Resumo:
Electrochemical reduction of exfoliated graphene oxide, prepared from pre-exfoliated graphite, in acetamide-urea-ammonium nitrate ternary eutectic melt results in few layer-graphene thin films. Negatively charged exfoliated graphene oxide is attached to positively charged cystamine monolyer self-assembled on a gold surface. Electrochemical reduction of the oriented graphene oxide film is carried out in a room temperature, ternary molten electrolyte. The reduced film is characterized by atomic force microscopy (AFM), conductive AFM, Fourier-transform infrared spectroscopy and Raman spectroscopy. Ternary eutectic melt is found to be a suitable medium for the regulated reduction of graphene oxide to reduced graphene oxide-based sheets on conducting surfaces. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Gd2O3:Eu3+ (4 mol%) nanophosphor co-doped with Li+ ions have been synthesized by low-temperature solution combustion technique in a short time. Powder X-ray diffractometer (PXRD), scanning electron microscopy (SEM), Fourier transform infrared spectroscopy (FT-IR), UV-VIS and photoluminescence (PL) techniques have been employed to characterize the synthesized nanoparticles. It is found that the lattice of Gd2O3:Eu3+ phosphor transforms from monoclinic to cubic as the Li+-ions are doped. Upon 254 nm excitation, the phosphor showed characteristic luminescence D-5(0) -> F-7(J) (J= 0-4) of the Eu3+ ions. The electronic transition located at 626 nm (D-5(0) -> F-7(2)) of Eu3+ ions was stronger than the magnetic dipole transition located at 595 nm (D-5(0) -> F-7(1)). Furthermore, the effects of the Li+ co-doping as well as calcinations temperature on the PL properties have been studied. The results show that incorporation of Li+ ions in Gd2O3:Eu3+ lattice could induce a remarkable improvement of their PL intensity. The emission intensity was observed to be enhanced four times than that of with out Li+-doped Gd2O3:Eu3+. (C) 2010 Elsevier B.V. All rights reserved,
Resumo:
Polyaniline/ZnFe2O4 nanocomposites were synthesized by a simple and inexpensive one-step in situ polymerization method in the presence of ZnFe2O4 nanoparticles. The structural, morphological, and electrical properties of the samples were characterized by wide angle X-ray diffraction (WAXD), Fourier transform infrared (FTIR) spectroscopy, scanning electron microscopy (SEM), and thermogravimetric analysis (TGA). WAXD and SEM revealed the formation of polyaniline/ZnFe2O4 nanocomposites. Infrared spectroscopy indicated that there was some interaction between the ZnFe2O4 nanoparticles and polyaniline. The dc electrical conductivity measurements were carried in the temperature range of 80 to 300 K. With increase in the doping concentration of ZnFe2O4, the conductivity of the nanocomposites found to be decreasing from 5.15 to 0.92 Scm(-1) and the temperature dependent resistivity follows ln rho(T) similar to T-1/2 behavior. The nanocomposites (80 wt % of ZnFe2O4) show a more negative magnetoresistance compared with that of pure polyaniline (PANI). These results suggest that the interaction between the polymer matrix PANI and zinc nanoparticles take place in these nanocomposites. (C) 2011 Wiley Periodicals, Inc. J Appl Polym Sci 120: 2856-2862, 2011
Resumo:
Dissolution of barium ion from aqueous suspensions of commercial nano-sized barium titanate powders (BaTiO3) has been studied at various pH values, solids loading, different time intervals and different electrolyte concentrations. Zeta potential measurements at various pH values and Fourier transform infrared spectroscopy study were also carried out to know the surface behaviour. Dissolution of Ba2+ depends on the suspension pH and stirring time period. The iso-electric points were found at 3.4 and 12.2 for as-received BaTiO3 powder and 2.3 for the leached BaTiO3. The Ba2+-leached BaTiO3 suspension retards further leaching of Ba2+ ions at different pH values, which favours the achievement of stable suspension.
