Resumo:
Structural, optical and magnetic studies of Co-doped ZnO have been carried out for bulk as well as thin films. The magnetic studies revealed the superparamagnetic nature for low-temperature synthesized samples, indicating the presence of cobalt metallic clusters, and this is supported by the optical studies. For the high-temperature sintered samples one obtains paramagnetism. The optical studies reveal the presence of Co2+ ions in the tetrahedral sites indicating proper doping. Interestingly, the films deposited by laser ablation from the paramagnetic target showed room temperature ferromagnetism. It appears that the magnetic nature of this system is process dependent.
Resumo:
It has been an outstanding problem that a semiconducting host in the bulk form can be doped to a large extent, while the same host in the nanocrystal form is found to resist any appreciable level of doping rather stubbornly, this problem being more acute in the wurtzite form compared to the zinc blende one. In contrast, our results based on the lattice parameter tuning in a ZnxCd1xS alloy nanocrystal system achieves 7.5% Mn2+ doping in a wurtzite nanocrystal, such a concentration being substantially higher compared to earlier reports even for nanocrystal hosts with the favorable zinc-blende structure. These results prove a consequence of local strains due to a size mismatch between the dopant and the host that can be avoided by optimizing the composition of the alloyed host. Additionally, the present approach opens up a new route to dope such nanocrystals to a macroscopic extent as required for many applications. Photophysical studies show that the quantum efficiency per Mn2+ ion decreases exponentially with the average number of Mn2+ ions per nanocrystal; en route, a high quantum efficiency of 25% is achieved for a range of compositions.
Resumo:
Thin films of antimony-doped tin oxide (SnO2:Sb) were prepared by spray pyrolysis using stannous chloride (SnCl2) and antimony trichloride (SbCl3) as precursors. The antimony doping was varied from 0 to 4 wt%. Scanning electron microscopy (SEM) revealed the surface morphology to be very smooth, yet grainy in nature. X-ray diffraction (XRD) shows films to have preferred orientation, which varies with the extent of antimony doping: undoped films prefer the (2 1 1) orientation, while the (3 0 1) orientation is preferred for doping levels of 0.5 and 1.0 wt%. For higher doping levels, the (2 0 0) orientation is preferred. This difference in preferred orientations is reflected in the SEM of the films. Atomic force microscopy (AFM) reveals that film roughness is not affected by antimony doping. The minimum sheet resistance (2.17 ohm/square) achieved in the present study is lower than values reported to date in SnO2:Sb films prepared from SnCl2 precursor. The Hall mobility of undoped SnO2 films was found to be 109.52 cm(2)/V s, which reduces to 2.55 cm(2)/ Vs for the films doped with 4 wt% of Sb. On the other hand, the carrier concentration, which is 1.23 x 10(19) cm(-3) in undoped films, increases to 2.89 x 10(21) cm(-3) for the films doped with 4 wt% of Sb. (c) 2004 Elsevier B.V. All rights reserved.
Resumo:
Graphene has generated, great sensation due to its amazing properties,and extensive research is being pursued on single as well as bi- and few-layer graphenes. In this Perspective, we highlight some aspects of graphene synthesis surface, magnetic, and mechanical properties, as well as effects of doping and indicate a few useful directions for future research.
Resumo:
Following growth doping technique highly luminescent (quantum yield >50%) Mn-doped ZnS nanocrystals are synthesized via colloidal synthetictechnique. The dopant emission has been optimized with varying reaction parameters and found the ratio of Zn and S as well as the percentage of introduced dopant in the reaction mixture are key factors for controlling the intensity. The method is simple, hassle free, and can be scalable to gram level without hindering the quality of nanocrystals. These nanocrystals retain their emission during various ligand exchange processes and aqueous dispersion.
Resumo:
Doping dependent current-voltage (I-V) and capacitance-voltage (C-V) measurements were carried out on polypyrrole devices in metal-polymer-metal sandwich structure. Temperature dependent I-V measurements infer that space-charge limited conduction (SCLC) with exponential trap distribution is appropriate for the moderately doped samples, whereas trap-free SCLC is observed in lightly doped samples. Trap densities and energies are estimated, the effective mobility is calculated using the Poole-Frenkel model, and the mobility exhibits thermally activated behavior. Frequency dependent capacitance-voltage characteristics show a peak near zero bias voltage, which implies that these devices are symmetric with a negligible barrier height at the metal-polymer interface. Low frequency capacitance measurements have revealed a negative capacitance at higher voltages due to the processes associated with the injection and redistribution of space-charges. (C) 2010 American Institute of Physics.
