233 resultados para Fracture surfaces
Resumo:
The fracture of eutectic Si particles dictates the fracture characteristics of Al-Si based cast alloys. The morphology of these particles is found to play an important role in fracture initiation. In the current study, the effects of strain rate, temperature, strain, and heat treatment on Si particle fracture under compression were investigated. Strain rates ranging from 3 x 10(-4)/s to 10(2)/s and three temperatures RT, 373 K, and 473 K (100 A degrees C and 200 A degrees C) are considered in this study. It is found that the Si particle fracture shows a small increase with increase in strain rate and decreases with increase in temperature at 10 pct strain. The flow stress at 10 pct strain exhibits the trend similar to particle fracture with strain rate and temperature. Particle fracture also increases with increase in strain. Large and elongated particles show a greater tendency for cracking. Most fracture occurs on particles oriented nearly perpendicular to the loading axis, and the cracks are found to occur almost parallel to the loading axis. At any strain rate, temperature, and strain, the Si particle fracture is greater for the heat-treated condition than for the non-heat-treated condition because of higher flow stress in the heat-treated condition. In addition to Si particle fracture, elongated Fe-rich intermetallic particles are also seen to fracture. These particles have specific crystallographic orientations and fracture along their major axis with the cleavage planes for their fracture being (100). Fracture of these particles might also play a role in the overall fracture behavior of this alloy since these particles cleave along their major axis leading to cracks longer than 200 mu m.
Resumo:
This paper deals with a combined forming and fracture limit diagram and void coalescence analysis for the aluminum alloy Al 1145 alloy sheets of 1.8 mm thickness, annealed at four different temperatures, namely 200, 250, 300, and 350 A degrees C. At different annealing temperatures these sheets were examined for their effects on microstructure, tensile properties, formability, void coalescence, and texture. Scanning electron microscope (SEM) images taken from the fractured surfaces were examined. The tensile properties and formability of sheet metals were correlated with fractography features and void analysis. The variation of formability parameters, normal anisotropy of sheet metals, and void coalescence parameters were compared with texture analysis.
Resumo:
Inspired by the Brazilian disk geometry we examine the utility of an edge cracked semicircular disk (ECSD) specimen for rapid assessment of fracture toughness of brittle materials using compressive loading. It is desirable to optimize the geometry towards a constant form factor F for evaluating K-I. In this investigation photoelastic and finite element results for K-I evaluation highlight the effect of loading modeled using a Hertzian. A Hertzian loading subtending 4 degrees at the center leads to a surprisingly constant form factor of 1.36. This special case is further analyzed by applying uniform pressure over a chord for facilitating testing.
Resumo:
Results of a high resolution photoemission and electrochemistry study of Se adsorption Au(111) and Ag(111) surfaces performed by immersion of pristine samples into an aqeuous solution of Na2Se are presented. Cyclic voltammetry on Au shows formation of selenium adsorbed species and the structures observed in reductive desorption are to the atomic and polymeric species observed in XPS. In the case of Au(111) XPS spectra in the Se(3d) region indeed show two main features attributed to Se chemisorbed atomically and polymeric Se-8 features.' Smaller structures due to other types of Se conformations were also observed. The Au(4f) peak line, shape does not show core level, shifts: indicative of Au selenide formation the case of silver, XPS spectra for the Ag(3d) show a broadening of the peak and a deconvolution into Ag-B bulk like Ag-Se components shows that the Ag-Se is located at a lower binding energy, an effect similar to oxidation and sulfidation of Ag. The Se(3d) XPS spectrum is found to be substantially different from the Au case and dominated by atomic type Se due to the selenide, though a smaller intensity Se structure at an energy similar to the Se-8 structure for Au is also observed. Changes in the valence band region. related to Se adsorption are reported.