Resumo:
The synthesis of ``smart structured'' conducting polymers and the fabrication of devices using them are important areas of research. However, conducting polymeric materials that are used in devices are susceptible to degradation due to oxygen and moisture. Thus, protection of such devices to ensure long-term stability is always desirable. Polymer nanocomposites are promising materials for the encapsulation of such devices. Therefore, it is important to develop suitable polymer nanocomposites as encapsulation materials to protect such devices. This work presents a technique based on grafting between surface-decorated gamma-alumina nanoparticles and polymer to make nanocomposites that can be used for the encapsulation of devices. Alumina was functionalized with allyltrimethoxysilane and used to conjugate polymer molecules (hydride-terminated polydimethylsiloxane) through a platinum-catalyzed hydrosilylation reaction. Fourier transform infrared spectroscopy, X-ray-photoelectron spectroscopy, and Raman spectroscopy were used to characterize the surface chemistry of the nanoparticles after surface modification. The grafting density of alkene groups on the surface of the modified nanoparticles was calculated using CHN and thermogravimetric analyses. The thermal stability of the composites was also evaluated using thermogravimetric analysis. The nanoindentation technique was used to analyze the mechanical characteristics of the composites. The densities of the composites were evaluated using a density gradient column, and the morphology of the composites was evaluated by scanning electron microscopy. All of our studies reveal that the composites have good thermal stability and mechanical flexibility and, thus, can potentially be used for the encapsulation of organic photovoltaic devices.
Resumo:
CuO nanowires are synthesized by heating Cu foil, rod and grid in ambient without employing a catalyst or gas flow at temperatures ranging from 400 to 800 degrees C for a duration of 1-12 h. Scanning electron microscopy (SEM) investigation reveals the formation of nanowires. The structure, morphology and phase of the as-synthesized nanowires are analyzed by various techniques such as X-ray diffraction (XRD), transmission electron microscopy (TEM), X-ray photoelectron spectroscopy (XPS), thermogravimetric analysis (TGA) and Fourier transform infrared spectroscopy (FTIR). It is found that these nanowires are composed of CuO phase and the underlying film is of Cu2O. A systematic study is carried out to find the possibilities for the transformation of one phase to another completely. A possible growth mechanism for the nanowires is also discussed. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
A new class of biodegradable copolyesters was synthesized by the catalyst-free melt condensation of sorbitol with citric acid, tartaric acid, and sebacic acid. The resulting polymers were designated as poly(sorbitol citric sebacate) p(SCS)] and poly(sorbitol tartaric sebacate) p(STS)]. The synthesized polymers were characterized by Fourier transform infrared spectroscopy, H-1-NMR spectroscopy, and differential scanning calorimetry analysis. Porous spongelike scaffolds were prepared with a salt-leaching technique and characterized with scanning electron microscopy. Tensile testing of the p(SCS) and p(STS) polymers showed that they exhibited a wide range of mechanical properties. The Young's modulus and tensile strengths of the polymers ranged from 1.06 +/- 0.12 to 462.65 +/- 34.21 MPa and from 0.45 +/- 0.04 to 20.32 +/- 2.54 MPa, respectively. In vitro degradation studies were performed on disc-shaped polymer samples. The half-life of the polymers ranged from 0.54 to 38.52 days. The percentage hydration of the polymers was in the range 9.36 +/- 1.26 to 78.25 +/- 1.91, with sol contents of 2-14%. At any given polymer composition, the Young's modulus and tensile strength of p(SCS) was higher than that of p(STS), whereas the degradation rates of p(SCS) was lower than that of p(STS). This was attributed to the structural difference between the citric and tartaric monomers and to the degree of crosslinking. (C) 2011 Wiley Periodicals, Inc. J Appl Polym Sci 121: 2861-2869, 2011
Resumo:
