149 resultados para Phase change material (PCM)
Resumo:
In this paper we explore the enhancement of solubility in a mechanically driven immiscible system experimentally using a mixture of Ag and Bi powders corresponding to a composition of Ag-5.1 at.% Bi. Increase in solubility can be correlated with the combination of sizes of both Ag and Bi at the nanometric scale. It is shown that complete solid solution of Ag-5.1 at.% Bi forms when the respective sizes of :Bi and Ag exceed 13 and 8 nm respectively. We have carried out a thermodynamic analysis of the size- and strain-dependent free energy landscape and compared the results to the initial mixture of microsized particles to rationalize the evolution of Ag solid solution. The agreement indicates that the emerging driving force for the formation of solid solution is primarily due to size reduction rather than the enhanced kinetics of mass transport due to mechanical driving. (c) 2011 Published by Elsevier Ltd. on behalf of Acta Materialia Inc.
Resumo:
Compositional dependent investigations of the bulk GeTe chalcogenides alloys added with different selenium concentrations are carried out by X-ray diffraction (XRD), Raman spectroscopy, X-ray photoelectron spectroscopy (XPS), electron probe micro-analyzer (EPMA) and differential scanning calorimetry (DSC). The measurements reveal that GeTe crystals are predominant in alloys up to 0.20 at.% of Se content indicating interstitial occupancy of Se in the Ge vacancies. Raman modes in the GeTe alloys changes to GeSe modes with the addition of Se. Amorphousness in the alloy increases with increase of Se and 0.50 at.% Se alloy forms a homogeneous amorphous phase with a mixture of Ge-Se and Te-Se bonds. Structural changes are explained with the help of bond theory of solids. Crystallization temperature is found to be increasing with increase of Se, which will enable the amorphous stability. For the optimum 0.50 at.% Se alloy, the melting temperature has reduced which will reduce the RESET current requirement for the phase change memory applications. (C) 2012 Elsevier B.V. All rights reserved.
Resumo:
Amorphous Ge15Te85-xSix thin film switching devices (1 <= x <= 6) have been deposited in sandwich geometry, on glass substrates with aluminum electrodes, by flash evaporation technique. These devices exhibit memory type electrical switching, like bulk Ge15Te85-xSix glasses. However, unlike the bulk glasses, a-Ge15Te85-xSix films exhibit a smooth electrical switching behavior. The electrical switching fields of a-Ge15Te85-xSix thin film samples are also comparable with other chalcogenide samples used in memory applications. The switching fields of a-Ge15Te85-xSix films have been found to increase with increasing Si concentration. Also, the optical band gap of a-Ge15Te85-xSix films is found to increase with Si content. The observed results have been understood on the basis of increase in network connectivity and rigidity with Si addition. (C) 2013 Elsevier Ltd. All rights reserved.
Resumo:
Phase change heat transfer in porous media finds applications in various geological flows and modern heat pipes. We present a study to show the effect of phase change on heat transfer in a porous channel. We show that the ratio of Jakob numbers based on wall superheat and inlet fluid subcooling governs the liquid-vapor interface location in the porous channel and below a critical value of the ratio, the liquid penetrates all the way to the extent of the channel in the flow direction. In such cases, the Nusselt number is higher due to the proximity of the liquid-vapor interface to the heat loads. For higher heat loads or lower subcooling of the liquid, the liquid-vapor interface is pushed toward the inlet, and heat transfer occurs through a wider vapor region thus resulting in a lower Nusselt number. This study is relevant in the designing of efficient two-phase heat exchangers such as capillary suction based heat pipes where a prior estimation of the interface location for the maximum heat load is required to ensure that the liquid-vapor interface is always inside the porous block for its operation.
