173 resultados para butyl radicals
Resumo:
Oxovanadium(IV) complexes [VO(L)(B)]Cl-2 (1-3), where L is bis(2-benzimidazolylmethyl)amine and B is 1,10-phenanthroline(phen),dipyrido[3,2-d:2',3'-f]quinoxaline(dpq) or dipyrido[3,2-a:2',3'-c]phenazine (dppz), have been prepared, characterized, and their photo-induced DNA and protein cleavage activity studied. The photocytotoxicity of complex 3 has been studied using adenocarcinoma A549 cells, The phen complex 1, structurally characterized by single-crystal X-ray crystallography, shows the presence of a vanadyl group in six-coordinate VON5 coordination geometry. The ligands L and phen display tridentate and bidentate N-donor chelating binding modes, respectively. The complexes exhibit a d-d band near 740 nm in 15% DMF-Tris-HCl buffer (pH 7.2). The phen and dpq complexes display an irreversible cathodic cyclic voltammetric response near -0.8 V in 20% DMF-Tris-HCl buffer having 0.1 M KCl as supporting electrolyte. The dppz complex 3 exhibits a quasi-reversible voltammogram near -0.6 V (vs SCE) that is assignable to the V(IV)-V(III)couple. The complexes bind to calf thymus DNA giving binding constant values in the range of 6.6 x 10(4)-2.9 x 10(5) M-1. The binding site size, thermal melting and viscosity binding data suggest DNA surface and/or groove binding nature of the complexes. The complexes show poor ``chemical nuclease'' activity in dark in the presence of 3-mercaptopropionic acid or hydrogen peroxide. The dpq and dppz complexes are efficient photocleavers of plasmid DNA in UV-A light of 365 nm via a mechanistic pathway that involves formation of both singlet oxygen and hydroxyl radicals. The complexes show significant photocleavage of DNA in near-IR light (>750 nm) via hydroxyl radical pathway. Among the three complexes, the dppz complex 3 shows significant BSA and lysozyme protein cleavage activity in UV-A light of 365 nm via hydroxyl radical pathway. The dppz complex 3 also exhibits photocytotoxicity in non-small cell lung carcinoma/human lung adenocarcinoma A549 cells giving IC50 value of 17 mu M in visible light(IC50 = 175 mu M in dark).
Resumo:
The 270 MHz 1H n.m.r. spectrum of benzyloxycarbonyl-Pro-N-methylamide in CDCl3 is exchange broadened at 293° K. Spectral lines due to two species are frozen out at 253° K and a dynamically averaged spectrum is obtained at 323° K. A selective broadening of the Cβ and Cγ resonances in the 13C n.m.r. spectrum is observed at 253° K, with a splitting of the Cβ and Cγ resonances into a pair of lines of unequal intensity. A similar broadening of Cβ and Cγ peaks is also detected in pivaloyl-Pro-N-methylamide where cis-trans interconversion about the imide bond is precluded by the bulky t-butyl group. The rate process is thus attributed to rotation about the Cα-CO bond (ψ) and a barrier (ΔG#) of 14kcal mol-1 is estimated. 13C n.m.r. data for pivaloyl-Pro-N-methylamide in a number of solvents is presented and the differences in the Cβ and Cγ chemical shifts are interpreted in terms of rotational isomerism about the Cα-CO bond.
Resumo:
Gabapentin, a widely used antiepileptic drug, crystallizes in multiple polymorphic forms. A new crystal form of gabapentin monohydrate in the space group Pbca is reported and the packing arrangement compared with that of a previously reported polymorph in the space group P2(1)/c [Ibers, J.A. (2001) Acta Crystallogr; C57:641]. Gabapentin polymorphs can also occur from a selection of one of the two distinct chair forms of the 1,1-disubstituted cyclohexane. Crystal structures of the E and Z isomers of 4-tert-butylgabapentin provide models for analyzing anticipated packing modes in the conformational isomers of gabapentin. The E isomer crystallized in the space group Pca2(1), while the Z isomer crystallized in the space group P2(1)/c. The crystal structure of E-4-tert-butylgabapentin provides the only example of a structure in a non-centrosymmetric space group. Crystal structures of the hydrochloride and hydrobromide salts of 4-tert-butyl derivatives are reported. The results suggest that for gabapentin, a large 'polymorph-space' may be anticipated, in view of the multiple conformational states that are accessible to the molecule.
