45 resultados para cast irons


Relevância:

20.00% 20.00%

Publicador:

Resumo:

There have been reported attempts of producing Cu based MMCs employing solid phase routes. In this work, copper was reinforced with short carbon fibres by pressure infiltration (squeeze casting) of molten metal through dry-separated carbon fibres. The resulting MMC's microstructure revealed uniform distribution of fibres with minimum amount of clustering. Hardness values are considerably higher than that for the unreinforced matrix. Addition of carbon fibres has brought in strain in the crystal lattice of the matrix, resulting in higher microhardness of MMCs and improved wear resistance. Tensile strength values of MMCs at elevated temperatures are considerably higher than that of the unreinforced matrix processed under identical conditions. (C) 1999 Kluwer Academic Publishers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Properties of cast aluminium matrix composites are greatly influenced by the nature of distribution of reinforcing phase in the matrix and matrix microstructural length scales, such as grain size, dendrite arm spacing, size and morphology of secondary matrix phases, etc. Earlier workers have shown that SIC reinforcements can act as heterogeneous nucleation sites for Si during solidification of Al-Si-SiC composites. The present study aims at a quantitative understanding of the effect of SiC reinforcements on secondary matrix phases, namely eutectic Si, during solidification of A356 Al-SiC composites. Effect of volume fraction of SiC particulate on size and shape of eutectic Si has been studied at different cooling rates. Results indicate that an increase in SiC volume fraction leads to a reduction in the size of eutectic Si and also changes its morphology from needle-like to equiaxed. This is attributed to the heterogeneous nucleation of eutectic Si on SiC particles. However, SiC particles are found to have negligible influence on DAS. Under all the solidification conditions studied in the present investigation, SiC particles are found to be rejected by the growing dendrites. (C) 1999 Elsevier Science Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effect of Fe content (0.2 to 0.6 pct) on the microstructure and mechanical properties of a cast Al-7Si-0.3Mg (LM 25/356) alloy has been investigated. Further, 1 pct mischmetal (MM) additions (a mixture of rare-earth (RE) elements) were made to these alloys, and their mechanical properties at room and at elevated temperatures (up to 200 degreesC) were evaluated. A structure-property correlation on this alloy was attempted using optical microstructure analysis, fractographs, X-ray diffraction, energy-dispersive analysis of X-rays (EDX), and quantitative metallography by image analysis. An increase in Fe content increased the volume percentage of Fe-bearing intermetallic compounds (beta and pi phases), contributing to the lower yield strength (YS), ultimate tensile strength (UTS), percentage elongation, and higher hardness. An addition of 1 pct MM to the alloys containing 0.2 and 0.6 pct Fe was found to refine the microstructure; modify the eutectic silicon and La, Ce, and Nd present in the MM; form different intermetallic compounds with Al, Si, Fe, and Mg; and improve the mechanical properties of the alloys both at room and elevated temperatures.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Processing maps have been developed for hot deformation of Mg-2Zn-1Mn alloy in as-cast condition and after homogenization with a view to evaluate the influence of homogenization. Hot compression data in the temperature range 300-500degreesC and strain rate range 0.001-100 s(-1) were used for generating the processing map. In the map for the as-cast alloy the domain of dynamic recrystallization occurring, at 450degreesC and 0.1 s(-1) has merged with another domain occurring at 500degreesC and 0.001 s(-1) representing grain boundary cracking. The latter domain is eliminated by homogenization and the dynamic recrystallization domain expanded with a higher peak efficiency occurring at 500 degreesC and 0.05 s(-1). The flow localization occurring at strain rates higher than 5 s(-1) is unaffected by homogenization.