196 resultados para ER-stress
Resumo:
n this paper, the influence of patch parameters on stress intensity factors in edge cracked plates is studied by employing transmission photoelasticity. Edge cracked plates made of photo-elastic material are patched on one side only by E glass-epoxy and carbon-epoxy unidirectional composites. The patch is located on the crack in such a way that the crack tip is not covered. Magnified isochromatic fringes are obtained by using a projection microscope of magnification 50, converted into a polariscope. Irwin's method is used to compute stress intensity factors from photoelastic data. The reduction in stress intensity factors is presented in graphical form as a function of patch parameters, namely stiffness, location and length. An empirical equation connecting reduction in stress intensity factor and these patch parameters is presented.
Resumo:
ErBa2Cu3O7 and Er0.5Y0.5Ba2Cu3O7 are both high-Tc superconductors attaining zero resistance above 80 K. Preliminary studies indicate that Yb1−xYxBa2Cu3O7 also exhibits zero resistance above 77 K.
Resumo:
In a beam whose depth is comparable to its span, the distribution of bending and shear stresses differs appreciably from those given by the ordinary flexural theory. In this paper, a general solution for the analysis of a rectangular, single-scan beam, under symmetrical loading is developed. The Multiple Fourier procedure is employed using four series by which it has been possible to satisfy all boundary and the resulting relation among the co-efficient are derives.
Resumo:
The use of the multiple Fourier method to analyses the stress distribution in the and regions of as a post-tensioned prestressed concrete beam had shown. The multiple Fourier method demonstrated have is a relatively new method for solving those problems for which the “Saint Vansant principle” is not applicable, The actual three-dimensional problem and a two-dimensional simplified representation of it are treated. The two-dimensional case is treated first and rather completely to gain further experience with multiple Fourier procedure, the appropriate Galerkin Vector for the three-dimensional case is found and the required relations between the arbitrary functions are stated.
Resumo:
Extensive molecular dynamics (MD) simulations have been performed in a B2-NiAl nanowire using an embedded atom method (EAM) potential. We show a stress induced B2 -> body-centered-tetragonal (BCT) phase transformation and a novel temperature and cross-section dependent pseudo-elastic/pseudo-plastic recovery from such an unstable BCT phase with a recoverable strain of similar to 30% as compared to 5-8% in polycrystalline materials. Such a temperature and cross-section dependent pseudo-elastic/pseudo-plastic strain recovery can be useful in various interesting applications of shape memory and strain sensing in nanoscale devices. Effects of size, temperature, and strain rate on the structural and mechanical properties have also been analyzed in detail. For a given size of the nanowire the yield stress of both the B2 and the BCT phases is found to decrease with increasing temperature, whereas for a given temperature and strain rate the yield stress of both the B2 and the BCT phase is found to increase with increase in the cross-sectional dimensions of the nanowire. A constant elastic modulus of similar to 80 GPa of the B2 phase is observed in the temperature range of 200-500 K for nanowires of cross-sectional dimensions in the range of 17.22-28.712 angstrom, whereas the elastic modulus of the BCT phase shows a decreasing trend with an increase in the temperature.
Resumo:
An experimental technique is proposed for the estimation of crack length as well as crack closure/opening stress during fatigue crack growth. A specially designed, single cantilever, crack opening displacement gauge is used to monitor these variables during fatigue crack propagation testing. The technique was experimentally validated through electronfractography.
Resumo:
The fatigue and fracture performance of a cracked plate can be substantially improved by providing patches as reinforcements. The effectiveness of the patches is related to the reduction they cause in the stress intensity factor (SIF) of the crack. So, for reliable design, one needs an accurate evaluation of the SIF in terms of the crack, patch and adhesive parameters. In this investigation, a centrally cracked large plate with a pair of symmetric bonded narrow patches, oriented normally to the crack line, is analysed by a continuum approach. The narrow patches are treated as transversely flexible line members. The formulation leads to an integral equation which is solved numerically using point collocation. The convergence is rapid. It is found that substantial reductions in SIF are possible with practicable patch dimensions and locations. The patch is more effective when placed on the crack than ahead of the crack. The present analysis indicates that a little distance inwards of the crack tip, not the crack tip itself, is the ideal location, for the patch.
