104 resultados para spray volume
Resumo:
The problem of spurious increase in volume fraction of second-phase particles during computer simulations of coarsening is examined. The origin of this problem is traced to the use of too long a time step (used for numerical integration of growth rates with respect to time) which leads to small particles with large negative growth rates shrinking to negative radii at the end of the time step. Such a shrinkage to negative sizes has the effect of pumping solute into the system. It is therefore suggested that the length of the time step be chosen in accordance with the size of the smallest particle present in the system. It is shown that spurious increase in particle Volume has a significant effect on the particle size distributions in the scaling regime (making them broader and more skewed in the Lifshitz-Slyozov-Wagner model). Its effect on coarsening kinetics, however, is found to be small.
Resumo:
Nebulized spray pyrolysis provides a good low?temperature chemical route for preparing thin films of PbTiO3, (Pb0.9,La0.1)TiO3 and Pb(Zr0.52,Ti0.48)O3. The films are a? or c? axis oriented, with spherical grains of ?30 nm and give satisfactory P?E hysteresis loops. © 1995 American Institute of Physics.
Resumo:
The technique of nebulized spray pyrolysis has been explored to find out whether oriented films of certain important oxides can be produced on single-crystal substrates by this relatively gentle method. Starting with acetylacetonate precursors, oriented films of metallic LaNiO3 containing nearly spherical grains (30 nm) have been obtained. Films of near-stoichiometric La4Ni3O10 and La3Ni2O7 showing metallic conductivity have been obtained by this method. This is indeed gratifying since it is difficult to prepare monophasic and stoichiometric bulk samples of these materials. Films of La2NiO4 show the expected semiconducting behavior. In the La-Cu-O system, starting with acetylacetonates, we have obtained films mainly comprising semiconducting La2Cu2O5, which is generally difficult to prepare in bulk form. More interestingly, nebulized spray pyrolysis gives excellent stoichiometric films of Pb(Zr0.52Ti0.48)O-3 consisting of nearly spherical grains (30 nm) which show ferroelectric behavior. The present investigation demonstrates that nebulized spray pyrolysis provides a useful and desirable route to deposite oriented films of complex oxide materials on single-crystal substrates.
Resumo:
Reported distress to an industrial structure from phosphate/sulfate contamination of kaolinitic foundation soil at an industrial location in Southern India prompted this laboratory study. The study examines the short-term effect of sodium sulfate/phosphate contamination on the swell/compression characteristics of a commercial kaolinite. Experimental results showed that the unsaturated contaminated kaolinite specimens exhibited slightly higher swell potentials and lower compressions than the unsaturated uncontaminated kaolinite specimens. It is suggested that the larger double layer promoted by the increased exchangeable sodium ion concentration is responsible for the slightly higher swell potentials and lower compressions of the unsaturated contaminated kaolinite specimens.
Resumo:
Devitrification of spray pyrolysed, amorphous ZrO2-Al2O3 solid solution produces nanocrystalline microstructures (grain sizes 10-20 nm). In this study, spray pyrolysed amorphous ZrO2-40 mol% Al2O3 powder displayed good sinterability during decomposition, after spraying, of the nitrate precursors up to 1023K. Hot pressing of fully pyrolysed, pre-sintered (more than 70% dense) pellets at 923K and 750 MPa produced an amorphous pellet with less than 2% porosity. The results indicate the possibility of producing dense, amorphous pellets that can be heat treated further to produce nanocrystalline microstructures conducive for superplasticity.
Resumo:
Nebulized spray pyrolysis of metal-organic precursors in methanol solution has been employed to prepare powders of TiO2, ZrO2 and PbZr0.5Ti0.5O3 (PZT). This process ensures complete decomposition of the precursors at relatively low temperatures. The particles have been examined by scanning and transmission electron microscopy as well as X-ray diffraction. As prepared, the particles are hollow agglomerates of diameter 0.1-1.6 mu m, but after heating to higher temperatures the ultimate size of the particles comprising the agglomerates are considerably smaller (0.1 mu m or less in diameter) and crystalline.
Resumo:
The next generation manufacturing technologies will draw on new developments in geometric modelling. Based on a comprehensive analysis of the desiderata of next generation geometric modellers, we present a critical review of the major modelling paradigms, namely, CSG, B-Rep, non-manifold, and voxel models. We present arguments to support the view that voxel-based modellers have attributes that make it the representation scheme of choice in meeting the emerging requirements of geometric modelling.
