by varying the nonlinearity.
Resumo:
We report the soft-X-ray absorption spectra at the oxygen K-edge of La1-xSrxCoO3-δ (x = 0.0, 0.1, 0.2, 0.3 and 0.4) series with experimentally determined δ values. We show that the doping of holes by replacing La3+ with Sr2+ induces states within the band gap of the insulating undoped compound for small x and these doped states have a very substantial oxygen 2p character. This indicates that the insulating compounds belong to the charge transfer insulator regime. With increasing Sr content, the doped states broaden into a band overlapping the top of the primarily oxygen p-derived band, leading to an insulator-metal transition at x ≥ 0.2.
Resumo:
Investigations of a variety of transition metal clusters by means of high-energy spectroscopies including BIS show the occurrence of a metal-insulator transition with decrease in the cluster size. The chemical reactivity of the clusters also varies significantly with the size. Among the many fascinating properties of the fullerenes C60 and C70, a noteworthy one is the interaction between metal clusters and fullerenes. Phase transitions of fullerenes involving orientational disorder and pressure-induced decrease in the band gap of C60 are other novel features of interest.
Resumo:
Thin films of titanium dioxide have been deposited using ion assisted deposition with oxygen ions in the energy range 100�500 eV and current densities up to 100 ?A/cm2. It has been observed that the refractive index of the films increases up to 300 eV and the extinction coefficient increased only nominally up to 300 eV. Optical band gap calculations have shown a strong dependence of the gap on the energy of incident ions. Beyond a critical energy and current density of the ions the refractive index and extinction coefficient of the films start deteriorating. It has also been found that beyond the critical values the optical band gap value decreases. The maximum refractive index obtained was 2.49 at an energy of 300 eV and 50 ?A/cm2 current density. Post?deposition annealing of the films at 500?°C resulted in a slight increase in refractive index without affecting the extinction coefficient. X?ray diffraction studies revealed a monophasic anatase structure in these films. ?
Resumo:
Poly(ethylene-co-vinyl acetate) (EVA) films were irradiated with a 1.2MeV electron beam at varied doses over the range 0-270kGy in order to investigate the modifications induced in its optical, electrical and thermal properties. It was observed that optical band gap and activation energy of EVA films decreased upon electron irradiation, whereas the transition dipole moment, oscillator strength and number of carbon atoms per cluster were found to increase upon irradiation. Further, the dielectric constant, the dielectric loss, and the ac conductivity of EVA films were found to increase with an increase in the dose of electron radiation. The result further showed that the thermal stability of EVA film samples increased upon electron irradiation.
Resumo:
We elucidate the relationship between effective mass and carrier concentration in an oxide semiconductor controlled by a double-doping mechanism. In this model oxide system, Sr1-xLaxTiO3-delta, we can tune the effective mass ranging from 6 to 20m(e) as a function of filling (carrier concentration) and the scattering mechanism, which are dependent on the chosen lanthanum-and oxygen-vacancy concentrations. The effective mass values were calculated from the Boltzmann transport equation using the measured transport properties of thin films of Sr1-xLaxTiO3-delta. We show that the effective mass decreases with carrier concentration in this large-band-gap, low-mobility oxide, and this behavior is contrary to the traditional high-mobility, small-effective-mass semiconductors.
Resumo:
CaSiO3:Eu3+ (1-5 mol%) red emitting phosphors have been synthesized by a low-temperature solution combustion method. The phosphors have been well characterized by powder X-ray diffraction (PXRD), Fourier transform infrared spectroscopy (FTIR), scanning electron microscopy (SEM) and optical spectroscopy. PXRD patterns reveal monoclinic CaSiO3 phase can be obtained at 900 degrees C. The SEM micrographs show the crystallites with irregular shape, mostly angular. Upon 254 nm excitation, the phosphor show characteristic fluorescence D-5(0) -> F-7(J) (J = 0, 1, 2, 3, 4) of the Eu3+ ions. The electronic transition located at 614 nm corresponding to D-5(0) -> F-7(2) of Eu3+ ions, which is stronger than the magnetic dipole transition located at 593 nm corresponding to D-5(0) -> F-7(1) of Eu3+ ions. Different pathways involved in emission process have been studied. Concentration quenching has been observed for Eu3+ concentration >4 mol%. UV-visible absorption shows an intense band at 240 nm in undoped and 270 nm in Eu3+ doped CaSiO3 which is attributed to oxygen to silicon (O-Si) ligand-to-metal charge-transfer (LMCT) band in the SiO32- group. The optical energy band gap is widened with increase of Eu3+ ion dopant. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Exposure with above band gap light and thermal annealing at a temperature near to glass transition temperature, of thermally evaporated amorphous (As2S3)(0.87)Sb-0.13 thin films of 1 mu m thickness, were found to be accompanied by structural effects, which in turn, lead to changes in the optical properties. The optical properties of thin films induced by illumination and annealing were studied by Fourier transform infrared spectroscopy, X-ray photoelectron spectroscopy and Raman spectroscopy. Photo darkening or photo bleaching was observed in the film depending upon the conditions of the light exposure or annealing. These changes of the optical properties are assigned to the change of homopolar bond densities. (C) 2010 Elsevier B.V. All rights reserved.