Resumo:
The photolytic and photocatalytic degradation of the copolymers poly(methyl methacrylate-co-butyl methacrylate) (MMA–BMA), poly(methyl methacrylate-co-ethyl acrylate) (MMA–EA) and poly(methyl methacrylate-co-methacrylic acid) (MMA–MAA) have been carried out in solution in the presence of solution combustion synthesized TiO2 (CS TiO2) and commercial Degussa P-25 TiO2 (DP 25). The degradation rates of the copolymers were compared with the respective homopolymers. The copolymers and the homopolymers degraded randomly along the chain. The degradation rate was determined using continuous distribution kinetics. For all the polymers, CS TiO2 exhibited superior photo-activity compared to the uncatalysed and DP 25 systems, owing to its high surface hydroxyl content and high specific surface area. The time evolution of the hydroxyl and hydroperoxide stretching vibration in the Fourier transform-infrared (FT-IR) spectra of the copolymers indicated that the degradation rate follows the order MMA–MAA > MMA–EA > MMA–BMA. The same order is observed for the rate coefficients of photocatalytic degradation. The photodegradation rate coefficients were compared with the activation energy of pyrolytic degradation. In degradation by pyrolysis, it was observed that MMA–BMA was the least stable followed by MMA–EA and MMA–MAA. The observed contrast in the order of thermal stability compared to the photo-stability of these copolymers was attributed to the two different mechanisms governing the scission of the polymer and the evolution of the products.
Resumo:
We report the quadratic nonlinearity of one- and two-electron oxidation products of the first series of transition metal complexes of meso-tetraphenylporphyrin (TPP). Among many MTPP complexes, only CuTPP and ZnTPP show reversible oxidation/reduction cycles as seen from cyclic voltammetry experiments. While centrosymmetric neutral metalloporphyrins have zero first hyperpolarizability, β, as expected, the cation radicals and dications of CuTPP and ZnTPP have very high β values. The one- and two-electron oxidation of the MTPPs leads to symmetry-breaking of the metal−porphyrin core, resulting in a large β value that is perhaps aided in part by contributions from the two-photon resonance enhancement. The calculated static first hyperpolarizabilities, β0, which are evaluated in the framework of density functional theory by a coupled perturbed Hartree−Fock method, support the experimental trend. The switching of optical nonlinearity has been achieved between the neutral and the one-electron oxidation products but not between the one- and the two-electron oxidation products since dications that are electrochemically reversible are unstable due to the formation of stable isoporphyrins in the presence of nucleophiles such as halides.
Resumo:
The transesterification of methyl butyrate, ethyl butyrate and butyl butyrate to geranyl butyrate was investigated in supercritical carbon dioxide. The effect of chain length of the butyrate on the rate of transesterification was investigated. The initial rates followed the trend: ethyl butyrate < butyl butyrate < methyl butyrate. The transesterification of butyl butyrate to geranyl butyrate in various supercritical fluids such as ethylene, methane, ethane was also examined. The initial rate of transesterification of butyl butyrate in different supercritical fluids followed the order: ScCO2 < ScC2H6 < ScC2H4 < ScCH4. The highest initial rate was obtained in supercritical methane and the reasons for this observation were proposed. The Ping-Pong Bi-Bi model with inhibition by both acid and alcohol was used to model the experimental data and determine the kinetics of the reaction. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Metribuzin, 4-amino-6-tert-butyl-3-methylthio- 1,2,4-triazin-5-one, exhibits polymorphic behaviour, crystallizing as plates and needles, driven by variation in solvent polarity, a delicate balance of weak intermolecular forces generating different molecular assemblies.
Resumo:
Two crystals structures of a nonapeptide (anhydrous and hydrated) containing the amino acid residue alpha, alpha-di-n-butylglycyl, reveal a mixed 3(10)/alpha-helical conformation. Residues 1-7 adopt phi, psi values in the helical region, with Val(8) being appreciably distorted. The Dbg residue has phi, psi values of -40, -37 degrees and -46, -40 degrees in two crystals with the two butyl side chains mostly extended in each. Peptide molecules in the crystals pack into helical columns. The crystal parameters are C50H91N9O12, space group P2(1), with a = 9.789(1) Angstrom, b = 20.240(2) Angstrom, c = 15.998(3) Angstrom, beta = 103.27(1); Z = 2, R = 10.3% for 1945 data observed >3 sigma(F) and C50H91N9O12. 3H(2)O, space group P2(1), with a = 9.747(3) Angstrom, b = 21.002(8) Angstrom, c = 15.885(6) Angstrom, beta = 102.22(3)degrees, Z = 2, R = 13.6% for 2535 data observed >3 sigma(F). The observation of a helical conformation at Dbg suggests that the higher homologs in the alpha, alpha-dialkylated glycine series also have a tendency to stabilize peptide helices. (C) Munksgaard 1996.
