93 resultados para styrene-butadiene rubber (SBR)


Relevância:

20.00% 20.00%

Publicador:

Resumo:

ASTM D2303 standard provides a method for evaluating the tracking and erosion resistance of polymeric insulators under ac voltages. In this paper, the above method has been extended for evaluating the performance of the insulators under dc stresses. Tests were conducted on polymeric silicone rubber (SR) insulators under positive and negative dc stresses. Micron sized Alumina trihydrate (uATH) and nano sized Alumina (nALU) were used as fillers in SR matrix to improve the resistance to tracking and erosion. Results suggest that SR composites perform better under negative dc than under positive dc voltages. Eroded mass and leakage current data support the above result. Samples with low concentration of nano alumina fillers performed on par with the samples with large loadings of uATH.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This is the first report on the study carried out on high-pressure free-radical initiated oxidated copolymerization of styrene (STY) with alpha-methylstyrene (AMS) at various temperatures (45-65degreesC) at constant pressure (100 psi) and then at various pressures (50-300 psi) keeping the temperature (50degreesC) constant. The compositions of the copolyperoxides obtained from the H-1 NMT spectra were utilized to determine the reactivity ratios of the monomers. The reactivity ratios indicate that STY forms an ideal copolyperoxide with AMS and the copolyperoxide is richer in AMS. The effect of temperature and oxygen pressure in the reactivity ratios of the monomers was studied. The rates of copolymerization (R-p) were used to determine the overall activation energies (E-a) and activation volume (DeltaV(#)) of copolymerization. The unusually higher values of the DeltaV(#) may be due to the pressurizing fluid oxygen which itself is a reactant in the copolymerization, the side reactions, and the chain-transfer reactions occuring during copolymerizations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The thermal degradation of a series of para-substituted poly(styrene peroxide)s with electron-donating [CH3, C(CH3)(3)] and electron-attracting (Br) substitutents are investigated by thermogravimetric analysis (TGA). The results indicate that the Hammett relationship can describe quantitatively the trends in maximum rate of polymer decomposition (T-max) observed in TGA and thus thermostability of substituted poly(styrene peroxide)s depends only on the electronic nature of substituents and their ability to stabilize macroradicals formed during chain scission. The experimental results are also substantiated by thermochemical calculations. (C) 2002 Elsevier Science Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Epoxy systems containing HTBN rubber material and reinforced with E-glass fibres, exposed to a fixed time duration in three separate media were subjected to compressive mode of deformation. The yield stress and fractographic features noted on the compression failed samples are reported in this work. The experiment reveals that the seawater exposed sample exhibits a drop in strength compared to dry (unexposed) sample. This kind of drop is maintained if the media is changed from seawater to distilled water. When HCl is included in seawater. the experiment shows a small rise in strength value. These changes have been attributed to various factors like medium ingress into samples assisting interface failure, the larger-sized Cl- influencing the extent of diffusion of medium into system and finally their participation in the deformation phenomena. The fractographic features reveal interface separations that show either scattered debris or a cleaner surface or display a whitish-coated matrix region depending on whether the tests are done on unexposed samples or on ones following the immersion in the media.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The three-point bending behavior of sandwich beams made up of jute epoxy skins and piecewise linear functionally graded (FG) rubber core reinforced with fly ash filler is investigated. This work studies the influence of the parameters such as weight fraction of fly ash, core to thickness ratio, and orientation of jute on specific bending modulus and strength. The load displacement response of the sandwich is traced to evaluate the specific modulus and strength. FG core samples are prepared by using conventional casting technique and sandwich by hand layup. Presence of gradation is quantified experimentally. Results of bending test indicate that specific modulus and strength are primarily governed by filler content and core to sandwich thickness ratio. FG sandwiches with different gradation configurations (uniform, linear, and piecewise linear) are modeled using finite element analysis (ANSYS 5.4) to evaluate specific strength which is subsequently compared with the experimental results and the best gradation configuration is presented. POLYM. COMPOS., 32:1541-1551, 2011. (C) 2011 Society of Plastics Engineers

