251 resultados para fracture resistance


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The characterisation of cracks is usually done using the well known three basic fracture modes, namely opening, shearing and tearing modes. In isotropic materials these modes are uncoupled and provide a convenient way to define the fracture parameters. It is well known that these fracture modes are coupled in anisotropic materials. In the case of orthotropic materials also, coupling exists between the fracture modes, unless the crack plane coincides with one of the axes of orthotropy. The strength of coupling depends upon the orientation of the axes of orthotropy with respect to the crack plane and so the energy release rate components associated with each of the modes vary with crack orientation. The variation, of these energy release rate components with the crack orientation with respect to orthotropic axes, is analyzed in this paper. Results indicate that in addition to the orthotropic planes there exists other planes with reference to which fracture modes are uncoupled.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

D.C. electrical conductivity of polyaniline (33%,40%) blended with PMMA was measured from 5K to 300mK. The conductivity behaviour is consistent with fluctuation induced tunneling. Magneto-resistance (MR) was measured between 300K and 2K. From 20K to 2K, a large positive MR was observed. At 2K, for low magnetic fields (<1 Tesla), a deviation from the normal H-2 behaviour was observed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Total strain controlled low cycle fatigue tests on 316L(N) stainless steel have been conducted in air at various strain rates in the temperature range of 773-873 K to identify the operative time-dependent mechanisms and to understand their influence on the cyclic deformation and fracture behaviour of the alloy. The cyclic stress response at all the testing conditions was marked by an initial hardening followed by stress saturation. A negative strain rate stress response is observed under specific testing conditions which is attributed to dynamic strain ageing (DSA). Transmission electron microscopy studies reveal that there is an increase in the dislocation density and enhanced slip planarity in the DSA regime. Fatigue life is found to decrease with a decrease in strain rate. The degradation in fatigue resistance is attributed to the detrimental effects associated with DSA and oxidation. Quantitative measurement of secondary cracks indicate that both transgranular and intergranular cracking are accelerated predominantly under conditions conducive to DSA.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In the present study a two dimensional model is first developed to show the behaviour of dense non-aqueous phase liquids (DNAPL) within a rough fracture. To consider the rough fracture, the fracture is imposed with variable apertures along its plane. It is found that DNAPL follows preferential pathways. In next part of the study the above model is further extended for non-isothermal DNAPL flow and DNAPL-water interphase mass transfer phenomenon. These two models are then coupled with joint deformation due to normal stresses. The primary focus of these models is specifically to elucidate the influence of joint alteration due to external stress and fluid pressures on flow driven energy transport and interphase mass transfer. For this, it is assumed that the critical value for joint alteration is associated with external stress and average of water and DNAPL pressures in multiphase system and the temporal and spatial evolution of joint alteration are determined for its further influence on energy transport and miscible phase transfer. The developed model has been studied to show the influence of deformation on DNAPL flow. Further this preliminary study demonstrates the influence of joint deformation on heat transport and phase miscibility via multiphase flow velocities. It is seen that the temperature profile changes and shows higher diffusivity due to deformation and although the interphase miscibility value decreases but the lateral dispersion increases to a considerably higher extent.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We demonstrate that the low-frequency resistance uctuations, or noise, in bilayer graphene is strongly connected to its band structure, and displays a minimum when the gap between the conduction and valence band is zero. Using double-gated bilayer graphene devices we have tuned the zero gap and charge neutrality points independently, which oers a versatile mechanism to investigate the low-energy band structure, charge localization and screening properties of bilayer graphene.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In a continuation of the authors' recent work, the ultimate tip resistance of a miniature cone using triaxial equipment was determined for samples of dry sand mixed with dry fly ash. The effect of (i) the proportion of fly ash, (ii) the relative density of samples, and (iii) the vertical overburden pressure was examined. It was noted that an addition of fly ash in sand for the same range of relative density leads to a significant reduction in the ultimate tip resistance of the cone (q(cu)). This occurs due to a decrease in the friction angle (phi) of the sample with an increase in the fly ash content for a given relative density. For phi greater than about 30 degrees, two widely used correlation curves from published literature, providing the relationships between q(cu) and phi for cohesionless soils, were found to provide satisfactory predictions, even for sand - fly ash mixtures. As was expected, the values of qcu increase continuously with an increase in the relative density of the soil mass and the vertical effective ( overburden) stress on the sample.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We demonstrate that the low-frequency resistance fluctuations, or noise, in bilayer graphene are strongly connected to its band structure and display a minimum when the gap between the conduction and valence band is zero. Using double-gated bilayer graphene devices we have tuned the zero gap and charge neutrality points independently, which offers a versatile mechanism to investigate the low-energy band structure, charge localization, and screening properties of bilayer graphene.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

