46 resultados para Ni-Cr-Mo-Ti


Relevância:

40.00% 40.00%

Publicador:

Resumo:

The effect of thermal cycling on the load-controlled tension-tension fatigue behavior of a Ni-Ti-Fe shape memory alloy (SMA) at room temperature was studied. Considerable strain accumulation was observed to occur in this alloy under both quasi-static and cyclic loading conditions. Though, in all cases, steady-state is reached within the first 50-100 cycles, the accumulated steady-state strain, epsilon(p.ss), is much smaller in thermally cycled alloy. As a result, the fatigue performance of them was found to be significantly enhanced vis-a-vis the as-solutionized alloy. Furthermore, under load-controlled conditions, the fatigue life of Ni-Ti-Fe alloys was found to be exclusively dependent on epsilon(p.ss). Observations made by profilometry and differential scanning calorimetry (DSC) indicate that the 200-500% enhancement in fatigue life of thermally cycled alloy is due to the homogeneous distribution of the accumulated fatigue strain. (C) 2010 Elsevier B.V. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

A structural investigation of cubic oxides (space group I23) of the formula Bi(26-x)M(x)O(40-delta) (M = Ti, Mn, Fe, Co, Ni and Pb) related to the Y-Bi2O3 phase has been carried out by the Rietveld profile analysis of high-resolution X-ray powder diffraction data in order to establish the cation distributions. Compositional dependence of the cation distribution has been examined in the case of Bi26-xCoxO40-delta (1 < x < 16). The study reveals that in Bi(26-X)M(X)O(40-delta) with M = Ti, Mn, Fe, Co or Pb, the M cations tend to occupy tetrahedral (2a) sites when x < 2 while the octahedral (24f) sites are shared by the excess Co or Ni cations with Bi atoms when x > 2. Also experimental magnetic moments of Mn, Co and Ni derivatives have been used to establish the valence state and distribution of these cations.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Melt spinning of Ti50Ni50 ? xCux (x = 10, 25, 40) alloys showed that the glass-forming ability is good for Cu-rich compositions and poor for Ni-rich compositions. The results of mechanical alloying experiments in the same system showed a reverse trend as far as the glass-forming ability is concerned. These contradictory results are explained in the light of thermodynamic and kinetic considerations. Crystallization results of the melt spun alloys are also presented.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

An amorphous phase has been synthesized by mechanical alloying in a planetary mill over a nickel content range of 10�70 at.% in the Ti---Ni system and a copper content range of 10�50 at.% in the Ti---Cu system. In the case of ternary Ti---Ni---Cu alloys the glass-forming composition range has been found to be given by x = 10�20 for Ti60Ni40 ? xCux, x = 10 � 30 for Ti50Ni50 ? xCux and x = 10 � 40 for Ti40Ni60 ? xCux alloys. The difficulty in the amorphization of copper-rich compositions is explained in the light of enthalpy composition diagrams calculated for the ternary solid solution and the amorphous phase.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The applicability of the confusion principle and size factor in glass formation has been explored by following different combinations of isoelectronic Ti, Zr and Hf metals. Four alloys of nominal composition Zr41.5Ti41.5Ni17, Zr41.5Hf41.5Ni17, Zr25Ti25Cu50 and Zr34Ti16Cu50 have been rapidly solidified to obtain an amorphous phase and their crystallisation behaviour has been studied. The Ti-Zr-Ni alloy crystallises in three steps. Initially this alloy precipitates icosahedral quasicrystalline phase, which on further heat treatment precipitates cF96 Zr2Ni phase. The Zr-Hf-Ni alloy can not be amorphised under the same experimental conditions. The amorphous Zr-Ti-Cu alloys at the initial stages of crystallisation phase-separateinto two amorphous phases and then on further heat treatment cF24 Cu5Zr and oC68 Cu10Zr7 phase are precipitated. The lower glass-forming abilityof Zr-Hf-Ni alloy and the crystallisation behaviour of the above alloys has been studied. The rationale behind nanoquasicrystallisation and the formation of other intermetallic phases has been explained.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Perovskite oxides LaMO3 (M = Cr, Co, Ni), have been successfully prepared using microwaves of 2.45 GHz. Microwave preparation is rapid, clean and energy efficient. Preparation of LaCrO3, LaCoO3 and LaNiO3 has been achieved in 3 min, 5 min and 10 min respectively. Direct reaction between component oxides is used for the preparation of LaCrO3 and LaCoO3, whereas nitrates are used as starting materials for LaNiO3 preparation. Products have been characterized using XRD, IR spectroscopy and SEM. Their dc electrical conductivity has also been studied and their fracture behaviour has been examined. All three microwave prepared oxide powders are of submicron size. These perovskite oxides have been sintered to very high densities using microwaves. Possible mechanisms of the microwave-material interaction both during preparation and during sintering have been discussed.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Diffusion couple technique is used to study interdiffusion in Nb-Mo, Nb-Ti and Nb-Zr systems. Interdiffusion coefficients at different temperatures and compositions are determined using the relation developed by Wagner. The change in activation energy for interdiffusion with composition is determined. Further, impurity diffusion coefficient of the species are determined and compared with the available data in literature.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