Resumo:
The work reported in this thesis is an attempt to enhance heat transfer in electronic devices with the use of impinging air jets on pin-finned heat sinks. The cooling per-formance of electronic devices has attracted increased attention owing to the demand of compact size, higher power densities and demands on system performance and re-liability. Although the technology of cooling has greatly advanced, the main cause of malfunction of the electronic devices remains overheating. The problem arises due to restriction of space and also due to high heat dissipation rates, which have increased from a fraction of a W/cm2to 100s of W /cm2. Although several researchers have at-tempted to address this at the design stage, unfortunately the speed of invention of cooling mechanism has not kept pace with the ever-increasing requirement of heat re- moval from electronic chips. As a result, efficient cooling of electronic chip remains a challenge in thermal engineering. Heat transfer can be enhanced by several ways like air cooling, liquid cooling, phase change cooling etc. However, in certain applications due to limitations on cost and weight, eg. air borne application, air cooling is imperative. The heat transfer can be increased by two ways. First, increasing the heat transfer coefficient (forced convec- tion), and second, increasing the surface area of heat transfer (finned heat sinks). From previous literature it was established that for a given volumetric air flow rate, jet im-pingement is the best option for enhancing heat transfer coefficient and for a given volume of heat sink material pin-finned heat sinks are the best option because of their high surface area to volume ratio. There are certain applications where very high jet velocities cannot be used because of limitations of noise and presence of delicate components. This process can further be improved by pulsating the jet. A steady jet often stabilizes the boundary layer on the surface to be cooled. Enhancement in the convective heat transfer can be achieved if the boundary layer is broken. Disruptions in the boundary layer can be caused by pulsating the impinging jet, i.e., making the jet unsteady. Besides, the pulsations lead to chaotic mixing, i.e., the fluid particles no more follow well defined streamlines but move unpredictably through the stagnation region. Thus the flow mimics turbulence at low Reynolds number. The pulsation should be done in such a way that the boundary layer can be disturbed periodically and yet adequate coolant is made available. So, that there is not much variation in temperature during one pulse cycle. From previous literature it was found that square waveform is most effective in enhancing heat transfer. In the present study the combined effect of pin-finned heat sink and impinging slot jet, both steady and unsteady, has been investigated for both laminar and turbulent flows. The effect of fin height and height of impingement has been studied. The jets have been pulsated in square waveform to study the effect of frequency and duty cycle. This thesis attempts to increase our understanding of the slot jet impingement on pin-finned heat sinks through numerical investigations. A systematic study is carried out using the finite-volume code FLUENT (Version 6.2) to solve the thermal and flow fields. The standard k-ε model for turbulence equations and two layer zonal model in wall function are used in the problem Pressure-velocity coupling is handled using the SIMPLE algorithm with a staggered grid. The parameters that affect the heat transfer coefficient are: height of the fins, total height of impingement, jet exit Reynolds number, frequency of the jet and duty cycle (percentage time the jet is flowing during one complete cycle of the pulse). From the studies carried out it was found that: a) beyond a certain height of the fin the rate of enhancement of heat transfer becomes very low with further increase in height, b) the heat transfer enhancement is much more sensitive to any changes at low Reynolds number than compared to high Reynolds number, c) for a given total height of impingement the use of fins and pulsated jet, increases the effective heat transfer coefficient by almost 200% for the same average Reynolds number, d) for all the cases it was observed that the optimum frequency of impingement is around 50 − 100 Hz and optimum duty cycle around 25-33.33%, e) in the case of turbulent jets the enhancement in heat transfer due to pulsations is very less compared to the enhancement in case of laminar jets.
Resumo:
An interesting topic for quite some time is an intermediate phase observed in chalcogenide glasses, which is related to network connectivity and rigidity. This phenomenon is exhibited by Si-Te-In glasses also. It has been addressed here by carrying out detailed thermal investigations by using Alternating Differential Scanning Calorimetry technique. An effort has also been made to determine the stability of these glasses using the data obtained from different thermodynamic quantities and crystallization kinetics of these glasses. Electrical switching behavior by recording I-V characteristics and variation of switching voltages with indium composition have been studied in these glasses for phase change memory applications. (C) 2011 Elsevier Inc. All rights reserved.
Resumo:
Abstract | Electrical switching which has applications in areas such as information storage, power control, etc is a scientifically interesting and technologically important phenomenon exhibited by glassy chalcogenide semiconductors. The phase change memories based on electrical switching appear to be the most promising next generation non-volatile memories, due to many attributes which include high endurance in write/read operations, shorter write/read time, high scalability, multi-bit capability, lower cost and a compatibility with complementary metal oxide semiconductor technology.Studies on the electrical switching behavior of chalcogenide glasses help us in identifying newer glasses which could be used for phase change memory applications. In particular, studies on the composition dependence of electrical switching parameters and investigations on the correlation between switching behavior with other material properties are necessary for the selection of proper compositions which make good memory materials.In this review, an attempt has been made to summarize the dependence of the electrical switching behavior of chalcogenide glasses with other material properties such as network topological effects, glass transition & crystallization temperature, activation energy for crystallization, thermal diffusivity, electrical resistivity and others.
