115 resultados para Amorphous selenium
Resumo:
We present the synthesis and properties of iodine incorporated amorphous carbon films. Optical studies depict a decrease in band gap with variation in iodine content and pyrolysis temperature. Tuning of the metal-insulator transition is achieved by varying the pyrolysis temperature and iodine concentration. Appreciable decrease in magnetoresistance is observed with iodine incorporation, but negative magnetoresistance typical behavior of metallic samples is not witnessed.
Resumo:
Abstract | Non-crystalline or glassy semiconductors are of great research interest for the fabrication of large area electronic systems such as displays and image sensors. Good uniformity over large areas, low temperature fabrication and the promise of low cost electronics on large area mechanically flexible and rigid substrates are some attractive features of these technologies. The article focusses on amorphous hydrogenated silicon thin film transistors, and reviews the problems, solutions and applications of these devices.
Resumo:
Densification characteristics of amorphous ZrO2-40 mol% Al2O3 powder with 3 to 15 mu m nominal particle size range, produced by spray pyrolysis, have been studied by conducting hot pressing experiments at 573, 723 and 873 K with uniaxial pressures of 250, 500 and 750 MPa. Most of the increase in relative density from the starting value of similar to 40% occurred during loading up to the desired pressure. The increments in density during 1 hour constant pressure dwells were less than 4% at all temperatures and pressure. Inter-particle bonding was not observed at 573 K. Correlation between the results with a viscous sintering model for hot pressing is not satisfactory for describing the behavior as normal viscous sintering.
Resumo:
The electrical switching behavior of amorphous GexSe35-xTe65 thin film samples has been studied in sandwich geometry of electrodes. It is found that these samples exhibit memory switching behavior, which is similar to that of bulk Ge-Se-Te glasses. As expected, the switching voltages of GexSe35-xTe65 thin film samples are lower compared to those of bulk samples. In both thin film amorphous and bulk glassy samples, the switching voltages are found to increase with the increase in Ge concentration, which is consistent with the increase in network connectivity with the addition of higher coordinated Ge atoms. A sharp increase is seen in the composition dependence of the switching fields of amorphous GexSe35-xTe65 films above x = 21, which can be associated with the stiffness transition. Further, the optical band gap of a-GexSe35-x Te-65 thin film samples, calculated from the absorption spectra, is found to show an increasing trend with the increase in Ge concentration, which is consistent with the variation of switching fields with composition. The increase in structural cross-linking with progressive addition of 4-fold coordinated Ge atoms is one of the main reasons for the observed increase in switching fields as well as band gaps of GexSe35-xTe65 samples. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Amorphous thin film Ge15Te85-xSnx (1 <= x <= 5) and Ge17Te83-xSnx (1 <= x <= 4) switching devices have been deposited in sandwich geometry using a flash evaporation technique, with aluminum as the top and bottom electrodes. Electrical switching studies indicate that these films exhibit memory type electrical switching behavior. The switching fields for both the series of samples have been found to decrease with increase in Sn concentration, which confirms that the metallicity effect on switching fields/voltages, commonly seen in bulk glassy chalcogenides, is valid in amorphous chalcogenide thin films also. In addition, there is no manifestation of rigidity percolation in the composition dependence of switching fields of Ge15Te85-xSnx and Ge17Te83-xSnx amorphous thin film samples. The observed composition dependence of switching fields of amorphous Ge15Te85-xSnx and Ge17Te83-xSnx thin films has been understood on the basis of Chemically Ordered Network model. The optical band gap for these samples, calculated from the absorption spectra, has been found to exhibit a decreasing trend with increasing Sn concentration, which is consistent with the composition dependence of switching fields.
Resumo:
Organoselenium compounds have attracted intense research owing to their unique biological properties as well as pharmaceutical significance. Progress has been made in developing reagents for incorporation of selenium in an efficient and controlled manner. Herein, we present a review on the recently developed selenium reagent, tetraethylammonium tetraselenotungstate, Et4N](2)WSe4 as a versatile selenium transfer reagent in organic synthesis. Tetraselenotungstate has been successfully used for the synthesis of a number of functionalized diselenides, sugar- and nucleoside-derived diselenides, seleno-cystines, selenohomocystines, selenoamides, selenoureas and sugar- and nucleoside-based cyclic-selenide derivatives. Additionally, this reagent has been employed for the ring opening of aziridines to synthesize a variety of beta-aminodiselenides. A new selena-aza-Payne type rearrangement of aziridinemethanoltosylates mediated by tetraselenotungstate for the synthesis of allyl amines is also discussed.
Resumo:
Electrical switching studies on amorphous Ge17Te83−xSnx thin films (1 ≤ x ≤ 4) has been done to find their suitability for Phase Change Memory application; Bulk ingots in glassy form are prepared using conventional melt quenching technique and the thin films are coated using flash evaporation technique. Samples are found to exhibit memory type of electrical switching behavior. The switching voltages of Ge17Te83−xSnx thin films have been found to decrease with increase in Sn concentration. The comparatively lower switching voltages of Ge17Te83−xSnx samples, make them suitable candidates for phase change memory applications.
