201 resultados para BLUE EMISSION
Resumo:
We report the synthesis of Eu3+-activated SrMoO4 phosphors by the facile nitrate-citrate gel combustion method. Powder XRD and Rietveld refinement data confirmed that these phosphors have a monophasic scheelite-type tetragonal structure with space group I4(1)/a (No. 88). FESEM micrographs indicate the agglomerated spherical particles. FTIR spectra showed four stretching and bending vibrational modes (2A(u) and 2E(u)). UV-Visible absorption spectroscopy illustrated that the optical band gap energy (E-g) values increase with increase in Eu3+ concentration. The host SrMoO4 phosphor exhibited an intense blue emission under UV excitation (368 nm). The Eu3+-activated SrMoO4 phosphors revealed characteristic luminescence due to Eu3+ ion corresponding to D-5(1) -> F-7(J) (J = 1,2) and D-5(0) -> F-7(J) (J = 1,2,3,4) transitions upon 465 nm excitation. The electric dipole transition located at 615 nm (D-5(0) -> F-7(2)) was stronger than the magnetic dipole transition located at 592 nm (D-5(0) -> F-7(1)). Intensity parameters (Omega(2), Omega(4)) and radiative properties such as transition probabilities (A(T)), radiative lifetime (tau(rad)) and branching ratio (beta) of Eu3+-activated SrMoO4 phosphors were calculated using the Judd-Ofelt theory. Based on the CIE chromaticity diagram, these phosphors can be promising materials for the development of blue and orange-red component in white LEDs. (C) 2015 Elsevier B.V. All rights reserved.
Resumo:
Nanocrystalline powders of Ba1-xMgxZr0.1Ti0.9O3 (x = 0.025-0.1) were synthesized via citrate assisted sol-gel method. Interestingly, the one with x = 0.05 in the system Ba1-xMgxZr0.1Ti0.9O3 exhibited fairly good piezoelectric response aside from the other physical properties. The phase and structural confirmation of synthesized powder was established by X-ray powder diffraction (XRD) and Raman Spectroscopic techniques. Two distinct Raman bands i.e., 303 and 723 cm(-1) characteristic of tetragonal phase were observed. Thermogravimetric analysis (TGA) was performed to evaluate the phase decomposition of the as-synthesized Ba0.95Mg0.05Zr0.1Ti0.9O3 sample as a function of temperature. The average crystallite size associated with Ba0.95Mg0.05Zr0.1Ti0.9O3 was calculated using Scherrer formula based on the XRD data and was found to be 25 nm. However, Scanning and Transmission Electron Microscopy studies revealed the average crystallite size to be in the range of 30-40 nm, respectively. Kubelka-Munk function was employed to determine the optical band gap of these nanocrystallites. A piezoelectric response of 26 pm/V was observed for Ba0.95Mg0.05Zr0.1Ti0.9O3 nanocrystal by Piezoresponse Force Microscopy (PFM) technique. Photoluminescence (PL) study carried out on these nanocrystals exhibited a blue emission (470 nm) at room temperature.
Resumo:
Cibacron blue is a potent inhibitor of 3-HBA-6-hydroxylase at a concentration < 1 mu M. Kinetic analyses revealed that at a concentration below 0.5 mu M the dye behaves as an uncompetitive inhibitor with respect to 3-HBA and competes with NADH for the same site on the enzyme. The alteration of the near-UV CD spectrum and quenching of the emission fluorescence of the enzyme by cibacron blue indicates a significant alteration in the environment of aromatic amino acid residues due to a stacking interaction and subtle conformatiodnal changes in the enzyme. The concentration-dependent quenching of the intrinsic fluorescence of the enzyme by cibacron blue was employed to determine the binding parameters such as association constant (K-a) and stoichiometry (r) for the enzyme-dye complex.