Resumo:
The RILEM work-of-fracture method for measuring the specific fracture energy of concrete from notched three-point bend specimens is still the most common method used throughout the world, despite the fact that the specific fracture energy so measured is known to vary with the size and shape of the test specimen. The reasons for this variation have also been known for nearly two decades, and two methods have been proposed in the literature to correct the measured size-dependent specific fracture energy (G(f)) in order to obtain a size-independent value (G(F)). It has also been proved recently, on the basis of a limited set of results on a single concrete mix with a compressive strength of 37 MPa, that when the size-dependent G(f) measured by the RILEM method is corrected following either of these two methods, the resulting specific fracture energy G(F) is very nearly the same and independent of the size of the specimen. In this paper, we will provide further evidence in support of this important conclusion using extensive independent test results of three different concrete mixes ranging in compressive strength from 57 to 122 MPa. (c) 2013 Elsevier Ltd. All rights reserved.
Resumo:
We interpret a normal surface in a (singular) three-manifold in terms of the homology of a chain complex. This allows us to study the relation between normal surfaces and their quadrilateral coordinates. Specifically, we give a proof of an (unpublished) observation independently given by Casson and Rubinstein saying that quadrilaterals determine a normal surface up to vertex linking spheres. We also characterize the quadrilateral coordinates that correspond to a normal surface in a (possibly ideal) triangulation.
Resumo:
This article reports the acoustic emission (AE) study of precursory micro-cracking activity and fracture behaviour of quasi-brittle materials such as concrete and cement mortar. In the present study, notched three-point bend specimens (TPB) were tested under crack mouth opening displacement (CMOD) control at a rate of 0.0004 mm/sec and the accompanying AE were recorded using a 8 channel AE monitoring system. The various AE statistical parameters including AE event rate , AE energy release rate , amplitude distribution for computing the AE based b-value, cumulative energy (I E) pound and ring down count (RDC) were used for the analysis. The results show that the micro-cracks initiated and grew at an early stage in mortar in the pre peak regime. While in the case of concrete, the micro-crack growth occurred during the peak load regime. However, both concrete and mortar showed three distinct stages of micro-cracking activity, namely initiation, stable growth and nucleation prior to the final failure. The AE statistical behavior of each individual stage is dependent on the number and size distribution of micro-cracks. The results obtained in the laboratory are useful to understand the various stages of micro-cracking activity during the fracture process in quasi-brittle materials such as concrete & mortar and extend them for field applications.
Resumo:
A droplet residing on a vibrating surface and in the pressure antinode of an asymmetric standing wave can spread radially outward and atomize. In this work, proper orthogonal decomposition through high speed imaging is shown to predict the likelihood of atomization for various viscous fluids based on prior information in the droplet spreading phase. Capillary instabilities are seen to affect ligament rupture. Viscous dissipation plays an important role in determining the wavelength of the most unstable mode during the inception phase of the ligaments. However, the highest ligament capillary number achieved was less than 1, and the influence of viscosity in the ligament growth and breakup phases is quite minimal. It is inferred from the data that the growth of a typical ligament is governed by a balance between the inertial force obtained from the inception phase and capillary forces. By including the effect of acoustic pressure field around the droplet, the dynamics of the ligament growth phase is revealed and the ligament growth profiles for different fluids are shown to collapse on a straight line using a new characteristic time scale.
Resumo:
Let X be an arbitrary complex surface and D subset of X a domain that has a noncompact group of holomorphic automorphisms. A characterization of those domains D that admit a smooth real analytic, finite type, boundary orbit accumulation point and whose closures are contained in a complete hyperbolic domain D' subset of X is obtained.
Resumo:
The study of the fracture behaviour of concrete structures using the fictitious crack model requires two fracture properties of the concrete mix, namely, the size-independent specific fracture energy G(F). and the corresponding tension softening relation sigma(w) between the residual stress carrying capacity sigma and the crack opening w in the fracture process zone ahead of a real crack. In this paper, bi-linear tension softening diagrams of three different concrete mixes, ranging in compressive strength from 57 to 122 MPa whose size-independent specific fracture energy has been previously determined, have been constructed in an inverse manner based on the concept of a non-linear hinge from the load-crack mouth opening plots of notched three-point bend beams. (C) 2013 Elsevier Ltd. All rights reserved.