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Demand for cost-effective manufacturing techniques led to the development of near-net-shape processes. Squeeze casting is one such established effort. This process enjoys the combined merits of casting and forging. Squeeze casting imparts soundness comparable to that of wrought products while maintaining isotropic nature. Aluminum alloys and zinc alloys have been successfully processed through squeeze casting, but copper and copper alloys do not seem to have been attempted. Considering the capability of squeeze casting process, it is reasonable to expect properties different from that of conventionally cast copper. This paper presents the details of a systematic investigation wherein optimum process parameters for the squeeze casting of pure copper were established. Microstructure of squeeze-cast copper has been found to be significantly different from that of conventionally cast copper, and the dendrite arm spacing is much smaller. In addition to the room temperature mechanical properties, elevated temperature properties of copper are also appreciably improved by squeeze casting.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, we report a significant improvement in mechanical and oxidation properties of near eutectic Nb-Si alloys by the addition of aluminum (Al) and control of microstructural length scale. A comparative study of two alloys Nb-18.79at%Si and Nb-12.3at%Si-9at%Al were carried out. The processing for microstructure refinements were carried out by vacuum suction casting in water cooled thick copper mould. It is shown that addition of Al suppresses Nb3Si phase and promotes beta Nb5Si3 phase under nonequilibrium solidification condition. The microstructural length scale and in particular eutectic spacing reduces significantly to 50-100 nm in suction cast ternary alloy. A detailed TEM study shows the presence of delta-Nb11Si4 phase in Nb matrix. The hardness of Nb solid solution can be increased as a consequence to a level observed in Nb3Si intermetallic due to the well oriented precipitates. Compression test yields the ultimate strength of 1.8 +/- 0.1 GPa and engineering strain of 2.3 +/- 0.03%. In comparison, the binary Nb-18.79 at% Si alloy possesses an ultimate strength of 1.35 +/- 0.1 GPa and strain of 0.2 +/- 0.01% when processed under identical conditions. The latter exhibits coarser microstructural length scale (300-400 nm) and a brittle behavior. The indentation fracture toughness of Al containing suction cast alloy shows a value of 20.2 +/- 0.5 MPa root m which represents a major improvement over bulk Nb-Si eutectic alloy. The detailed thermal studies confirm a multifold improvement in oxidation resistance up to 1000 degrees C. (C) 2012 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Disks of a cast Al-7 % Si alloy were processed through high-pressure torsion (HPT) for 1/4, 1/2, 1, 5, and 10 revolutions under a pressure of 6.0 GPa and at temperatures of 298 and 445 K. The hardness of the samples after processing was significantly higher than in the cast sample, and the hardness profiles across the samples became more uniform with increasing numbers of turns. Processing at higher temperature gave lower hardness values. Experiments were conducted to examine the effects of HPT processing on various microstructural aspects of the cast Al-7 % Si alloy such as the grain size, the Taylor factor, and the fraction of high-angle grain boundaries. The results demonstrate that there is a correlation between trends in the microhardness values and the observed microstructures.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Aluminum scandium binary alloys represent a promising precipitation-hardening alloy system. However, the hardness of the binary alloys decreases with the rapid coarsening of Al3Sc precipitate during high-temperature aging. In the current study, we report a new approach to compensate for the loss of mechanical properties by combining rapid solidification with very small ternary addition of transition metal Ni. This addition yields dispersion, and at a critical concentration improves the mechanical properties. We explore additions of a maximum of 0.06 at. pct of Nickel to a binary Al-0.14 at. pct Sc alloy, which yield nickel-rich dispersions. We report two kinds of biphasic dispersions containing AlNi2Sc/Al9Ni2 and alpha-Al/Al9Ni2 phase combinations. The maximum improvement in mechanical properties occurs with the addition of 0.045 at. pct Ni with a yield strength of 239 +/- A 7 MPa for an aging treatment at 583 K (310 A degrees C) for 15 hours. DOI: 10.1007/s11661-013-1624-z (C) The Minerals, Metals & Materials Society and ASM International 2013