Resumo:
Aqueous solutions of acetates and nitrates of zinc and cobalt have been spray decomposed to study the production of extended solid solutions in the ZnO-CoO system. Examination of the products of a variety of synthesis conditions indicates that up to 70% CoO may be retained in the solid solution in the wurzite phase, even though a comparison of the equilibrium solubility in the phase diagram might be expected to favor the formation of a rock-salt-based solid solution.
Resumo:
We propose a new method for evaluating the adsorbed phase volume during physisorption of several gases on activated carbon specimens. We treat the adsorbed phase as another equilibrium phase which satisfies the Gibbs equation and hence assume that the law of rectilinear diameters is applicable. Since invariably the bulk gas phase densities are known along measured isotherms, the constants of the adsorbed phase volume can be regressed from the experimental data. We take the Dubinin-Astakhov isotherm as the model for verifying our hypothesis since it is one of the few equations that accounts for adsorbed phase volume changes. In addition, the pseudo-saturation pressure in the supercritical region is calculated by letting the index of the temperature term in Dubinin's equation to be temperature dependent. Based on over 50 combinations of activated carbons and adsorbates (nitrogen, oxygen, argon, carbon dioxide, hydrocarbons and halocarbon refrigerants) it is observed that the proposed changes fit experimental data quite well.
Resumo:
The role of matrix microstructure on the fracture of Al-alloy composites with 60 vol% alumina particulates was studied. The matrix composition and microstructure were systematically varied by changing the infiltration temperature and heat treatment. Characterization was carried out by a combination of metallography, hardness measurements, and fracture studies conducted on compact tension specimens to study the fracture toughness and crack growth in the composites. The composites showed a rise in crack resistance with crack extension (R curves) due to bridges of intact matrix ligaments formed in the crack wake. The steady-state or plateau toughness reached upon stable crack growth was observed to be more sensitive to the process temperature rather than to the heat treatment. Fracture in the composites was predominantly by particle fracture, extensive deformation, and void nucleation in the matrix. Void nucleation occurred in the matrix in the as-solutionized and peak-aged conditions and preferentially near the interface in the underaged and overaged conditions. Micromechanical models based on crack bridging by intact ductile ligaments were modified by a plastic constraint factor from estimates of the plastic zone formed under indentations, and are shown to be adequate in predicting the steady-state toughness of the composite.
Resumo:
Fracture toughness and fracture mechanisms in Al2O3/Al composites are described. The unique flexibility offered by pressureless infiltration of molten Al alloys into porous alumina preforms was utilized to investigate the effect of microstructural scale and matrix properties on the fracture toughness and the shape of the crack resistance curves (R-curves). The results indicate that the observed increment in toughness is due to crack bridging by intact matrix ligaments behind the crack tip. The deformation behavior of the matrix, which is shown to be dependent on the microstructural constraints, is the key parameter that influences both the steady-state toughness and the shape of the R-curves. Previously proposed models based on crack bridging by intact ductile particles in a ceramic matrix have been modified by the inclusion of an experimentally determined plastic constraint factor (P) that determines the deformation of the ductile phase and are shown to be adequate in predicting the toughness increment in the composites. Micromechanical models to predict the crack tip profile and the bridge lengths (L) correlate well with the observed behavior and indicate that the composites can be classified as (i) short-range toughened and (ii) long-range toughened on the basis of their microstructural characteristics.
Resumo:
Liquid phase co-spray forming (LPCSF) was employed to produce two Al-Si-Pb alloys. The preforms thus obtained were then subjected to hot extrusion at different extrusion ratios. Following extrusion, the materials were tensile tested at room temperature. The distribution of Pb particles and the microstructural characterization in as-formed preforms and in the extruded rods were studied on the basis of SEM observation. The influence of the Pb content on the mechanical properties was investigated. (C) 2002 Published by Elsevier Science B.V.
Resumo:
ZrO2–Al2O3 powders were synthesized by spray pyrolysis. These powders were sintered at 1 GPa in the temperature range of 700–1100 °C. The microstructural evolution and densification are reported in this paper. The application of 1 Gpa pressure lowers the crystallization temperature from ∼850 to <700 °C. Similarly, the transformation temperature under 1 GPa pressure for γ → α–Al2O3 reduces from ∼1100 to 700–800 °C range, and that for t → m ZrO2 reduces from ∼1050 to 700–800 °C range. It was possible to obtain highly dense nanocrystalline ZrO2–Al2O3 composite at temperatures as low as 700 °C. The effect of high pressure on nucleation and transformation of phases is discussed.