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In order to improve the tracking and erosion performance of outdoor polymeric silicone rubber (SR) insulators used in HV power transmission lines, micron sized inorganic fillers are usually added to the base SR matrix. In addition, insulators used in high voltage dc transmission lines are designed to have increased creepage distance to mitigate the tracking and erosion problems. ASTM D2303 standard gives a procedure for finding the tracking and erosion resistance of outdoor polymeric insulator weathershed material samples under laboratory conditions for ac voltages. In this paper, inclined plane (IP) tracking and erosion tests similar to ASTM D2303 were conducted under both positive and negative dc voltages for silicone rubber samples filled with micron and nano sized particles to understand the phenomena occurring during such tests. Micron sized Alumina Trihydrate (ATH) and nano sized alumina fillers were added to silicone rubber matrix to improve the resistance to tracking and erosion. The leakage current during the tests and the eroded mass at the end of the tests were monitored. Scanning Electron Microscopy (SEM) and Energy dispersive Xray (EDX) studies were conducted to understand the filler dispersion and the changes in surface morphology in both nanocomposite and microcomposite samples. The results suggest that nanocomposites performed better than microcomposites even for a small filler loading (4%) for both positive and negative dc stresses. It was also seen that the tracking and erosion performance of silicone rubber is better under negative dc as compared to positive dc voltage. EDX studies showed migration of different ions onto the surface of the sample during the IP test under positive dc which has led to an inferior performance as compared to the performance under negative dc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Corona discharge is recognized as one of the mechanisms that can influence the surface hydrophobicity of Silicone Rubber (SR) because of the chemical changes that occur on its surface. In this study SR samples were exposed to positive and negative DC corona for 25 and 50 hours using a needle-plane electrode system. Hydrophobicity changes were monitored using a sessile drop contact angle measurement facility. The physical changes on the surface were studied using Scanning Electron Microscopy (SEM) and surface roughness measurements. The effect of positive dc corona was found to be different from that of negative dc corona. Significant surface degradation and loss of hydrophobicity was found in the case of negative dc corona exposed samples. Significant improvement in the above mentioned properties were obtained by adding small quantities of nSIL into the SR matrix.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Multiwall carbon nanotubes (MWNTs) were anchored onto graphene oxide sheets (GOs) via diazonium and C-C coupling reactions and characterized by spectroscopic and electron microscopic techniques. The thus synthesized MWNT-GO hybrid was then melt mixed with 50/50 polyamide6-maleic anhydride-modified acrylonitrile-butadiene-styrene (PA6-mABS) blend to design materials with high dielectric constant (30) and low dielectric loss. The phase morphology was studied by SEM and it was observed that the MWNT-GO hybrid was selectively localized in the PA6 phase of the blend. The 30 scales with the concentration of MWNT-GO in the blends, which interestingly showed a very low dielectric loss (< 0.2) making them potential candidate for capacitors. In addition, the dynamic storage modulus scales with the fraction of MWNT-GO in the blends, demonstrating their reinforcing capability as well.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Corona is an unavoidable phenomena in high voltage power transmission system, in spite of suitably designed insulator accessories and transmission line hardware. It is a proven fact that the continuous occurrence of corona can subject the polymeric insulator to a severe degradation. Further, moisture in the air has a positive influence on the corona activity. This paper presents the methodology to evaluate the corona performance of the silicone rubber housing material with simultaneous application of cold fog. Analysis conducted after corona treatment by the Fourier Transform Infrared Spectroscopy (FTIR) present an interesting results showing a higher hydroxylation of sample surface under the moisture application than in the normal condition for both AC and DC excitation. FTIR spectrum also indicates the presence of nitric acid on the treated surface with coldfog application. Results obtained from SEM analysis are also presented.