94 resultados para high strength
Resumo:
With many innovations in process technology, forging is establishing itself as a precision manufacturing process: as forging is used to produce complex shapes in difficult materials, it requires dies of complex configuration of high strength and of wear-resistant materials. Extensive research and development work is being undertaken, internationally, to analyse the stresses in forging dies and the flow of material in forged components. Identification of the location, size and shape of dead-metal zones is required for component design. Further, knowledge of the strain distribution in the flowing metal indicates the degree to which the component is being work hardened. Such information is helpful in the selection of process parameters such as dimensional allowances and interface lubrication, as well as in the determination of post-forging operations such as heat treatment and machining. In the presently reported work the effect of aperture width and initial specimen height on the strain distribution in the plane-strain extrusion forging of machined lead billets is observed: the distortion of grids inscribed on the face of the specimen gives the strain distribution. The stress-equilibrium approach is used to optimise a model of flow in extrusion forging, which model is found to be effective in estimating the size of the dead-metal zone. The work carried out so far indicates that the methodology of using the stress-equilibrium approach to develop models of flow in closed-die forging can be a useful tool in component, process and die design.
Resumo:
Recent studies (I-7) clearly indicate a strong dependence of fatigue threshold parameter, A K on grain size in several alloy systems. Attempts to explain these observations on the basis of crat~tortuosity (1,8), fracture surface roughness (5,9) and crack closure (6) appear to present a fairly clear picture of the mechanisms that cause a reduction in crack growth rates at threshold. In general, it has been shown that coarse grained microstructures exhibit higher fatigue threshold in low carbon steels (1,5) aluminium alloys (7) and titanium alloys (6). In spite of these observations, there exists (10-1#) considerable uncertainity about the manner in which the AK~L depends on prior austenitic grain size in quenched and tempered steels. Studies in quenched and tempered steels demonstrating both an increase (3,12,14) as well as a decrease (11,12) in AKth with an increase in prior austenitic grain size can be sought to illustrate this point. Occasionally , the absence of any sensitivity of AKth to the variations in prior austenitJc grain size has also been reported (11,13). While a few investigators (5-7) comfortably rationalised the grain size effects on AK~L on the basis of crack closure by a comparison in terms of the closure-free component of the thresho~Ifc~, AK -f such an approach has yet to be extended to high strength steels, An attempt has been made in t~et ,pthrg sent study to explai. n the effect of pri, or austeniti.c grain size on &Kth on the basis of crack closure measurements in a high strength steel.
Resumo:
An attempt has been made experimentally to investigate the acoustic emission (AE) energy release in high-strength concrete (HSC) beams subjected to monotonically increasing load. Acoustic emission energy release during the fracture process of the HSC beams is measured. Stress waves released during the fracture process in materials cause acoustic emissions. AE energy released during the fracture of a notched three-point bend plain concrete beam specimens having 28-day compressive strengths of 50.0 MPa, 69.0 MPa and 78.0 MPa and mortar (cement: sand (1: 4) by weight) specimens are studied. Mortar consists of one part cement and four parts sand by weight. The specimens were tested by a material testing system of 1200 kN capacity employing crack mouth opening displacement control at the rate of 0.0004 mm/s. The fracture energy and the AE energy released during the fracture process of all the tested TPB and mortar specimens are compared and discussed. The observations made in the present experimental study have some applications for monitoring the integrity of structures.
Resumo:
A novel stress induced martenistic phase transformation is reported in an initial B2-CuZr nanowire of cross-sectional dimensions in the range of 19.44 x 19.44-38.88 x 38.88 angstrom(2) and temperature in the range of 10-400 K under both tensile and compressive loading. Extensive Molecular Dynamic simulations are performed using an inter-atomic potential of type Finnis and Sinclair. The nanowire shows a phase transformation from an initial B2 phase to BCT (body-centered-tetragonal) phase with failure strain of similar to 40% in tension, whereas in compression, comparatively a small B2 -> BCT phase transformation is observed with failure strain of similar to 25%. Size and temperature dependent deformation mechanisms which control ultimately the B2 -> BCT phase transformation are found to be completely different for tensile and compressive loadings. Under tensile loading, small cross-sectional nanowire shows a single step phase transformation, i.e. B2 -> BCT via twinning along {100} plane, whereas nanowires with larger cross-sectional area show a two step phase transformation, i.e. B2 -> R phase -> BCT along with intermediate hardening. In the first step, nanowire shows phase transformation from B2 -> R phase via twinning along {100} plane, afterwards the nanowire deforms via twinning along {110} plane which cause further transformation from R phase -> BCT phase. Under compressive loading, the nanowire shows crushing along {100} plane after a single step phase transformation from B2 -> BCT. Proper tailoring of such size and temperature dependent phase transformation can be useful in designing nanowire for high strength applications with corrosion and fatigue resistance. (C) 2009 Elsevier Ltd. All rights reserved.
