Automated synthesis of mechanical designs is an important step towards the development of an intelligent CAD system. Research into methods for supporting conceptual design using automated synthesis has attracted much attention in the past decades. The research work presented here is based on an empirical study of the process of synthesis of multiple state mechanical devices. As a background to the work, the paper explores concepts of what mechanical device, state, single state and multiple state are, and in the context of the above observational studies, attempts to identify the outstanding issues for supporting multiple state synthesis of mechanical devices.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Electrical transport measurements on ultrathin single-crystalline Au nanowires, synthesized via a wet chemical route, show an unexpected insulating behavior. The linear response electrical resistance exhibits a power-law dependence on temperature. In addition, the variation of current over a wide range of temperature and voltage obeys a universal scaling relation that provides compelling evidence for a non-Fermi liquid behavior. Our results demonstrate that the quantum ground state In ultrathin nanowires of simple metallic systems can be radically different from their bulk counterparts and can be described In terms of a Tomonaga-Luttinger liquid (TLL), in the presence of remarkably strong electron-electron interactions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The approach taken in this paper in order to modify the scattering features of electrons and phonons and improve the figure of merit (ZT) of thermoelectric PbTe is to alter the microstructure at constant chemistry. A lamellar pattern of PbTe/GeTe at the nano- and microscale was produced in Pb(0.36)Ge(0.64)Te alloy by the diffusional decomposition of a supersaturated solid solution. The mechanism of nanostructuration is most likely a discontinuous spinodal decomposition. A simple model relating the interface velocity to the observed lamellar spacing is proposed. The effects of nanostructuration in Pb(0.36)Ge(0.64)Te alloy on the electrical and thermal conductivity, thermopower and ZT were investigated. It was shown that nanostructuration through the formation of a lamellar pattern of PbTe/GeTe is unlikely to provide a significant improvement due to the occurrence of discontinuous coarsening. However, the present study allows an analysis of possible strategies to improve thermoelectric materials via optimal design of the microstructure and optimized heat treatment. (C) 2011 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The solubility of oxygen in liquid gallium in the temperature range 775 –1125 °C and in liquid gallium-copper alloys at 1100 °C, in equilibrium with β-Ga2O3, has been measured by an isopiestic equilibrium technique. The solubility of oxygen in pure gallium is given by the equation log (at.% O) = −7380/T + 4.264 (±0.03) Using recently measured values for the standard free energy of formation of β-Ga2O3 and assuming that oxygen obeys Sievert's law up to the saturation limit, the standard free energy of solution of oxygen in liquid gallium may be calculated : View the MathML sourceΔ°298 = −52 680 + 6.53T (±200) cal where the standard state for dissolved oxygen is an infinitely dilute solution in which the activity is equal to atomic per cent. The effect of copper on the activity of oxygen dissolved in liquid gallium is found to be in good agreement with that predicted by a recent quasichemical model in which it was assumed that each oxygen is interstitially coordinated to four metal atoms and that the nearest neighbour metal atoms lose approximately half their metallic cohesive energies.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The solubility of oxygen in liquid germanium in the temperature range 1233 to 1397 K, and in liquid germanium-copper alloys at 1373 K, in equilibrium with GeO2 has been measured by the phase equilibration technique. The solubility of oxygen in pure germanium is given by the relation R470 log(at. pct 0)=-6470/T+4.24 (±0.07). The standard free energy of solution of oxygen in liquid germanium is calculated from the saturation solubility, and recently measured values for the free energy of formation of GeO2, assuming that oxygen obeys Sievert’s law up to the saturation limit. For the reaction, 1/2 O2(g)→ OGe ΔG° =-39,000 + 3.21T (±500) cal = -163,200 + 13.43T (±2100) J. where the standard state for dissolved oxygen is that which makes the value of activity equal to the concentration (in at. pct), in the limit, as concentration approaches zero. The effect of copper on the activity of oxygen dissolved in liquid germanium is found to be in good agreement with that predicted by a quasichemical model in which each oxygen was assumed to be bonded to four metal atoms and the nearest neighbor metal atoms to an oxygen atom are assumed to lose approximately half of their metallic bonds.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Measurements on the solid electrolyte cell(Ar -b H2 ~ H2S/CaS + CaF2 ~- ( P t ) / / C a F 2 / / ( P t )-~- CaF2 ~ CaS/H2S ~- H2 ~- At) show that the emf of the cell is directly related through the Nernst equation to the difference in sulfur potentials established at the two Ar ~- H2 ~ H2S/electrode interfaces. The electrodes are designed to convert the sulfur potential gradient across the calcium fluoride electrolyte into an equivalent fluorine potential gradient with the aid of the reaction, CaF2(s) ~ 1~ S2(g)-e CaS(s) ~- F2(g). The response time of the probe varies from approximately 9 hr at 990~ to 2.5 hr at 1225~ The conversion of calcium sulfide and/or calcium fluoride into calcium oxide should not be a problem in anticipated commercial coal gasification systems. Suggestions are presented for improving the cell for such commercial applications.