Adsorption, electrokinetic, microflotation, and flocculation studies have been carried out on sphalerite and galena minerals using extracellular polysaccharides (ECP) isolated from Bacillus polymyxa. The adsorption density of ECP onto galena is found to be higher than that onto sphalerite. The adsorption of ECP onto sphalerite is found to increase from pH 3 to about pH 7, where a maximum is attained, and thereafter continuously decreases. With respect to galena, the adsorption density of ECP steadily increases with increased pH. The addition of ECP correspondingly reduces the negative electrophoretic mobilities of sphalerite and galena in absolute magnitude without shifting their isoelectric points. However, the magnitude of the reduction in the electrophoretic mobility values is found to be greater for galena compared to that for sphalerite. Microflotation tests show that galena is depressed while sphalerite is floated using ECP in the entire pH range investigated. Selective flotation tests on a synthetic mixture of galena and sphalerite corroborate that sphalerite could be floated from galena at pH 9-9.5 using ECP as a depressant for galena. Flocculation tests reveal that in the pH range 9-11, sphalerite is dispersed and galena is flocculated in the presence of ECP. Dissolution tests indicate release of the lattice metal ions from galena and sphalerite, while co-precipitation tests confirm chemical interaction between lead or zinc ions and ECP. Fourier transform infrared spectroscopic studies provide evidence in support of hydrogen bonding and chemical interaction for the adsorption of ECP onto galena/sphalerite surfaces. (C) 2002 Elsevier Science (USA).
Resumo:
The most stable vinyl polyperoxide, namely, poly(indene peroxide) (PINDP), an alternating copolymer of indene and oxygen, was synthesized by the oxidative polymerization of indene. It was characterized by H-1-NMR and C-13-NMR, Fourier transform infrared, differential scanning calorimetry, direct pyrolysis mass spectrometry, and gas chromatography mass spectrometry studies. The overall activation energy for the degradation and the glass-transition temperature of PINDP were 47 kcal/mol and 327 K respectively, which were very high compared to those of other vinyl polyperoxides. (C) 2002 Wiley Periodicals, Inc.
Resumo:
We report the characterization of carbonaceous aluminium oxide, Al2O3:C, films grown on Si(100) by metalorganic chemical vapor deposition. The focus is on the study of the effects of carbon on the dielectric properties of aluminium oxide in a qualitative manner. The carbon present in the aluminium oxide film derives from aluminium acetylacetonate used as the source of aluminium. As-grown films comprise nanometer-sized grains of alumina (∼ 20–50 nm) in an amorphous carbonaceous matrix, as examined by X-ray diffractometry (XRD) and transmission electron microscopy (TEM). The films are shiny; they are smooth as observed by scanning electron microscopy (SEM). An attempt has been made to explore the defects (viz., oxide charge density) in the aluminium oxide films using room temperature high frequency capacitance – voltage (C-V) and current–voltage (I-V) measurements. The hysteresis and stretch-out in the high frequency C-V plots is indicative of charge trapping. The role of heteroatoms, as characterized by X-ray photoelectron spectroscopy (XPS) and Fourier transform infrared (FTIR) spectroscopy, in the transport of charge in Al2O3:C films is discussed.
Resumo:
The thiocarbohydrazone Schiff-base ligand with a nitrogen and sulphur donor was synthesized through condensation of pyridine-2-carbaldehyde and thiocarbohydrazide. Schiff-base ligands have the ability to conjugate with metal salts. A series of metal complexes with a general formula [MCl(2)(H(2)L)]center dot nH(2)O (M=Ni, Co, Cu and Zn) were synthesized by forming complexes of the N(1),N5-bis[pyridine-2-methylene]thiocarbohydrazone (H2L) Schiff-base ligand. These metal complexes and ligand were characterized by using ultraviolet-visible (UV-Vis), Fourier Transform Infrared (FT-IR), (1)H and (13)C NMR spectroscopy and mass spectroscopy, physicochemical characterization, CHNS and conductivity. The biological activity of the synthesized ligand was investigated by using Escherichia coli DNA as target. The DNA interaction of the synthesized ligand and complexes on E. coli plasmid DNA was investigated in the aqueous medium by UV-Vis spectroscopy and the binding constant (K(b)) was calculated. The DNA binding studies showed that the metal complexes had an improved interaction due to trans-geometrical isomers of the complexes than ligand isomers in cis-positions. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Noble metal ion substituted CeO(2) in the form of Ce(0.98)M(0.02)O(2-delta) solid solution (where M = Pt, Pd, Cu) are the new generation catalysts with applications in three-way exhaust catalysis. While adsorption of CO on noble metals ions is well-known, adsorption of CO on noble metal ions has not been studied because creating exclusive ionic sites has been difficult. Using first-principles density functional theory (DFT) we have shown that CO gets adsorbed on the noble metal Pt(2+), Pd(2+), Cu(2+) ionic sites in the respective compounds, and the net energy of the overall system decreases. Adsorption of CO on metal ions is also confirmed by Fourier transform infrared spectroscopy (FTIR).
