238 resultados para Immersion calorimetry
Resumo:
Glaiis transitions of As-Se glasses have been investigated over a wide range of compositions by using differential scanning calorimetry. The variation of Tg with composition has been interpreted on the basis of a bond-lattice model.
Resumo:
Transparent SrBi2B2O7 glasses were prepared via melt-quenching technique and characterized using differential scanning calorimetry and x-ray powder diffraction. The ac conductivities of the glasses were studied as a function of frequency (100 Hz-10 MHz) at different temperatures. The frequency dependence of conductivity has been analyzed using Almond-West expression. The exponent n was nearly unaffected by temperature. Impedance and modulus spectroscopies were employed to further examine the electrical data. Dielectric relaxation exhibited a stretched exponential behavior with a stretching exponent beta independent of temperature. From conductivity analysis we have proposed that the charge transport occurs through the participation of nonbridging oxygen (NBO), which switches positions in a facile manner. The stretched exponential behavior appears to be a direct consequence of the NBO switching mechanism of charge transport.
Resumo:
In this research fabrication of crystalline PbZrO3 (PZ) nanoparticles and their phase transformation behavior is investigated. A novel sol-gel method was used for the synthesis of air-stable and precipitate-free diol-based sol of PZ, which was dried at 150 degrees C and then calcined at 300-700 degrees C for 1 h. The morphology, crystallinity and phase formation of as synthesized nanoparticles were studied by the selected-area electron diffraction (SAED), X-ray diffraction (XRD), thermal gravimetric analysis/differential scanning calorimetry (TGA-DSC), and high resolution transmission electron microscope (HRTEM). The XRD, SAED, and TGA-DSC analyses confirmed the tetragonal lead rich zirconia phase (t-Z phase) and monoclinic zirconia phase (m-Z phase) as the intermediate phases during the calcinations process followed by crystallization of single orthorhombic PZ phase at about 700 degrees C. The average PZ particle size was observed about 20 nm as confirmed by TEM study. Energy-dispersive X-ray spectroscopy (EDX) analysis demonstrated that stoichiometric PbZrO3 was formed.
Resumo:
Lipopolysaccharide (LPS), the major cell wall constituent of Gram-negative bacteria, evokes a multitude of biological effects in mammals including pyrogenicity and toxic shock syndrome. Polymyxin B (PmB), a polycationic cyclic peptide, is known to neutralize most of its activities. The nature of the interaction of PmB with LPS and lipid A was investigated by isothermal titration calorimetry. PmB binds to LPS as well as lipid A stoichiometrically and non-co-operatively with micromolar affinity. These interactions are driven primarily by a favourable change in entropy (delta S) and are endothermic in nature. These positive changes in enthalpies decrease with increasing temperature, yielding a heat capacity change, delta Cp, of -2385 J.mol-1.degree-1 for PmB-LPS interactions while the binding of PmB to lipid A displays a delta Cp of -2259 J.mol-1.degree-1. The negative heat capacity changes provide strong evidence for the role of hydrophobic interactions as the driving force for the association of PmB with LPS and lipid A. A correlation of the energetics of these interactions with analyses of the molecular models of PmB suggests that a cluster of solvent-exposed non-polar amino acid side-chains that line one surface of the molecule, together with a ring of positively charged residues on its other surface, are responsible for its strong and stoichiometric binding to LPS.
Resumo:
The possibility of using spin-probe electron spin resonance (ESR) as a tool to study glass transition temperature, T g, of polymer electrolytes is explored in 4 hydroxy 2,2,6,6 tetramethylpiperidine N oxyl (TEMPOL) doped composite polymer electrolyte (PEG)46LiClO4 dispersed with nanoparticles of hydrotalcite. The T g is estimated from the measured values of T 50G, the temperature at which the extrema separation 2A zz of the broad powder spectrum decreases to 50 G. In another method, the correlation time τc for the spin probe dynamics was determined by computer simulation of the ESR spectra and T g has been identified as the temperature at which τc begins to show temperature dependence. While both methods give values of T g close to those obtained from differential scanning calorimetry, it is concluded that more work is required to establish spin-probe ESR as a reliable technique for the determination of T g.
Resumo:
Transparent glasses of SrBi2B2O7 (SBBO) were fabricated via the conventional melt-quenching technique. The amorphous and the glassy nature of the as-quenched samples were, respectively, confirmed by X-ray powder diffraction (XRD) and differential scanning calorimetry (DSC). The glass transition (T (g)) and the crystallization parameters [crystallization activation energy (E (cr)) and Avrami exponent (n)] were evaluated under non-isothermal conditions using DSC. There was a close agreement between the activation energies for the crystallization process determined by Augis and Bennet and Kissinger methods. The variation of local activation energy [E (c)(x)] that was determined by Ozawa method, decreased with the fraction of crystallization (x). The Avrami exponent (n(x)) increased with the increase in fraction of crystallization (x) suggesting that there was a change over in the crystallization process from the surface to the bulk.
