478 resultados para optical testing
Resumo:
The bipolar point spread function (PSF) corresponding to the Wiener filter tor correcting linear-motion-blurred pictures is implemented in a noncoherent optical processor. The following two approaches are taken for this implementation: (1) the PSF is modulated and biased so that the resulting function is non-negative and (2) the PSF is split into its positive and sign-reversed negative parts, and these two parts are dealt with separately. The phase problem associated with arriving at the pupil function from these modified PSFs is solved using both analytical and combined analytical-iterative techniques available in the literature. The designed pupil functions are experimentally implemented, and deblurring in a noncoherent processor is demonstrated. The postprocessing required (i.e., demodulation in the first approach to modulating the PSF and intensity subtraction in the second approach) are carried out either in a coherent processor or with the help of a PC-based vision system. The deblurred outputs are presented.
Resumo:
Hard, low stress diamond-like carbon films have been deposited by plasma assisted chemical vapour deposition technique, The various substrates include soft IR components like ZnS and ZnSe windows, Gaseous precursors such as propene, ethyl alcohol and acetone have been used to synthesize the films to study the nature of precursors in determining the film compatibility with the underlying component (substrate), The residual compressive stresses, the Young's modulus and the adhesion energy of the films have been estimated to be 10(10) dynes/cm(2), 10(10) N/m(2) and 1000 ergs/cm(2) respectively. To alleviate film failure, a study on the effects of additive gases such as hydrogen and the use of buffer layers such as ZrO2, has been undertaken, The diamond-like carbon films produced here are hard (5000 kg/mm(2)), specularly smooth in the wavelength region from 2.5 mu m to 20 mu m, with no microstructural features and have excellent adhesion on ZnS and ZnSe windows. The figure of merit of these films for aero-space applications has been evaluated by subjecting the film-buffer layer ZnS or ZnSe composite stack to wind, dust and rain erosion studies and by establishing the integrity of the specular IR transmittance of the stack upto 16 or 20 mu m as the case may be.
Resumo:
Strain-rate effects on the low-cycle fatigue (LCF) behavior of a NIMONIC PE-16 superalloy have been evaluated in the temperature range of 523 to 923 K. Total-strain-controlled fatigue tests were per-formed at a strain amplitude of +/-0.6 pct on samples possessing two different prior microstructures: microstructure A, in the solution-annealed condition (free of gamma' and carbides); and microstructure B, in a double-aged condition with gamma' of 18-nm diameter and M23C6 carbides. The cyclic stress response behavior of the alloy was found to depend on the prior microstructure, testing temperature, and strain rate. A softening regime was found to be associated with shearing of ordered gamma' that were either formed during testing or present in the prior microstructure. Various manifestations of dynamic strain aging (DSA) included negative strain rate-stress response, serrations on the stress-strain hysteresis loops, and increased work-hardening rate. The calculated activation energy matched well with that for self-diffusion of Al and Ti in the matrix. Fatigue life increased with an increase in strain rate from 3 x 10(-5) to 3 x 10(-3) s-1, but decreased with further increases in strain rate. At 723 and 823 K and low strain rates, DSA influenced the deformation and fracture behavior of the alloy. Dynamic strain aging increased the strain localization in planar slip bands, and impingement of these bands caused internal grain-boundary cracks and reduced fatigue life. However, at 923 K and low strain rates, fatigue crack initiation and propagation were accelerated by high-temperature oxidation, and the reduced fatigue life was attributed to oxidation-fatigue interaction. Fatigue life was maximum at the intermediate strain rates, where strain localization was lower. Strain localization as a function of strain rate and temperature was quantified by optical and scanning electron microscopy and correlated with fatigue life.
Resumo:
We present a method for measuring the local velocities and first-order variations in velocities in a timevarying image. The scheme is an extension of the generalized gradient model that encompasses the local variation of velocity within a local patch of the image. Motion within a patch is analyzed in parallel by 42 different spatiotemporal filters derived from 6 linearly independent spatiotemporal kernels. No constraints are imposed on the image structure, and there is no need for smoothness constraints on the velocity field. The aperture problem does not arise so long as there is some two-dimensional structure in the patch being analyzed. Among the advantages of the scheme is that there is no requirement to calculate second or higher derivatives of the image function. This makes the scheme robust in the presence of noise. The spatiotemporal kernels are of simple form, involving Gaussian functions, and are biologically plausible receptive fields. The validity of the scheme is demonstrated by application to both synthetic and real video images sequences and by direct comparison with another recently published scheme Biol. Cybern. 63, 185 (1990)] for the measurement of complex optical flow.
