830 resultados para Roasting (Metallurgy)
Resumo:
The evolution of microstructure and texture during room temperature compression of commercially pure Ti with four different initial orientations were studied under quasi-static and dynamic loading conditions. At a low strain rate (epsilon)over dot = 3 x 10(-4) s(-1) the different initial textures yielded the same end texture, despite different microstructural evolution in terms of twin boundaries. High strain rate deformation at (epsilon)over dot = 1.5 x 10(3) s(-1) was characterized by extensive twinning and evolution of a texture that was similar to that at low strain rate with minor differences. However, there was a significant difference in the strength of the texture for different orientations that was absent for low strain rate deformed samples at high strain rate. A viscoplastic self-consistent model with a secant approach was used to corroborate the experimental results by simulation. (C) 2011 Published by Elsevier Ltd. on behalf of Acta Materialia Inc.
Resumo:
In this paper the effects of constant and cyclic power loads on the evolution of interfacial reaction layers in lead-free solder interconnections are presented. Firstly, the differences in the growth behavior of intermetallic compound (IMC) layers at the cathode and anode sides of the interconnections are rationalized. This is done by considering the changes in the intrinsic fluxes of elements owing to electromigration as well as taking into account the fact that the growth of Cu3Sn and Cu6Sn5 are coupled via interfacial reactions. In this way, better understanding of the effect of electron flux on the growth of each individual layer in the Cu-Sn system can be achieved. Secondly, it is shown that there is a distinct difference between steady-state current stressing (constant current, constant temperature) and power cycling with alternating on- and off-cycle periods (accompanied by a change of temperature). The reasons behind the observed differences are subsequently discussed. Finally, special care is taken to ensure that the current densities are chosen in such a way that there is no risk for even partial melting of the solder interconnections.
Resumo:
The deformation characteristics of as-cast 304 stainless steel under compression in the temperature range 20-600 degrees C and strain rate range 0.001-100 s(-1) have been studied with a view to characterizing the flow instabilities occurring in the microstructure. Ar strain rates of less than 0.05 s(-1), as-cast 304 stainless steel exhibits flow localization in the temperature range 20-600 degrees C, whereas dynamic strain ageing occurs at intermediate temperatures and below 5 s(-1). At room temperatures and strain rates of less than 0.05 s(-1), martensite formation is observed. To avoid the above microstructural instabilities warm working should be carried out at strain rates greater than 10 s(-1) in the temperature range 400-600 degrees C and cold working could be done in the range of about 0.05-0.8 s(-1). The continuum criterion developed on the basis of the principles of maximum rate of entropy production and separability of the dissipation function, predicts accurately all of the above instability features. (C) 1997 Elsevier Science S.A.
Resumo:
Interaction of Bacillus polymyxa with calcite, hematite, corundum and quartz resulted in significant surface chemical changes not only of the cells but also in the minerals. Both the cell surfaces as well as quartz particles were rendered more hydrophobic after mutual interaction, whilst the rest of the minerals exhibited enhanced hydrophilicity after interaction with the bacteria. The bacteria were also observed to be capable of dissolving calcite, hematite and corundum and biosorbing the dissolved metal ions to varying extents. An excess of polysaccharides could be observed on biotreated calcite, hematite and corundum while the predominance of a protein-based metabolic product was evident on quartz surfaces. The utility of bioprocessing in the beneficiation of the above minerals through bioflotation and bioflocculation is demonstrated. (C) 1997 Elsevier Science Ltd.
Resumo:
A pseudo 2-D mathematical model has been developed to simulate a cupola with one row and two rows of tuyere. The simulation results predicted higher spout temperature and combustion ratio for cupola with two rows of tuyere compared to that with one row. Further, the model has been used to study the effect of the distance of separation between the two rows of tuyere on cupola performance. The computed results shows that the spout temperature increases with tuyere level separation and attains the maximum at an optimum distance of separation between two rows of tuyere. Above the optimum, the spout temperature starts decreasing. The exit gas temperature and combustion ratio increases monotonously with the increase in tuyere level separation. These results agree well with the reported experimental observations. The mechanism behind the improved cupola performance with two rows of tuyere has been deduced from the computed temperature and composition profiles inside the cupola.