Resumo:
The carrier type reversal (CTR) from p- to n-type in semiconducting chalcogenide glasses is an important and a long standing problem in glass science. Ge-Se glasses exhibit CTR when the metallic elements Bi and Pb are added. For example, bulk Ge42-xSe58Pbx glasses exhibit CTR around 8-9 at. % of Pb. These glasses have been prepared by melt quenching method. Glass transition temperature (T-g), Specific heat change between the liquid and the glassy states (Delta C-p) at T-g and the nonreversing heat flow (Delta H-nr) measured by modulated differential scanning calorimetry exhibit anomalies at 9 at. % of Pb. These observed anomalies are interpreted on the basis of the nano scale phase separation occurring in these glasses.
Resumo:
The isobaric heat capacity of CaCu3Ti4O12 (CCTO) was measured from 300 to 1100 K using differential scanning calorimetry (DSC). The results were verified using drop calorimetric measurement of enthalpy increment (H-T - H-298.15) at T= 973 and 1073 K. The samples were dropped from room temperature into a calorimeter maintained at high temperature. The results show small negative deviation from Neumann-Kopp rule. The enthalpy and entropy increments are computed as a function of temperature and compared with values available in the literature. The results obtained in this study are consistent with available information on enthalpy and Gibbs energy of formation of CCTO.
Resumo:
Two new donor-acceptor type liquid crystalline semiconductors based on benzothiazole have been synthesized. Their structural, photophysical and electronic properties were investigated using X-ray diffraction, atomic force microscopy, cyclic voltammetry, UV-Vis, photoluminescence, and Raman spectroscopy. The liquid crystalline behaviour of the molecules was thoroughly examined by differential scanning calorimetry (DSC) and optical polarizing microscope. The DSC and thermogravimetric analysis (TGA) show that these materials posses excellent thermal stability and have decomposition temperatures in excess of 300 degrees C. Beyond 160 degrees C both molecules show a smectic A liquid crystalline phase that exists till about 240 degrees C. Field-effect transistors were fabricated by vacuum evaporating the semiconductor layer using standard bottom gate/top contact geometry. The devices exhibit p-channel behaviour with hole mobilities of 10(-2) cm(2)/Vs. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
The β-phase aging response of Cu–Al–Ni single crystal shape memory alloys (SMAs) within the temperature range of 473–573 K has been investigated. Alloys in austenitic (Cu–14.1Al–4Ni wt.%, alloy A) and martensitic (Cu–13.4Al–4Ni wt.%, alloy M) conditions at room temperature were considered. Aged samples show presence of β1′ and γ1′ martensites in both the alloys and formation of γ2 precipitates in the alloy A. The differential scanning calorimetry (DSC) thermograms of the aged samples show increase in transformation temperatures as well as transformation hysteresis with aging. Dynamic mechanical analysis (DMA) was conducted on both the alloys to ascertain the role of precipitates and martensitic transition on tan δ, which characterizes the damping behaviour of the material. With aging, a steady decrease in tan δ value was observed in both the alloys, which was attributed to the decrease in the number of interfaces per unit area with increasing aging temperature. Moreover, in alloy A, as the volume fraction of precipitate increases with aging, the movement of martensitic interfaces is restricted causing a decreased tan δ.
Resumo:
We report the binding energy of various nucleobases (guanine (G), adenine (A), thymine (T) and cytosine (C)) with (5,5) single-walled carbon nanotube (SWNT) calculated using first-principle Hartre–Fock method (HF) together with classical force field. The binding energy without including the solvation effects of water decreases in the order G>A>T>C. The inclusion of solvation energy changes the order of binding preference to be G>T>A>C. Using isothermal titration (micro) calorimetry experiments, we also show the relative binding affinity to be T>A>C, in agreement with our calculations.