Resumo:
This work presents an electrochemical technique for the polymerization and copolymerization of thiophene derivatives like 7,9-dithiophene-2yl-8H-cyclopenta[a]acenaphthalene-8-one and 3-hexylthiophene. The structural characterization of chemically synthesized monomers and electro-chemically synthesized polymers was carried out by nuclear magnetic resonance and Fourier transform infrared spectroscopy. Thermal characterizations indicate that copolymer has increased thermal stability than that of homopolymer. Morphological studies of the polymerized films carried out by scanning electron microscopy shows network structure of copolymer. Optical properties of the homopolymers and copolymer were studied by UV-visible spectrometer and it was observed that band gap of copolymer is less than the homopolymers. HOMO and LUMO levels, band gap values of the respective polymers were also calculated from the cyclic voltammetry technique with various scan rates. By the peak current obtained from various scan rates shows that all polymerization reactions are diffusion controlled process. Charge transfer resistances of polymers were determined using Nyquist plots. Conductivity of synthesized polymers shows higher conductivity for copolymer than homopolymers. (C) 2011 Elsevier Ltd. All rights reserved.
Resumo:
Bilayer thin films of Te/As(2)S(3) were prepared from Te and As(2)S(3) by thermal technique under high vacuum. Optical constants were calculated by analysing the transmission spectrum in the spectral range 400-1100 nm. The optical band gap decreases with the addition of Te to As(2)S(3). The decrease of optical band gap has been explained on the basis of density of states and the increase in disorder in the system. We have irradiated the as-deposited films using a diode pumped solid state laser of 532 nm wavelength to study photo-diffusion of Te into As(2)S(3). The changes were characterised by Fourier Transform Infrared and X-ray Photoelectron Spectroscopy (XPS). The optical band gap is found to be decreased with the light irradiation which is proposed due to homopolar bond formation. The core level peaks in XPS spectra give information about different bond formation. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Micrometre-scale polypyrrole (PPy) structures are synthesised for electrochemical supercapacitor applications by a facile electrochemical route. Globular polypyrrole microstructures of size < 5 μm are grown on stainless steel (SS-304) substrate by electro-polymerisation of pyrrole on oxygen microbubble templates electrochemically generated and stabilised in the presence of surfactant/supporting electrolyte/ dopant b-naphthalene sulfonic acid (b-NSA). Microstructures obtained with scan range of 0??1.6 V (against Ag/AgCl) are uniformly distributed over the surface with high coverage density of 5 x 105 to 8 x 10 cm-2. Fourier transform infrared spectroscopy and X-ray photoelectron spectroscopy revealed that the formed microstructures are of Β-NSA doped PPy. Scanning electron microscopy showed the uniform spread and good coverage of microstructures over the substrate. Supercapacitor properties of PPy films are investigated by cyclic voltammetry, electrochemical impedance spectroscopy and galvanostatic charge/discharge methods with 1.0 M KCl as electrolyte in a three-electrode electrochemical cell. Specific capacitance of 583 Fg-1 is obtained, which is greater than the values (350-400 Fg-1 highest) usually reported for this material. Electrochemical impedance spectroscopy proves the superc