In this paper, we present a modified k - epsilon model capable of addressing turbulent weld-pool convection in a GMAW process, taking into account the morphology of the phase change interface during a Gas Metal Arc Welding (GMAW) process. A three-dimensional turbulence mathematical model has been developed to study the heat transfer and fluid flow within the weld pool by considering the combined effect of three driving forces, viz., buoyancy, Lorentz force and surface tension (Marangoni convection). Mass and energy transports by the droplets are considered through the thermal analysis of the electrode. The falling droplet's heat addition to the molten pool is considered to be a volumetric heat source distributed in an imaginary cylindrical cavity ("cavity model") within the weld pool. This nature of heat source distribution takes into account the momentum and the thermal, energy of the falling droplets. The numerically predicted weld pool dimensions both from turbulence and laminar models are then compared with the experimental post-weld results sectioned across the weld axis. The above comparison enables us to analyze the overall effects of turbulent convection on the nature of heat and fluid flow and hence on the weld pool shape/size during the arc welding processes.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, a numerical model for friction welding of thixo-cast materials is developed, which includes a coupling of thermal effect and plastic deformation using a finite element method (FEM). As the constitutive equations for flow behavior of materials for a thixo-cast material are expected to be different from those of conventionally cast material of the same alloy, the necessary material data are experimentally determined from isothermal hot compression tests of the A356 thixocast alloy. The Johnson-Cook model has been employed to represent the flow behavior of the thixocast A356 alloy. The purpose of this FEM analysis is to provide better understanding of the friction welding process of thixo-cast material, and to obtain optimized process parameters before an actual welding is carried out.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Welding parameters like welding speed, rotation speed, plunge depth, shoulder diameter etc., influence the weld zone properties, microstructure of friction stir welds, and forming behavior of welded sheets in a synergistic fashion. The main aims of the present work are to (1) analyze the effect of welding speed, rotation speed, plunge depth, and shoulder diameter on the formation of internal defects during friction stir welding (FSW), (2) study the effect on axial force and torque during welding, (c) optimize the welding parameters for producing internal defect-free welds, and (d) propose and validate a simple criterion to identify defect-free weld formation. The base material used for FSW throughout the work is Al 6061T6 having a thickness value of 2.1 mm. Only butt welding of sheets is aimed in the present work. It is observed from the present analysis that higher welding speed, higher rotation speed, and higher plunge depth are preferred for producing a weld without internal defects. All the shoulder diameters used for FSW in the present work produced defect-free welds. The axial force and torque are not constant and a large variation is seen with respect to FSW parameters that produced defective welds. In the case of defect-free weld formation, the axial force and torque are relatively constant. A simple criterion, (a,tau/a,p)(defective) > (a,tau/a,p)(defect free) and (a,F/a,p)(defective) > (a,F/a,p)(defect free), is proposed with this observation for identifying the onset of defect-free weld formation. Here F is axial force, tau is torque, and p is welding speed or tool rotation speed or plunge depth. The same criterion is validated with respect to Al 5xxx base material. Even in this case, the axial force and torque remained constant while producing defect-free welds.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper highlights the role of globular microstructure on the weldability of semi-solid processed aluminum alloys via high temperature flow behavior. The investigation was carried out on the joining of thixocast A356 aluminum alloy components by friction welding. A thermomechanical model was developed to predict the temperature and stress distributions, as well as to identify the suitable and safe range of parameters. Good comparisons between numerical and experimental results were observed. In addition, metallographic examinations and hardness and tensile tests of the welded samples were carried out. It was found that the tensile strength of the joint is higher than the tensile strength of the parent material for the optimum set of parameters. (C) 2014 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A sound weld was obtained between 2024-T3 Al alloy and AZ31B-O Mg alloy dissimilar metal plates of 5 mm thickness, at a rotational speed of 300 rev min(-1) and at a welding speed of 50 mm min(-1). One of the parameter studied was, the effect of interface offset variation, on the quality and properties of the welded samples and on the thickness of intermetallic layer formed in the welded samples. The intermetallic layer at the midst of the weld volume contains intermetallic compounds Al12Mg17 and Al3Mg2. Highest tensile strength of 106.86 MPa, corresponding tensile joint efficiency of 44.52% and corresponding elongation 1.33% were obtained for the tensile sample, with interface offset of 0.66 mm from zero interface offset in retreating side and with approximate least intermetallic thickness of 1.2 mu m. Dissimilar friction stir welded joint samples had failed completely in brittle fracture mode; the position of tensile fracture