Resumo:
The development of scaffolds for neural tissue engineering application requires an understanding of cell adhesion, proliferation, and migration of neuronal cells. Considering the potential application of carbon as scaffold materials and the lack of understanding of compatibility of amorphous carbon with neuronal cells, the carbon-based materials in the forms of carbon films and continuous electrospun carbon nanofibers having average diameter of approximate to 200 nm are being investigated with or without ultraviolet (UV) and oxy-plasma (OP) treatments for cytocompatibility property using mouse Neuroblastoma (N2a) and rat Schwann cells (RT4-D6P2T). The use of Raman spectroscopy in combination with Fourier transform infrared (FTIR) and X-ray diffraction establishes the amorphous nature and surface-bonding characteristics of the studied carbon materials. Although both UV and OP treatments make carbon surfaces more hydrophilic, the cell viability of N2a cells is statistically more significant on OP treated fibers/films compared to UV fiber/film substrates after 4 days in culture. The electrospun carbon fibrous substrate provides the physical guidance to the cultured Schwann cells. Overall, the experimental results of this study demonstrate that the electrospun amorphous carbon nanofibrous scaffolds can be used as a suitable biomaterial substrate for supporting cell adhesion and proliferation of neuronal cells in the context of their applications as artificial nerve implants. (c) 2013 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 2013.
Resumo:
This study deals with the influence of Er-doping level and thermal annealing on the optical properties of amorphous Ge-Ga-S thin films. Nominal compositions of (GeS2)(75)(Ga2S3)(25) doped with high concentrations of 2.1 and 2.4 mol% Er2S3 (corresponding to 1.2 and 1.4 at% Er, respectively) have been chosen for this work. The results have been related to those obtained for the un-doped samples. The values of the refractive index, the absorption coefficient and optical band gap have been determined from the transmittance data. It has been found that the optical band gap of un-doped and 2.1 mol% Er2S3-doped films slightly increases with annealing temperature, whereas at 2.4 mol% Er2S3-doping level it is decreased. The dependences of the optical parameters on the erbium concentration and effect of annealing in the temperature range of 100-200 degrees C have been evaluated and discussed in relation to possible structural changes.
Resumo:
Results of a high resolution photoemission and electrochemistry study of Se adsorption Au(111) and Ag(111) surfaces performed by immersion of pristine samples into an aqeuous solution of Na2Se are presented. Cyclic voltammetry on Au shows formation of selenium adsorbed species and the structures observed in reductive desorption are to the atomic and polymeric species observed in XPS. In the case of Au(111) XPS spectra in the Se(3d) region indeed show two main features attributed to Se chemisorbed atomically and polymeric Se-8 features.' Smaller structures due to other types of Se conformations were also observed. The Au(4f) peak line, shape does not show core level, shifts: indicative of Au selenide formation the case of silver, XPS spectra for the Ag(3d) show a broadening of the peak and a deconvolution into Ag-B bulk like Ag-Se components shows that the Ag-Se is located at a lower binding energy, an effect similar to oxidation and sulfidation of Ag. The Se(3d) XPS spectrum is found to be substantially different from the Au case and dominated by atomic type Se due to the selenide, though a smaller intensity Se structure at an energy similar to the Se-8 structure for Au is also observed. Changes in the valence band region. related to Se adsorption are reported.
Resumo:
Electrical switching studies on amorphous Si15Te75Ge10 thin film devices reveal the existence of two distinct, stable low-resistance, SET states, achieved by varying the electrical input to the device. The multiple resistance levels can be attributed to multi-stage crystallization, as observed from temperature dependant resistance studies. The devices are tested for their ability to be RESET with minimal resistance degradation; further, they exhibit a minimal drift in the SET resistance value even after several months of switching. (c) 2013 Elsevier B.V. All rights reserved.
Resumo:
Fourier Transform Infrared (FTIR) spectroscopic analysis has been carried out on the hydrogenated amorphous silicon (a-Si:H) thin films deposited by DC, pulsed DC (PDC) and RF sputtering process to get insight regarding the total hydrogen concentration (C-H) in the films, configuration of hydrogen bonding, density of the films (decided by the vacancy and void incorporation) and the microstructure factor (R*) which varies with the type of sputtering carried out at the same processing conditions. The hydrogen incorporation is found to be more in RF sputter deposited films as compared to PDC and DC sputter deposited films. All the films were broadly divided into two regions namely vacancy dominated and void dominated regions. At low hydrogen dilutions the films are vacancy dominated and at high hydrogen dilutions they are void dominated. This demarcation is at C-H = 23 at.% H for RF, C-H = 18 at.% H for PDC and C-H = 14 at.% H for DC sputter deposited films. The microstructure structure factor R* is found to be as low as 0.029 for DC sputter deposited films at low C-H. For a given C-H, DC sputter deposited films have low R* as compared to PDC and RF sputter deposited films. Signature of dihydride incorporation is found to be more in DC sputter deposited films at low C-H.
Resumo:
Amorphous thin chalcogenide Si15Te85-xGex films (x: 5, 9, 10, 11, 12) are prepared by flash evaporation and the temperature dependence of resistance of these films has been studied in the temperature range 25-250 degrees C. All the compositions show a linear variation of resistance in this temperature range. Apart from the linear variation, a sharp reduction in resistance at one or at two distinct temperatures (T-TR1/T-TR2) is seen. Thin films annealed at these temperatures, when subjected to X-ray diffraction studies suggest that the dominant crystalline phase at T-TR1 and at T-TR2 is the same and the two dips are associated with varying levels of crystallization. This is also reflected in the atomic force microscopic (AFM) study. Further, the resistance of these two phases shows no drift when the films are annealed for varying lengths of time (10 min to 120 min) suggesting the stability of the phases.