Resumo:
Analytical short time solution of moving boundary in heat conduction in a cylindrical mould under prescribed flux boundary condition has been studied in this paper. Partial differential equations are converted to integro-differential equations. These integro-differential equations which are coupled have been solved analytically for short time by choosing suitable series expansions for the unknown quantitities.
Resumo:
Attempts were made to produce directionally solidified, specifically grain aligned Al-6 wt pct Ni eutectic alloy using a laboratory scale ESR unit. For this purpose sand cast alloy electrodes were electroslag remelted under different mold conditions. The grain structure of the ingots obtained from these meltings showed that insulated silica molds gave the best vertical alignment of grains along the length of the ingot. The NiAl3 fibers within the grains tended to fan out and there was only a preferred alignment of fibers along the growth direction under the conditions of our experiments. The ESR parameters most suitable for vertical alignment of eutectic grains have been identified. In some electroslag remelting trials ingots were grown on a seed ingot. This resulted in a fewer vertical grains compared to the case when no seed ingot was used. The sand cast specimen of the eutectic exhibited a maximum tensile strength of around 88.2 MN/m2 (9.0 kg/mm2) whereas conventional ESR using water cooled mold gave strength value of 98.0 MN/m2 (10 kg/mm2). The directionally solidified ESR material showed longitudinal tensile strength as high as 213.7 MN/m2 (21.8 kg/mm2) which could be further increased to 220.6 MN/m2 (22.5 kg/mm2) by using the seed ingot. The average growth rate was varied between 5 to 25 mm/min during electroslag remelting in this study. The flow stresses, tangent modulus and ultimate tensile strength of directionally solidified eutectic increased with increasing growth rates.
Resumo:
Nanocrystalline Fe53Co47 alloy was synthesized by a single-step transmetallation chemical method at room temperature. The Fe53Co47 alloy nanoparticles of 77 and 47 wt% were dispersed in silica matrix by the sol-gel process using tetraethyl orthosilcate. Structural studies reveal that the as-prepared alloy powders are in bcc phase and silica is in an amorphous state. The phase-transition temperature and Mossbauer spectra analysis of the Fe-Co alloy establishes the homogeneous alloy formation. A saturation magnetization of 218 emu/g was obtained for pure FeCo alloy at room temperature. Scanning electron microscopic analysis demonstrates the hollow-sphere morphology for FeCo alloy particles. Magnetic nanocomposite consisting of 47 wt% FeCo-silica shows enhanced thermal stability over the native FeCo alloy. Electrical and dielectric properties of 47 wt% FeCo-silica nanocomposites were investigated as a function of frequency and temperature. It was found that the dielectric constants and dielectric loss were stable throughout the measured temperature (310-373 K). Our results indicate that FeCo-silica nanocomposite is a promising candidate for high-frequency applications. (C) 2010 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim
Resumo:
Thermodynamic properties of three oxides of niobium have been measured using solid state electrochemical cells incorporating yttria-doped thoria (YDT) as the electrolyte in the temperature range T = (1000 to 1300) K. The standard Gibbs energies of formation of NbO, NbO2, and NbO2.422 from the elements can be expressed as: Delta(f)G(NbO)(o) +/- 547/J . mol(-1) = -414 986 + 86.861(T/K) Delta(f)G(NbO2)(o) +/- 548/J . mol(-1) = -779 864 + 164.438(T/K) Delta(f)G(NbO2.422)(o) +/- 775/J . mol(-1) = -911 045 + 197.932(T/K) The results are discussed in comparison with thermodynamic data reported in the literature. The new results refine data for NbO and NbO2 presented in standard data compilations. There are no data in thermodynamic compilations for NbO2.422 (Nb12O29). In the absence of the heat capacity and enthalpy of formation measurements, only the Gibbs energy of formation of NbO2.422 can be assessed. The free energy of formation of stoichiometric Nb2O5 is evaluated on the basis of measurements on NbO2.422 and information available in the literature on phase boundary compositions and isothermal variation of nonstoichiometric parameter with oxygen potential for Nb2O5-x. The results suggest a minor revision of data for Nb2O5. A minimum in the Gibbs energy of mixing for the system Nb-O occurs in the nonstoichiometric domain of Nb2O5-x with x = 0.036.