was located at the midst of intermetallic layer, which had maximum hardness and minimum ductility. The nano hardness values fluctuate in the weld nugget owing to dynamic recrystallization of alloy materials and formation of brittle intermetallic compounds of alloy materials in the weld nugget; maximum hardness of 10.74 GPa occurred for the sample with least intermetallic thickness of 1.2 mu m. (C) 2014 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We present results for electron beam welding of a binary Ti/Ni dissimilar metal couple. The difference in physical properties of the base metals and metallurgical features (thermodynamics and kinetics) of the system influence both macroscopic transport and microstructure development in the weld. Microstructures near the fusion interfaces are markedly different from those inside the weld region. At the Ti side, Ti2Ni dendrites are observed to grow toward the fusion interface, while in the Ni side, layered growth of gamma-Ni, Ni3Ti, and Ni3Ti + NiTi eutectic is observed. Different morphologies of the latter eutectic constitute the predominant microstructure inside the weld metal region. These results are compared and contrasted with those from laser welding of the same binary couple, and a scheme of solidification is proposed to explain the observations. This highlights notable departures from welding of similar and other dissimilar metals such as a significant asymmetry in heat transport that governs progress of solidification from each side of the couple, and a lack of unique liquidus isotherm characterizing the liquid-solid front.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Lasers are very efficient in heating localized regions and hence they find a wide application in surface treatment processes. The surface of a material can be selectively modified to give superior wear and corrosion resistance. In laser surface-melting and welding problems, the high temperature gradient prevailing in the free surface induces a surface-tension gradient which is the dominant driving force for convection (known as thermo-capillary or Marangoni convection). It has been reported that the surface-tension driven convection plays a dominant role in determining the melt pool shape. In most of the earlier works on laser-melting and related problems, the finite difference method (FDM) has been used to solve the Navier Stokes equations [1]. Since the Reynolds number is quite high in these cases, upwinding has been used. Though upwinding gives physically realistic solutions even on a coarse grid, the results are inaccurate. McLay and Carey have solved the thermo-capillary flow in welding problems by an implicit finite element method [2]. They used the conventional Galerkin finite element method (FEM) which requires that the pressure be interpolated by one order lower than velocity (mixed interpolation). This restricts the choice of elements to certain higher order elements which need numerical integration for evaluation of element matrices. The implicit algorithm yields a system of nonlinear, unsymmetric equations which are not positive definite. Computations would be possible only with large mainframe computers.Sluzalec [3] has modeled the pulsed laser-melting problem by an explicit method (FEM). He has used the six-node triangular element with mixed interpolation. Since he has considered the buoyancy induced flow only, the velocity values are small. In the present work, an equal order explicit FEM is used to compute the thermo-capillary flow in the laser surface-melting problem. As this method permits equal order interpolation, there is no restriction in the choice of elements. Even linear elements such as the three-node triangular elements can be used. As the governing equations are solved in a sequential manner, the computer memory requirement is less. The finite element formulation is discussed in this paper along with typical numerical results.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We investigate the events near the fusion interfaces of dissimilar welds using a phase-field model developed for single-phase solidification of binary alloys. The parameters used here correspond to the dissimilar welding of a Ni/Cu couple. The events at the Ni and the Cu interface are very different, which illustrate the importance of the phase diagram through the slope of the liquidus curves. In the Ni side, where the liquidus temperature decreases with increasing alloying, solutal melting of the base metal takes place; the resolidification, with continuously increasing solid composition, is very sluggish until the interface encounters a homogeneous melt composition. The growth difficulty of the base metal increases with increasing initial melt composition, which is equivalent to a steeper slope of the liquidus curve. In the Cu side, the initial conditions result in a deeply undercooled melt and contributions from both constrained and unconstrained modes of growth are observed. The simulations bring out the possibility of nucleation of a concentrated solid phase from the melt, and a secondary melting of the substrate due to the associated recalescence event. The results for the Ni and Cu interfaces can be used to understand more complex dissimilar weld interfaces involving multiphase solidification.