Resumo:
Stiffness, strength, and toughness are the three primary attributes of a material, in terms of its mechanical properties. Bulk metallic glasses (BMGs) are known to exhibit elastic moduli at a fraction lower than crystalline alloys and have extraordinary strength. However, the reported values of fracture toughness of BMGs are highly variable; some BMGs such as the Zr-based ones have toughness values that are comparable to some high strength steels and titanium alloys, whereas there are also BMGs that are almost as brittle as silicate glasses. Invariably, monolithic BMGs exhibit no or low crack growth resistance and tend to become brittle upon structural relaxation. Despite its critical importance for the use of BMGs as structural materials, the fracture toughness of BMGs is relatively poorly understood. In this paper, we review the available literature to summarize the current understanding of the mechanics and micromechanisms of BMG toughness and highlight the needs for future research in this important area.
Resumo:
This paper presents results of triaxial compression tests on sand reinforced with different types of geosynthetics in different layer configurations to study the effect of quantity of reinforcement and tensile strength of the geosynthetic material on the mechanical behavior of geosynthetic-reinforced sand. The reinforcement types used are woven geotextile, geogrid, and polyester film. The layer configurations used are two, three, four, and eight horizontal reinforcing layers in a triaxial test sample. From the triaxial tests, it is found that the geosynthetic reinforcement imparts cohesive strength to otherwise cohesionless sand. The effect of reinforcement on the friction angle was found to be insignificant. The magnitude of imparted apparent cohesion is found to depend not only on the tensile strength of the geosynthetic material but also the surface roughness changes during loading. Special triaxial tests using rice flour as the reinforced medium, microscopic images, and surface roughness studies revealed the effect of indent formation on the surface of polyester film, which was the reason for the unusually high strength exhibited by the sand reinforced with polyester film.
Resumo:
This paper presents test results for 22 high strength deformed bars and nine mild steel bars subjected to monotonic repeated and reversed axial loading to determine the stress-strain behavior. Equations have been proposed for the stress-strain curves and have been compared with test results. Satisfactory agreement was obtained.
Resumo:
This paper presents test results for 22 high strength deformed bars and nine mild steel bars subjected to monotonic repeated and reversed axial loading to determine the stress-strain behavior. Equations have been proposed for the stress-strain curves and have been compared with test results. Satisfactory agreement was obtained.
Resumo:
An attempt has been made to systematically investigate the effects of microstructural parameters, such as the prior austenite grain size (PAGS), in influencing the resistance to fatigue crack growth (FCG) in the near-threshold region under three different temper levels in a quenched and tempered high-strength steel. By austenitizing at various temperatures, the PAGS was varied from about 0.7 to 96 μm. The microstructures with these grain sizes were tempered at 200 °C, 400 °C, and 530 °C and tested for fatigue thresholds and crack closure. It has been found that, in general, three different trends in the dependence of both the total threshold stress intensity range, ΔK th , and the intrinsic threshold stress intensity range, ΔK eff, th , on the PAGS are observable. By considering in detail the factors such as cyclic stress-strain behavior, environmental effects on FCG, and embrittlement during tempering, the present observations could be rationalized. The strong dependence of ΔK th and ΔK eff, th on PAGS in microstructures tempered at 530 °C has been primarily attributed to cyclic softening and thereby the strong interaction of the crack tip deformation field with the grain boundary. On the other hand, a less strong dependence of ΔK th and ΔK eff, th on PAGS is suggested to be caused by the cyclic hardening behavior of lightly tempered microstructures occurring in 200 °C temper. In both microstructures, crack closure influenced near-threshold FCG (NTFCG) to a significant extent, and its magnitude was large at large grain sizes. Microstructures tempered at the intermediate temperatures failed to show a systematic variation of ΔKth and ΔKeff, th with PAGS. The mechanisms of intergranular fracture vary between grain sizes in this temper. A transition from “microstructure-sensitive” to “microstructure-insensitive” crack growth has been found to occur when the zone of cyclic deformation at the crack tip becomes more or less equal to PAGS. Detailed observations on fracture morphology and crack paths corroborate the grain size effects on fatigue thresholds and crack closure.
