268 resultados para Bismuth tellurite glasses
Resumo:
Lithium silicophosphate glasses have been prepared by a sol-gel route over a wide range of compositions. Their structural and electrical properties have been investigated. Infrared spectroscopic studies show the presence of hydroxyl groups attached to Si and P. MAS NMR investigations provide evidence for the presence of different phosphatic units in the structure. The variations of de conductivities at 423 K and activation energies have been studied as a function of composition, and both exhibit an increasing trend with the ratio of nonbridging oxygen to bridging oxygen in the structure. Ac conductivity behavior shows that the power law exponent, s, is temperature dependent and exhibits a minimum. Relaxation behavior has been examined in detail using an electrical modulus formalism, and modulus data were fitted to Kohlraush-William-Watts stretched exponential function. A structural model has been proposed and the unusual properties exhibited by this unique system of glasses have been rationalized using this model. Ion transport in these glasses appears to be confined to unidimensional conduits defined by modified phosphate chains and interspersed with unmodified silica units.
Resumo:
Neutron diffraction measurement is carried out on GexSe1-x glasses, where 0.1 less than or equal to x less than or equal to 0.4, in a Q interval of 0.55-13.8 Angstrom(-1). The first sharp diffraction peak (FSDP) in the structure factor, S(Q), shows a systematic increase in the intensity and shifts to a lower Q with increasing Ge concentration. The coherence length of FSDP increases with x and becomes maximum for 0.33 less than or equal to x less than or equal to 0.4. The Monte-Carlo method, due to Soper, is used to generate S(Q) and also the pair correlation function, g(r). The generated S(Q) is in agreement with the experimental data for all x. Analysis of the first four peaks in the total correlation function, T(r), shows that the short range order in GeSe2 glass is due to Ge(Se-1/2)(4) tetrahedra, in agreement with earlier reports. Se-rich glasses contain Se-chains which are cross-linked with Ge(Se-1/2)(4) tetrahedra. Ge-2(Se-1/2)(6) molecular units are the basic structural units in Ge-rich, x = 0.4, glass. For x = 0.2, 0.33 and 0.4 there is evidence for some of the tetrahedra being in an edge-shared configuration. The number of edge-shared tetrahedra in these glasses increase with increasing Ge content.
Resumo:
The thermal properties and electrical-switching behavior of semiconducting chalcogenide SbxSe55-xTe45 (2 <= x <= 9) glasses have been investigated by alternating differential scanning calorimetry and electrical-switching experiments, respectively. The addition of Sb is found to enhance the glass forming tendency and stability as revealed by the decrease in non-reversing enthalpy Delta H-nr. and an increase in the glass-transition width Delta T-g. Further, the glass-transition temperature of SbxSe55-xTe45 glasses, which is a measure of network connectivity, exhibits a subtle increase, suggesting a meager network growth with the addition of Sb. The crystallization temperature is also observed to increase with Sb content. The SbxSe55-xTe45 glasses (2 <= x <= 9) are found to exhibit memory type of electrical switching, which can be attributed to the polymeric nature of network and high devitrifying ability. The metallicity factor has been found to dominate over the network connectivity and rigidity in the compositional dependence of switching voltage. which shows a profound decrease with the addition of Sb.
Resumo:
Barium lanthanum bismuth titanate (Ba1−(3/2)xLaxBi4Ti4O15, x = 0–0.4) ceramics were fabricated using the powders synthesized via the solid-state reaction route. X-ray powder diffraction analysis confirmed the above compositions to be monophasic and belonged to the m = 4 member of the Aurivillius family of oxides. The effect of the partial presence of La3+ on Ba2+ sites on the microstructure, dielectric and relaxor behaviour of BaBi4Ti4O15 (BBT) ceramics was investigated. For the compositions pertaining to x ≤ 0.1, the dielectric constant at both room temperature and in the vicinity of the temperature of the dielectric maximum (Tm) of the parent phase (BBT) increased significantly with an increase in x while Tm remained almost constant. Tm shifted towards lower temperatures accompanied by a decrease in the magnitude of the dielectric maximum (εm) with an increase in the lanthanum content (0.1 < x ≤ 0.4). The dielectric relaxation was modelled using the Vogel–Fulcher relation and a decrease in the activation energy for frequency dispersion with increasing x was observed. The frequency dispersion of Tm was found to decrease with an increase in lanthanum doping, and for compositions corresponding to x ≥ 0.3, Tm was frequency independent. Well-developed P(polarization)–E(electric field) hysteresis loops were observed at 150 °C for all the samples and the remanent polarization (2Pr) was improved from 6.3 µC cm−2 for pure BBT to 13.4 µC cm−2 for Ba0.7La0.2Bi4Ti4O15 ceramics. Dc conductivities and associated activation energies were evaluated using impedance spectroscopy.