Resumo:
Body-centered-tetragonal (BCT) ZnS nanocrystals have been synthesized, for the first time to the best of our knowledge, by using the chemical coprecipitation method at higher synthesis temperatures of 65 and 95 degrees C. It is confirmed from X-ray diffraction (XRD) studies that in the high-temperature-synthesized samples, cubic and BCT phases coexist, in contrast to the room-temperature-synthesized sample, which consists of only cubic phase with sizes of the particles lying between 2 and 3 nm. The sizes of BCT phase nanocrystals are bigger than those of cubic phase of ZnS. The presence of BCT phase of ZnS in the samples is increased from 40 to 90% when the temperature of synthesis is increased from 65 to 95 degrees C. The nanocrystalline nature and UV-Vis absorption characteristics of the prepared samples have been studied with a transmission electron microscope (TEM) and a UV-Visible pectrophotometer, respectively. The room-temperature-synthesized ZnS sample shows photoluminescence (PL) emission in the blue region with multiple peaks, whereas the high-temperature-synthesized samples show PL emissions in the visible region. The Gaussian fittings of the measured PL spectra shows that three PL peaks at 429, 477, and 525 nm are appeared in the 65 degrees C sample and two peaks at 491 and 540 nm appear in the 95 degrees C sample with the enhanced PL intensity of the green peak at 540 nm. (C) 2010 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim
Resumo:
In this paper, recent results on band A emission in chemical vapor-deposited diamond films have been analyzed within a vibronic model. The blue-band A (2.8 eV) spectra from undoped diamond films grown by two different techniques have been simulated using the same phonon density distribution g(Omega) and Huang-Rhys factor (S). The same g(Omega) at higher S gives a good fit with the green band A (2.32 eV) as well. This model provides a reasonable alternative approach to the long standing donor-acceptor pair recombination model.
Resumo:
The synthesis, hydrogelation, and aggregation-induced emission switching of the phenylenedivinylene bis-N-octyl pyridinium salt is described. Hydrogelation occurs as a consequence of pi-stacking, van der Waals, and electrostatic interactions that lead to a high gel melting temperature and significant mechanical properties at a very low weight percentage of the gelator. A morphology transition from fiber-to-coil-to-tube was observed depending on the concentration of the gelator. Variation in the added salt type, salt concentrations, or temperature profoundly influenced the order of aggregation of the gelator molecules in aqueous solution. Formation of a novel chromophore assembly in this way leads to an aggregation-induced switch of the emission colors. The emission color switches from sky blue to white to orange depending upon the extent of aggregation through mere addition of external inorganic salts. Remarkably, the salt effect on the assembly of such cationic phenylenedivinylenes in water follow the behavior predicted from the well-known Hofmeister effects. Mechanistic insights for these aggregation processes were obtained through the counterion exchange studies. The aggregation-induced emission switching that leads to a room-temperature white-light emission from a single chromophore in a single solvent (water) is highly promising for optoelectronic applications.
Resumo:
Porous fungus-like ZnO nanostructures have been synthesized by simple thermal annealing of the hydrothermally synthesized sheet-like ZnS(en)(0.5) complex precursor in air at 600 degrees C. Structural and morphological changes occurring during ZnS(en)(0.5) -> ZnS -> ZnO transformations have been observed closely by annealing the as-synthesized precursor at 100-600 degrees C. Wurtzite ZnS nanosheets and ZnS-ZnO composites are obtained at temperatures of 400 degrees C and 500 degrees C, respectively. Thermal decomposition and oxidation of the ZnS(en) 0.5 nanosheets have been confirmed by differential scanning calorimetry and thermo-gravimetric analysis. The visible light driven photocatalytic degradation of methylene blue dye has been demonstrated in the synthesized samples. ZnS-ZnO composite shows the highest dye degradation efficiency of 74% due to the formation of surface complex as well as higher visible light absorption as a result of band-gap narrowing effect. The porous ZnO nanostructures show efficient visible photoluminescence (PL) emission with a colour coordinate of (0.29, 0.35), which is close to that of white light (0.33, 0.33). The efficient visible PL emission as well as visible light driven photocatalytic activity of the materials synthesized in the present work might be very attractive for their applications in future optoelectronic devices, including in white light emitting devices.
