Rapid solidification, mechanical alloying and devitrificaiton of precursor metallic glasses are all possible routes for the synthesis of nanocrystals and nanocomposites, though their efficacy is system dependent. In a comprehensive study of alloys across the Ti-Ni phase diagram, nanocrystals of Ti and Ni and nanocomposites of alpha -Ti and Ti sub 2 Ni, Ti sub 2 Ni and TiNi and beta -Ti and glass have been produced. By the addition of Al, devitrification of metallic glasses created by mechanical alloying led to nanocrystalline intermetallic compounds. The evolution of these nanocrystalline microstructures has been rationalized on the basis of thermodynamic and kinetic considerations involving the metastable phase diagram for this system.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Nano-sized bimetallic dispersoids consisting of (Pb) and beta-(Sn) phases of eutectic composition (Pb26.1Sn73.9) embedded in aluminum and Al-Cu-Fe quasicrystalline matrices have been prepared by rapid solidification processing. The two phases, face centered cubic (Pb) and body center tetragonal, beta-(Sn) solid solution co-exist in all the embedded nanoparticles at room temperature. The phases bear crystallographic orientation relationship with the matrix. In situ TEM study has been carried out for the alloy particles to study the melting and the solidification behavior. The detailed microscopic observations indicate formation of a single-phase metastable fcc (Pb) in the nano-particles prior to the melting during heating. Solidification of these particles begins with nucleation of fcc (Pb), which phase separates into fcc (Pb) and beta-(Sn) lamellae in the solid state. In situ X-ray diffraction study is carried out to obtain lattice parameter of metastable fcc (Pb) and thereby an estimate of amount of Sn dissolved in the metastable (Pb) prior to the melting. The results are discussed in terms of a metastable phase diagram between fcc Pb and fcc Sn and invoking the size effect on the metastable phase diagram. The size factor is found to play a critical role in deciding the pathway of phase transformation as well as the extension of solid solubility of Sn in fcc (Pb) in the nano-particles.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The well-known classical nucleation theory (CNT) for the free energy barrier towards formation of a nucleus of critical size of the new stable phase within the parent metastable phase fails to take into account the influence of other metastable phases having density/order intermediate between the parent metastable phase and the final stable phase. This lacuna can be more serious than capillary approximation or spherical shape assumption made in CNT. This issue is particularly significant in ice nucleation because liquid water shows rich phase diagram consisting of two (high and low density) liquid phases in supercooled state. The explanations of thermodynamic and dynamic anomalies of supercooled water often invoke the possible influence of a liquid-liquid transition between two metastable liquid phases. To investigate both the role of thermodynamic anomalies and presence of distinct metastable liquid phases in supercooled water on ice nucleation, we employ density functional theoretical approach to find nucleation free energy barrier in different regions of phase diagram. The theory makes a number of striking predictions, such as a dramatic lowering of nucleation barrier due to presence of a metastable intermediate phase and crossover in the dependence of free energy barrier on temperature near liquid-liquid critical point. These predictions can be tested by computer simulations as well as by controlled experiments. (C) 2014 AIP Publishing LLC.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The(1-x) BiFeO3-(x) PbTiO3 solid solution exhibiting a Morphotropic Phase Boundary (MPB) has attracted considerable attention recently because of its unique features such as multiferroic, high Curie point (T-C similar to 700 degrees C) and giant tetragonality (c/a -1 similar to 0.19). Different research groups have reported different composition range of MPB for this system. In this work we have conclusively proved that the wide composition range of MPB reported in the literature is due to kinetic arrest of the metastable rhombohedral phase and that if sufficient temperature and time is allowed the metastable phase disappears. The genuine MPB was found to be x=0.27 for which the tetragonal and the rhombohedral phases are in thermodynamic equilibrium. In-situ high temperature structural study of x=0.27 revealed the sluggish kinetics associated with the temperature induced structural transformation. Neutron powder diffraction study revealed that themagnetic ordering at room temperature occurs in the rhombohedral phase. The magnetic structure was found to be commensurate G-type antiferromagnetic with magnetic moments parallel to the c-direction (of the hexagonal cell). The present study suggests that the equilibrium properties in this solid solution series should be sought for x=0.27.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Thermoelectric properties of semiconducting beta-FeSi2 containing a homogeneous distribution of Si secondary phase have been studied. The synthesis was carried out using arc melting followed by the densification by uniaxial hot pressing. Endogenous beta-FeSi2/Si composites were produced by the eutectoid decomposition of high-temperature alpha-Fe2Si5 phase. The aging heat treatments have been carried out at various temperatures below the equilibrium eutectoid temperature for various durations in order to tune the size of the eutectoid product. Thermal properties of the samples were studied in the temperature range of 100-350 A degrees C. The microstructural investigations support the fact that the finest microstructure generated through the eutectoid decomposition of the alpha-Fe2Si5 metastable phase is responsible of the phonon scattering. The results suggest an opportunity to produce bulk iron silicide alloys with reduced thermal conductivity in order to enhance its thermoelectric performance.