19 resultados para NUTRIÇÃO MINERAL


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Studies were carried out to assess the utility of the cellular and extracellular constituents of Bacillus megaterium for the flotation of sphalerite and galena minerals. Based on the flotation results on the individual minerals, it was observed that sphalerite was preferentially floated compared to galena. A maximum selectivity index (SI) value of 11.7 was achieved in the presence of the soluble fraction of the thermolysed cells, which was higher than that obtained with the intact cells (SI of 6.5) and the insoluble fraction of the thermolysed cells (SI of 9.6). The results of the various enzymatic treatment tests revealed that extracellular DNA played a vital role in the selective flotation of sphalerite. A noteworthy finding was that the single-stranded DNA (ssDNA) had a higher biocollector capacity vis-A -vis the double-stranded DNA (dsDNA), leading to better flotation efficiency. About 95 % recovery of sphalerite could be achieved from the mineral mixture by the combined addition of the ssDNA with the non-DNA components of the bacterial cells, resulting in a maximum SI of 19.1. Calcium and phosphate components of the nutrient media were found to be essential for better selectivity of separation of sphalerite. The mechanisms of microbe-mineral interaction are discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Milling is an energy intensive process and it is considered as one of the most energy inefficient processes. Electrical and mechanical shock loading can be used to develop a pre-treatment methodology to enhance energy efficiency of comminution and liberation of minerals. Coal and Banded Hematite Jasper (BHJ) Iron ores samples were taken for the study to know the effect of shock loading. These samples were exposed to 5 electric shocks of 300 kV using an electric shock loading device. A diaphragmless shock tube was used to produce 3 and 6 compressed air shocks of Mach number 2.12 to treat the coal and Iron ore samples. Microscopic, comminution and liberation studies were carried out to compare the effectiveness of these approaches. It was found that electric shock loading can comminute the coal samples more effectively and increases the yield of carbon by 40% at 1.6 gm/cc density over the untreated coal samples. Mechanical shock loading showed improved milling performance for both the materials and 12.90% and 8.1% reduction in the D-80 of the particles was observed during grinding for treated samples of coal and iron, respectively. Liberation of minerals in BHJ Iron ore was found unaffected due to low intensity of the mechanical shock waves and non conductivity of minerals. Compressed air based shock loading is easier to operate than electrical shock loading and it needs to be explored further to improve the energy efficacy of comminution. (C) 2014 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A comparative study of two bacterial strains namely, Bacillus licheniformis and Bacillus firmus in the production of bioflocculants was made. The highest bioflocculant yield of 16.55 g/L was obtained from B. licheniformis (L) and 10 g/L from B. firmus (F). The bioflocculants obtained from the bacterial species were water soluble and insoluble in organic solvents. FTIR spectral analysis revealed the presence of hydroxyl, carboxyl and sugar derivatives in the bioflocculants. Thermal characterization by differential scanning calorimetry (DSC) showed the crystalline transition and the melting point (T-m) at 90-100 degrees C. Effects of bioflocculant dosage and pH on the flocculation of clay fines were evaluated. Highest bioflocculation efficiency on kaolin clay suspensions was observed at an optimum bioflocculant dosage of 5 g/L. The optimum pH range for the maximum bioflocculation was at pH 7-9. Bioflocculants exhibited high efficiency in dye decolorization. The maximum Cr (VI) removal was found to be 85 % for L (bioflocculant dosage at 2 g/L). This study demonstrates that microbial bioflocculants find potential applications in mineral processing such as selective flocculation of mineral fines, decolorization of dye solutions and in the remediation of toxic metal solutions. (C) 2015 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The selective flotation of sphalerite from a sphalerite-galena mineral mixture was achieved using cellular components of Paenibacillus polymyxa after adaptation to the above minerals. The soluble and insoluble fractions of the thermolysed bacterial cells adapted to sphalerite yielded higher flotation recoveries of sphalerite with selectivity indices ranging between 22 and 29. The protein profile for the unadapted and mineral-stressed cells was found to differ distinctly, attesting to variation in the yield and nature of extra-cellular polymeric substances. The changes induced in the bacterial cell wall components after adaptation to sphalerite or galena with respect to the contents of phosphate, uronic acid and acetylated sugars of P. polymyxa were quantified. In keeping with these changes, a marginal morphological transition of P. polymyxa from rods to spheres was observed. The role of the dissolved metal ions from the minerals as well as that of the constituents of extracellular secretions in modulating the surface potential of the mineral-stressed cells were demonstrated. These studies highlighted that, mineral stress led to qualitative and quantitative changes in the cellular components, which facilitated the enhancement of flotation selectivity of sphalerite.