Resumo:
This article presents the details of estimation of fracture parameters for high strength concrete (HSC, HSC1) and ultra high strength concrete (UHSC). Brief details about characterization of ingredients of HSC, HSC1 and UHSC have been provided. Experiments have been carried out on beams made up of HSC, HSC1 and UHSC considering various sizes and notch depths. Fracture characteristics such as size independent fracture energy (G(f)), size of fracture process zone (C-f), fracture toughness (K-IC) and crack tip opening displacement (CTODc) have been estimated based on the experimental observations. From the studies, it is observed that (i) UHSC has high fracture energy and ductility inspite of having a very low value of C-f; (ii) relatively much more homogeneous than other concretes, because of absence of coarse aggregates and well-graded smaller size particles; (iii) the critical SIF (K-IC) values are increasing with increase of beam depth and decreasing with increase of notch depth. Generally, it can be noted that there is significant increase in fracture toughness and CTODc. They are about 7 times in HSC1 and about 10 times in UHSC compared to those in HSC; (iv) for notch-to-depth ratio 0.1, Bazant's size effect model slightly overestimates the maximum failure loads compared to experimental observations and Karihaloo's model slightly underestimates the maximum failure loads. For the notch-to-depth ratio ranging from 0.2 to 0.4 for the case of UHSC, it can be observed that, both the size effect models predict more or less similar maximum failure loads compared to corresponding experimental values.
Resumo:
The fracture characteristics of Al-Si based eutectic alloy are investigated in the unmodified and modified conditions under compression. The investigations are carried out at different strain rates and temperatures. Fracture of the alloy starts with eutectic Si particle fracture and modification plays an important role in particle fracture. The fraction of fractured particles is found to be always lesser in the modified condition than in the unmodified condition. Particle fracture increases with increase in strain. It is found that the Si particle fracture shows an increase with increase in strain rate and decreases with increase in temperature at 10% strain. Large and elongated particles show a greater tendency for fracture in the unmodified and modified conditions. Particle orientation plays an important role on fracture and the cracks are found to occur almost in a direction normal to the tensile strain imposed upon the particles by the deforming matrix in the unmodified alloy. The modified alloy shows a random distribution of fractured particles and crack orientation. The criteria of fracture based on dislocation pile-up mechanism and fiber loading explain the observed difference in particle fracture characteristics due to modification. The particle fracture for the modified alloy is also discussed in terms of Weibull statistics and the existing models of dispersion hardening. Particle/matrix interface decohesion is observed at higher strain rates and temperatures in the modified alloy. Dendritic rotation of 10 degrees is also observed at higher strain rates, which can increase the amount of particle fracture. (C) 2013 Elsevier B.V. All rights reserved.
Resumo:
A fracture mechanism map (FMM) is a powerful tool which correlates the fracture behavior of a material to its microstructural characteristics in an explicit and convenient way. In the FMM for solder joints, an effective thickness of the interfacial intermetallic compound (IMC) layer (t (eff)) and the solder yield strength (sigma (ys,eff)) are used as abscissa and ordinate axes, respectively, as these two predominantly affect the fracture behavior of solder joints. Earlier, a definition of t (eff), based on the uniform thickness of IMC (t (u)) and the average height of the IMC scallops (t (s)), was proposed and shown to aptly explain the fracture behavior of solder joints on Cu. This paper presents a more general definition of t (eff) that is more widely applicable to a range of metallizations, including Cu and electroless nickel immersion gold (ENIG). Using this new definition of t (eff), mode I FMM for SAC387/Cu joints has been updated and its validity was confirmed. A preliminary FMM for SAC387/Cu joints with ENIG metallization is also presented.
Resumo:
In this work, the fracture behavior of magnesium single crystals is studied by conducting experiments with notched three point bend specimens of three crystallographic orientations. In the first and second orientations, the c-axis is along the normal to the flat surface of the notch, while in the third it is aligned with the notch front. For all the orientations, in situ electron back scattered diffraction observations made around the notch root show profuse tensile twinning of {10 (1) over bar2} type. Further, in the first two orientations basal and prismatic slip traces are identified from optical metallography. The width of the most prominent twin saturates at around 120-150 mu m, while twins continue to nucleate farther away to accommodate plastic deformation. In all the orientations, crack initiation occurs before the attainment of peak load and the crack grows stably along twin-matrix interface before deflecting at twin-twin intersections. Results show that profuse tensile twinning is an important energy dissipating mechanism that enhances the fracture toughness. (C) 2013 Elsevier B.V. All rights reserved.