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Continuous CO2 laser welding of an Fe-Cu dissimilar couple in a butt-weld geometry at different process conditions is studied. The process conditions are varied to identify and characterize the microstructural features that are independent of the welding mode. The study presents a characterization of the microstructure and mechanical properties of the welds. Detailed microstructural analysis of the weld/base-metal interface shows features that are different on the two sides of the weld. The iron side can grow into the weld with a local change in length scale, whereas the interface on the copper side indicates a barrier to growth. The interface is jagged, and a banded microstructure consisting of iron-rich layers could be observed next to the weld/Cu interface. The observations suggest that solidification initiates inside the melt, where iron and copper are mixed due to convective flow. The transmission electron microscopy (TEM) of the weld region also indicates the occasional presence of droplets of iron and copper. The microstructural observations are rationalized using arguments drawn from a thermodynamic analysis of the Fe-Cu system.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Lithium-containing aluminium alloys are of considerable current interest in the aerospace and aircraft industries because lithium additions to aluminium improve the modulus and decrease the density compared to conventional aluminium alloys. Few commercial aluminium-lithium alloys have emerged for use in the aerospace industry. One such candidate is 8090, a precipitation-hardenable Al-Li-Cu-Mg alloy. The influence of electron-beam welding on the microstructure and mechanical properties of alloy 8090 material has been evaluated through microscopical observations and mechanical tests. Microscopic observations of the electronbeam welds revealed an absence of microporosity and hot cracking, but revealed presence of microporosity in the transverse section of the weld. Mechanical tests revealed the electronbeam weld to have lower strength, elongation and joint efficiency. A change in microscopic fracture mode was observed for the welded material when compared to the unwelded counterpart. An attempt is made to rationalize the behaviour in terms of competing mechanistic effects involving the grain structure of the material, the role of matrix deformation characteristics, grain-boundary chemistry and grain-boundary failure.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Joining of dissimilar metals involves a number of scientific issues, the modelling of which offers unique challenges. This review discusses the complexities in different joining processes and dissimilar combinations, and the corresponding computational techniques that have the potential to address the same. Future directions in modelling at both macroscopic and microscopic scales are also suggested.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The evaluation of the creep deformation and fracture behavior of a 2.25Cr-1Mo steel base metal, a 2.25Cr-1Mo/2.25Cr-1Mo similar weld joint, and a 2.25Cr-1Mo/Alloy 800 dissimilar weld joint at 823 K over a stress range of 90 to WO MPa has been carried out. The specimens for creep testing were taken from single-V weld pads fabricated by a shielded metal arc-welding process using 2.25Cr-1Mo steel (for similar-joint) and INCONEL 182 (for dissimilar-joint) electrodes. The weld pads were subsequently given a postweld hear treatment (PWHT) of 973 K for I hour. The microstructure and microhardness of the weld joints were evaluated in the as-welded, postweld heat-treated, and creep-tested conditions. The heat-affected zone (HAZ) of similar weld joint consisted of bainite in the coarse-prior-austenitic-grain (CPAG) region near the fusion line, followed by bainite in the fine-prior-austenitic-grain (FPAG) and intercritical regions merging with the unaffected base metal. In addition to the HAZ structures in the 2.25Cr-1Mo steel, the dissimilar weld joint displayed a definite INCONEL/2.25Cr-1Mo weld interface structure present either as a sharp line or as a diffuse region. A hardness trough was observed in the intercritical region of the HAZ in both weld joints, while a maxima in hardness was seen at the weld interface of the dissimilar weld joint. Both weld joints exhibited significantly lower rupture lives compared to the 2.25Cr-1Mo base metal. The dissimilar weld joint exhibited poor rupture life compared to the similar weld joint, at applied stresses lower than 130 MPa. In both weld joints, the strain distribution across the specimen gage length during creep testing varied significantly. During creep testing, localization of deformation occurred in the intercritical HAZ. In the similar weld joint, at all stress levels investigated, and in the dissimilar weld joint, at stresses greater than or equal to 150 MPa, the creep failure occulted in the intercritical HAZ. The fracture occurred by transgranular mode with a large number of dimples. At stresses below 150 MPa, the failure in the dissimilar weld joint occurred in the CPAG HAZ near to the weld interface. The failure occurred by extensive intergranular creep cavity formation.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A systematic procedure is outlined for scaling analysis of momentum and heat transfer in gas tungsten arc weld pools. With suitable selections of non-dimentionalised parameters, the governing equations coupled with appropriate boundary conditions are first scaled, and the relative significance of various terms appearing in them is analysed accordingly. The analysis is then used to predict the orders of magnitude of some important quantities, such as the velocity scene lit the top surface, velocity boundary layer thickness, maximum temperature increase in the pool, and time required for initiation of melting. Some of the quantities predicted from the scaling analysis can also be used for optimised selection of appropriate grid size and time steps for full numerical simulation of the process. The scaling predictions are finally assessed by comparison with numerical results quoted in the literature, and a good qualitative agreement is observed.