An equiatomic NiTiCuFe multi-component alloy with simple body-centered cubic (bcc) and face-centered cubic solid-solution phases in the microstructure was processed by vacuum induction melting furnace under dynamic Ar atmosphere. High-temperature uniaxial compression experiments were conducted on it in the temperature range of 1073 K to 1303 K (800 degrees C to 1030 degrees C) and strain rate range of 10(-3) to 10(-1) s(-1). The data generated were analyzed with the aid of the dynamic materials model through which power dissipation efficiency and instability maps were generated so as to identify the governing deformation mechanisms that are operative in different temperature-strain rate regimes with the aid of complementary microstructural analysis of the deformed specimens. Results indicate that the stable domain for the high temperature deformation of the multi-component alloy occurs in the temperature range of 1173 K to 1303 K (900 degrees C to 1030 degrees C) and (epsilon) over dot range of 10(-3) to 10(-1.2) s(-1), and the deformation is unstable at T = 1073 K to 1153 K (800 degrees C to 880 degrees C) and (epsilon) over dot = 10(-3) to 10(-1.4) s(-1) as well as T = 1223 K to 1293 K (950 degrees C to 1020 degrees C) and (epsilon) over dot = 10(-1.4) to 10(-1) s(-1), with adiabatic shear banding, localized plastic flow, or cracking being the unstable mechanisms. A constitutive equation that describes the flow stress of NiTiCuFe multi-component alloy as a function of strain rate and deformation temperature was also determined. (C) The Minerals, Metals & Materials Society and ASM International 2015

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Since the discovery 1] of gamma' precipitate (L1(2) - Co-3 (Al, W)) in the Co-Al-W ternary system, there has been an increased interest in Co-based superalloys. Since these alloys have two phase microstructures (gamma + gamma') similar to Ni-based superalloys 2], they are viable candidates in high temperature applications, particularly in land-based turbines. The role of alloying on stability of the gamma' phase has been an active area of research. In this study, electronic structure calculations were done to probe the effect of alloying in Co3W with L1(2) structure. Compositions of type Co-3(W, X), (where X/Y = Mn, Fe, Ni, Pt, Cr, Al, Si, V, W, Ta, Ti, Nb, Hf, Zr and Mo) were studied. Effect of alloying on equilibrium lattice parameters and ground state energies was used to calculate Vegard's coefficients and site preference related data. The effect of alloying on the stability of the L1(2) structure vis a vis other geometrically close packed ordered structures was also studied for a range of Co3X compounds. Results suggest that the penchant of element for the W sublattice can be predicted by comparing heats of formation of Co3X in different structures.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The present paper reports a new class of Co based superalloys that has gamma-gamma' microstructure and exhibits much lower density compared to other commercially available Co superalloys including Co-Al-W based alloys. The basic composition is Co-10Al-5Mo (at%) with addition of 2 at% Ta for stabilization of gamma' phase. The gamma-gamma' microstructure evolves through solutionising and aging treatment. Using first principles calculations, we observe that Ta plays a crucial role in stabilizing gamma' phase. By addition of Ta in the basic stoichiometric composition Co-3(Al, Mo), the enthalpy of formation (Delta H-f) of L1(2) structure (gamma' phase) becomes more negative in comparison to DO19 structure. The All of the L12 structure becomes further more negative by the occupancy of Ni and Ti atoms in the lattice suggesting an increase in the stability of the gamma' precipitates. Among large number of alloys studied experimentally, the paper presents results of detailed investigations on Co-10Al-5Mo-2Ta, Co-30Ni-10Al-5Mo-2Ta and Co-30Ni-10Al-5Mo-2Ta-2Ti. To evaluate the role alloying elements, atom probe tomography investigations were carried out to obtain partition coefficients for the constituent elements. The results show strong partitioning of Ni, Al, Ta and Ti in ordered gamma' precipitates. 2015 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

We present results for electron beam welding of a binary Ti/Ni dissimilar metal couple. The difference in physical properties of the base metals and metallurgical features (thermodynamics and kinetics) of the system influence both macroscopic transport and microstructure development in the weld. Microstructures near the fusion interfaces are markedly different from those inside the weld region. At the Ti side, Ti2Ni dendrites are observed to grow toward the fusion interface, while in the Ni side, layered growth of gamma-Ni, Ni3Ti, and Ni3Ti + NiTi eutectic is observed. Different morphologies of the latter eutectic constitute the predominant microstructure inside the weld metal region. These results are compared and contrasted with those from laser welding of the same binary couple, and a scheme of solidification is proposed to explain the observations. This highlights notable departures from welding of similar and other dissimilar metals such as a significant asymmetry in heat transport that governs progress of solidification from each side of the couple, and a lack of unique liquidus isotherm characterizing the liquid-solid front.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

We report on the effect of resputtering on the properties of nanocrystalline Ni-Ti alloy thin films deposited using co-sputtering of Ni and Ti targets. In order to facilitate the formation of nanocrystalline phases, films were deposited at room temperature and 573 K (300 A degrees C) with substrate bias voltage of -100 V. The influence of substrate material on the composition, surface topography microstructure, and phase formations of nanocrystalline Ni-Ti thin films was also systematically investigated. The preferential resputtering of Ti adatoms was lesser for Ni-Ti films deposited on quartz substrate owing to high surface roughness of 4.87 nm compared to roughness value of 1.27 nm for Si(100) substrate.