108 resultados para conditions of contact


Relevância:

90.00% 90.00%

Publicador:

Resumo:

The optimum conditions for producing cast aluminium alloy-mica particle composites, by stirring mica particles (40 to 120 mgrm) in molten aluminium alloys (above their liquidus temperatures), followed by casting in permanent moulds, are described. Addition of magnesium either as pieces along with mica particles on the surface of the melts or as a previously added alloying element was found to be necessary to disperse appreciable quantities (1.5 to 2 wt.%) of mica particles in the melts and retain them as uniform dispersions in castings under the conditions of present investigation. These castings can be remelted and degassed with nitrogen at least once with the retention of about 80% mica particles in the castings. Electron probe micro-analysis of these cast composites showed that magnesium added to the surface of the melt along with mica has a tendency to segregate around the mica particles, apparently improving the dispersability for mica particles in liquid aluminium alloys. The mechanical properties of the aluminium alloy-mica particle composite decrease with an increase in mica content, however, even at 2.2% the composite has a tensile strength of 14.22 kg mm–2 with 1.1% elongation, a compression strength of 42.61 kg mm–2, and an impact strength of 0.30 kgm cm–2. The properties are adequate for certain bearing applications, and the aluminium-mica composite bearings were found to run under boundary lubrication, semi-dry and dry friction conditions whereas the matrix alloy (without mica) bearings seized or showed stick slip under the same conditions.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The seizure resistance of cast graphite-aluminium composite alloys containing graphite particles of various sizes was studied using a Hohman wear tester. If the graphite content is more than 2% these alloys can be selfmated without seizure under conditions of boundary lubrication. The size and shape of the graphite particles had no significant effect on seizure resistance. Owing to the extensive deformation and fragmentation of graphite, the low yield strength of the aluminium matrix and the low flow stress of the graphite particles, a continuous layer of graphite is formed on the mating surfaces even after a short running-in period. This layer persisted even after extensive wear deformation.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Interference fits are used extensively in aircraft structural joints because of their improved fatigue performance. Recent advances in analysis of these joints have increased understanding of the nonlinear load-contact and load-interfacial slip variations in these joints. Experimental work in these problems is lacking due to difficulties in determining partial contact and partial slip along the pin-hole interface. In this paper, an experimental procedure is enumerated for determining load-contact relations in interference/clearance fits, using photoelastic models and applying a technique for detecting progress of separation/contact up to predetermined locations. The study incorporates a detailed procedure for model making, controlling interference, locating break of contact up to known locations around the interface, estimating optically the degree of interference, determining interfacial friction and evaluating stresses in the sheet. Experiments, simulating joints in large sheets, were carried out under both pin and plate loads. The present studies provide load-separation behavior in interference joint with finite interfacial friction.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

A new mode of driven nonlinear vibrations of a stretched string is investigated with reference to conditions of existence, properties, and regions of stability. It is shown that this mode exhibits negative resistance properties at all frequencies and driving force amplitudes. Discovery of this mode helps to fill certain gaps in the theory of forced nonlinear vibrations of strings.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The activity of glutamine synthetase fromAspergillus niger was significantly lowered under conditions of citric acid fermentation. The intracellular pH of the organism as determined by bromophenol blue dye distribution and fluorescein diacetate uptake methods was relatively constant between 6•0–6•5, when the pH of the external medium was varied between 2•3–7•0.Aspergillus niger glutamine synthetase was rapidly inactivated under acidic pH conditions and Mn2+ ions partially protected the enzyme against this inactivation. Mn2+-dependent glutamine synthetase activity was higher at acidic pH (6•0) compared to Mg2+-supported activity. While the concentration of Mg2+ required to optimally activate glutamine synthetase at pH 6•0 was very high (≥ 50 mM), Mn2+ was effective at 4 mM. Higher concentrations of Mn2+ were inhibitory. The inhibition of both Mn2+ and Mg2+-dependent reactions by citrate, 2-oxoglutarate and ATP were probably due to their ability to chelate divalent ions rather than as regulatory molecules. This suggestion was supported by the observation that a metal ion chelator, EDTA also produced similar effects. Of the end-products of the pathway, only histidine, carbamyl phosphate, AMP and ADP inhibitedAspergillus niger glutamine synthetase. The inhibitions were more pronounced when Mn2+ was the metal ion activator and greater inhibition was observed at lower pH values. These results permit us to postulate that glutamine synthesis may be markedly inhibited when the fungus is grown under conditions suitable for citric acid production and this block may result in delinking carbon and nitrogen metabolism leading to acidogenesis.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

