111 resultados para Refractive-index distribution
Resumo:
The variation of the linear electro-optic effect in (-)-2-(alpha-methylbenzylamino)-5-nitropyridine with the wavelength of the incident light at room temperature has been measured. The reduced half-wave voltages have been found to have the values 2.1, 2.8, and 6.0 kV at 488, 514.5, and 632.8 nm respectively and the corresponding values of the linear electro-optic coefficient have been evaluated.;The interpretation of the results in terms of the structures of the molecule and the crystal is discussed. The thermal variation of the birefringence has also been investigated and the coefficient for the temperature variation of the refractive index difference is found to have the value (d Delta n/dT)=9.3X10(-5) K-1.
Resumo:
Transparent BaNaB9O15 (BNBO), BaLiB9O15 (BLBO) and SrLiB9O15 (SLBO) glasses were fabricated via the conventional melt-quenching technique. X-ray diffraction (XRD) and Differential thermal analysis (DTA) studies carried out on the as-quenched glasses confirmed their amorphous and glassy nature, respectively. The optical properties for these as-quenched glasses were investigated. The refractive index, optical band gap. Urbach energy and Fermi energy were determined. The average electronic polarizability calculated from the refractive index expression. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Thin films of zirconia have been synthesized using reactive DC magnetron sputtering. It has been found that films with good optical constants, high refractive index (1.9 at 600 nm) and low extinction coefficient can be prepared al ambient temperatures. The optical constants and band gnp and hence the composition nle dependent on the deposition parameters such as target power, rate of deposition and oxygen background pressure. Thermal annealing of the films revealed that tile films showed optical and crystalline inhomogeneity and also large variations in optical constants.
Resumo:
A study of the linear electro?optic effect in single crystals of the organic compound, 4?nitro�4??methylbenzylidene aniline is reported. The reduced half?wave voltages have been found to have values 2.8, 1.3, and 1.1 kV at 632.8, 514.5, and 488.0 nm, respectively and the corresponding values of the largest linear electro?optic coefficient have been calculated. The thermal variation of the birefringence has also been investigated and the temperature variation of the refractive index difference is found to have the value, d?n/dT = 15.8 × 10?5 K?1.
Resumo:
Thin films of Bismuth Vanadate Bi2VO5.5 (BiV) have been deposited on amorphous quartz and polycrystalline silicon substrates by r.f. sputtering technique and characterised for their structural and optical properties. The os-deposited films at room temperature are found to be amorphous and transparent over the spectral range of 0.55 mu m to 12 mu m. Post-deposition annealing at 400 degrees C in air shows the formation of the BiV crystalline phase. The optical constants namely refractive index. extinction coefficient and optical bandgap of both amorphous and crystalline films have been determined. The refractive index of the as-deposited film is around 2.4 at 0.7 mu m and drops to 2.26 at 1.56 mu m. The optical bandgap of the material has been determined from the computed values of the absorption coefficients.
Resumo:
The dependence of optical constants, structure and composition of titania thin films on the process parameters has been investigated. Films were deposited using both reactive electron beam evaporation and ion Assisted Deposition(IAD). If has been observed that the refractive index of IAD films is higher than that for the reactively deposited films, without much difference in the extinction coefficient. Electron paramagnetic resonance has been used to estimate qualitatively the presence of non-stoichiometry in the films. It has been found that these spectra correlate very well the optical behaviour of the films. X-ray diffraction studies revealed that the neutral oxygen deposited films were stress free, while the IAD films showed tensile stress. The lattice parameters showed anisotropic change with ion beam parameters.
Resumo:
Optical and structural properties of reactive ion beam sputter deposited CeO2 films as a function of oxygen partial pressures (P-O2) and substrate temperatures (T-s) have been investigated. The films deposited at ambient temperature with P-O2 of 0.01 Pa have shown a refractive index of 2.36 which increased to 2.44 at 400 degrees C. Refractive index and extinction coefficient are sensitive up to a T-s of similar to 200 degrees C. Raman spectroscopy and X-ray diffraction (XRD) have been used to characterise the structural properties. A preferential orientation of (220) was observed up to a T-s of 200 degrees C and it changed to (200) at 400 degrees C: and above. Raman line broadening, peak shift and XRD broadening indicate the formation of nanocrystalline phase for the films deposited up to a substrate temperature of 300 degrees C. However, crystallinity of the films were better for T-s values above 300 degrees C. In general both optical and structural properties were unusual compared to the films deposited by conventional electron beam evaporation, but were similar in some aspects to those deposited by ion-assisted deposition. Apart from thermal effects, this behavior is also attributed to the bombardment of backscattered ions/neutrals on the growing film as well as the higher kinetic energy of the condensing species, together resulting in increased packing density. (C) 1997 Elsevier Science S.A.
Resumo:
Glass samples with compositions (100-2x)SrB4O7-xBaO-xTiO(2) (10 less than or equal to x less than or equal to 40) were prepared by conventional melt quenching and the influence of the addition of BaO-TiO2 on the structural, dielectric and optical properties of SBO glasses was studied The molar volume, glass transition temperature and the optical polarisability of the glass samples were found to decrease with increase in BaO-TiO2 content while the refractive index and optical band gap increase with increase in BaO-TiO2 content.
