516 resultados para Dielectric materials


Relevância:

30.00% 30.00%

Publicador:

Resumo:

The results of the studies on the effect of rare earth Nd doping on the phase formation behavior and electrical properties of sol-gel derived Pb-1.05(Zr0.53Ti0.47)O-3 (PZT) thin films are presented. The perovskite phase is obtained up to 5 at. % doping and beyond that pyrochlore phase was found to coexist with the perovskite phase in all the films. The transition temperature of undoped lead zirconate titanate (PZT) film was found to be reduced with Nd doping. The Nd doped films also exhibited typical relaxor-type behavior and a diffuse phase transition, similar to that observed in relaxor materials. The introduction of Nd into the PZT lattice probably introduces disorder in the B site of ABO(3) lattice, which causes the observed dielectric relaxation. Efforts were made to isolate the irreversible component contributions in low field dielectric and high field polarization switching behavior. (C) 2001 American Institute of Physics.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Single crystals of a-hopeite exhibiting high transparency were grown by single diffusion gel growth technique. Single crystal X-ray diffraction analysis reveals that the crystal belongs to orthorhombic system. The values of several structural and physical parameters have been determined for the grown crystal. The optical absorption study reveals the transparency of the crystal and is noticed in the entire visible region and the cut-off wavelength was found to be 230 nm. The optical band gap found to be at 3.25 eV. The dependence of extinction co-efficient (k) and the refractive index (n) on the wavelength was also shown. The dielectric constant and dielectric loss of the crystal was studied as a function of frequency and temperature. Transport properties of the grown crystal have been studied from the Cole-Cole plot. (C) 2010 Elsevier GmbH. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Recently, there has been growing interest in Ca modified BaTiO3 structures due to their larger electro-optic coefficients for their use in optical storage of information over conventional BaTiO3 crystals. Barium Calcium Titanate (BCT) shows promising applications in advanced laser systems, optical interconnects and optical storage devices. BaTiO3 thin films of varied Ca (3 at. % - 15 at. %) doping were deposited using pulsed laser ablation (KrF excimer laser) technique over Pt/Si substrates. The stoichiometric and the compositional analysis were carried out using EDAX and SIMS. The dielectric studies were done at the frequency regime of 40 Hz to 100 kHz at different ambient temperatures from 200 K to 600 K. The BCT thin films exhibited diffuse phase transition, which was of a typical non lead relaxor behavior and had high dielectric constant and low dielectric loss. The phase transition for the different compositions of BCT thin films was near the room temperature, showing a marked departure from the bulk phase transition. The C - V and the hysteresis behavior confirmed the ferroelectric nature below the phase transition and paraelectric at the room temperature.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Bi2Nbx V1−xO5.5 ceramics with x ranging from 0.01 to 0.5 have been prepared. The crystal system transforms from an orthorhombic to tetragonal at x 3= 0.1 and it persists until x = 0.5. Scanning electron microscopic (SEM) investigations carried out on thermally etched Bi2NbxV1−xO5.5 ceramics confirm that the grain size decreases markedly (18 μm to 4 μm) with increasing x. The shift in the Curie temperature (725 K) toward lower temperatures, with increasing x, is established by Differential Scanning Calorimetry (DSC). The dielectric constants as well as the loss tangent (tan δ) decrease with increasing x at room temperature.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