An analysis of gas absorption accompanied by chemical reaction in the presence of interfacial resistance is presented. The analysis indicates that the effect of interfacial resistance on interphase mass transfer is significantly higher in presence of a reaction compared to the pure absorption case. For fixed values of surface resistance and contact time, the difference between the amount of gas transferred across the interface with and without surface resistance increases as the value of reaction velocity increases. For ranges of contact time and surface resistance of practical relevance, the influence of surface resistance is too high to be neglected while designing gas-liquid contactors.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

For the purposes of obtaining a number of components with nearly identical thickness distributions over the substrate area and of minimizing the inhomogeneities of the film, it is logical to presume that a substrate rotating on its own axis and revolving around another axis will give more uniformity in film thickness than a substrate only revolving around one axis. In relation to the practical applications, an investigation has been undertaken to study the refinement that can be achieved by using a planar planetary substrate holder. It is shown theoretically that the use of the planetary substrate holder under ideal conditions of source and geometry does not offer any further improvement in uniformity of thickness over the conventional rotary work-holder. It is also shown that the geometrical parameters alone have little influence over the uniformity achieved on a planetary substrate, because of the complex cyclidal motion of any point on it. However, for any given geometry, a non-integral speed ratio of the planetary substrate and the work-holder shows considerably less variation in thickness over the substrate area.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

For the prediction of response of footings subjected to horizontal vibration, different types of contact shear distributions and displacement conditions are to be considered. Solutions using elastic half-space theory are not available for all the cases of shear distribution and displacement conditions. In this paper, solutions are obtained for the cases in which solutions are not available and the relevant coefficients are presented in tables which could be used in the appropriate equations for the prediction of dynamic response. Spring constants are evaluated and tabulated for different displacement and shear distribution conditions.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The role of heme in the synthesis of cytochrome c oxidase has been investigated in the mold Neurospora crassa. Iron-deficient cultures of the mold have low levels of cytochrome oxidase and delta-aminolevulinate dehydratase, the latter being the rate-limiting enzyme of the heme-biosynthetic pathway in this organism. Addition of iron to the iron-deficient cultures results in an immediate increase in the levels of delta-aminolevulinate dehydratase followed by an increase in the rate of heme synthesis and cytochrome oxidase levels. The rate of precursor labeling of the mitochondrial subunits of cytochrome oxidase is decreased preferentially under conditions of iron deficiency and addition of iron corrects this picture. Exogenous hemin addition which prevents iron-mediated induction of delta-aminolevulinate dehydratase also inhibits the increase in the activity of cytochrome oxidase and the enhanced precursor labeling of the mitochondrial subunits of cytochrome oxidase. Protein synthesis on mitoribosomes measured in vivo and in vitro is decreased under conditions of heme deficiency. Hemin addition in vitro to mitochondrial lysates prepared from heme-deficient mycelia restores a near normal rate of protein synthesis. It is concluded that heme is required for the optimal rate of translation on mitoribosomes.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The simple quasi-steady analysis of the combustion of a liquid fuel droplet in an oxidising atmosphere provides unsatisfactory explanations for several experimental observations. It's prediction of values for the burning constant (K), the flame-to-droplet diameter ratio ( ) and the flame temperature (Tf) have been found to be amgibuous if not completely inaccurate. A critical survey of the literature has led us to a detailed examination of the effects of unsteadiness and variable properties. The work published to date indicates that the gas-phase unsteadiness is relatively short and therefore quite insignificant.A new theoretical analysis based on heat transfer within the droplet is presented here. It shows that the condensed-phase unsteadiness lasts for about 20â??25% of the total burning time. It is concluded that the discrepancies between experimental observations and the predictions of the constant-property quasi-steady analysis cannot be attributed either to gas-phase or condensed-phase unsteadiness.An analytical model of quasi-steady droplet combustion with variable thermodynamic and transport properties and non-unity Lewis numbers will be examined. Further findings reveal a significant improvement in the prediction of combustion parameters, particularly of K, when consideration is given to variations of cp and λ with the temperature and concentrations of several species. Tf is accurately predicted when the required conditions of incomplete combustion or low ( ) at the flame are met. Further refinement through realistic Lewis numbers predicts ( ) meaningfully.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Al-10.98 pct Si-4.9 pct Ni ternary eutectic alloy was unidirectionally solidified at growth rates from 1.39μm/sec to 6.95μm/sec. Binary Al-Ni and Al-Si eutectics prepared from the same purity metals were also solidified under similar conditions to characterize the growth conditions under the conditions of present study. NiAl3 phase appeared as fibers in the binary Al-Ni eutectic and silicon appeared as irregular plates in the binary Al-Si eutectic. However, in the ternary Al-Si-Ni eutectic alloy both NiAl3 and silicon phases appeared as irregular plates dispersed in α-Al phase, without any regular repctitive arrangement. The size and spacing of NiAl3 and Si platelets in cone shaped colonies decreased with an increase in the growth rate of the ternary eutectic. Examination of specimen quenched during unidirectional solidification indicated that the ternary eutectic grows with a non-planar interface with both Si and NiAl3 phases protruding into the liquid. It is concluded that it will be difficult to grow regular ternary eutectic structures even if only one phase has a high entropy of melting. The tensile strength and modulus of unidirectionally solidified Al-Si-Ni eutectic was lower than the chill cast alloys of the same composition, and decreased with a decrease in growth rate. Tensile modulus and strength of ternary Al-Si-Ni eutectic alloys was greater than binary Al-Si eutectic alloy under similar growth conditions, both in the chill cast and in unidirectionally solidified conditions.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