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Polypropylene and natural rubber blends with multiwalled carbon nanotube (PP/NR + MWCNT nanocomposites) were prepared by melt mixing. The melt rheological behaviour of neat PP and PP/NR blends filled with different loadings (1, 3, 5, 7 wt%) of MWCNT was studied. The effect of PP/NR blends (with compositions, 80/20,50/50, 20/80 by wt) on the rheological percolation threshold was investigated. It was found that blending PP with NR (80/20 and 50/50 composition) reduced the rheological percolation threshold from 5 wt% to 3 wt% MWCNT. The melt rheological behaviour of the MWCNT filled PP/NR blends was correlated with the morphology observations from high resolution transmission electron microscopic (HRTEM) images. In predicting the thermodynamically favoured location of MWCNT in PP/NR blend, the specific interaction of phospholipids in NR phase with MWCNTs was considered quantitatively. The MWCNTs were selectively localised in the NR phase. The percolation mechanism in MWCNT filled PP/NR blends was discussed and for each blend composition, the percolation mechanism was found to be different. (C) 2015 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Electromagnetic shielding has become important for various electrical systems because of the electromagnetic pollution caused by the large scale use of electronic devices operating at different frequencies and power levels. Traditionally used metallic shields lack flexibility and hence may not be the right choice for certain applications. In such situations, filled polymer composites provide a good alternative for electromagnetic shielding applications. Being polymer based, they are easy to manufacture and can be molded into the required geometry and shape. In this study, the shielding properties of multiwalled carbon nanotubes and carbon nanofibers filled silicone rubber are studied. The conductivity and the shielding effectiveness of the composites were measured at different filler loadings. Both the fillers are able to make the base polymer conducting even at very low filler loadings. The conductivity and the shielding effectiveness improved when the filler loading was above the percolation threshold.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This is the first report on studies carried out in detail on high-pressure oxygen copolymerization (> 50 psi) of the vinyl monomers styrene and alpha-methylstyrene (AMS). The saturation pressure of oxygen for AMS oxidation, hitherto obscure, is found to be 300 psi. Whereas the ease of oxidation is more favorable for styrene, the rate and yield of polyperoxide formation are higher for AMS. This is explained on the basis of the reactivity of the corresponding alkyl and peroxy radicals. Below 50 degrees C, degradation of the poly(styrene peroxide) formed is about 2.5 times less than that observed above 50 degrees C, so much so that it gives a break in the rate curve, and thereafter the rate is lowered. Normal free radical kinetics is followed before the break point, after which the monomer and initiator exponents become unusually high. This is interpreted on the basis of chain transfer to the degradation products. The low molecular weight of polyperoxides has been attributed to the (i) low reactivity of RO(2)(.) toward the monomer, (ii) chain transfer to degradation products, (iii) facile cleavage of O-O bond, followed by unzipping to nonradical products, and (iv) higher stability of the reinitiating radicals. At lower temperatures, (i) predominates, whereas at higher temperatures, chiefly (ii)-(iv) are the case.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The present work focuses on simulation of nonlinear mechanical behaviors of adhesively bonded DLS (double lap shear) joints for variable extension rates and temperatures using the implicit ABAQUS solver. Load-displacement curves of DLS joints at nine combinations of extension rates and environmental temperatures are initially obtained by conducting tensile tests in a UTM. The joint specimens are made from dual phase (DP) steel coupons bonded with a rubber-toughened adhesive. It is shown that the shell-solid model of a DLS joint, in which substrates are modeled with shell elements and adhesive with solid elements, can effectively predict the mechanical behavior of the joint. Exponent Drucker-Prager or Von Mises yield criterion together with nonlinear isotropic hardening is used for the simulation of DLS joint tests. It has been found that at a low temperature (-20 degrees C), both Von Mises and exponent Drucker-Prager criteria give close prediction of experimental load-extension curves. However. at a high temperature (82 degrees C), Von Mises condition tends to yield a perceptibly softer joint behavior, while the corresponding response obtained using exponent Drucker-Prager criterion is much closer to the experimental load-displacement curve.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

It has been observed that poly(styrene peroxide) with a high molecular weight is thermally less stable than the same polymer with a low molecular weight. This has been explained as being due to the strain on the O-O bond due to the greater polymer chain length.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Multistress aging of outdoor composite polymeric insulators continues to be a topic of interest for power transmission research community. Aging due to dry conditions alone at elevated temperatures and electric stress in the presence of UV radiation environment probably has not been explored. This paper deals with long-term accelerated multistress aging under the above conditions on full-scale 11 kV distribution class composite silicone rubber insulators. To evaluate the long-term synergistic effect of electric stress, temperature and UV radiation on insulators, they were subjected to accelerated aging in a specially designed multistress-aging chamber for 12000 hours. Chemical, physical and electrical changes due to degradation have been assessed using various techniques. It has been found that the content of low molecular weight molecules and hydrophobicity reduced significantly. Also, due to oxidation and aging there is appreciable increase in surface roughness and weight percentage of oxygen. Study is under progress and only intermediate results are presented in this paper.