Resumo:
Chitosan grafted poly(alkyl methacrylate)s (namely chitosan grafted poly(methyl methacrylate) (ChgPMMA), chitosan grafted poly(ethyl methacrylate)(ChgPEMA), chitosan grafted poly(butyl methacrylate) (ChgPBMA) and chitosan grafted poly(hexyl methacrylate) (ChgPHMA)) were synthesized and characterized by using FT-IR and C-13 NMR techniques. The adsorption batch experiments on these grafted copolymers were conducted by using an anionic sulfonated dye. Orange-G. A pseudo-second-order kinetic model was used to determine the kinetics of adsorption. The effect of grafting, effect of process variables and the effect of different sulfonated anionic dyes (Orange-C, Congo Red, Remazol Brill Blue R and Methyl Blue) on the adsorption kinetics was determined. The Langmuir and Freundlich models were used to fit the adsorption isotherms and from the values of correlation coefficients (R-2), it was observed that the experimental data fits very well to the Langmuir model. The values of the maximum adsorption capacity of the adsorbents follow the order: ChgPMMA > ChgPEMA > ChgPBMA > ChgPHMA > chitosan. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Dinuclear ((VVV)-V-IV) oxophenoxovanadates of general formula [V2O3L] have been synthesized in excellent yields by reacting bis(acetylacetonato)oxovanadium(IV) with H3L in a 2:1 ratio in acetone under an N-2 atmosphere. Here L3- is the deprotonated form of 2,6-bis[{{(2-hydroxybenzyl)(N',N'-(dimethylamino)ethyl)}amino}methyl]-4-methylphenol (H3L1), 2,6-bis[{{(5-methyl-2-hydroxybenzyl)(N',N'-(dimethylamino)ethyl)}amino}methyl]-4-methylphenol (H3L2) 2,6-bis[ {{(5-tert-butyl-2-hydroxybenzyl)(N',N'-(dimethylamino)ethyl)}amino}methyl]-4-methylphenoI (H3L3), 2,6-bis[{{(5-chloro-2-hydroxybenzyl)(N',N'-(dimethylamino)ethyl)}amino}methyl]-4-methylphenol (H3L4) , 2,6-bis[{{(5-bromo-2-hydroxybenzyl)(N',N'-(dimethylamino)ethyl)}amino}methyl]-4-methylphenol (H3L5), or 2,6-bis[{{(5-methoxy-2-hydroxybenzyl)(N',N'-(dimethylamino)ethyl)}amino}methyl]-4-methylphenol (H3L6). In [V2O3L1], both the metal atoms have distorted octahedral geometry. The relative disposition of two terminal V=O groups in the complex is essentially cis. The O=V...V=O torsion angle is 24.6(2)degrees. The V-O-oxo-V and V-O-phenoxo-V angles are 117.5(4) and 93.4(3)degrees, respectively. The V...V bond distance is 3.173(5) Angstrom. X-ray crystallography, IR, UV-vis, and H-1 and V-51 NMR measurements show that the mixed-valence complexes contain two indistinguishable vanadium atoms (type 111). The thermal ellipsoids of O2, O4, C10, C14, and C15 also suggests a type III complex in the solid state. EPR spectra of solid complexes at 77 K display a single line indicating the localization of the odd electron (3d(xy)(1)). Valence localization at 77 K is also consistent with the V-51 hyperfine structure of the axial EPR spectra (3d(xy)(1) ground state) of the complexes in frozen (77 K) dichloromethane solution: S = 1/2, g(parallel to) similar to 1.94, g(perpendicular to) similar to 1.98, A(parallel to) similar to 166 x 10(-4) cm(-1), and A(perpendicular to) similar to 68 x 10(-4) cm(-1). In contrast isotropic room-temperature solution spectra of the family have 15 hyperfine lines (g(iso) similar to 1.974 and A(iso) similar to 50 x 10(-4) cm(-1)) revealing that the unpaired electron is delocalized between the metal centers. Crystal data for the [V2O3L1].CH2Cl2 complex are as follows: chemical formula, C32H43O6N4C12V2; crystal system, monoclinic; space group, C2/c; a = 18.461(4), b = 17.230(3), c = 13.700(3) Angstrom; beta = 117.88(3)degrees; Z = 8.