Resumo:
The structural integrity of any member subjected to a load gets impaired due to the presence of cracks or crack-like defects. The notch severity is one of the several parameters that promotes the brittle fracture. The most severe one is an ideal crack with infinitesimal width and infinitesimal or zero root radius. Though analytical investigations can handle an ideal crack, experimental work, either to validate the analytical conclusions or to impose the bounds, needs to be carried out on models or specimens containing the cracks which are far from the ideal ones. Thus instead of an ideal crack with infinitesimal width the actual model will have a slot or a slit of finite width and instead of a crack ending in zero root radius, the model contains a slot having a finite root radius. Another factor of great significance at the root is the notch angle along which the transition from the slot to the root takes place. This paper is concerned with the photoelastic determination of the notch stress intensity factor in the case of a “crack” subjected to Mode 1 deformation.
Resumo:
The importance of interlaminar stresses has prompted a fresh look at the theory of laminated plates. An important feature in modelling such laminates is the need to provide for continuity of some strains and stresses, while at the same time allowing for the discontinuities in the others. A new modelling possibility is examined in this paper. The procedure allows for discontinuities in the in-plane stresses and transverse strains and continuity in the in-plane strains and transverse stresses. This theory is in the form of a heirarchy of formulations each representing an iterative step. Application of the theory is illustrated by considering the example of an infinite laminated strip subjected to sinusoidal loading.
Resumo:
A simple mathematical model depicting blood flow in the capillary is developed with an emphasis on the permeability property of the blood vessel based on Starling's hypothesis. In this study the effect of inertia has been neglected in comparison with the viscosity on the basis of the smallness of the Reynolds number of the flow in the capillary. The capillary blood vessel is approximated by a circular cylindrical tube with a permeable wall. The blood is represented by a couple stress fluid. With such an ideal model the velocity and pressure fields are determined. It is shown that an increase in the couple stress parameter increases the resistance to the flow and thereby decreases the volume rate flow. A comparison of the results with those of the Newtonian case has also been made.
Resumo:
This paper reports an experimental investigation carried out, using the photoelastic technique, to determine the Mode I stress intensity factor in case of cracks of varying a/w ratio in single edge-notch specimens. The photoelastic information was analysed using the several methods proposed by earlier workers. The experimental results are compared with the analytical expressions.
Resumo:
The stress corrosion cracking (SCC) characteristics of agr-titanium sheets in a bromine-methanol solution have been studied in the annealed and cold-rolled conditions using longitudinal and transverse specimens. The times to failure for annealed longitudinal specimens were longer than those for similarly tested transverse specimens. The cold-rolled specimens developed resistance to SCC, but failed by cleavage when notched, unlike the intergranular separation in annealed titanium. The apparent activation energy was found to be texture dependent and was in the range 30 to 51 kJ mol–1 for annealed titanium, and 15kJ mol–1 for cold-rolled titanium. The dependence of SCC behaviour on the texture is related to the changes in the crack initiation times. These are caused by changes in the passivation and repassivation characteristics of the particular thickness plane. The thickness planes are identified with the help of X-ray pole figures obtained on annealed and cold-rolled material. On the basis of the activation energy and the electrochemical measurements, the mechanism of SCC in annealed titanium is identified to be the one involving stress-aided anodic dissolution. On the other hand, the results on the cold-rolled titanium are in support of the hydrogen embrittlement mechanism consisting of hydride precipitation. The cleavage planes identified from the texture data match with the reported habit planes for hydride formation.
Resumo:
Free proline content in Ragi (Eleusine coracana) leaves increased markedly (6 to 85 fold) as the degree of water stress, created by polyethylene gylcol treatment, was prolonged There was also a marginal increase in soluble proteins in the stressed leaves as compared to that in the controls. Water stress stimulated the activities of ornithine aminotransferase and pyrroline-5-carboxylate reductase, the enzymes of proline biosynthesis and markedly inhibited the enzymes involved in proline degradation viz., proline oxidase and pyrroline-5-carboxylate dehydrogenase. These results suggest that increase in free proline content of Ragi leaves could be due to enhanced activities of the enzymes synthesizing proline but more importantly due to severe inhibition of the enzymes degrading proline. These observations establish for the first time, the pathway of proline metabolism in plants by way of detection of the activities of all the enzymes involved and also highlight the role of these enzymes in proline accumulation during water stress.
Resumo:
An experimental investigation dealing with the influence of stress path on the shear behaviour of a layered soil prepared in the laboratory is described. Specimens trimmed in vertical and horizontal directions have been sheared under three different stress paths in compression and extension tests. Either in compression or extension, the stress–strain behaviour of the specimens with both orientations was apparently the same, although the volume change behaviour was different. The effective stress parameters C′ and ′ were found to be unique and independent of the stress path and two principal orientations. However, the values of ′ in extension tests were 6–7° higher than those in compression tests.