364 resultados para Solvent-free


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Sn4+-doped In2O3 (ITO) is a benchmark transparent conducting oxide material. We prepared ligand-free but colloidal ITO (8nm, 10% Sn4+) nanocrystals (NCs) by using a post-synthesis surface-modification reaction. (CH3)(3)OBF4 removes the native oleylamine ligand from NC surfaces to give ligand-free, positively charged NCs that form a colloidal dispersion in polar solvents. Both oleylamine-capped and ligand-free ITO NCs exhibit intense absorption peaks, due to localized surface plasmon resonance (LSPR) at around =1950nm. Compared with oleylamine-capped NCs, the electrical resistivity of ligand-free ITO NCs is lower by an order of magnitude (approximate to 35mcm(-1)). Resistivity over a wide range of temperatures can be consistently described as a composite of metallic ITO grains embedded in an insulating matrix by using a simple equivalent circuit, which provides an insight into the conduction mechanism in these systems.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nanocrystalline powders of Ba1-xMgxZr0.1Ti0.9O3 (x = 0.025-0.1) were synthesized via citrate assisted sol-gel method. Interestingly, the one with x = 0.05 in the system Ba1-xMgxZr0.1Ti0.9O3 exhibited fairly good piezoelectric response aside from the other physical properties. The phase and structural confirmation of synthesized powder was established by X-ray powder diffraction (XRD) and Raman Spectroscopic techniques. Two distinct Raman bands i.e., 303 and 723 cm(-1) characteristic of tetragonal phase were observed. Thermogravimetric analysis (TGA) was performed to evaluate the phase decomposition of the as-synthesized Ba0.95Mg0.05Zr0.1Ti0.9O3 sample as a function of temperature. The average crystallite size associated with Ba0.95Mg0.05Zr0.1Ti0.9O3 was calculated using Scherrer formula based on the XRD data and was found to be 25 nm. However, Scanning and Transmission Electron Microscopy studies revealed the average crystallite size to be in the range of 30-40 nm, respectively. Kubelka-Munk function was employed to determine the optical band gap of these nanocrystallites. A piezoelectric response of 26 pm/V was observed for Ba0.95Mg0.05Zr0.1Ti0.9O3 nanocrystal by Piezoresponse Force Microscopy (PFM) technique. Photoluminescence (PL) study carried out on these nanocrystals exhibited a blue emission (470 nm) at room temperature.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Dynamics of contact free (levitated) drying of nanofluid droplets is ubiquitous in many application domains ranging from spray drying to pharmaceutics. Controlling the final morphology (macro to micro scales) of the dried out sample poses some serious challenges. Evaporation of solvent and agglomeration of particles leads to porous shell formation in acoustically levitated nanosilica droplets. The capillary pressure due to evaporation across the menisci at the nanoscale pores causes buckling of the shell which leads to ring and bowl shaped final structures. Acoustics plays a crucial role in flattening of droplets which is a prerequisite for initiation of buckling in the shell: Introduction of mixed nanocolloids (sodium dodecyl sulfate + nanosilica) reduces evaporation rate, disrupts formation of porous shell, and enhances mechanical strength of the shell, all of which restricts the process of buckling. Although buckling is completely arrested in such surfactant added droplets, controlled external heating using laser enhances evaporation through the pores in the shell due to thermally induced structural changes and rearrangement of SDS aggregates which reinitializes buckling in such droplets, Furthermore, inclusion of anilinium hydrochloride into the nanoparticle laden droplets produces ions which adsorb and modify the morphology of sodium dodecyl sulfate crystals and reinitializes buckling in the shell (irrespective of external heating conditions). The kinetics of buckling is determined by the combined effect of morphology of the colloidal particles, particle/aggregate diffusion rate within the droplet, and the rate of evaporation of water. The buckling dynamics leads to cavity formation which grows subsequently to yield final structures with drastically different morphological features. The cavity growth is controlled by evaporation through the nanoscate pores and exhibits a universal trend irrespective of heating rate and nanoparticle type.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Na0.5Bi0.5TiO3- based lead-free piezoelectrics exhibiting giant piezostrain are technologically interesting materials for actuator applications. The lack of clarity with regard to the structure of the nonpolar phase of this system has hindered the understanding of the structural mechanism associated with the giant piezostrain and other related phenomena. In this paper, we have investigated the structure and field-induced phase transformation behavior of a model system (0.94 - x) Na0.5Bi0.5TiO3-0.06BaTiO(3)-xK(0.5)Na(0.5)NbO(3) (0.0 <= x <= 0.025). A detailed structural analysis using neutron powder diffraction revealed that the nonpolar phase is neither cubic nor a mixture of rhombohedral (R3c) and tetragonal (P4bm) phases as commonly reported in literature but exhibits a long-period modulated structure, which is most probably of the type root 2 x root 2 x n with n = 16. Our results suggest that the giant piezoelectric strain is associated with a field-induced phase transformation of the long-period modulated structure to rhombohedral R3c structure above a critical field. We also demonstrate that the giant piezostrain is lost if the system retains a fraction of the field-induced R3c phase. A possible correlation among depolarization temperature, giant piezostrain, and its electrical fatigue behavior has also been indicated.