Resumo:
Formation of oxygen radicals during reduction of H2O2 or diperoxovanadate with vanadyl sulfate or ferrous sulfate was indicated by the 1:2:2:1 electron spin resonance (ESR) signals of the DMPO adduct typical of standard radical dotOH radical. Signals derived from diperoxovanadate remained unchanged in the presence of ethanol in contrast to those from H2O2. This gave the clue that they represent a different radical, possibly radical dotOV(O2)2+, formed on breaking a peroxo-bridge of diperoxovanadate complex. The above reaction mixtures evolved dioxygen or, when NADH was present, oxidized it rapidly which was accompanied by consumption of dioxygen. Operation of a cycle of peroxovanadates including this new radical is suggested to explain these redox activities both with vanadyl and ferrous sulfates. It can be triggered by ferrous ions released from cellular stores in the presence of catalytic amounts of peroxovanadates.
Resumo:
Pseudo-acid chlorides of five 4′-substituted o-benzoylbenzoic acids are converted into a mixture of dilactones with sodium iodide in acetone. The meso-isomer is always formed to a larger extent than the (±)-mixture. These results imply that the radicals involved are not planar.
Resumo:
The ultrasonic degradation of poly (styrene-co-methyl methacrylate) (SMMA), poly (styrene-co-ethyl methacrylate) (SEMA) and poly (styrene-co-butyl methacrylate) (SBMA) copolymers of different compositions was studied. The copolymers were synthesized and NMR spectroscopy was used to determine the composition, and the glass transition temperatures were determined by DSC. The reactivity ratios were determined by the Kelen-Tudos method and it indicated that the copolymers were random. The effect of solvent, temperature and copolymer composition on the ultrasonic degradation rate of these copolymers was investigated. A model based on continuous distribution kinetics was employed to study the degradation kinetics. The degradation rate coefficients of the copolymers decreased with an increase in the styrene content in the copolymer. At any particular copolymer composition the rate of degradation follows the order: SBMA >SEMA > SMMA. Thermogravimetric analysis (TGA) of the copolymers was carried in order to assess their thermal stability. The same order of degradation was observed for the thermal degradation of the copolymers as that observed for ultrasonic degradation. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
The kinetics of dimerization of 4-substituted- and unsubstituted o-benzoylbenzoyl chlorides, with iodide ion can be described by the expression, rate =k2[acid chloride][iodide]. The value for the reaction in dimethylformamide solution is –0·38. The entropy of activation for the reaction is –34·2 cal mol–1 K–1 and the activation energy is 10·7 kcal mol–1. These results have been interpreted as evidence for the formation of pseudo-iodide in the rate-determining step and its fast decomposition to radicals which combine to give a mixture of stereoisomeric dilactones.
Resumo:
Durability is central to the commercialization of polymer electrolyte fuel cells (PEFCs). The incorporation of TiO2 with platinum (Pt) ameliorates both the stability and catalytic activity of cathodes in relation to pristine Pt cathodes currently being used in PEFCs. PEFC cathodes comprising carbon-supported Pt-TiO2 (Pt-TiO2/C) exhibit higher durability in relation to Pt/C cathodes as evidenced by cell polarization, impedance, and cyclic voltammetry data. The degradation in performance of the Pt-TiO2/C cathodes is 10% after 5000 test cycles as against 28% for Pt/C cathodes. These data are in conformity with the electrochemical surface area and impedance values. Pt-TiO2/C cathodes can withstand even 10,000 test cycles with nominal effect on their performance. X-ray diffraction, transmission electron microscope, and cross-sectional field-emission-scanning electron microscope studies on the catalytic electrodes reflect that incorporating TiO2 with Pt helps in mitigating the aggregation of Pt particles and protects the Nafion membrane against peroxide radicals formed during the cathodic reduction of oxygen. (C) 2010 The Electrochemical Society. [DOI: 10.1149/1.3421970] All rights reserved.