Resumo:
A controllable synthesis of phase pure wurtzite (WZ) ZnS nanostructures has been reported in this work at a low temperature of similar to 220 degrees C using ethylenediamine as the soft template and by varying the molar concentration of zinc to sulphur precursors as well as by using different precursors. A significant reduction in the formation temperature required for the synthesis of phase pure WZ ZnS has been observed. A strong correlation has been observed between the morphology of the synthesized ZnS nanostructures and the precursors used during synthesis. It has been found from Scanning Electron Microscope (SEM) and Transmission Electron Microscope (TEM) image analyses that the morphology of the ZnS nanocrystals changes from a block-like to a belt-like structure having an average length of similar to 450 nm when the molar ratio of zinc to sulphur source is increased from 1 : 1 to 1 : 3. An oriented attachment (OA) growth mechanism has been used to explain the observed shape evolution of the synthesized nanostructures. The synthesized nanostructures have been characterized by the X-ray diffraction technique as well as by UV-Vis absorption and photoluminescence (PL) emission spectroscopy. The as-synthesized nanobelts exhibit defect related visible PL emission. On isochronal annealing of the nanobelts in air in the temperature range of 100-600 degrees C, it has been found that white light emission with a Commission Internationale de I'Eclairage 1931 (CIE) chromaticity coordinate of (0.30, 0.34), close to that of white light (0.33, 0.33), can be obtained from the ZnO nanostructures obtained at an annealing temperature of 600 degrees C. UV light driven degradation of methylene blue (MB) dye aqueous solution has also been demonstrated using as-synthesized nanobelts and similar to 98% dye degradation has been observed within only 40 min of light irradiation. The synthesized nanobelts with visible light emission and having dye degradation activity can be used effectively in future optoelectronic devices and in water purification for cleaning of dyes.
Resumo:
Although semiconductor quantum dots are promising materials for displays and lighting due to their tunable emissions, these materials also suffer from the serious disadvantage of self-absorption of emitted light. The reabsorption of emitted light is a serious loss mechanism in practical situations because most phosphors exhibit subunity quantum yields. Manganese-based phosphors that also exhibit high stability and quantum efficiency do not suffer from this problem but in turn lack emission tunability, seriously affecting their practical utility. Here, we present a class of manganese-doped quantum dot materials, where strain is used to tune the wavelength of the dopant emission, extending the otherwise limited emission tunability over the yellow-orange range for manganese ions to almost the entire visible spectrum covering all colors from blue to red. These new materials thus combine the advantages of both quantum dots and conventional doped phosphors, thereby opening new possibilities for a wide range of applications in the future.
Resumo:
Dual photoluminescence (PL) emission characteristics of Mn2+ doped ZnS (ZnS:Mn) quantum dots (QDs) have drawn a lot of attention recently. However, here we report the effect of thermal annealing on the PL emission characteristics of uncapped ZnS:Mn QDs of average sizes similar to 2-3 nm, synthesized by simple chemical precipitation method by using de-ionized (DI) water at room temperature. As-synthesized samples show dual PL emissions, having one UV PL band centred at similar to 400 nm and the other in the visible region similar to 610 nm. But when the samples are isochronally annealed for 2 h at 100-600 degrees C temperature range in air, similar to 90% quenching of Mn2+ related visible PL emission intensity takes place at the annealing temperature of 600 degrees C. X-ray diffraction data show that the as-synthesized cubic ZnS has been converted to wurtzite ZnO at 600 degrees C annealing temperature. The nanostructural properties of the samples are also determined by transmission electron micrograph, electron probe micro-analyser and UV-vis spectrophotometry. The photocatalytic property of the annealed ZnS:Mn sample has been demonstrated and photo-degradation efficiency of the as-synthesized and 600 degrees C annealed ZnS:Mn sample has been found out to be similar to 35% and similar to 61%, respectively, for the degradation of methylene blue dye under visible light irradiation. The synthesized QDs may find significant applications in future optoelectronic devices. (C) 2014 Elsevier B.V. All rights reserved.