Resumo:
Detailed high-temperature compression creep experiments on a pure 3 mol% yttria-stabilized tetragonal zirconia (3YTZ) and 3YTZ doped with 4.8 wt% TiO2 revealed that both materials exhibit a similar transition in stress exponents from n similar to 1 to n similar to 2 with a decrease in stress. The stress exponent of 1 and the inverse grain size dependence p of similar to 3 are consistent with the Coble diffusion creep at high stresses; the increase in stress exponent at low stresses is attributed to an interface-controlled diffusion creep process. Measurements revealed that grain-boundary sliding contributes to >similar to 50% of the total strain in both regions with n similar to 1 and n similar to 2, indicating the operation of the same fundamental deformation process in both regions. The creep data indicate that doping with TiO2 leads to an increase in the grain-boundary diffusion coefficients. The increase observed in the dihedral angle with doping is also consistent with the increase in grain boundary diffusion coefficient and the reported enhanced ductility in such materials.
Resumo:
Electronic transport in the high temperature paramagnetic regime of the colossal magnetoresistive oxides, La(1-x)A(x)MnO(3), A=Ca, Sr, Ba, x similar or equal to 0.1-0.3, has been investigated using resistivity measurements. The main motivation for this work is to relook into the actual magnitude of the activation energy for transport in a number of manganites and study its variation as a function of hole doping (x), average A-site cation radius (< r(A)>), cationic disorder (sigma(2)) and strain (epsilon(zz)). We show that contrary to current practice, the description of a single activation energy in this phase is not entirely accurate. Our results clearly reveal a strong dependence of the activation energy on the hole doping as well as disorder. Comparing the results across different substituent species with different < r(A)> reveals the importance of sigma(2) as a metric to qualify any analysis based on (r(A)). (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
We mention here an unusual disorder effect in manganites, namely the ubiquitous hopping behavior for electron transport observed in them over a wide range of doping. We argue that the implied Anderson localization is intrinsic to manganites, because of the existence of polarons in them which are spatially localized, generally at random sites (unless there is polaron ordering). We have developed a microscopic two fluid lb model for manganites, where l denotes lattice site localized l polarons, and b denotes band electrons. Using this, and the self-consistent theory of localization, we show that the occupied b states are Anderson localized in a large range of doping due to the scattering of b electrons from l polarons. Numerical simulations which further include the effect of long range Coulomb interactions support this, as well the existence of a novel polaronic Coulomb glass. A consequence is the inevitable hopping behaviour for electron transport observed in doped insulating manganites.
Resumo:
We demonstrate a top-gated field effect transistor made of a reduced graphene oxide (RGO) monolayer (graphene) by dielectrophoresis. The Raman spectrum of RGO flakes of typical size of 5 mu m x 5 mu m shows a single 2D band at 2687 cm(-1), characteristic of single-layer graphene.The two-probe current-voltage measurements of RGO flakes, deposited in between the patterned electrodes with a gap of 2.5 mu m using ac dielectrophoresis, show ohmic behavior with a resistance of similar to 37 k Omega. The temperature dependence of the resistance (R) of RGO measured between 305 K and 393 K yields a temperature coefficient of resistance [dR/dT]/R similar to -9.5 x 10(-4)/K, the same as that of mechanically exfoliated single-layer graphene. The field-effect transistor action was obtained by electrochemical top-gating using a solid polymer electrolyte (PEO + LiClO4) and Pt wire. The ambipolar nature of graphene flakes is observed up to a doping level of similar to 6 x 10(12)/cm(2) and carrier mobility of similar to 50 cm(2)/V s. The source-drain current characteristics show a tendency of current saturation at high source-drain voltage which is analyzed quantitatively by a diffusive transport model. (C) 2010 Elsevier Ltd. All rights reserved.
Resumo:
KO2 is a molecular solid consisting of oxygen dimers. K present in the lattice donates an electron which goes on to occupy the O p levels.As the basic electronic structure is similar to that of an oxygen molecule, except for broadening due to solid state effects, KO2 represents the realization of the doping of oxygen molecules arranged in a lattice. These considerations alone result in magnetism with high ordering temperatures as our calculations reveal. However, we find that the high temperature structure is unstable to an orbital ordering (OO) transition. The microscopic considerations driving the OO transition, however, are electrostatic interactions instead of the often encountered superexchange driven ordering within the Kugel-Khomskii model often used to describe the OO. This OO transition is also found to preclude any possibility of high magnetic ordering temperatures, which otherwise seemed possible.