Resumo:
During outbreaks, locust swarms can contain millions of insects travelling thousands of kilometers while devastating vegetation and crops. Such large-scale spatial organization is preceded locally by a dramatic density-dependent phenotypic transition in multiple traits. Behaviourally, low-density solitarious individuals avoid contact with one another; above a critical local density, they undergo a rapid behavioural transition to the gregarious phase whereby they exhibit mutual attraction. Although proximate causes of this phase polyphenism have been widely studied, the ultimate driving factors remain unclear. Using an individual-based evolutionary model, we reveal that cannibalism, a striking feature of locust ecology, could lead to the evolution of density-dependent behavioural phase-change in juvenile locusts. We show that this behavioural strategy minimizes risk associated with cannibalistic interactions and may account for the empirically observed persistence of locust groups during outbreaks. Our results provide a parsimonious explanation for the evolution of behavioural plasticity in locusts.
Resumo:
Infrared spectra of solid formamide are reported as a function of temperature. Solid formamide samples were prepared at 30 K and then annealed to higher temperatures (300 K) with infrared transmission spectra being recorded over the entire temperature range. The NH2 vibrations of the formamide molecule were found to be particularly very sensitive to temperature change. The IR spectra revealed a phase change occurring in solid formamide between 155 and 165 K. Spectral changes observed above and below the phase transition may be attributed to a rearrangement between formamide dimers and the formation of polymers is proposed at higher temperatures.
Resumo:
Selenium doped thin films of GeTe alloys were investigated for their structural modifications by X-ray Diffraction, Fourier Transform Infrared Spectroscopy, X-ray photoelectron Spectroscopy (XPS) and Raman Spectroscopy. The band gap increase from 0.69 to 1.10 eV with increasing Se addition signifies the possibility of band gap tuning in the material. Disorder decreases, band widens and conductivity saturates about 0.20 at.% of Se addition. Structural changes are explained by the bond theory of solids. The as-deposited films are amorphous and 0.50 at.% Se alloy forms a homogeneous amorphous phase with a mixture of Ge-Se and Te-Se bonds. The XPS core level spectra and Raman spectra investigation clearly indicate the formation of Ge-Se, GeTe2 and Te-Se bonds with Se addition. Crystallization temperature is found to be increasing with Se and the 0.10 at.% Se alloy is found to have a higher resistance contrast compared to other Se concentration alloys. Up to 0.10 at.% of Se addition can enhance GeTe phase change memory properties. (C) 2013 Elsevier B.V. All rights reserved.
Resumo:
The paper reports phase evolution in mechanically driven Ag-15 at. pct Sn alloy powder starting with elemental powders in order to establish the feasibility of designing nanocomposites of a Ag-Sn solid solution. This alloy lies in the phase field of the hexagonal zeta-phase which is a well-known Hume-Rothery electron compound with an electron-to-atom ratio of about 1.45 and hexagonal crystal structure (a = 0.2966 nm, c = 0.4782 nm). Through a systematic use of X-ray diffraction and transmission electron microscopy, the results establish the formation of the zeta-phase which co-exists with the Ag solid solution during the initial phase of milling. Mechanical milling for long duration (55 hours) destabilizes the zeta-phase. A complete solid solution of Ag with a grain size of similar to 8 nm could be achieved after 60 hours of milling. Additional milling can induce decomposition of the solid solution that results in a reappearance of zeta-phase. We present a detailed thermodynamic calculation which indicates that complete Ag solid solution of the present alloy composition would be possible if the crystallites size can be reduced below a certain critical size. In particular, we show that both Ag and zeta-phase grain sizes need to be taken into account for determining the metastable equilibrium and the phase change that has been experimentally observed. Finally, we argue that recrystallization processes set a limit to the achievable size of the nanoparticles with metastable Ag solid solution.
Resumo:
Temperature dependent acoustic phonon behavior of PbWO4 and BaWO4 using Brillouin spectroscopy has been explained for the first time. Low temperature Brillouin studies on PbWO4 and BaWO4 have been carried out from 320-20 K. In PbWO4, we observe a change in acoustic phonon mode behavior around 180 K. But in the case of BaWO4, we have observed two types of change in acoustic phonon mode behavior at 240 K and 130 K. The change in Brillouin shift omega and the slope d omega/dT are the order parameter for all kinds of phase transitions. Since we do not see hysteresis on acoustic phonon mode behavior in the reverse temperature experiments, these second order phase transitions are no related to structural phase change and could be related to acoustic phonon coupled electronic transitions. In PbWO4 he temperature driven phase transition at 180 K could be due to changes in he environment around he lead vacancy (V-pb(2-)) changes the electronic states. In the case of BaWO4, the phase transition at 240 K shows he decrease in penetration depth of WO3 impurity. So it becomes more metallic. The transition at 130 K could be he same electronic transitions as that of PbWO4 as function of temperature. The sound velocity and elastic moduli of BaWO4 shows that it could be the prominent material for acousto-optic device applications. (C) 2014 Elsevier Ltd. All rights reserved.