Resumo:
Semieonducting GaxTe~oo-x (17 -< x _< 25) glasses have been prepared by melt quenching method and thermal crystallization studies carried out using differential scanning calorimetry. On heating, virgin GaxTel0o-x glasses exhibit one glass transition and two crystallization reactions.The first crystallization reaction corresponds to the precipitation of hexagonal Te and the second one to the crystallization of the matrix into zinc blende Ga2Te3 phase. If GaxTeloo-x glasses are quenched to ambient temperature from Tcrl and reheated, they exhibit the phenomenon of double glass transition.
Resumo:
Raman bandwidths and bandshapes of some molecular and ionic glasses have been investigated through the glass-transition region. Widths of both polarised and depolarised bands exhibit step-like changes during the glass transition. Molecular and ionic glasses differ with respect to the magnitude and the nature of variations in bandwidths and reorientational times. An attempt has been made to understand the changes in bandwidths around the glass-transition temperature.
Resumo:
In order to investigate the factors determining the relative stabilities of layered perovskite and pyrochlore structures of transition metal oxides containing trivalent bismuth, several ternary and quaternary oxides have been investigated. While d0 cations stabilize the layered perovskite structure, cations containing partially-filled d orbitals (which suppress ferroelectric distortion of MO6 octahedra) seem to favor pyrochlore-related structures. Thus, the vanadium analogue of the layered perovskite Bi4Ti3O12 cannot be prepared; instead the composition consists of a mixture of pyrochlore-type Bi1.33V2O6, Bi2O3, and Bi metal. The distortion of Bi1.33V2O6 to orthorhombic symmetry is probably due to an ordering of anion vacancies in the pyrochlore structure. None of the other pyrochlores investigated, Bi2NbCrO7, Bi2NbFeO7, TlBiM2O7 (M = Nb, Ta), shows evidence for cation ordering in the X-Ray diffraction patterns, as indeed established by structure refinement of TlBiNb2O7.
Resumo:
A study of the effect of bismuth dopant on the electronic transport properties of the amorphous semiconductors Ge20S80-xBix under high pressure (up to 140 kbar) has been carried out down to liquid-nitrogen temperature. The experiments reveal that the electronic conduction is strongly composition dependent and is thermally activated with a single activation energy at all pressures and for all compositions. A remarkable resemblance between the electronic conduction process, x-ray diffraction studies, and differential thermal analysis results is revealed. It is proposed that the n-type conduction in germanium chalcogenides doped with a large Bi concentration is due to the effect of Bi dopants on the positive correlation energy defects present in germanium chalcogenides. The impurity-induced chemical modification of the network creates a favorable environment for such an interaction.
Resumo:
Recent observation of n-type conduction in amorphous Ge20Ss_xBix at large bismuth concentrations (x = 11), which otherwise shows p-type conduction, has aroused considerable interest in the international scientific community [1]. The mechanism of such impurity incorporation in a germanium chalcogenide glass is not understood and is a topic of current interest. In our recent publications [2-10] we have brought to light some hitherto unknown and interesting features of bismuth dopants in chalcogen-rich Ge-X (X -- S, Se) glassy compositions. In this communication we present our new results of investigations on vitreous semiconductors Ge20S80 Bi using electron microscopy, electron diffraction of as-prepared and annealed/pressure quenched compositions. Our results provide conclusive support to the formation of composite clusters containing all the three elements, germanium, sulphur and bismuth, which crystallize in simpler stoichiometric compounds Bi2S3 and GeS2.