Resumo:
We have investigated the electronic structure of Ba1-xKxBiO3 (0<x<0.4) by x-ray photoelectron spectroscopy. The Bi(4f) core levels show a normal valency of +3 as in Bi2O3 and we find no evidence for the disproportionation of Bi4+ to Bi3+ and Bi5+. Instead, we find that BaBiO3 has mixed valent O2- and O1- ions. As the potassium doping is increased, the binding energy of the O2- ions in the O(1s) photoelectron spectra steadily decreases from 529.7 to 528.8 eV. The effect of lowering the O(1s) binding energy is to raise the O(2p) band towards EF and at the superconducting composition a finite density of O(2p) states is observed near EF. Similarly, the Ba(5p) binding energies decrease with potassium doping, indicating increased metallicity. The behavior of the O(1s), Ba(5p), and the valence band resembles that of all the cuprate superconductors and we conclude that in all these oxide superconductors, a hole in the (filled) O(2p) band is the carrier responsible for superconductivity, which predicts hole conduction in the Ba-K-Bi-O and Ba-Pb-Bi-O systems.
Resumo:
We report transport and magnetic properties of a different class of highly conducting polyaniline, doped with boron trihalides BX3 (X=F, Cl, and Br). In order to understand the transport mechanism we analyze the temperature dependence of resistivity of a large number of samples, made by pelletizing doped polyaniline powder and by doping films of polyaniline. We find that the charge transport in this class of conducting polyaniline is driven by the charging-energy limited transport of charge carriers, in contrast to the quasi-one-dimensional variable range hopping conduction prevalent in conventional proton-doped polyaniline samples. Magnetic susceptibility provides further insight into the unusually high intrinsic conductivity behavior.
Resumo:
Pristine and long-chain functionalized single-walled carbon nanotubes (SWNTs) were incorporated successfully in supramolecular organogels formed by an all-trans tri(p-phenylenevinylene) bis-aldoxime to give rise to new nanocomposites with interesting mechanical, thermal and electrical properties. Variable-temperature UV-vis and fluorescence spectra reveal both pristine and functionalized SWNTs promote aggregation of the gelator molecules and result in quenching of the UV-vis and fluorescence intensity. Electron microscopy and confocal microscopy show the existence of a densely packed and directionally aligned fibrous network in the resulting nanocomposites. Differential scanning calorimetry (DSC) of the composites shows that incorporation of SWNTs increases the gel formation temperature. The DSC of the xerogels of 1-SWNT composites indicates formation of different thermotropic mesophases which is also evident from polarized optical microscopy. The reinforced aggregation of the gelators on SWNT doping was reflected in the mechanical properties of the composites. Rheology of the composites demonstrates the formation of a rigid and viscoelastic solid-like assembly on SWNT incorporation. The composites from gel-SWNTs were found to be semiconducting in nature and showed enhanced electrical conductivity compared to that of the native organogel. Upon irradiation with a near IR laser at 1064 nm for 5 min it was possible to selectively induce a gel-to-sol phase transition of the nanocomposites, while irradiation for even 30 min of the native organogel under identical conditions did not cause any gel-to-sol conversion.
Resumo:
Gd2O3:Eu3+ (0.5-8.0 mol%) nanophosphors have been prepared by low temperature solution combustion method using metal nitrates as oxidizers and oxalyl dihydrazide (ODH) as a fuel. The phosphors are well characterized by powder X-ray diffraction (PXRD), scanning electron microscopy (SEM), Fourier transform infrared spectroscopy (FT-IR) and photoluminescence (PL) techniques. PXRD patterns of as-formed and calcined (800 degrees C, 3 h) Gd2O3 powders exhibit monoclinic phase with mean crystallite sizes ranging from 20 to 50 nm. Eu3+ doping changes the structure from monoclinic to mixed phase of monoclinic and cubic. SEM micrographs shows the products are foamy, agglomerated and fluffy in nature due to the large amount of gases liberated during combustion reaction. Upon 254 nm excitation the photoluminescence of the Gd2O3:Eu3+ particles show red emission at 611 nm corresponding to D-5(0)-> F-7(2) transition. It is observed that PL intensity increases with calcination temperature. This might be attributed to better crystallization and eliminates the defects, which serve as centers of non-radiative relaxation for nanomaterials. It is observed that the optical energy gap (E-g) is widened with increase Eu3+ content. (C) 2010 Elsevier B.V. All rights reserved.