34 resultados para performance degradation
Resumo:
In the present study, amino-silane modified layered organosilicates were used to reinforce cyclic olefin copolymer to enhance the thermal, mechanical and moisture impermeable barrier properties. The optimum clay loading (4%) in the nanocomposite increases the thermal stability of the film while further loading decreases film stability. Water absorption behavior at 62 degrees C was carried out and compared with the behavior at room temperature and 48 degrees C. The stiffness of the matrix increases with clay content and the recorded strain to failure for the composite films was lower than the neat film. Dynamic mechanical analysis show higher storage modulus and low loss modulus for 2.5-4 wt% clay loading. Calcium degradation test and device encapsulation also show the evidence of optimum clay loading of 4 wt% for improved low water vapor transmission rates compared to other nanocomposite films. (C) 2014 Elsevier Ltd. All rights reserved.
Resumo:
Corona is an unavoidable phenomena in high voltage power transmission system, in spite of suitably designed insulator accessories and transmission line hardware. It is a proven fact that the continuous occurrence of corona can subject the polymeric insulator to a severe degradation. Further, moisture in the air has a positive influence on the corona activity. This paper presents the methodology to evaluate the corona performance of the silicone rubber housing material with simultaneous application of cold fog. Analysis conducted after corona treatment by the Fourier Transform Infrared Spectroscopy (FTIR) present an interesting results showing a higher hydroxylation of sample surface under the moisture application than in the normal condition for both AC and DC excitation. FTIR spectrum also indicates the presence of nitric acid on the treated surface with coldfog application. Results obtained from SEM analysis are also presented.
Resumo:
We report the synthesis of nitrogen doped vertically aligned multi-walled (MWNCNTs) carbon nanotubes by pyrolysis and its catalytic performance for degradation of methylene blue (MB) dye & oxygen reduction reaction (ORR). The degradation of MB was monitored spectrophotometrically with time. Kinetic studies show the degradation of MB follows a first order kinetic with rate constant k=0.0178 min(-1). The present rate constant is better than that reported for various supported/non-supported semiconducting nanomaterials. Further ORR performance in alkaline media makes MWNCNTs a promising cost-effective, fuel crossover tolerance, metal-free, eco-friendly cathode catalyst for direct alcohol fuel cell.
Resumo:
Corona discharges resulting from the metal parts of insulators and the line hardware affect the long term performance of the polymeric insulators used for outdoor application and can lead to its eventual failure. The authors previous work, involved in developing a new methodology to evaluate the performance of polymeric shed materials subjected to corona stresses in the presence of natural fog condition, results revealed more surface hydroxylation thereby resulting in more loss of hydropobhicity. With the increase in industrialization, there is an increase in acidic component of the rain as well as the fog (moisture). The present work, reports the effect of acid fog on the corona performance of the polymeric insulators for both AC and DC excitation, interesting results are obtained. A comparison of the experimental investigations revealed that the acidic fog has more effect than that of the normal fog. This fact has been confirmed by physico-chemical analysis like the scanning electron microscopy (SEM), Fourier transform infrared spectroscopy (FTIR), x-ray photoelectron spectroscopy (XPS) and contact angle measurement. The effect of DC corona is found to be lesser in comparison with the AC; however the hydroxylation induced by the DC corona under the presence of fog is similar with that of AC excitation.