Resumo:
Herein we report the synthesis, characterization, and potential application of his (4- (7,9,10-triphenylfluoranthen-8-yl)pheny)sulfone (TPFDPSO2) and 2,8-bis (7,9,10-triphenylfluoranthen-8-yl) dibenzo b, d]-thiophene 5,5-dioxide (TPFDBTO2) as electron transport as well as light-emitting materials. These fluoranthene derivatives were synthesized by oxidation of their corresponding parent sulfide compounds, which were prepared via Diels-Alder reaction. These materials exhibit deep blue fluorescence emission in both solution and thin film, high photoluminescence quantum yield (PLQY), thermal and electrochemical stability over a wide potential range. Hole- and electron-only devices were fabricated to study the charge transport characteristics, and predominant electron transport property comparable with that of a well-known electron transport material, Alq(3), was observed. Furthermore, bilayer electroluminescent devices were fabricated utilizing these fluoranthene derivatives as electron transport as well as emitting layer, and device performance was compared with that of their parent sulfide molecules. The electroluminescence (EL) devices fabricated with these molecules displayed bright sky blue color emission and 5-fold improvement in external quantum efficiency (EQE) with respect to their parent compounds.
Resumo:
We have synthesized a series of 4'-aryl substituted 2,2':6',2 `'-terpyridine (terpy) derivatives, namely 4'-(4-methylphenyl)-2,2':6',2 `'-terpyridine (C-1), 4'-(2-furyl)-2,2':6'2 `'-terpyridine (C-2), and 4'-(3,4,5-trimethoxyphenyl)-2,2':6',2 `'-terpyridine (C-3). The synthesized terpy compounds were characterized by elemental analyses, FTIR, NMR (H-1 and C-13), and ESI-Mass spectrometry. Photophysical, electrochemical and thermal properties of terpy compounds were systematically studied. Maximum excitation band was observed between 240 and 330 nm using UV-visible spectra, and maximum emission peaks from PL spectra were observed at 385, 405 and 440 nm for C-1, C-2 and C-3 respectively. Fluorescence lifetime (tau) of the fluorophores was found to be 035 and 1.55 ns at the excitation wavelength of 406 nm for C-1 and C-2 respectively, and tau value for C-3 was found to be 0.29 ns at the excitation wavelength of 468 nm. We noticed that the calculated values of HOMO energy levels were increased from 5.96 (C-1) to 6.08 (C-3) eV, which confirms that C-3 derivative is more electrons donating in nature. The calculated electrochemical band gaps were 2.95, 2.82 and 3.02 eV for C-1, C-2 and C-3 respectively. These blue fluorescent emitter derivatives can be used as an electron transport and electroluminescent material to design the blue fluorescent organic light emitting diode (OLED) applications. (C) 2015 Elsevier B.V: All rights reserved.
Resumo:
Here, we report the hydrothermal synthesis of boron-doped CNPs (B-CNPs) with different size/atomic percentage of doping and size-independent color tunability from red to blue. The variation of size/atomic percentage of B is achieved by simply varying the reaction time, while the color tunability is obtained by diluting the solution. With dilution, the luminescence spectra are not only blue-shifted, the intensity increases as well. The huge blue-shift in the emission energy (similar to 1 eV) is believed to be due to the increase in the interparticle distance. The quantum yield with optimum dilution is found to increase with boron doping though it is very low as compared to CNPs and nitrogen-doped CNPs. Finally, we show that B-CNPs with a quantum yield of 0.5% can be used for bioimaging applications. (C) 2015 Elsevier Ltd. All rights reserved.
Resumo:
CdS nanoparticles exhibit size dependent optical and electrical properties. We report here the photocurrent and I-V characteristic studies of CdS nanoparticle devices. A sizable short circuit photocurrent was observed in the detection range governed by the size of the clusters. We speculate on the mechanisms leading to the photocurrent and emission in these nanometer scale systems.
Resumo:
The interaction of Cibacron blue F3GA with ribosome inactivating proteins, ricin, ricin A-chain and momordin has been investigated using difference absorption spectroscopy. Ricin was found to bind the dye with a 20- and 2-fold lower affinity than ricin A-chain and momordin, respectively. A time dependent increase in the amplitude of Cibacron blue difference spectrum in the presence of ricin was observed on addition of beta-mercaptoethanol. Analysis of the kinetic profile of this increase showed a biphasic phenomenon and the observed rates were found to be independent of the concentration of beta-mercaptoethanol. Kinetics of reduction of the intersubunit disulphide bond in ricin by beta-mercaptoethanol showed that reduction pet se is a second order reaction. Therefore, the observed changes in the difference spectra of Cibacron blue probably indicate a slow change in the conformation of ricin, triggered by reduction of the intersubunit disulphide bond.