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Pure Y2O3 and Y2O3---ZrO2 solid solutions have been prepared by melt atomization and by pyrolysis of nitrate solutions. Extended solubility is readily achieved in both techniques for the entire composition range investigated: melts with 0–30% ZrO2 and precursors with 0–50% ZrO2. However, solidification of under cooled droplets yields almost exclusively single phase powders with the structure of cubic yttria (D53). In contrast, the pyrolysis route leads to a sequence of metastable microstructures beginning with a nanocrystalline disordered fluorite-based (C1) solid solution. Further heating leads to the evolution of much larger (micron size) flake crystals with a {001} texture, concurrent with partial ordering of the oxygen ions to the sites occupied in the D53 structure. The driving force for ordering and the rate of grain growth decrease with increasing ZrO2 addition. Abrupt heating to high temperatures or electron irradiation can induce ordering without substantial grain growth. There is no significant reduction in porosity during the recrystallization, which with the other observations suggests that grain growth is driven by the free energy available for the ordering transformation from fluorite to the yttria structure. This route offers opportunities for single crystal thin film development at relatively low processing temperatures.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Pure Y2O3 and Y2O3-ZrO2 solid solutions have been prepared by melt atomization and by pyrolysis of nitrate solutions. Extended solubility is readily achieved in both techniques for the entire composition range investigated: melts with 0-30% ZrO2 and precursors with 0-50% ZrO2. However, solidification of under cooled droplets yields almost exclusively single phase powders with the structure of cubic yttria (D5(3)). In contrast, the pyrolysis route leads to a sequence of metastable microstructures beginning with a nanocrystalline disordered fluorite-based (C1) solid solution. Further heating leads to the evolution of much larger (micron size) flake crystals with a {001} texture, concurrent with partial ordering of the oxygen ions to the sites occupied in the D5(3) structure. The driving force for ordering and the rate of grain growth decrease with increasing ZrO2 addition. Abrupt heating to high temperatures or electron irradiation can induce ordering without substantial grain growth. There is no significant reduction in porosity during the recrystallization, which with the other observations suggests that grain growth is driven by the free energy available for the ordering transformation from fluorite to the yttria structure. This route offers opportunities for single crystal thin film development at relatively low processing temperatures.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Temperature-time study of the magnetoelectric multiferroic (1-x)BiFeO3-(x)PbTiO3 by x-ray and electron diffraction on the reported morphotropic phase boundary (MPB) compositions revealed that this MPB does not correspond to the equilibrium state. The MPB like state is rather of metastable nature and arise due to kinetic arrest of metastable rhombohedral (R3c) phase, along with the equilibrium tetragonal (P4mm) phase. The life time of the metastable R3c nuclei is very sensitive to composition and temperature, and nearly diverges at x -> 0.27. The MPB like state appears only if the system is cooled before the metastable R3c nuclei could vanish. These findings resolve the long standing controversy with regard to seemingly erratic phase formation behaviour reported by different groups and provides a rational basis for developing genuine equilibrium MPB compositions in this system for better piezoelectric properties. (C) 2013 AIP Publishing LLC.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

When quenched with liquid N-2, a room temperature liquid, 4-fluorobenzoyl chloride, generates a new crystalline form that appears to be polytypic to the previously reported form. The structural and energetic correlations between these forms trace a crystallization pathway of the compound.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

For decades it has been a well-known fact that among the few ferroelectric compounds in the perovskite family, namely, BaTiO3, KNbO3, PbTiO3, and Na1/2Bi1/2TiO3, the dielectric and piezoelectric properties of BaTiO3 are considerably higher than the others in polycrystalline form at room temperature. Further, similar to ferroelectric alloys exhibiting morphotropic phase boundary, single crystals of BaTiO3 exhibit anomalously large piezoelectric response when poled away from the direction of spontaneous polarization at room temperature. These anomalous features in BaTiO3 remained unexplained so far from the structural standpoint. In this work, we have used high-resolution synchrotron x-ray powder diffraction, atomic resolution aberration-corrected transmission electron microscopy, in conjunction with a powder poling technique, to reveal that at 300 K (i) the equilibrium state of BaTiO3 is characterized by coexistence of metastable monoclinic Pm and orthorhombic (Amm2) phases along with the tetragonal phase, and (ii) strong electric field switches the polarization direction from the 001] direction towards the 101] direction. These results suggest that BaTiO3 at room temperature is within an instability regime, and that this instability is the fundamental factor responsible for the anomalous dielectric and piezoelectric properties of BaTiO3 as compared to the other homologous ferroelectric perovskite compounds at room temperature. Pure BaTiO3 at room temperature is therefore more akin to lead-based ferroelectric alloys close to the morphotropic phase boundary where polarization rotation and field induced ferroelectric-ferroelectric phase transformations play a fundamental role in influencing the dielectric and piezoelectric behavior.