Resumo:

The hot deformation behavior of α brass with varying zinc contents in the range 3%–30% was characterized using hot compression testing in the temperature range 600–900 °C and strain rate range 0.001–100 s−1. On the basis of the flow stress data, processing maps showing the variation of the efficiency of power dissipation (given by Image where m is the strain rate sensitivity) with temperature and strain rate were obtained. α brass exhibits a domain of dynamic recrystallization (DRX) at temperatures greater than 0.85Tm and at strain rates lower than 1 s−1. The maximum efficiency of power dissipation increases with increasing zinc content and is in the range 33%–53%. The DRX domain shifts to lower strain rates for higher zinc contents and the strain rate for peak efficiency is in the range 0.0001–0.05 s−1. The results indicate that the DRX in α brass is controlled by the rate of interface formation (nucleation) which depends on the diffusion-controlled process of thermal recovery by climb.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The electrical properties of Co1−xZnxFe2O4 (x=0–1) spinel ferrites were investigated by impedance spectroscopy. The grain‐boundary resistance was found to increase as a function of composition up to x=0.6, and decreases beyond x=0.6. The variation in the bulk resistance and the activation energy as a function of composition is found to exhibit a similar trend whereas the grain resistance appears to be an independent parameter. The observed results suggest that the bulk properties of solid solution spinel ferrites are primarily controlled by the grain‐boundary phase.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

he solvation of (2,3,7,8,12,13,17,18-octabromo-5,10,15,20-tetraphenylporphyrinato)zinc(II)[Zn(obtpp)], in twelve different solvents results in large red shifts of the B and Q bands of the porphyrin accompanied by enhanced absorbance ratios of the Q bands. These observations are ascribed to the destabilisation of the highest occupied molecular orbital a2u of the porphyrin arising from a flow of charge from the axial ligand to the porphyrin ring through the zinc(II) ion. The binding constants of adducts of [Zn(obtpp)] with neutral bases have been found to be an order of magnitude greater than those observed for the corresponding adducts of (5,10,15,20-tetraphenylporphyrinato)-zinc and vary in the order piperidine > imidazole > pyridine > 3-methylpyridine > pyridine-3-carbaldehyde. The enhanced binding constants and large spectral shifts are interpreted in terms of the electrophilicity of [Zn(obtpp)] induced by the electron-withdrawing bromine substituents in the porphyrin core. The structure of [Zn(obtpp)(PrCN)2] has been determined; it reveals six-co-ordinated zinc(II) with two long Zn–N distance [2.51(4), 2.59(3)Å]. The porphyrin is non-planar and displays a saddle-shaped conformation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We demonstrate that the structural and optical properties of a sol-gel deposited zinc oxide thin film can be tuned by varying the composition of the sol, consisting of ethylene glycol and glycerol. A systematic study of the effect of the composition of sol on the mean grain size, thickness, and defect density of the zinc oxide film is presented. About 20% glycerol content in the sol is observed to improve the quality of the film, as evaluated by X-ray diffraction and photoluminescence studies. Thus, optimizing the composition of the sol for about 60 nm thick ZnO film using 20% glycerol resulted in the zinc oxide film that is about 80% transparent in visible spectrum, exhibiting electrical resistivity of about 18 Omega cm and field-effect mobility of 0.78 cm(2)/(V s). (C) 2010 The Electrochemical Society. DOI: 10.1149/1.3515894] All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Zinc forms two types of complexes with o-vanillin salicyloylhydrazone. The H-1 and C-13 nmr studies suggest that it coordinates with azomethine nitrogen, the carbonyl oxygen and with one or both of the phenolic oxygens. The H-1-H-1 and H-1 decoupled C-13-C-13 two-dimensional nuclear Overhauser and exchange spectra show that there is an exchange between the two types of complexes.