Resumo:
Glass nanocomposites in the system (100 - x)Li2B4O7-xSrBi(2)Ta(2)O(9) (0 less than or equal to x less than or equal to 22.5, in molar ratio) were fabricated via a melt quenching technique followed by controlled heat-treatment. The as-quenched samples were confirmed to be glassy and amorphous by differential thermal analysis (DTA) and X-ray powder diffraction (XRD) techniques, respectively. The phase formation and crystallite size of the heat-treated samples (glass nanocomposites) were monitored by XRD and transmission electron microscopy (TEM). The relative permittivities (epsilon(tau)') of the glass nanocomposites for different compositions were found to lie in between that of the parent host glass (Li2B4O7) and strontium bismuth tantalate (SBT) ceramic in the frequency range 100 Hz-40 MHz at 300 K, whereas the dielectric loss (D) of the glass nanocomposite was less than that of both the parent phases. Among the various dielectric models employed to predict the effective relative permittivity of the glass nanocomposite, the one obtained using the Maxwell's model was in good agreement with the experimentally observed value. Impedance analysis was employed to rationalize the electrical behavior of the glasses and glass nanocomposites. The pyroelectric response of the glasses and glass nanocomposites was monitored as a function of temperature and the pyroelectric coefficient for glass and glass nanocomposite (x = 20) at 300 K were 27 muC m(-2) K-1 and 53 muC m(-2) K-1, respectively. The ferroelectric behavior of these glass nanocomposites was established by P vs. E hysteresis loop studies. The remnant polarization (P-r) of the glass nanocomposite increases with increase in SBT content. The coercive field (E-c) and P-r for the glass nanocomposite (x = 20) were 727 V cm(-1) and 0.527 muC cm(-2), respectively. The optical transmission properties of these glass nanocomposites were found to be composition dependent. The refractive index (n = 1.722), optical polarizability (am = 1.266 6 10 23 cm 3) and third-order nonlinear optical susceptibility (x(3) = 3.046 6 10(-21) cm(3)) of the glass nanocomposite (x = 15) were larger than those of the as-quenched glass. Second harmonic generation (SHG) was observed in transparent glass nanocomposites and the d(eff) for the glass nanocomposite (x = 20) was found to be 0.373 pm V-1.
Direct measurement of phase of foreward-scattered light using polarization heterodyne interferometer
Resumo:
We describe direct measurement of phase of ballistic photons transmitted through objects hidden in a turbid medium using a polarization interferometer employing a rotating analyzer. The unwrapped phase difference measurements from interferometry was possible for medium levels of turbidity and accurate phase measurement from the sinusoidal intensity was not detectable when l/l* is increased beyond 4.3. The measured phase on reconstruction using standard tomographic algorithms resulted in the recovery of the refractive index profile of the object hidden in the turbid medium.
Resumo:
Single crystals of a-hopeite exhibiting high transparency were grown by single diffusion gel growth technique. Single crystal X-ray diffraction analysis reveals that the crystal belongs to orthorhombic system. The values of several structural and physical parameters have been determined for the grown crystal. The optical absorption study reveals the transparency of the crystal and is noticed in the entire visible region and the cut-off wavelength was found to be 230 nm. The optical band gap found to be at 3.25 eV. The dependence of extinction co-efficient (k) and the refractive index (n) on the wavelength was also shown. The dielectric constant and dielectric loss of the crystal was studied as a function of frequency and temperature. Transport properties of the grown crystal have been studied from the Cole-Cole plot. (C) 2010 Elsevier GmbH. All rights reserved.
Resumo:
Aluminum oxide films have been prepared by ion assisted deposition using argon ions with energy in the range 300 to 1000 eV and current density in the range 50 to 220 μA/cm2. The influence of ion energy and current density on the optical and structural properties has been investigated. The refractive index, packing density, and extinction coefficient are found to be very sensitive to the ion beam parameters and substrate temperatures. The as-deposited films were found to be amorphous and could be transformed into crystalline phase on annealing. However, the crystalline phases were different in films prepared at ambient and elevated substrate temperatures.
Resumo:
Structural, optical and nanomechanical properties of nanocrystalline Zinc Telluride (ZnTe) films of thickness upto 10 microns deposited at room temperature on borosilicate glass substrates are reported. X-ray diffraction patterns reveal that the films were preferentially oriented along the (1 1 1) direction. The maximum refractive index of the films was 2.74 at a wavelength of 2000 nm. The optical band gap showed strong thickness dependence. The average film hardness and Young's modulus obtained from load-displacement curves and analyzed by Oliver-Pharr method were 4 and 70 GPa respectively. Hardness of (1 1 1) oriented ZnTe thin films exhibited almost 5 times higher value than bulk. The studies show clearly that the hardness increases with decreasing indentation size, for indents between 30 and 300 nm in depth indicating the existence of indentation size effect. The coefficient of friction for these films as obtained from the nanoscratch test was ~0.4.
Resumo:
Structural, optical and nanomechanical properties of nanocrystalline Zinc Telluride (ZnTe) films of thickness upto 10 microns deposited at room temperature on borosilicate glass substrates are reported. X-ray diffraction patterns reveal that the films were preferentially oriented along the (1 1 1) direction. The maximum refractive index of the films was 2.74 at a wavelength of 2000 nm. The optical band gap showed strong thickness dependence. The average film hardness and Young's modulus obtained from load-displacement curves and analyzed by Oliver-Pharr method were 4 and 70 GPa respectively. Hardness of (1 1 1) oriented ZnTe thin films exhibited almost 5 times higher value than bulk. The studies show clearly that the hardness increases with decreasing indentation size, for indents between 30 and 300 nm in depth indicating the existence of indentation size effect. The coefficient of friction for these films as obtained from the nanoscratch test was ~0.4.
Resumo:
Multiple beam interference of light in a wedge is considered when the wedge is filled with an absorbing medium. The aim is to examine a method that may give values of both the real and the imaginary parts of the refractive index of the absorbing medium. We propose here a method to determine these quantities from simple techniques like fringe counting and interferometry, by using as the incident wave either a single Gaussian beam or two parallel Gaussian beams.