Resumo:
The formation of anomalous indentations, with two opposite faces describing a pin-cushion effect and the other two faces normal, in long elongated grains of an extruded Mg-2Al-1Zn alloy is reported. Subsurface microstructural observations combined with Schmid factor calculations suggest that extension twinning accompanied by basal slip are the reasons for these. Johnson's expanding cavity model is invoked for further substantiation. (C) 2010 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
The effect of thermal cycling on the load-controlled tension-tension fatigue behavior of a Ni-Ti-Fe shape memory alloy (SMA) at room temperature was studied. Considerable strain accumulation was observed to occur in this alloy under both quasi-static and cyclic loading conditions. Though, in all cases, steady-state is reached within the first 50-100 cycles, the accumulated steady-state strain, epsilon(p.ss), is much smaller in thermally cycled alloy. As a result, the fatigue performance of them was found to be significantly enhanced vis-a-vis the as-solutionized alloy. Furthermore, under load-controlled conditions, the fatigue life of Ni-Ti-Fe alloys was found to be exclusively dependent on epsilon(p.ss). Observations made by profilometry and differential scanning calorimetry (DSC) indicate that the 200-500% enhancement in fatigue life of thermally cycled alloy is due to the homogeneous distribution of the accumulated fatigue strain. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Addition of boron in small quantities to various titanium alloys have shown significant improvement in mechanical behavior of materials. In the present study, electron back-scatter diffraction (EBSD) techniques have been applied to investigate the deformation microstructure evolution in boron modified two-phase titanium alloy Ti-6Al-4V. The alloy was hot compressed at 750 degrees C up to 50% height reduction at two different strain rates (10(-3) s(-1) and 1 s(-1)). The EBSD analyses indicated significant differences in deformed microstructure of the base alloy and the alloy containing boron. A strong subgrain formation tendency was observed along with inhomogeneous distribution of dislocations inside large a colonies of Ti64. In contrast, a colonies were relatively strain free for Ti64 + B, with more uniform dislocation density distribution. The observed difference is attributed to microstructural modifications viz, grain size refinement and presence of TiB particles at grain boundary produced due to boron addition. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
The chemical potentials of SrO in two-phase fields (TiO2 + SrTiO3) (SrTiO3 + Sr4Ti3O10) (Sr4Ti3O10 + Sr3Ti2O7) and (Sr3Ti2O7 + Sr2TiO4) of the pseudo-binary system (SrO + TiO2) have been measured in the temperature range (900 to 1250) K relative to pure SrO as the reference state using solid-state galvanic cells incorporating single crystal SrF2 as the electrolyte The cells were operated under pure oxygen at ambient pressure The standard Gibbs free energies of formation of strontium titanates SrTiO3 Sr4Ti3O10 Sr3Ti2O7 and Sr2TiO4 from their component binary oxides were derived from the reversible electromotive force (EMF) of the cells For the formation of the four compounds from their component oxides TiO2 with rutile structure and SrO the standard Gibbs free energy changes are given by Delta G((ox))(SrTiO3) +/- 89/(J mol(-1)) = -121878 + 3 881(T/K) Delta G((ox))(Sr4Ti3O10) +/- 284/(J mol(-1)) = -409197 + 14 749(T/K) Delta G((ox))(Sr3Ti2O7) +/- 190/(J mol(-1)) = -285827 + 10 022(T/K) Delta G((ox))(Sr2TiO4) +/- 110/(J mol(-1))= -159385 + 3 770(T/K) The reference state for solid TiO2 is the rutile form The results of this study are in good agreement with Gibbs free energy of formation data reported in the literature for SrTiO3 but differ significantly with data for Sr4Ti3O10 For Si3Ti2O7 and Si2TiO4 experimental measurements are not available in the literature for direct comparison with the results obtained in this study (C) 2010 Elsevier Ltd All rights reserved
Resumo:
Thermal expansion of several compositions of Sr and Mg-doped LaGaO3 including an A-site deficient composition (La0.9Sr0.1)(0.98)(Ga0.8Mg0.2)O-2.821 were measured in the temperature range from 298 to 1273 K. The effect of doping on thermal expansion was studied by varying the composition at one site of the perovskite structure (either A or B), while keeping the composition at the other site invariant. Thermal expansion varied nonlinearly with temperature and exhibited an inflexion between 550 and 620 K, probably related to the change in crystal structure from orthorhombic to rhombohedral. The dependence of average thermal expansion coefficient (alpha (av)) on the dopant concentration on either A or B site of the perovskite structure was found to be linear, when the composition at the other site was kept constant. Mg doping on the B-site had a greater effect on the average thermal expansion coefficient than Sr doping on the A-site. Cation deficiency at the A-site decreases thermal expansion when compositions at both sites are held constant.