DC electric field induced dielectric properties of 0.7Pb(Mg1/3Nb2/3)O3-0.3PbTiO3 (PMN-PT) thin films were studied as a function of frequency at different temperatures. It was observed that the dielectric constant (ε) and dissipation factor (tanδ) were decreased in presence of bias field. The temperature of dielectric maxima was found to increase with increasing bias level. The low temperature (dielectric permittivity was suppressed with the application of dc bias. After a certain bias voltage the relaxor property of films was disappeared i.e. the films exhibited normal ferroelectric behavior. Since the absence of long range interaction among the nanopolar clusters in PMN and its family is believed to be the origin of relaxor behavior, disappearance of relaxor nature in PMN-PT (70/30) films could be attributed to manifestation of long-range order at higher bias voltage. This was observed in the temperature dependence of dielectric constant i.e. the films neither exhibited any frequency dispersion in the temperature of dielectric maximum (Tm) nor showed any diffused phase transition. The relaxor property of PMN-PT thin films was studied in terms of diffused phase transition together with frequency dispersion of the temperature of dielectric maximum (Tm). Vogel-Fulcher relation was used to analyze the frequency dependence of temperature of dielectric maximum.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The dielectric response of BaBi2Nb2O9 (BBN) thin films has been studied as a function of frequency over a wide range of temperatures. Both dielectric constant and loss tangent of BBN thin films showed a ‘power law’ dependence with frequency, which was analyzed using the Jonscher's universal dielectric response model. Theoretical fits were utilized to compare the experimental results and also to estimate the value of temperature dependence parameters such as n(T) and a(T) used in the Jonscher's model. The room temperature dielectric constant (ε') of the BBN thin films was 214 with a loss tangent (tanδ) of 0.04 at a frequency of 100 kHz. The films exhibited the second order dielectric phase transition from ferroelectric to paraelectric state at a temperature of 220 °C. The nature of phase transition was confirmed from the temperature dependence of dielectric constant and sponteneous polarization,respectively. The calculated Currie constant for BBN thin films was 4 × 105°C.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A study was done on pulsed laser deposited relaxor ferroelectric thin films of 0.7Pb(Mg1/3Nb2/3)O3-0.3PbTiO3 (PMN-PT) deposited on platinized silicon substrates with template layers to observe the influence of the template layers on physical and electrical properties. Initial results, showed that perovskite phase (80% by volume) was obtained through proper selection of the processing conditions on Pt/Ti/SiO2/Si substrates. The films were grown at 300°C and then annealed in a rapid thermal annealing furnace in the temperature range of 750-850°C to induce crystallization. Comparison of the films annealed at different temperatures revealed a change in crystallinity, perovskite phase formation and grain size. These results were further used to improve the quality of the perovskite PMN-PT phase by inserting thin layers of TiO2 on the Pt substrate. These resulted in an increase in perovskite phase in the films even at lower annealing temperatures. Dielectric studies on the PMN-PT films show very high values of dielectric constant (1300) at room temperature, which further improved with the insertion of the template seed layer. The relaxor properties of the PMN-PT were correlated with Vogel-Fulcher theory to determine the actual nature of the relaxation process.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Relaxor ferroelectric thin films of 0.7Pb(Mg1/3Nb2/3)O-3-0.3PbTiO(3) (PMN-PT) deposited on platinized silicon substrates with and without template layers were studied. Perovskite phase (80% by volume) was obtained through proper selection of the processing conditions on bare Pt/Ti/SiO2/Si substrates. The films were initially grown at 300 degreesC using pulsed-laser ablation and subsequently annealed in a rapid thermal annealing furnace in the temperature range of 750-850 degreesC to induce crystallization. Comparison of microstructure of the films annealed at different temperatures showed change in perovskite phase formation and grain size etc. Results from compositional analysis of the films revealed that the films initially possessed high content of lead percentage, which subsequently decreased after annealing at temperature 750-850 degreesC. Films with highest perovskite content were found to form at 820-840 degreesC on Pt substrates where the Pb content was near stoichiometric. Further improvement in the formation of perovskite PMN-PT phase was obtained by using buffer layers of La0.5Sr0.5CoO3 (LSCO) on the Pt substrate. This resulted 100% perovskite phase formation in the films deposited at 650 degreesC. Dielectric studies on the PMN-PT films with LSCO template layers showed high values of relative dielectric constant (3800) with a loss factor (tan delta) of 0.035 at a frequency of 1 kHz at room temperature. (C) 2002 Elsevier Science B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Combining experiments with first-principles calculations, we show that site-specific doping of Mn into SrTiO(3) has a decisive influence on the dielectric properties of these doped systems. We find that phonon contributions to the dielectric constant invariably decrease sharply on doping at any site. However, a sizable, random dipolar contribution only for Mn at the Sr site arises from a strong off-centric displacement of Mn in spite of Mn being in a non-d(0) state; this leads to a large dielectric constant at higher temperatures and gives rise to a relaxor ferroelectric behavior at lower temperatures. We also investigate magnetic properties in detail and critically reevaluate the possibility of a true multiglass state in such systems.

Relevância:

30.00% 30.00%

Publicador:

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Titanium dioxide (TiO(2)) and silicon dioxide (SiO(2)) thin films and their mixed films were synthesized by the sol-gel spin coating method using titanium tetra isopropoxide (TTIP) and tetra ethyl ortho silicate (TEOS) as the precursor materials for TiO(2) and SiO(2) respectively. The pure and composite films of TiO(2) and SiO(2) were deposited on glass and silicon substrates. The optical properties were studied for different compositions of TiO(2) and SiO(2) sols and the refractive index and optical band gap energies were estimated. MOS capacitors were fabricated using TiO(2) films on p-silicon (1 0 0) substrates. The current-voltage (I-V) and capacitance-voltage (C-V) characteristics were studied and the electrical resistivity and dielectric constant were estimated for the films annealed at 200 degrees C for their possible use in optoelectronic applications. (C) 2011 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Large single crystal of triglycine sulphate (dimension 100 mm along monoclinic b-axis and 15 mm in diameter) was grown using the unidirectional solution growth technique. The X-ray diffraction studies confirmed the growth/long axis to be b-axis (polar axis). The dielectric studies were carried out at various temperatures to establish the phase transition temperature. The frequency response of the dielectric constant, dielectric loss and impedance of the crystal along the growth axis, was monitored. These are typically characterized by strong resonance peaks in the kHz region. The piezoelectric coefficients like stiffness constant (C), elastic coefficient (S), electromechanical coupling coefficient (k) and d (31) were calculated using the resonance-antiresonance method. Polarization (P)-Electric field (E) hysteresis loops were recorded at various temperatures to find the temperature-dependent spontaneous polarization of the grown crystal. The pyroelectric coefficients were determined from the pyroelectric current measurement by the Byer and Roundy method. The ferroelectric domain patterns were recorded on (010) plane using scanning electron microscopy and optical microscopy.