123 resultados para PEROXYOXALATE CHEMI-LUMINESCENCE


Relevância:

10.00% 10.00%

Publicador:

Resumo:

Interaction of CdSe and ZnO nanocrystals with electron-donating tetrathiafulvalene (TTF) and electron-withdrawing tetracyanoethylene (TCNE) has been investigated. Isothermal calorimetry shows CdSe nanocrystals interact more strongly with TCNE than TTF. Interaction of larger CdSe nanocrystals with TCNE causes a red-shift in the band-edge emission because of agglomeration, while the smaller CdSe nanocrystals, exhibiting stronger interaction with TCNE modify the optical gap of the nanocrystal. Luminescence of CdSe gets quenched sharply after addition of both TTF and TCNE. ZnO nanocrystals also exhibit luminescence quenching to lesser extent. Defect-emission of ZnO nanocrystals gets red or blue-shifted after interaction with TTF or TCNE respectively. (C) 2012 Elsevier B. V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We report the synthesis of trigonal and tetragonal phase GeO2 films/microrods from a Ge wafer/powder by thermal oxidation. Both trigonal and tetragonal GeO2 exhibit excitation-dependent luminescence. Trigonal GeO2 exhibits strong green luminescence while tetragonal GeO2 exhibits strong blue luminescence when excited with ultra-violet light. Yellow-red luminescence is observed when both the phases are excited with green light. The emission wavelength varies almost linearly with the excitation wavelength both for trigonal and tetragonal GeO2. The variation is significant in the case of tetragonal GeO2, indicating a potential wavelength converter material.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Li+-doped Gd2O3:Eu3+ phosphors have been studied as potential red phosphors for application to field emission displays. The Li+-doped and undoped Gd2O3:Eu3+ phosphors were synthesized by low temperature solution combustion method. The enhanced luminescence was regarded as the result of the creation of oxygen vacancies due to the Gd3+ sites occupied by Li+ ions, the alteration of the crystal field surrounding the activator Eu3+ ions owing to the incorporation of Li+ into interstial sites. The result in a remarkable increase on photoluminescence and the strong emission was observed at 612 nm by a factor of 4.1 in comparison with that of undoped sample.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

alpha-Fe2O3 nanoparticles were synthesized by a low temperature solution combustion method. The structural, magnetic and luminescence properties were studied. Powder X-ray diffraction (PXRD) pattern of alpha-Fe2O3 exhibits pure rhombohedral structure. SEM micrographs reveal the dumbbell shaped particles. The EPR spectrum shows an intense resonance signal at g approximate to 5.61 corresponding to isolated Fe3+ ions situated in axially distorted sites, whereas the g approximate to 2.30 is due to Fe3+ ions coupled by exchange interaction. Raman studies show A(1g) (225 cm(-1)) and E-g (293 and 409 cm(-1)) phonon modes. The absorption at 300 nm results from the ligand to metal charge transfer transitions whereas the 540 nm peak is mainly due to the (6)A(1) + (6)A(1) —> T-4(1)(4G) + T-4(1)(4G) excitation of an Fe3+-Fe3+ pair. A prominent TL glow peak was observed at 140 C at heating rate of 5 degrees C s(-1). The trapping parameters namely activation energy (E), frequency factor (s) and order of kinetics (b) were evaluated and discussed. (C) 2012 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