Resumo:
Transparent SrLiB9O15 (SLBO) glasses were fabricated via the conventional melt-quenching technique. X-ray powder diffraction and differential thermal analysis carried out on the as-quenched samples confirmed their amorphous and glassy nature, respectively. The dielectric constants in the 100 Hz to 10 MHz frequency range for SLBO glasses were measured as a function of temperature (300–1023 K). The dielectric relaxation characteristics were rationalized using the electric modulus formalism. The electrode polarization effect was subtracted from the low-frequency dielectric constant to have an insight into the intrinsic dielectric behavior of SLBO glasses. The imaginary part of electric modulus spectra was modeled using an approximate solution of Kohlrausch–Williams–Watts relation. The dielectric constant for the as-quenched glass increased with increasing temperature and exhibited anomalies in the vicinity of the glass transition and crystallization temperatures.
Resumo:
High pressure resistivity measurements on Se100-xTex, glasses for 0≤x≤30 are reported. Two composition regions, where the transport and transformation behaviour are different, are identified. For 0≤x≤6, there is a first-order-like transformation to metallic crystalline states, while for x>6 the transformation appears to be continuous. Glass-transition temperatures also show differences in trends as a function of composition around 6% Te. An attempt is made to explain the composition-dependent trends on the basis of known structural features of selenium glasses and of the nature of tellurium bonding. At concentrations with up to 6% tellurium, Te most likely enters selenium chain terminations, substituting for negatively charged Se1- defects, while at larger concentrations, tellurium probably enters chains and rings by a random substitution.
Resumo:
Resistivity behaviour of PbO---PbX2 (X=F,Cl) glasses has been investigated as a function of pressure at laboratory temperature. All PbO---PbX2 glasses undergo crystallization under pressure and the resistivities of crystallized samples are lower than the corresponding glasses. Transitions in PbO---PbF2 glasses exhibit a first order behaviour while transitions in PbO---PbCl2 glasses possess features of a continuous transition. The differences in the pressure behaviour of the two glass systems have been attributed to the differences in the ionic sizes of F− and Cl− ions and also to pressure induced modifications of Pb---O bonding.
Resumo:
Reaction of bismuth metal with WO$_3$ in the absence of oxygen yields interesting bronze-like phases. From analytical electron microscopy and X-ray photoelectron spectroscopy, the product phases are found to have the general composition Bi$_x$ WO$_3$ with bismuth in the 3+ state. Structural investigations made with high resolution electron micrscopy and cognate techniques reveal that when x < 0.02, a perovskite bronze is formed. When x $\geqslant$ 0.02, however, intergrowth tungsten bronzes (i.t.b.) containing varying widths of the WO$_3$ slab are formed, the lattice periodicity being in the range 2.3-5.1 nm in a direction perpendicular to the WO$_3$ slabs. Image-matching studies indicate that the bismuth atoms are in the tunnels of the hexagonal tungsten bronze (h.t.b.) strips and the h.t.b. strips always remain one-tunnel wide. Annealed samples show a satellite structure around the superlattice spots in the electron diffraction patterns, possibly owing to ordering of the bismuth atoms in the tunnels. The i.t.b. phases show recurrent intergrowths extending up to 100 nm in several crystals. The periodicity varies considerably within the same crystal wherever there is disordered intergrowth, but unit cell dimensions can be assigned from X-ray and electron diffraction patterns. The maximum value of x in the i.t.b. phases is ca. 0.07 and there is no evidence for the i.t.b. phase progressively giving way to the h.t.b. phase with increase in x. Hexagonal tungsten bronzes that contain bismuth with x up to 0.02 can be formed by starting from hexagonal WO$_3$, but the h.t.b. phase seems to be metastable. Optical, magnetic and electron transport properties of the i.t.b. phases have been measured and it appears that the electrons become itinerant when x > 0.05.