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The stereology, variant distribution and coarsening behavior of semicoherent alpha(hcp) precipitates in a beta(bcc) matrix of a Ti5553 alloy has been analyzed, and a dominant 3-variant cluster has been observed in which the variants are related to each other by an axis-angle pair <<11(2)over bar> 0 >/60 degrees. Shape and spatial distribution independent elastic self and interaction energies for all pairwise and triplet combinations of a have been calculated and it is found that the 3-cluster combination that is experimentally observed most frequently has the lowest energy for the semicoherent state. The coarsening behavior of the delta distribution follows LSW kinetics after an initial transient, and has been modeled by phase field methods. (C) 2016 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Texture evolution in a low cost beta titanium alloy was studied for different modes of rolling and heat treatments. The alloy was cold rolled by unidirectional and multi-step cross rolling. The cold rolled material was either aged directly or recrystallized and then aged. The evolution of texture in alpha and beta phases were studied. The rolling texture of beta phase that is characterized by the gamma fiber is stronger for MSCR than UDR; while the trend is reversed on recrystallization. The mode of rolling affects alpha transformation texture on aging with smaller alpha lath size and stronger alpha texture in UDR than in MSCR. The defect structure in beta phase influences the evolution of a texture on aging. A stronger defect structure in beta phase leads to variant selection with the rolled samples showing fewer variants than the recrystallized samples.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

It is conjectured that the hard sphere system has several distinct solid phases, all but one of which are metastable. The bifurcation theory analysis of freezing is extended to the description of the transition between a supercooled liquid and a disordered solid by defining a restricted phase space for the disordered solid. This approach leads to the prediction of a first order transition between a supercooled hard sphere fluid and a disordered metastable hard sphere solid. The results of the calculation are in qualitative agreement with the results of Woodcock's molecular dynamics computer simulations. The Journal of Chemical Physics is copyrighted by The American Institute of Physics.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

We focus on athermal phase transitions where in discrete and dissipative avalanches are observed in physical observables as the system jumps from one metastable state to another, when driven by an external field. Using higher order statistics of time dependent avalanches, or noise, in electrical resistivity during temperature-driven martensite transformation in thin nickel-titanium films, we demonstrate evidence suggesting the existence of a singular `global instability' or divergence of the correlation length as a function of temperature at the transition. These results not only establish a mapping of non-equilibrium first order phase transition and equilibrium critical phenomena, but perhaps also call for a re-evaluation of many existing experimental claims of self-organized criticality.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The compounds Pb2PtO4 and PbPt2O4 were synthesized from an intimate mixture of yellow PbO and Pt metal powders by heating under pure oxygen gas at 973 K for periods up to 600 ks with intermediate grinding and recompacting. Both compounds were found to decompose on heating in pure oxygen to PbO and Pt, apparently in conflict with the requirements for equilibrium phase relations in the ternary system Pb–Pt–O. The oxygen chemical potential corresponding to the three-phase mixtures, Pb2PtO4 + PbO + Pt and PbPt2O4 + PbO + Pt were measured as a function of temperature using solid-state electrochemical cells incorporating yttria-stabilized zirconia as the solid electrolyte and pure oxygen gas at 0.1 MPa pressure as the reference electrode. The standard Gibbs free energies of formation of the ternary oxides were derived from the measurements. Analysis of the results indicated that the equilibrium involving three condensed phases Pb2PtO4 + PbO + Pt is metastable. Under equilibrium conditions, Pb2PtO4 should have decomposed to a mixture of PbO and PbPt2O4. Measurement of the oxygen potential corresponding to this equilibrium decomposition as a function of temperature indicated that decomposition temperature in pure oxygen is 1014(±2) K. This was further confirmed by direct determination of phase relations in the ternary Pb–Pt–O by equilibrating several compositions at 1023 K for periods up to 850 ks and phase identification of quenched samples using X-ray diffraction (XRD), scanning electron microscopy (SEM) and energy dispersive X-ray spectroscopy (EDS). Only one ternary oxide PbPt2O4 was stable at 1023 K under equilibrium conditions. Alloys and intermetallic compounds along the Pb–Pt binary were in equilibrium with PbO.