YAlO3:Ni2+ (0.1 mol%) doped nanophosphor was synthesised by a low temperature solution combustion method. Powder X-ray diffraction (PXRD) confirms the orthorhombic phase of yttrium aluminate (YAlO3) along with traces of Y3Al5O12. Scanning Electron microscopy (SEM) shows that the powder particles appears to be spherical in shape with large agglomeration. The average crystallite sizes appeared to be in the range 45-90 nm and the same was confirmed by transmission electron microscopy (TEM) and Williamson-Hall (W-H) plots. Electron Paramagnetic Resonance (EPR) and photoluminescence (PL) studies reveal that Ni2+ ions are in octahedral coordination. Thermoluminescence (TL) glow curve consists of two peaks with the main peak at similar to 224 degrees C and a shouldered peak at 285 degrees C was recorded in the range 0.2-15 kGy gamma-irradiated samples. The TL intensity was found to be increasing linearly for 224 degrees C and 285 degrees C peaks up to 1 kGy and thereafter it shows sub-linear (up to 8 kGy) and saturation behavior. The trap parameters namely activation energy (E), order of kinetics (b), frequency factor (s) at different gamma-doses were determined using Chens glow peak shape and Luschiks methods then the results are discussed in detail. Simple glow peak structure, the 224 degrees C peak in YAlO3:Ni2+ nanophosphor can be used in personal dosimetry. (C) 2012 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We demonstrate electronic energy transfer between resonance states of 2 and 2.8 nm CdTe quantum dots in aqueous media using steady-state photoluminescence spectroscopy without using any external linker molecule. With increasing concentration of larger dots, there is subsequent quenching of luminescence in smaller dots accompanied by the enhancement of luminescence in larger dots. Our experimental evidence suggests that there is long-range resonance energy transfer among electronic excitations, specifically from the electronically confined states of the smaller dots to the higher excited states of the larger dots.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Here, we report for the first time a simple thermal oxidation strategy for the large area synthesis of Ge/GeO2 nanoholes from Ge and studied the luminescence of Ge/GeO2 and hole formation mechanism through phase and luminescence mapping. Photoluminescence mapping reveals that the emission in the visible range is only from the hole region, which provokes the necessity of the nanoholes. Such materials can also be used to convert ultraviolet to visible radiation for detection by conventional phototubes and to coat blue or ultraviolet diodes to obtain white light.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Wafer/microcrystallites of oxidized Ge with holes/nanoholes synthesized by thermal oxidation strategy from Ge wafer/microcrystallites can convert one wavelength to another. Both oxidized Ge wafer and microcrystallites shows excitation- and power-dependent luminescence. Red-shift is observed as the excitation wavelength is increased, while blue-shift is observed as power density is increased. Over all, blue-green-yellow-orange luminescence is observed depending on the excitation wavelength and the morphology of oxidized Ge. The various defects level associated with germanium-oxygen vacancies in GeO2 and Ge/GeO2 interface are responsible for the excitation-dependent luminescence. Being a light-conversion material, oxidized Ge is expected to find potential applications in solid-state lighting, photovoltaic devices and photocatalysis.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

ZnO films have been grown via a vapour phase transport (VPT) on soda lime glass (SLG) and indium-tin oxide (ITO) coated glass. ZnO film on ITO had traces of Zn and C which gives them a dark appearance while that appears yellowish-white on SLG. X-ray photoelectron spectroscopy studies confirm the traces of C in the form of C-O. The photoluminescence studies reveal a prominent green luminescence band for ZnO film on ITO. (C) 2013 Author(s).