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The compounds Zn(C12H8N2)](2)C12N2H8(COO)(2)](2)center dot(C6H12O)center dot(H2O), I, Zn(C12H8N2)]C12N2H8(COO)(2)], II, Cd(C12H8N2)(H2O)]C12N2H8(COO)(2)]center dot(H2O), III, Zn(C10N2H8)]C12N2H8(COO)(2)]center dot 0.5(C10N2H8), IV, Cd(C12N2H8(COO)(2)center dot H2O], V, and Zn-3(mu(2)-O)(mu(3)-O)(3)]C12N2H8(COO)(2)], VI, have been synthesized by using a biphasic approach (I, III, V, VI) or regular hydrothermal method (II, IV). The compounds exhibit one (I and II), two (In), and three dimensionally (IV, V, VI) extended structures. The flexible azodibenzoate ligand gives rise to a 3-fold interpenetration (IV) when the synthesis was carried out using normal hydrothermal methods. The biphasic approach forms structures without any interpenetrations, especially in the three-dimensional structures of V and VI. Formation of Cd2O2 dimers in V and extended M-O(H)-M two-dimensional layers in VI suggests the subtle structural control achieved by the biphasic method. Transformation studies indicate that it is possible to transform I to II. Lewis acid catalytic studies have been performed to evaluate the role of the coordination environment in such reactions. All the compounds have been characterized by a variety of techniques that includes powder X-ray diffraction, infrared, thermogravitric analysis, UV-vis, photoluminescence studies.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Spermatidal transition protein, TP2, was purified from rat testes by Hg-affinity chromatography. The present study reports the details of the zinc-metalloprotein nature of TP2 by employing the Zn-65-blotting technique. Chemical modification of cysteine by iodoacetic acid, and histidine by diethylpyrocarbonate, resulted in a near complete inhibition of Zn-65-binding to TP2. The (65)Zinc-binding was localized to the V8 protease-derived N-terminal two-third polypeptide fragment. Circular dichroism spectroscopy studies of TP2 (zinc pre-incubated) and its V8 protease-derived polypeptide fragments revealed that the N-terminal fragment has a Type I-beta-turn spectrum, while the C-terminal fragment has a small but significant alpha-helical structure. EDTA altered the circular dichroism spectrum of TP2 and the N-terminal fragment (zinc binding domain) but not that of the C-terminal fragment.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The absorption spectrum in the visible range and the, ESR spectrum of vanadyl sulfate were lost on addition of diperoxovanadate. The V-51-NMR spectra revealed that diperoxovanadate was reduced to vanadate and its oligomers. With excess vanadyl, tetrameric vanadate was found to be the major product, During this reaction oxygen was released into the medium. The oxygen-release reaction was inhibited by a variety of organic ligands-imidazole, benzoate, formate, mannitol, ethanol, Tris, DMPO, malate, and asparagine. An oxygen-consuming reaction emerged at high concentrations of some of these compounds, e.g. benzoate and ethanol. Using DMPO as the spin-trap, an oxygen-radical species with a 1:2:2:1 type of ESR spectrum was detected in the reaction mixtures resulting from vanadyl oxidation by diperoxovanadate which was unaffected by addition of catalase or ethanol. The results showed that secondary oxygen-exchange reactions occur which depend on and utilize the intermediates in the primary reaction during diperoxovanadate-dependent oxidation of vanadyl sulfate.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Photoinduced electron transfer (ET) reactions in the zinc porphyrin-crown ether (ZnPCE) supramolecule, in which one crown ether moiety containing Eu3+ as electron acceptor is covalently linked to zinc porphyrin (ZnP), were studied by flash photolysis. In methanol solutions, highly efficient charge separation occurs via intramolecular ET from (ZnP)-Zn-3 to Eu3+ encapsulated in the crown ether void (k(1) = (3 +/- 1) X 10(3) s(-1)) and intramolecular ET from 3ZnP to uncomplexed Eu2+ (k(2) = (2.5 +/- 0.5) X 10(3) s(-1)). Intermolecular ET from Eu2+ escaped from the crown ether void to ZnP.+ (k(tau) = (4.3 +/- 0.7) X 10(8) M(-1) s(-1)) seems to be the main pathway of charge recombination.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Layered lanthanide sulfate compounds with three different structures have been prepared and characterized. The compounds C10H10N2] La(SO4)(2)]center dot 2H(2)O (I), C10H10N2] La(SO4)(2)(H2O)(2)](2) (Ha), C10H10N2]Pr(SO4)(2)(H2O)(2)](2) (IIb), C10H10N2]Nd-2(SO4)(4)(H2O)(2)](2) (IIIa), C10H10N2]Sm-2(SO4)(4)(H2O)(2)](2) (IIIb), and C10H10N2]Eu-2(SO4)(4)(H2O)(2)] 2 (IIIC) have anionic lanthanide sulfate layers separated by protonated bipyridine molecules. The layers are formed by the connectivity between the lanthanide polyhedra and sulfate tetrahedra. The formation of a two-dimensional La-O-La layer (la), Pr-O-Pr chains (IIb), and a tetramer cluster (IIIa) is noteworthy. The compounds exhibit honeycomb (I), square (IIa, IIb), and honeycomb (IIIa-IIIc) net arrangements, when the connectivity between the lanthanide ions is considered. Optical studies indicate the observation of characteristic metal-centered emission at room temperature. The Nd compound (IIIa) exhibits a two-photon upconversion behavior.