Resumo:
Phase relations in the system Ca-Pb-O at 1100 K have been determined by equilibrating 18 compositions in the ternary and identifying the phases present in quenched samples by X-ray diffraction and energy dispersive X-ray analysis (EDX). Only one ternary compound Ca2PbO4 was found to be present. The compound coexists with CaO and PbO. The intermetallic compounds Ca2Pb, Ca5Pb3 and CaPb and liquid alloys are in equilibrium with CaO. The standard Gibbs energies of formation of Ca2PbO4 (880 - 1100 K) and Pb3O4 (770 - 910 K) were determined using solid-state cells based on yttria-stabilized zirconia as the solid electrolyte. Pure oxygen gas at 0.1 MPa was used as the reference electrode. For measurements on Ca2PbO4, a novel cell design with three electrodes in series, separated by solid electrolyte membranes, was used to avoid polarization of the electrode containing three solid phases. Two three-phase electrodes were used. The first absorbs the electrochemical flux of oxygen from the reference electrode to the measuring electrode. The other three-phase electrode, which is unaffected by the oxygen flux through the solid electrolyte, is used for electromotive force (EMF) measurement. The results from EMF studies were cross-checked using thermogravimetry (TG) under controlled oxygen partial pressures. The stability of Pb3O4 was investigated using a conventional solid-state cell with RuO2 electrodes. The results can be summarized by the following equations: 2CaO + PbO +1/2O(2) --> Ca2PbO4 Delta(r)G degrees/J mol(-1) = (- 128340 + 93.21 T/K) +/- 200 3PbO + 1/2O(2) --> Pb3O4 Delta(r)G degrees/J mol(-1) = (- 70060 + 77.5 T/K) +/- 150
Resumo:
Distribution of particle reinforcements in cast composites is determined by the morphology of the solidification front. Interestingly, during solidification, the morphology of the interface is intrinsically affected by the presence of dispersed reinforcements. Thus the dispersoid distribution and length scale of matrix microstructure is a result of the interplay between these two. A proper combination of material and process parameters can be used to obtain composites with tailored microstructures. This requires the generation of a broad data base and optimization of the complete solidification process. The length scale of soldification microtructure has a large influence on the mechanical properties of the composites. This presentation addresses the concept of a particle distribution map which can help in predicting particle distribution under different solidification conditions Future research directions have also been indicated.
Resumo:
This paper deals with the development of a new model for the cooling process on the runout table of hot strip mills, The suitability of different numerical methods for the solution of the proposed model equation from the point of view of accuracy and computation time are studied, Parallel solutions for the model equation are proposed.
Resumo:
Rapid solidification of a ternary Al-Cu-Zr alloy results in a nanocomposite microstructure. In this study, melt spinning a Al82Cu15Zr3 alloy has resulted in the combined occurrence of, (a) 0.5 mu m sized grains of Al solid solution and (b) fine grains (10-20 nm) of intermetallic Al2Cu (theta) and alpha-Al, along side each other. The larger alpha-Al grains contain nanometric GP zones, with the Zr addition resulting in a grain refinement. In the other type of microstructure Zr promotes simultaneous nucleation of nanosized grains of the two equilibrium phases, Al2Cu and alpha-Al. Both these lead to a very high hardness of similar to 540 VHN for this alloy and can be used as a candidate for a high strength alloy with good ductility at a low strain rate.
