349 resultados para a-Si film
Resumo:
The increase in optical band gap (photo bleaching) due to light illumination was studied at room temperature as well as at low (4.2 K) temperature for Sb/As2S3 multilayered film of 640 nm thickness by Fourier Transform Infrared Technique. The interdiffusion of Sb into As2S3 matrix results the formation of Sb-As2S3 ternary solid solutions which is explained by the change in optical band gap (E-g), absorption coefficient (alpha), Tauc parameter (B-1/2), Urbach edge (E-e). At the same time, photo darkening phenomena was observed in (As2S3)(0.93)Sb-0.07 film of same thickness both at low and room temperatures. From our X-ray Photoelectron Spectroscopy measurements,we are able to show that some of the As-As, S-S and Sb-Sb bonds are converted into As-S and S-Sb bonds in case of multilayers. We found that the energetically favoured heteropolar bond formation take place by a phonon-assisted mechanism using the lone pair pi electrons of S-2(0). But in case of (As2S3)(0.93)Sb-0.02 film, the homopolar bonds are playing a major role. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
The dependence of barrier height on the metal work function of metal-SiO2-p-Si Schottky barrier diodes was investigated and nonlinearity was found. This is explained by the theoretical model proposed recently by Chattopadhyay and Daw. The values of interface trap density and fixed charge density of the insulating layer of the diodes were calculated using this model and found to be appreciably different from those estimated by the usual method.
Resumo:
Metallic glasses are of interest because of their mechanical properties. They are ductile as well as brittle. This is true of Pd77.5Cu6Si16.5, a ternary glassy alloy. Actually, the most stable metallic glasses are those which are alloys of noble or transition metals A general formula is postulated as T70–80G30-20where T stands for one or several 3d transition elements, and includes the metalloid glass formers. Another general formula is A3B to A5B where B is a metalloid. A computer method utilising the MIGAP computer program of Kaufman is used to calculate the miscibility gap over a range of temperatures. The precipitation of a secondary crystalline phase is postulated around 1500K. This could produce a dispersed phase composite with interesting high temperature-strength properties.
Resumo:
PbSnS2 thin film has been prepared for the first time by spray pyrolysis technique on FTO substrate at 570K. The preliminary optical and structural characteristics of the film have been reported. The optical studies showed that the value of the fundamental absorption edge lies at 1.47eV and a low energy absorption band tail has been observed. The prepared film is p- type electrical conductivity, polycrystalline in nature and has an orthorhombic crystal structure. The value of an average grain size of the film is 350Å.
Resumo:
InN quantum dots (QDs) were fabricated on Si(111) substrate by droplet epitaxy using an RF plasma-assisted MBE system. Variation of the growth parameters, such as growth temperature and deposition time, allowed us to control the characteristic size and density of the QDs. As the growth temperature was increased from 100 C to 300 degrees C, an enlargement of QD size and a drop in dot density were observed, which was led by the limitation of surface diffusion of adatoms with the limited thermal energy. Atomic force microscopy (AFM) and scanning electron microscopy (SEM) were used to assess the QDs size and density. The chemical bonding configurations of InN QDs were examined by X-ray photo-electron spectroscopy (XPS). Fourier transform infrared (FTIR) spectrum of the deposited InN QDs shows the presence of In-N bond. Temperature-dependent photoluminescence (PL) measurements showed that the emission peak energies of the InN QDs are sensitive to temperature and show a strong peak emission at 0.79 eV.
Resumo:
The electrochemical properties of the film-covered anode/solution interface in the magnesium/ manganese dioxide dry cell have been evaluated. The most plausible electrical equivalent circuit description of the Mg/solution interface with the passive film intact, has been identified. These results are based on the analysis of ac impedance and voltage transient measurements made on the dry cell under conditions which cause no damage to the protective passive film on the anode. The study demonstrates the complementary character of impedance and transient measurements when widely different frequency ranges are sampled in each type of investigation. The values and temperature dependence of the anode-film resistance, film capacitance, double-layer capacitance and charge-transfer resistance of the film-covered magnesium/solution interface have been determined. The magnitude of these values and its implications in understanding the important performance aspects of the magnesium/manganese dioxide dry cell are discussed. The study may be extended, in principle, to Li, Al and Ca batteries.
Resumo:
The electrochemical properties of the film-covered anode/solution interface in the magnesium/ manganese dioxide dry cell have been evaluated. The most plausible electrical equivalent circuit description of the Mg/solution interface with the passive film intact, has been identified. These results are based on the analysis of ac impedance and voltage transient measurements made on the dry cell under conditions which cause no damage to the protective passive film on the anode. The study demonstrates the complementary character of impedance and transient measurements when widely different frequency ranges are sampled in each type of investigation. The values and temperature dependence of the anode-film resistance, film capacitance, double-layer capacitance and charge-transfer resistance of the film-covered magnesium/solution interface have been determined. The magnitude of these values and its implications in understanding the important performance aspects of the magnesium/manganese dioxide dry cell are discussed. The study may be extended, in principle, to Li, Al and Ca batteries.