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nonliving waste biomass consisting of Aspergillus niger attached to wheat bran was used as a biosorbent for the removal of copper and zinc from aqueous solutions. Copper and zinc uptake by the biomass obeyed Langmuir isotherms. The binding capacity of the biomass for copper was found to be higher than that for zinc. The metal uptake, expressed in milligrams per gram of biomass, was found to be a function of: the initial metal concentration (with the uptake decreasing with increasing initial concentration), the biomass loading (with the uptake decreasing with increasing biomass loading) and pH (with the uptake increasing with increasing pH in the range of 1.5 and 6.0). The metal uptake was significantly affected in the presence of a co-ion. The uptake of copper by the biomass decreased in the presence of zinc and vice versa. The decrease in metal uptake was dependent on the concentrations of metals in the two-component aqueous solutions. The effect of copper on zinc uptake was more pronounced than the effect of zinc on copper uptake.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Studies have been carried out in glasses containing Fe2O3, V2O5, and Fe2O3 + V2O5. Mossbauer studies in the ZnO-B2O3-Fe2O3 system show that iron is present as Fe3+ with tetrahedral coordination and that the isomer shift and the quadrupole splitting decrease with increase of Fe2O3 Content; similarly, the isomer shift and quadrupole splitting are also found to decrease with increasing ZnO. On the other hand, in the Na2O-ZnO-B2O3-Fe2O3 system, the isomer shift increases with Na2O or ZnO while the quadrupole splitting is fairly insensitive. Electron paramagnetic resonance in the ZnO-B2O3-Fe2O3 system shows signals at g = 4.20 and 2.0, whose intensity and linewidth show strong dependence on Fe2O3 content. In the ZnO-B2O3-V2O5 system, electron paramagnetic resonance shows that vanadium is present as the vanadyl complex, and the hyperfine coupling constants, A(parallel-to) and A(perpendicular-to) decrease with increasing V2O5 content; on the other hand, g(parallel-to) decreases and g(perpendicular-to) increases slightly, indicating an increase in tetragonal distortion. Zinc borate glasses containing Fe2O3 + V2O5 do not show the hyperfine structure of V4+ due to the interaction between Fe3+ and V4+

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report a reversible phase transformation of platelet-shaped ZnS nanostructures between wurtzite (WZ) and zinc blende (ZB) phases by reversible insertion/ ejection of dopant Mn(II) ions induced by a thermocyclic process. In a reaction flask loaded with WZ ZnS platelets and Mn molecular precursors, during heating Mn ions are incorporated and change the phase of the host nanostructures to ZB; during cooling Mn ions are spontaneously ejected, returning the host nanoplatelets to the original WZ phase. These reversible changes are monitored for several cycles with PL, EPR, XRD, and HRTEM. Interestingly, the (0001) WZ platelets transform to (110) ZB following a nucleation and growth process triggered by a local increase/depletion of the Mn2+ concentration in the nanocrystals.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report a reversible phase transformation of platelet-shaped ZnS nanostructures between wurtzite (WZ) and zinc blende (ZB) phases by reversible insertion/ ejection of dopant Mn(II) ions induced by a thermocyclic process. In a reaction flask loaded with WZ ZnS platelets and Mn molecular precursors, during heating Mn ions are incorporated and change the phase of the host nanostructures to ZB; during cooling Mn ions are spontaneously ejected, returning the host nanoplatelets to the original WZ phase. These reversible changes are monitored for several cycles with PL, EPR, XRD, and HRTEM. Interestingly, the (0001) WZ platelets transform to (110) ZB following a nucleation and growth process triggered by a local increase/depletion of the Mn2+ concentration in the nanocrystals.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fluorescent zinc complexes have recently attracted a lot of interest owing to their vast applications in cellular imaging. We report the synthesis as well as physical, chemical and biological studies of a novel zinc glyoxalbis(4-methyl-4-phenyl-3-thiosemicarbazone), Zn (GTSC)](3), complex. As compared with the well-studied zinc biacetylbis(4-methyl-3-thiosemicarbazone), Zn(ATSM), complex, which was used as a reference, Zn(GTSC)](3) had 2.5-fold higher fluorescence. When cellular fluorescence was measured using flow cytometry, we observed that Zn(GTSC)](3) had 3.4-fold to 12-fold higher fluorescence than Zn(ATSM) in various cell lines (n = 9) of different tissue origin. Confocal fluorescence microscopy results showed that Zn(GTSC)](3) appeared to have a nuclear localization within 30 mm of addition to MCF7 cells. Moreover, Zn(GTSC)](3) showed minimal cytotoxicity compared with Zn(ATSM), suggesting that Zn(GTSC)](3) may be less deleterious to cells when used as an imaging agent. Our data suggest that the novel Zn(GTSC)](3) complex can potentially serve as a biocompatible fluorescent imaging agent for live cells.