Resumo:
Constant-stress tensile creep experiments on a superplastic 3-mol%-yttria-stabilized tetragonal zirconia composite with 20 wt% alumina revealed that cavities nucleate relatively early during tensile deformation. The number of cavities nucleated increases with increasing imposed stress. The cavities nucleate at triple points associated largely with an alumina grain, and then grow rapidly in a cracklike manner to attain dimensions on the order of the grain facet size. It is suggested that coarser-grained superplastic ceramics exhibit lower ductility due to the ease in formation of such grain boundary facet-cracks and their interlinkage to form a macroscopic crack of critical dimensions.
Resumo:
Limestone rejects from Bagalkot mines have been beneficiated by froth flotation with a view to reducing the magnesia content. In order to ascertain the effect of the main parameters such as sodium oleate concentration, sodium silicate concentration and pH on the MgO content, statistically designed experiments have been performed. The results indicate that under the optimum conditions arrived at limestone rejects could be beneficiated to produce a concentrate with magnesia. content meeting the specifications for cement manufacture.
Resumo:
Devitrification of spray pyrolysed, amorphous ZrO2-Al2O3 solid solution produces nanocrystalline microstructures (grain sizes 10-20 nm). In this study, spray pyrolysed amorphous ZrO2-40 mol% Al2O3 powder displayed good sinterability during decomposition, after spraying, of the nitrate precursors up to 1023K. Hot pressing of fully pyrolysed, pre-sintered (more than 70% dense) pellets at 923K and 750 MPa produced an amorphous pellet with less than 2% porosity. The results indicate the possibility of producing dense, amorphous pellets that can be heat treated further to produce nanocrystalline microstructures conducive for superplasticity.
Resumo:
Plate-shaped products resulting from martensitic, diffusional, and mixed mode transformations in zirconium-base alloys are compared. in the present study. These alloys are particularly suitable for the comparison in view of the fact that the lattice correspondence between the parent beta (bcc) and the product alpha (hcp) or gamma-hydride (fct) phases are remarkably similar for different types of transformations. Crystallographic features such as orientation relations, habit planes, and interface structures associated with these transformations have been compared:, with a view toward examining whether the transformation mechanisms have characteristic imprints on these experimental observables. Martensites exhibiting dislocated lath, internally twinned plate, and self-accommodating three-plate cluster morphologies have been encountered in Zr-2.5Nb alloy. Habit planes corresponding to all these morphologies have been found to be consistent with the predictions based on the invariant plane strain (IFS) criterion. Different morphologies have been found to reflect the manner in which the neighboring martensite variants are assembled. Lattice-invariant shears (LISs) for all these cases have been identified to be either {10 (1) over bar 1}(alpha) ((1) over bar 123)(alpha) slip or twinning on (10 (1) over bar 1)(alpha) planes. Widmanstatten alpha precipitates, forming in a step-quenching treatment, have been shown to have a lath morphology, the alpha/beta interface being decorated with a periodic array of (c + a) dislocations at a spacing of 8 to 10 nm. The line vectors of these dislocations are nearly parallel to the invariant lines. The alpha precipitates, forming in the retained beta phase on aging, exhibit an internally twinned structure with a zigzag habit plane. Average habit planes for the morphologies have been found to lie near the {103}(beta) - {113}(beta) poles, which are close to the specific variant of the {112}(beta) plane, which transforms into a prismatic plane of the type {1 (1) over bar 00}(alpha). The crystallography of the formation of the gamma-hydride phase (fct) from both the alpha and beta phases is seen to match the IFS predictions. While the beta-gamma transformation can be treated approximately as a simple shear on the basal plane involving a change in the stacking sequence, the alpha-gamma transformation call be conceptually broken into a alpha --> beta transformation following the Burgers correspondence and the simple beta-gamma shear process. The active eutectoid decomposition in the Zr-Cu system, beta --> alpha + beta', has been described in terms of cooperative growth of the alpha phase from the beta phase through the Burgers correspondence and of the partially ordered beta' (structurally similar to the equilibrium Zr2Cu phase) through an ordering process. Similarities and differences in crystallographic features of these transformations have been discussed. and the importance of the invariant line vector in deciding the geometry of the corresponding habit planes has been pointed out.