Resumo:
The addition of small amounts of B to Ti-6Al-4V alloy reduces the as-cast grain size by an order of magnitude and introduces TiB phase into the microstructure. The effects of these microstructural modifications on both the high cycle fatigue and cyclic stress-strain response were investigated. Experimental results show that B addition markedly enhances the fatigue strength of the alloy; however, the influence of prior-beta grain size was found to be only marginal. The presence of TiB particles in the matrix appears to be beneficial with the addition of 0.55 wt.% B to Ti-6Al-4V enhancing the fatigue strength by more than 50%. Strain-controlled fatigue experiments reveal softening in the cyclic stress-strain response, which increases with the B content in the alloy. Transmission electron microscopy of the fatigued specimens indicates that generation of dislocations during cyclic loading and creation of twins due to strain incompatibility between the matrix and the TiB phase are possible reasons for the observed softening. (c) 2010 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
In this article, we examine the unusual plastic deformation under uniaxial compression of an Al2O3-15 mol % Y2O3 (A15Y) glass synthesized by a wet chemical route At a low temperature of 650-725 degrees C, plastic deformation of this glass is largely non-viscous through shear instabilities In contrast deformation near the crystallization temperature (850 degrees C) occurs homogeneously with work hardening and with a monotonic increase in the true density of the glass by 10-12% accompanied by an increase in hardness (H) and elastic modulus (E) of up to 100% We hypothesize a phenomenon of molecular densification of the amorphous structure through a hierarchy of multiple phases, analogous to density- or entropy-driven amorphous to-amorphous phase transitions (polyamorphism) These results suggest that the present method of preparation and the unusual behavior can trigger a search for many more systems that display such behavior (C) 2010 Acta Materialia Inc Published by Elsevier Ltd All rights reserved
Resumo:
Research on conducting polymers, organic light emitting diodes and organic solar cells has been an exciting field for the past decade. The challenge with these organic devices is the long term stability of the active material. Organic materials are susceptible to chemical degradation in the presence of oxygen and moisture. The sensitivity of these materials towards oxygen and moisture makes it imperative to protect them by encapsulation. Polymer nanocomposites can be used as encapsulation materials in order to prevent material degradation. In the present work, amine functionalized alumina was used as a cross-linking and reinforcing material for the polymer matrix in order to fabricate the composites to be used for encapsulation of devices. Fourier transform infrared spectroscopy, X-ray photoelectron spectroscopy and Raman spectroscopy were used to elucidate the surface chemistry. Thermogravimetric analysis techniques and CHN analysis were used to quantify grafting density of amine groups over the surface of the nanoparticles. Mechanical characterizations of the composites with various loadings were carried out with dynamic mechanical analyzer. It was observed that the composites have good thermal stability and mechanical flexibility, which are important for an encapsulant. The morphology of the composites was evaluated using scanning electron microscopy and atomic force microscopy.
Resumo:
Several methods for improving the strength of metallic materials are available and correlations between strength and various microstructural features have been established. The purpose of this paper is to review parallel developments favouring improved fracture resistance. Resistance to fracture in monotonie loading, cyclic loading and when fracture is environment-aided have been considered in steels, aluminium alloys and anisotropic materials. Finally, the question of optimising alloy behaviour is discussed.
Resumo:
The phase diagram of the Ni-W-O system at 1200 K was established by metallographic and X-ray identification of the phases present after equilibration at controlled oxygen potentials. The oxygen partial pressures over the samples were fixed by metered streams of CO+CO2 gas mixtures. There was only one ternary oxide, nickel tungstate (NiWO4), in the Ni-W-O system at a total pressure of 1 atm, and this compound decomposed to a mixture of Ni+WO2.72 on lowering the oxygen potential. The Gibbs' free energy of formation of NiWO4 was determined from the measurement of the e.m.f. of the solid oxide galvanic cell, Pt, Ni+NiWO4+WO2.72/CaO-ZrO2/Ni+NiO, Pt and thermodynamic properties of tungsten and nickel oxides available in the literature. For the reaction, NiO(s)+WO3(s)rarrNiWO4(s) DeltaG°=–10500–0.708 T (±250) cal mol–1.