Resumo:
The conformation, organization, and phase transitions of alkyl chains in organic-inorganic hybrids based on the double pervoskite-slab lead iodides, (CH3NH3)(CH3(CH2)(n)NH3)(2)Pb2I7 (n = 11, 13, 15, 17) have been investigated by X-ray diffraction, calorimetry, and infrared vibrational spectroscopy. In these hybrid solids, double pervoskite (CH3NH3)Pb2I7 slabs are interleaved with alkyl ammonium chains with the anchored alkyl chains arranged as tilted bilayers and adopting a planar all-trans conformation at room temperature. The (CH3NH3)(CH3(CH2)(n)NH3)(2)Pb2I7 compounds exhibit a single reversible phase transition above room temperature with the associated enthalpy change varying linearly with alkyl chain length. This transition corresponds to the melting in two-dimensions of the alkyl chains of the anchored bilayer and is characterized by increased conformational disorder of the methylene units of the chain and loss of tilt angle coherence leading to an increase in the interslab spacing. By monitoring features in the infrared spectra that are characteristic of the global conformation of the alkyl chains, a quantitative relation between conformational disorder and melting of the anchored bilayer is established. It is found that, irrespective of the alkyl chain length, melting occurs when at least 60% of the chains in the anchored bilayer of (CH3NH3)(CH3(CH2)(n)NH3)(2)Pb2I7 have one or more gauche defects. This concentration is determined by the underlying lattice to which the alkyl chains are anchored.
Resumo:
Transparent glasses of BaNaB9O15 (BNBO) were fabricated via the conventional melt-quenching technique. The amorphous and the glassy nature of the as-quenched samples were, respectively, confirmed by x-ray powder diffraction and differential scanning calorimetry (DSC). The glass transition and crystallization parameters were evaluated under non-isothermal conditions using DSC. The correlation between the heating rate dependent glass transition and the crystallization temperatures was studied and the Kauzmann temperature was deduced for BNBO glass plates and powdered samples. The values of the Kauzmann temperature for the plates and powdered samples were 776 K and 768 K, respectively. An approximation- free method was used to evaluate the crystallization kinetic parameters for the BNBO glass samples. The effect of the sample thickness on the crystallization kinetics of BNBO glasses was also investigated.
Resumo:
The standard free energy of formation of titanium boride (TiB2) Was measured by the Electro Motive Force (EMF) method (by using yttria doped thoria (YDT) as the solid electrolyte). Two galvanic cells viz. Cell (I): Pt, TiB2 (s), TiO2 (s), B (s) vertical bar YDT vertical bar NiO (s), Ni (s), Pt and cell (II): Pt, TiB2 (s), TiO2 (s), B (s) vertical bar YDT vertical bar FeO (s). Fe (s), Pt were constructed in order to determine the Delta(f)G degrees, of TiB2. Enthalpy increments on TiB2 were measured by using inverse drop calorimetry over the temperature range 583-1769 K. The heat capacity, entropy and the free energy function have been derived from these experimental data in the temperature range 298-1800 K. The mean value of the standard enthalpy of formation of TiB2 (Delta H-f(298)degrees (TiB2)) was obtained by combining these Delta(f)G degrees, values and the free energy functions of TiB2 derived from the drop calorimetry data. The mean values of Delta H-f(298)degrees (TiB2) derived from the Delta(f)G degrees, data obtained from cell I and II were -322 +/- 1.2 kJ mol(-1) and -323.3 +/- 2.1 kJ mol(-1), respectively. These values were found to be in very good agreement with the assessed data. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
The time evolution of the film thickness and domain formation of octadecylamine molecules adsorbed oil a mica surface is investigated Using atomic force microscopy. The adsorbed Film thickness is determined by measuring the height profile across the mica-amine interface of a mica surface partially immersed in a 15 mM solution of octadecylamine in chloroform. Using this novel procedure, adsorption of amine on mica is found to occur in three distinct stages, with morphologically distinct domain Formation and growth occurring during each stage. In the first stage, where adsorption is primarily in the thin-film regime, all average Film thickness of 0.2 (+/- 0.3) nm is formed for exposure times below 30 s and 0.8 (+/- 0.2) nm for 60 s of immersion time. During this stage, large sample spanning domains are observed. The second stage, which occurs between 60-300 s, is associated with it regime of rapid film growth, and the film thickness increases from about 0.8 to 25 nm during this stage. Once the thick-film regime is established, further exposure to the amine solution results in all increase in the domain area, and it regime of lateral domain growth is observed. In this stage, the domain area coverage grows from 38 to 75%, and the FTIR spectra reveal an increased level of crystallinity in the film. Using it diffusion-controlled model and it two-step Langmuir isotherm, the time evolution of the film growth is quantitatively captured. The model predicts the time at which the thin to thick film transition occurs as well its the time required for complete film growth at longer times. The Ward-Tordai equation is also solved to determine the model parameters in the monolayer (thin-film) regime, which occurs during the initial stages of film growth.