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The paper reports effect of small ternary addition of In on the microstructure, mechanical property and oxidation behaviour of a near eutectic suction cast Nb-19.1 at-%Si-1.5 at-%In alloy. The observed microstructure consists of a combination of two kinds of lamellar structure. They are metal-intermetallic combinations of Nb-ss-beta-Nb5Si3 and Nb-ss-alpha-Nb5Si3 respectively having 40-60 nm lamellar spacings. The alloy gives compressive strength of 3 GPa and engineering strain of similar to 3% at room temperature. The composite structure also exhibits a large improvement in oxidation resistance at high temperature (1000 degrees C).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The solidification pathways of Nb rich Nb-Si alloys when processed under non-equilibrium conditions require understanding. Continuing with our earlier work on alloying additions in single eutectic composition 1,2], we report a detailed characterization of the microstructures of Nb-Si binary alloys with wide composition range (10-25 at% Si). The alloys are processed using chilled copper mould suction casting. This has allowed us to correlate the evolution of microstructure and phases with different possible solidification pathways. Finally these are correlated with mechanical properties through studies on deformation using mechanical testing under indentation and compressive loads. It is shown that microstructure modification can significantly influence the plasticity of these alloys.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The stress states in Si particles of cast Al-Si based alloys depend on its morphology and the heat treatment given to the alloy. The Si particles fracture less on modification and fracture more in the heat treated condition. An attempt has been made in this work to study the effect of heat treatment and Si modification on the stress states of the particles. Such understanding will be valuable for predicting the ductility of the alloy. The stress states of Si particles are estimated by Raman technique and compared with the microstructure-based FEM simulations. Combination of Electron Back-Scattered Diffraction (EBSD) and frequency shift, polarized micro-Raman technique is applied to determine the stress states in Si particles with (111) orientations. Stress states are measured in the as-received state and under uniaxial compression. The residual stress, the stress in the elastic-plastic regime and the stress which causes fracture of the particles is estimated by Raman technique. FEM study demonstrates that the stress distribution is uniform in modified Si, whereas the unmodified Si shows higher and more complex stress states. The onset of plastic flow is observed at sharp corners of the particles and is followed by localization of strain between particles. Clustering of particles generates more inhomogeneous plastic strain in the matrix. Particle stress estimated by Raman technique is in agreement with FEM calculations. (C) 2014 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effects of combined additions of Ca and Sb on the microstructure and tensile properties of AZ91D alloy fabricated by squeeze-casting have been investigated. For comparison, the same has also been studied with and without individual additions of Ca and Sb. The results indicate that both individual and combined additions refine the grain size and beta-Mg17Al12 phase, which is more pronounced with combined additions. Besides alpha-Mg and beta-Mg17Al12 phases, a new reticular Al2Ca and rod-shaped Mg3Sb2 phases are formed following individual additions of Ca and Sb in the AZ91D alloy. With combined additions, an additional Ca2Sb phase is formed suppressing Mg3Sb2 phase. Additions of both Ca and Sb increase yield strength (YS) at both ambient and elevated temperatures up to 200 degrees C. However, both ductility and ultimate tensile strength (UTS) decrease first up to 150 degrees C and then increase at 200 degrees C. The increase in YS is attributed to the refinement of grain size, whereas, ductility and UTS are deteriorated by the presence of brittle Al2Ca, Mg3Sb2 and Ca2Sb phases. The best tensile properties are obtained in the AZXY9110 alloy owing to the presence of lesser amount of brittle Al2Ca and Ca2Sb phases resulted from the optimum content of 1.0Ca and 0.3Sb (wt%). The fracture surface of the tensile specimen tested at ambient temperature reveals cleavage failure that changes to quasi-cleavage at 200 degrees C. The squeeze-cast alloys exhibited better tensile properties as compared to that of the gravity-cast alloys nullifying the detrimental effects of Ca and/or Sb additions. (C) 2014 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

It has been previously reported that the addition of boron to Ti-6Al-4V results in significant refinement of the as-cast microstructure and enhancement in the strain hardening. However, the mechanism for the latter effect has not been adequately studied. The aim of this study was to understand the reasons for the enhancement in room temperature strain hardening on addition of boron to as cast Ti-6Al-4V alloy. A study was conducted on slip transmission using SEM, TEM, optical profilometry and four point probe resistivity measurements on un-deformed and deformed samples of Ti-6Al-4V-xB with five levels of boron. Optical profilometry was used to quantify the magnitude of offsets on slip traces which in turn provided information about the extent of planar or multiple slip. Studies on deformed samples reveal that while lath boundaries appear to easily permit dislocation slip transmission, colony boundaries are potent barriers to slip. From TEM studies it was also observed that while alloys containing lower boron underwent planar slip, deformation was more homogeneous in higher boron alloys due to multiple slip resulting from large number of colony boundaries. Multiple slip is also proposed to be the prime cause of the enhanced strain hardening.