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Structural, iono (IL) and thermoluminescence (TL) studies of Zn2SiO4:Sm3+ (1-5 mol%) nanophosphor bombarded with swift heavy ions in the fluence range 3.91 x 10(12)-21.48 x 10(12) cm(-2) have been carried out. The average crystallite sizes for pristine and ion irradiated for 3.91 x 10(12) ions cm(-2) and 21.48 x 10(12) ions cm(-2) were found to be 34, 26 and 20 nm. With increase of ion fluence, the intensity of XRD peaks decreases and FWHM increases. The peak broadening indicates the stress induced point/clusters defects produced due to heavy ion irradiation. IL studies were carried out for different Sm3+ concentrations in Zn2SiO4 by irradiating with ion fluence of 15.62 x 10(12) ions cm(-2). The characteristic emission peaks at similar to 562, 599, 646 and 701 nm were recorded by exciting Si7+ ions in the fluence range 3.91 x 10(12)-21.48 x 10(12) ions cm(-2). These peaks were attributed to (4)G(5/2)-> H-6(5/2) (562 nm), (4)G(5/2)-> H-6(7/2) (599 nm), (4)G(5/2)-> H-6(9/2) (646 nm), and (4)G(5/2)-> H-6(5/2) (701 nm) transitions of Sm3+. The highest emission was recorded at 3 mol% of Sm3+ doped Zn2SiO4. TL studies were carried out for 3 mol% Sm3+ concentration in the fluence range 3.91 x 10(12)-21.48 x 10(12) ions cm(-2). Two U glow peaks at 152 and 223 degrees C were recorded. The kinetic parameters (E, b, and s), were estimated using Chen's peak shape method. Simple glow curve structure (223 degrees C), highly resistive, increase in TL. intensity up to 19.53 x 10(12) ions cm(-2), simple trap distribution makes Zn2SiO4:Sm3+ (3 mol%) phosphor highly useful in radiation dosimetry.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Studies were carried on the growth behavior of InN nanodots by plasma assisted molecular beam epitaxy on bare Si(100) substrates and their structural, optical, electrical properties. The growth was carried out by two different methods such as, (i) mono-step growth process at a low temperature and a (ii) bi-step growth process with the combination of low and high temperatures for the formation of single crystalline nanodots with well defined crystallographic facets due to cluster migration. Low temperature photoluminescence shows a free excitonic (FE) luminescence at 0.80 eV. The Raman spectroscopy and X-ray diffraction studies reveal that the nanodots as well as the film were of wurtzite structure and strain free.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Although weak interactions, such as C-H center dot center dot center dot O and pi-stacking, are generally considered to be insignificant, it is their reorganization that holds the key for many a solid-state phenomenon, such as phase transitions, plastic deformation, elastic flexibility, and mechanochromic luminescence in solid-state fluorophores. Despite this, the role of weak interactions in these dynamic phenomena is poorly understood. In this study, we investigate two co-crystal polymorphs of caffeine:4-chloro-3-nitrobenzoic acid, which have close structural similarity (2D layered structures), but surprisingly show distinct mechanical behavior. Form I is brittle, but shows shear-induced phase instability and, upon grinding, converts to Form II, which is soft and plastically shearable. This observation is in contrast to those reported in earlier studies on aspirin, wherein the metastable drug forms are softer and convert to stable and harder forms upon stressing To establish a molecular level understanding, have investigated the two co-crystal polymorphs I and II by single crystal X-ray diffraction, nanoindentation to quantify mechanical properties, and theoretical calculations. The lower hardness (from nanoindentation) and smooth potential surfaces (from theoretical studies) for shearing of layers in Form II allowed us to rationalize the role of stronger intralayer (sp(2))C-H center dot center dot center dot O and nonspecific interlayer pi-stacking interactions in the structure of II. Although the Form I also possesses the same type of interactions, its strength is clearly opposite, that is, weaker intralayer (sp(3))C-H center dot center dot center dot O and specific interlayer pi-stacking interactions. Hence, Form I is harder than Form IL Theoretical calculations and indentation on (111) of Form I suggested the low resistance of this face to mechanical stress; thus, Form I converts to II upon mechanical action. Hence, our approach demonstrates the usefulness of multiple techniques for establishing the role of weak noncovalent interactions in solid-state dynamic phenomena, such as stress induced phase transformation, and hence is important in the context of solid-state pharmaceutical chemistry and crystal engineering.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This article presents the investigation of the coordination behavior of a newly synthesized tricarboxylate ligand, obtained by joining imidazole dicarboxylic acid and 4-carboxybenzyl moieties cbimdaH(3), 1-(4-carboxybenzyl)-1H-imidazole-4,5-dicarboxylic acid]. Two novel coordination polymers were obtained through solvothermal reactions under similar conditions namely Sr(cbimdaH)(H2O)](n) (1) and Cd-2(cbimdaH)(2)(H2O)(6)](n)center dot(DMF)(3n)(H2O)(3n) (2), with the ligand behaving as a dianionic tricarboxylate linker. The single crystal X-ray structures show that while 1 forms a 3D coordination polymer, 2 forms a 1D polymer which is further assembled in three dimensions through supramolecular interactions (H-bonding). Complex 1 consists of Sr2+ ions in a distorted dodecahedral coordination geometry, while 2 consists of Cd2+ ions in distorted pentagonal bipyramidal geometries. A topology study reveals that 1 has a new topology based on the 5,6-coordinated 3D net architecture. The luminescence properties of the complexes in the solid state and their thermal stabilities were studied.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We report the synthesis of Pr6O11 microspheres self-assembled from ultra-small nanocrystals formed by the microwave irradiation of a solution of a salt of Pr in ethylene glycol (EG). The as-prepared product consists of microspheres measuring 200 to 500 nm in diameter and made of <5 nm nano-crystallites. The surface of these microspheres/nanocrystals is covered/capped with an organic layer of ethylene glycol as shown by TEM analysis and confirmed by IR spectroscopy measurements. The as-prepared product shows blue-green emission under excitation, which changes to orange-red when the product is annealed in air at 600 degrees C for 2 h. This change in luminescence behaviour can be attributed to presence of ethylene glycol layer in the as-prepared product. The samples were characterized by X-ray powder diffraction (XRD), field emission scanning electron microscopy (FE-SEM), IR Spectroscopy (IR), transmission electron microscopy (TEM), and thermogravimetric analysis (TGA). (C) 2013 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Despite being a particularly good emitter, use of divalent Eu has been seriously limited. This is because severe reducing environments or special hosts are needed during synthesis of divalent Eu containing phosphors. In this work we stabilize Eu in its 2+ state (in CaAl2O4) using an open-air solution combustion reaction. The impact of fuel (F) to oxidizer (O) molar ratios (F/O = 0.5-2.0) on luminescence properties is explored. Chromaticity of Eu:CaAl2O4 depends sensitively on the F/O ratio. In general, higher F/O inhibits Eu3+ and promotes Eu2+ formation, which in turn improves the quality of the blue phosphor. EPR spectra show inhomogeneous broadening effects with the increase in F/O ratio, which suggests that disorder creation is promoted when F/O is increase. This is also confirmed by an increase in emission line width in PL spectra, when F/O is increased. (C) 2013 Elsevier B.V. All rights reserved.