Resumo:
The nuclear, aerospace, naval and missile industries place emphasis on materials with high structural integrity and reliable performance so as to meet certain stringent requirements in service. Strength is not the only criterion for selection. Properties such as fatigue resistance. impact toughness and fracture toughness are equally important. Electroslag refining (ESR) has been used widely and successfully over the years for improving the fatigue resistance, creep resistance, impact strength and fracture toughness of steels and alloy steels. But application of ESR to aluminium alloys is only a recent endeavour. A high-strength aircraft aluminium alloy IS: 7670 was therefore chosen for studies on the fatigue strength and the impact and fracture toughness. The results indicate that the fatigue resistance is considerably improved after refining and that the impact strength and fracture toughness of the refined alloy are comparable with that of the unrefined alloy.
Resumo:
Mechanical alloying (MA) pioneered by Benjamin is a technique for the extension of solid solubility in systems where the equilibrium solid solubility is limited. This technique has, in recent years, emerged as a novel alternate route for rapid solidification processing (RSP) for the production of metastable crystalline, quasicrystalline, amorphous phases and nanocrystalline materials. The glass-forming composition range (GFR), in general, is found to be much wider in case of MA in comparison with RSP. The amorphous powders produced by MA can be compacted to bulk shapes and sizes and can be used as precursors to obtain high strength materials. This paper reports the work done on solid state amorphization by MA in Ti-Ni-Cu and Al-Ti systems where a wide GFR has been obtained. Al-Ti is a classic case where no glass formation has been observed by RSP, while a GFR of 25–90 at.% Ti has been obtained in this system, thus demonstrating the superiority of MA over RSP. The free energy calculations made to explain GFR are also presented.
Resumo:
Owing to their high strength-to-weight ratio, excellent mechanical properties and corrosion resistance, titanium (Ti) and its alloys, especially (alpha+beta) alloys like Ti-6Al-4V is the backbone materials for aerospace, energy, and chemical industries. Trace boron addition (similar to 0.1 wt. %) to the alloy Ti-6Al-4V produces a reduction in as-cast grain size by roughly an order of magnitude resulting in enhanced ductility, higher stiffness, strength and good fracture resistance. Boron addition could also affect the evolution of texture and microstructure in the material. The solidification microstructures of Boron free as well as Boron containing Ti-6Al-4V are found to be almost homogeneous from periphery towards the center of as-cast ingot in terms of both alpha-colony size and distribution. Boron addition substantially reduces alpha-colony size (similar to 50-80 mu m). A gradual change in alpha texture from periphery towards the center has been observed with orientations close to specific texture components suggesting the formation of texture zones. The mechanism of texture evolution can be visualized as a result of variant selection during solidification through (alpha+beta) phase field.
Resumo:
Rapid solidification of a ternary Al-Cu-Zr alloy results in a nanocomposite microstructure. In this study, melt spinning a Al82Cu15Zr3 alloy has resulted in the combined occurrence of, (a) 0.5 mu m sized grains of Al solid solution and (b) fine grains (10-20 nm) of intermetallic Al2Cu (theta) and alpha-Al, along side each other. The larger alpha-Al grains contain nanometric GP zones, with the Zr addition resulting in a grain refinement. In the other type of microstructure Zr promotes simultaneous nucleation of nanosized grains of the two equilibrium phases, Al2Cu and alpha-Al. Both these lead to a very high hardness of similar to 540 VHN for this alloy and can be used as a candidate for a high strength alloy with good ductility at a low strain rate.
Resumo:
Full-scale test embankments, with and without geotextile reinforcement, were constructed on soft Bangkok clay. The performances of these embankments are evaluated and compared with each other on the basis of field measurements and FEM analysis. The analyses of failure mechanisms and the investigations on the embankment stability using undrained conditions were also done to determine the critical embankment height and the corresponding geotextile strain. The high-strength geotextile can reduce the plastic deformation in the underlying foundation soil, increase the collapse height of the embankment on soft ground, and produce a two-step failure mechanism. In this case study, the critical strain in the geotextile corresponding to the primary failure of foundation soils may be taken as 2.5-3% irrespective of the geotextile reinforcement stiffness. (C) 2002 Elsevier Science Ltd. All rights reserved.
Resumo:
This article presents the deformation behavior of high-strength pearlitic steel deformed by triaxial compression to achieve ultra-fine ferrite grain size with fragmented cementite. The consequent evolution of microstructure and texture has been studied using scanning electron microscopy, electron back-scatter diffraction, and X-ray diffraction. The synergistic effect of diffusion and deformation leads to the uniform dissolution of cementite at higher temperature. At lower temperature, significant grain refinement of ferrite phase occurs by deformation and exhibits a characteristic deformation texture. In contrast, the high-temperature deformed sample shows a weaker texture with cube component for the ferrite phase, indicating the occurrence of recrystallization. The different mechanisms responsible for the refinement of ferrite as well as the fragmentation of cementite and their interaction with each other have been analyzed. Viscoplastic self-consistent simulation was employed to understand deformation texture in the ferrite phase during triaxial compression.