Resumo:
Polycrystalline diamond coatings are grown on Si (100) substrate by hot filament CVD technique. We investigate here the effect of substrate roughening on the substrate temperature and methane concentration required to maintain high quality, high growth rate and faceted morphology of the diamond coatings. It has been shown that as we increase the substrate roughness from 0.05 mu m to 0.91 mu m (centre line average or CLA) there is enhancement in deposited film quality (Raman peak intensity ratio of sp (3) to non-sp (3) content increases from 1.65 to 7.13) and the substrate temperature can be brought down to 640A degrees C without any additional substrate heating. The coatings grown at adverse conditions for sp (3) deposition has cauliflower morphology with nanocrystalline grains and coatings grown under favourable sp (3) condition gives clear faceted grains.
Resumo:
Highly stable silver nanoparticles (Ag NPs) in agar-agar (Ag/agar) as inorganic-organic hybrid were obtained as free-standing film by in situ reduction of silver nitrate by ethanol. The antimicrobial activity of Ag/agar film on Escherichia coli (E. coil), Staphylococcus aureus (S. aureus), and Candida albicans (C albicans) was evaluated in a nutrient broth and also in saline solution. In particular, films were repeatedly tested for antimicrobial activity after recycling. UV-vis absorption and TEM studies were carried out on films at different stages and morphological studies on microbes were carried out by SEM. Results showed spherical Ag NPs of size 15-25 nm, having sharp surface plasmon resonance (SPR) band. The antimicrobial activity of Ag/agar film was found to be in the order, C. albicans > E. coil > S. aureus, and antimicrobial activity against C. albicans was almost maintained even after the third cycle. Whereas, in case of E. coil and S. aureus there was a sharp decline in antimicrobial activity after the second cycle. Agglomeration of Ag NPs in Ag/agar film on exposure to microbes was observed by TEM studies. Cytotoxic experiments carried out on HeLa cells showed a threshold Ag NPs concentration of 60 mu g/mL, much higher than the minimum inhibition concentration of Ag NPs (25.8 mu g/mL) for E. coli. The mechanical strength of the film determined by nanoindentation technique showed almost retention of the strength even after repeated cycle. (C) 2010 Elsevier Ltd. All rights reserved.
Resumo:
Curves for the uniformity in film thickness on spherical substrates are drawn for various geometries. The optimum source-to-substrate height for maximum uniformity of the film thickness is determined. These data are approximated to achieve uniform thickness on a large number of small planar substrates loaded on a large spherical substrate holder, the appropriate geometry being selected on the basis of the radius of curvature of the substrate holder.
Resumo:
Microwave switches operating in the X band were designed and fabricated using amorphous chalcogenide semiconductors of composition GexTeyAsz. Threshold devices were shown to operate as microwave modulators at modulation frequencies of up to 100 MHz. No delay time was observed at the highest frequency although the modulation efficiency decreased above 10 MHz owing to the finite recovery time which was approximately 0.3 × 10−8s. The devices can also be used as variolossers, the insertion loss being 0.5 dB in the OFF state and increasing on switching from 5 dB at 1 mA device current to 18 dB at 100 mA.The behaviour of the threshold switches can be explained in terms of the formation of a conducting filament in the ON state with a constant current density of 2 × 104Acm−2 that is shunted by the device capacitance. The OFF state conductivity σ varies as ωn (0.5 < n < 1) which is characteristic of hopping in localized states. However, there was evidence of a decrease in n or a saturation of the conductivity at high frequencies.As a result of phase separation memory switches require no holding current in the ON state and may be used as novel latching semiconductor phase-shifters.
Resumo:
The electrical switching behavior of amorphous Al23Te77 thin film devices, deposited by flash evaporation, has been studied in co-planar geometry. It is found that these samples exhibit memory type electrical switching. Scanning Electron Microscopic studies show the formation of a crystalline filament in the electrode region which is responsible for switching of the device from high resistance OFF state to low resistance ON state. It is also found that the switching behavior of thin film Al-Te samples is similar to that of bulk samples, with the threshold fields of bulk samples being higher. This has been understood on the basis of higher thermal conductance in bulk, which reduces the Joule heating and temperature rise in the electrode region. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Large-area PVDF thin films have been prepared and characterized for quasi-static and high frequency dynamic strain sensing applications. These films are prepared using hot press method and the piezoelectric phase (beta-phase) has been achieved by thermo-mechanical treatment and poling under DC field. The fabricated films have been characterized for quasi-static strain sensing and the linear strain-voltage relationship obtained is promising. In order to evaluate the ultrasonic sensing properties, a PZT wafer has been used to launch Lamb waves in a metal beam on which the PVDF film sensor is bonded at a distance. The voltage signals obtained from the PVDF films have been compared with another PZT wafer sensor placed on the opposite surface of the beam as a reference signal. Due to higher stiffness and higher thickness of the PZT wafer sensors, certain resonance patterns significantly degrade the sensor sensitivity curves. Whereas, the present results show that the large-area PVDF sensors can be superior with the signal amplitude comparable to that of PZT sensors and with no resonance-induced effect, which is due to low mechanical impedance, smaller thickness and larger area of the PVDF film. Moreover, the developed PVDF sensors are able to capture both A(0) and S-0 modes of Lamb wave, whereas the PZT sensors captures only A(0) mode in the same scale of voltage output. This shows promises in using large-area PVDF films with various surface patterns on structures for distributed sensing and structural health monitoring under quasi-static, vibration and ultrasonic situations. (C) 2010 Elsevier B.V. All rights reserved.