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conductivity measurements as a function of temperature and partial pressures of SOs, SO2, and O2, and transference experiments indicate that the transport number of Na + ions is unity in Na2SO4-I. A concentration cell based on this electrolyte Pt, O2' + SO2' + SOs'/Na2SO4-I/SOa" + SO~" + O~", Pt produces emf's that are in agreement with those calculated from the Nernst equation when equilibrium is assumed between the gas species at the electrodes. The cell can be used for monitoring the SO#SOs pollution in air, and in combination with an oxygen probe can be used for the determination of SO=/SOs concentrations in coal combustion reactors, for the evaluation of the partial pressure of $2 in coal gasification systems, and for emission control in nonferrous smelters using sulfide ores. The probe is similar to that developed recently by Gauthier et aL (4, 5) using K=SO4 as the electrolyte, but can operate at higher pressures of SO3. Because of the greater polarizing power of the Na+ ion compared to the K + ion, Na2S207 is less stable and can be formed only at a considerably higher pressure of S03 than that required for K~20~.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The solubility limit of oxygen in liquid antimony has been measured by a novel isopiestic technique in the temperature range 995--1175 deg K. The results can be expressed by the equation log c = --5500/T + 3.754 ( plus/minus 0.04) with c in at.% O and T in deg K. The oxygen potential over Sb + O alloys equilibrium with Sb2O3 has been measured by a solid state cell using a fully stabilized CaO.ZrO2 electrolyte. The cell was designed to contain the Sb + Sb2O3 mixture in a closed volume, that the vaporization of the oxide can be minimized and true equilibrium attained. The Gibbs free energy of the reaction 2 Sb(s) + 3/2 O2 = Sb2O3(s) is Delta G deg = --719560 + 274.51 T( plus/minus 500) and Sb(l) + 3/2 O2 = Sb2O3(l), Delta G deg = --704711 + ( plus/minus 500) ( Delta G deg in J/mole, T in deg K). The combination of these results with Sieverts' law yields the standard free energy of solution of oxygen in liquid antimony according to the reaction 1/2 O2 = \O\Sb,at.% as Delta G deg = --129620 + 14.23 T ( plus/minus 950). The standard enthalopy and entropy of the solution of oxygen in Sb are compared with values for other metal- oyxgen systems, and with the standard enthalpies of formation of corresponding oxides. The resulting correlations permit the estimation of the standard free energy of solution of oxygen in pure metals for which experimental information is lacking. 24 ref.--AA

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A critical revi<:w of the possibilities of measuring the ~artlal pressure of sulfur using solid state galvanic cells )'n;;cd on AgI, C" , B-alumina, CaO-Zr02' Na2S04-I and doped ;:":;, ,,,Ilil "Iltl ,,11: auxiliary "jectrodes are presentlOu. SOIll..., df tllc!iL' sYHtcmH h,}vu inherent limltntlol1$ when <:xl'o" ...d to environments contilining both oxygen and sulfur. Electrode polarization due to electronic conduction in the solid electrolyte is a significant factor limiting the ;lC'e,"'acy of isotlwrm:l1 cell",. The electrochemical flux of{lit' !'\)ndlwl Ill}: Ion LhnHO',h tht' ('!('ctrojyt(~ C:Ul },(,! llIinlnliz(,{j pfUjJL!f cell. dL:~) i.t',11. Noni!:iot.herm~ll cells \.Jlth temperaLure compensated reference electrodes have a number of advantages over thC'ir isothermal counterparts.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The limiting solubility of oxygen in liquid nickel in equilibrium withα-alumina and nickel aluminate has been measured by inert gas fusion analysis of suction samples in the temperature range 1730 to 1975 K. The corresponding oxygen potential has been monitored by a solid electrolyte cell consisting of calcia stabilized zirconia as the electrolyte and Mo + MoO2 as the reference electrode. The results can be summarized by the following equations: log(at. pct O) = \frac - 10,005T + 4.944 ( ±0.015)log(atpctO)=T−10005+4944(0015) % MathType!MTEF!2!1!+-% feaafiart1ev1aaatCvAUfeBSjuyZL2yd9gzLbvyNv2CaerbuLwBLn DmO2 /4.606RT = log P O2 1/2 = \frac - 13,550T + 4.411 ( ±0.009)O24606RT=logPO212=T−13550+4411(0009) From simultaneous measurements of the potential and concentration of oxygen in melts, not in thermodynamic equilibrium with alumina and aluminate phases, information on the composition dependence of the activity coefficient and the standard free energy of solution of oxygen is obtained. For the reaction, $\frac{1}{2} O_2 \to \underset{\raise0.3em\hbox{$Missing close brace ΔG o = -72,930 - 7.11T (±840) J gr.at.–1 = + 0.216 at. pct OlogfO=T−500+0216atpctO where the standard state for dissolved oxygen is that which makes the value of activity equal to the concentration (in at. pct) in the limit as concentration approaches zero. The oxygen solubility in liquid nickel in equilibrium with solid NiO, evaluated from thermodynamic data, is compared with information reported in the literature. Implications of the results to the deoxidation equilibria of aluminum in nickel are discussed.