En 52 steel has been electroslag refined and the resultant effects of refining on its mechanical properties have been assessed. It was found that refining caused a decrease in fatigue crack growth rates and increases in fatigue strength, fracture toughness, Charpy fracture energy and tensile ductility. Fatigue crack growth rates in region I and in region III were found to be considerably lower in the electroslag refined steel: they were unaffected in region II. The fracture toughness values for the electroslag refined steel are nearly twice those estimated for the unrefined steel. Measurements on heat-treated samples have shown that the electroslag refined steel has a better response to heat-treatment. The improvement in the mechanical properties is explained in terms of the removal of nonmetallic inclusions and a reduction in the sulphur content of the steel.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The AISI 4340 steel has been electroslag refined and the improvement in mechanical properties has been assessed. Electroslag refining (ESR) has improved tensile ductility, plane strain fracture toughness, Charpy fracture energy, and has decreased fatigue crack growth rates. The KIC values for the ESR steel are nearly twice those estimated in the unrefined steel and higher than those obtained in the vacuum arc remelted steel. Fatigue crack growth rates in region I and in region III are found to be decreased considerably in the ESR steel, while they are unaffected in region II. Measurements on heat treated samples have shown that the ESR steel has a better response to heat treatment. Both the suggested heat treatments namely austenitizing at 1140–1470 K as well as the conventional heat treatment of austenitizing at 1140 K have been followed. The improvement in the mechanical properties of ESR steel has been explained on the basis of removal of nonmetallic inclusions and reduction in sulfur content in the steel.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The changes in the tensile properties and fracture mode brought about by heat treatment of Fe-12Cr-6Al ferritic stainless steel have been studied. A favourable combination of high strength and good ductility is obtained by heating the material at 1370 K for 2 h followed by a water quench. The high-temperature treatment results in carbide dissolution as well as an increase in the grain size. The mechanism of strengthening has been evaluated from the apparent activation energy (28 kJ mol–1) and is identified to be the unpinning of dislocations from the atmosphere of carbon atoms. As the heat-treatment temperature is increased, the fracture behaviour changes from ductile to brittle mode and this is related to the changes in grain size and friction stress.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The occurrence of a maximum in the percentage of intergranular fracture on the fracture surface during the transition from intermediate to low fatigue crack growth rates has been observed for a high strength steel. It is suggested that transgranular planar slip leading to slip localization is essential in promoting intergranular fracture when the cyclic plastic zone size becomes equal to the prior austenite grain size.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

One of the problems associated with outdoor polymeric insulators is tracking and erosion of the weathershed which can directly influence the reliability of the power system. Flame retardants are added to the base material to enhance its tracking and erosion resistance. Hydroxide fillers are regarded as the best flame retardants. This paper deals with studies related to nano - sized magnesium dihydroxide (MDH) and micron-sized Alumina Trihydrate (ATH) fillers as flame retardants in RTV silicone rubber. Tracking and erosion resistance studies were carried out on MDH and ATH silicone rubber composites using an inclined plane tracking and erosion (IPT) resistance tester. The MDH filled (5% by wt) composites performed much better than ATH composites in terms of eroded mass, depth of erosion, width and length of erosion. The eroded mass of MDH composite is 49.8 % that of ATH composite which can be attributed to high surface area and higher thermal stability of MDH nanofillers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The grain size dependencies of the yield and fracture stresses in hot rolled Mg-12.7 at % Cd alloy have been measured in the temperature range 77 to 420 K and are found to be in accordance with HalI-Petch type of equations. In hot rolled Mg-12.7 Cd alloy, the HalI-Petch intercept a w is higher than that in hot rolled magnesium, while the slope ky is comparable. The fracture is intercrystalline at 77 K, mixed mode at 300 K and ductile at 420 K. The above flow and fracture behaviours are interpreted in terms of the complimentary effects of texture hardening and solid solution strengthening.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

New antiretroviral drugs that offer large genetic barriers to resistance, such as the recently approved inhibitors of HIV-1 protease, tipranavir and darunavir, present promising weapons to avert the failure of current therapies for HIV infection. Optimal treatment strategies with the new drugs, however, are yet to be established. A key limitation is the poor understanding of the process by which HIV surmounts large genetic barriers to resistance. Extant models of HIV dynamics are predicated on the predominance of deterministic forces underlying the emergence of resistant genomes. In contrast, stochastic forces may dominate, especially when the genetic barrier is large, and delay the emergence of resistant genomes. We develop a mathematical model of HIV dynamics under the influence of an antiretroviral drug to predict the waiting time for the emergence of genomes that carry the requisite mutations to overcome the genetic barrier of the drug. We apply our model to describe the development of resistance to tipranavir in in vitro serial passage experiments. Model predictions of the times of emergence of different mutant genomes with increasing resistance to tipranavir are in quantitative agreement with experiments, indicating that our model captures the dynamics of the development of resistance to antiretroviral drugs accurately. Further, model predictions provide insights into the influence of underlying evolutionary processes such as recombination on the development of resistance, and suggest guidelines for drug design: drugs that offer large genetic barriers to resistance with resistance sites tightly localized on the viral genome and exhibiting positive epistatic interactions maximally inhibit the emergence of resistant genomes.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Using computer modeling of three-dimensional structures and structural information available on the crystal structures of HIV-1 protease, we investigated the structural effects of mutations, in treatment-naive and treatment-exposed individuals from India and postulated mechanisms of resistance in clade C variants. A large number of models (14) have been generated by computational mutation of the available crystal structures of drug bound proteases. Localized energy minimization was carried out in and around the sites of mutation in order to optimize the geometry of interactions present. Most of the mutations result in structural differences at the flap that favors the semiopen state of the enzyme. Some of the mutations were also found to confer resistance by affecting the geometry of the active site. The E35D mutation affects the flap structure in clade B strains and E35N and E35K mutation, seen in our modeled strains, have a more profound effect. Common polymorphisms at positions 36 and 63 in clade C also affected flap structure. Apart from a few other residues Gln-58, Asn-83, Asn-88, and Gln-92 and their interactions are important for the transition from the closed to the open state. Development of protease inhibitors by structure-based design requires investigation of mechanisms operative for clade C to improve the efficacy of therapy.