δ-Aminolevulinate (ALA) dehydratase, the second and rate limiting enzyme of the heme biosynthetic pathway in the mold Neurospora crassa is induced maximally in 30 min by the addition of iron to iron-deficient cultures. The induction of the enzyme is blocked by cycloheximide, protoporphyrin, 8-azaguanine and cordycepin. Iron also brings about an increase in poly(A)-containing RNA synthesis under conditions of induction. The iron dependent increase in poly(A)-containing RNA synthesis is blocked by protoporphyrin. It is suggested that at the time intervals examined, bulk of the messenger RNA synthesized in response to iron addition represents the messenger for ALA dehydratase.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The denaturation of β-lactoglobulin-A by heat and guanidine hydrochloride at pH 2 has been investigated. The effect of ethylene glycol on the thermal denaturation at this pH has also been studied. The conditions of the experiments have been chosen so as to eliminate complications arising out of disulfide interchange, changes in the degree of association of the protein during denaturation, and intermolecular aggregation. The physical parameters characterizing the denatured states of the protein which are produced by heat and guanidine hydrochloride have been determined. The thermodynamic parameters for these transitions have been estimated using a two-state hypothesis in each case. Both the physical and thermodynamic parameters indicate that the heat-denatured state of β-lactoglobulin-A retains about 15-20% of residual structure which is destroyed on adding guanidine hydrochloride.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Asymmetric rolling of commercially pure magnesium was carried out at three different temperatures: room temperature, 200 degrees C and 350 degrees C. Systematic analysis of microstructures, grain size distributions, texture and misorientation distributions were performed using electron backscattered diffraction in a field emission gun scanning electron microscope. The results were compared with conventional (symmetric) rolling carried out under the same conditions of temperature and strain rate. Simulations of deformation texture evolution were performed using the viscoplastic self-consistent polycrystal plasticity model. The main trends of texture evolution are faithfully reproduced by the simulations for the tests at room temperature. The deviations that appear for the textures obtained at high temperature can be explained by the occurrence of dynamic recrystallization. Finally, the mechanisms of texture evolution in magnesium during asymmetric and symmetric rolling are explained with the help of ideal orientations, grain velocity fields and divergence maps displayed in orientation space.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

By “phenotypic plasticity” we refer to the capacity of a genotype to exhibit different phenotypes, whether in the same or in different environments. We have previously demonstrated that phenotypic plasticity can improve the degree of adaptation achieved via natural selection (Behera & Nanjundiah, 1995). That result was obtained from a genetic algorithm model of haploid genotypes (idealized as one-dimensional strings of genes) evolving in a fixed environment. Here, the dynamics of evolution is examined under conditions of a cyclically varying environment. We find that the rate of evolution, as well as the extent of adaptation (as measured by mean population fitness) is lowered because of environmental cycling. The decrease is adaptation caused by a varying environment can, however, be partly or wholly compensated by an increase in the degree of plasticity that a genotype is capable of. Also, the reduction of population fitness caused by a variable environment can be partially offset by decreasing the total number of genetic loci. We conjecture that an increase in genome size may have been among the factors responsible for the evolution of phenotypic plasticity.