Resumo:
The advent of high intensity lasers coupled with the recent advances in crystal technology has led to rapid progress in the field of nonlinear optics. This article traces the history of materials development that has taken place over the past forty odd years and dwells on the current status in this important area. The materials aspect is discussed under three classes viz. inorganic, organic and semiorganic crystals. In the end, some of the crystal growth work that has been carried out in author's laboratory is presented.
Resumo:
Attempts to prepare hydrogen-bond-directed nonlinear optical materials from a 1:1 molar mixture Of D-(+)-dibenzoyltartaric acid (DBT, I) and 4-aminopyridine (4-AP, II) resulted in two salts of different stoichiometry. One of them crystallizes in an unusual 1.5:1 (acid:base) monohydrate salt form III while the other one crystallizes as 1:1 (acid:base) salt IV. Crystal structures of both of the salts were determined from single-crystal X-ray diffraction data. The salt III crystallizes in a monoclinic space group C2 with a = 30.339(l), b = 7.881(2), c = 14.355(1) angstrom, beta = 97.48(1)degrees, V = 3403.1(9) angstrom3, Z = 4, R(w) = 0.058, R(w)= 0.058. The salt IV also crystallizes in a monoclinic space group P2(1) with a = 7.500(1), b = 14.968(2), c = 10.370(1) angstrom, beta = 102.67(1)degrees, V = 1135.9(2) angstrom3, Z = 2, R = 0.043, R(w) = 0.043. Interestingly, two DBT molecules with distinctly different conformation are present in the same crystal lattice of salt III. Extensive hydrogen-bonding interactions are found in both of the salts, and both of them show SHG intensity 1.4-1.6 times that of urea.
Resumo:
Optimum design of dynamic fracture test rigs demands a thorough appreciation of beam vibration under impact. Analyses invariably presume rigid anvils, and neglect overhang effects. The beam response predicted analytically and numerically in this paper highlights the significant role of anvil rigidity and beam overhangs on the impact dynamics of three point bend (3PB) specimens.
Resumo:
Optical absorption and photoluminescence studies have been carried out at room temperature in 25 R2O-25 GeO2-49.5 B2O3-0.5 Nd2O3 glass systems, (Composition in mol%, R= Li, Na, K and Rb). Judd Ofelt Intensity parameters and other parameters like Racah (E-1, E-2 and E-3), Slater-Condon-Shortley (F-2, F-4 and F-6) Spin-Orbit Coupling (xi(4f)) and Configuration Interaction (alpha,beta and gamma) for Nd3+ ion in the glass system are calculated. The variation of the 02 parameters are interpreted in terms of the covalency of the RE ion in the glass matrix. Further the hypersensitive transition I-4(9/2) -> (4)G(5/2), (2)G(7/2) is analyzed with respect to the intensity ratio I-L/I-S and is found to be dependent on the type of alkali in the glass matrix. The Photoluminescence studies do not show any appreciable shift in the peak emission wavelength of the F-4(3/2) to I-4(11/2) transition with the change in alkali type. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
We present a method for measuring the local velocities and first-order variations in velocities in a time-varying image. The scheme is an extension of the generalized gradient model that encompasses the local variation of velocity within a local patch of the image. Motion within a patch is analyzed in parallel by 42 different spatiotemporal filters derived from 6 linearly independent spatiotemporal kernels. No constraints are imposed on the image structure, and there is no need for smoothness constraints on the velocity field. The aperture problem does not arise so long as there is some two-dimensional structure in the patch being analyzed. Among the advantages of the scheme is that there is no requirement to calculate second or higher derivatives of the image function. This makes the scheme robust in the presence of noise. The spatiotemporal kernels are of simple form, involving Gaussian functions, and are biologically plausible receptive fields. The validity of the scheme is demonstrated by application to both synthetic and real video images sequences and by direct comparison with another recently published scheme [Biol. Cybern. 63, 185 (1990)] for the measurement of complex optical flow.
Resumo:
We highlight our recent experimental work on an efficient molecular nonlinear optical crystal, 3-methoxy 4-hydroxy benzaldehyde (MHBA). Optical quality single crystals of MHBA were grown from mixtures of solvents and from melt. The overall absorption and transparency window were improved by growing them in a mixture of chloroform and acetone. The grown crystals were characterized for their optical transmission, mechanical hardness and laser damage. We have observed a strong correlation between mechanical properties and laser induced damage.
Resumo:
Transparent BaNaB9O15 (BNBO), BaLiB9O15 (BLBO) and SrLiB9O15 (SLBO) glasses were fabricated via the conventional melt-quenching technique. X-ray diffraction (XRD) and Differential thermal analysis (DTA) studies carried out on the as-quenched glasses confirmed their amorphous and glassy nature, respectively. The optical properties for these as-quenched glasses were investigated. The refractive index, optical band gap. Urbach energy and Fermi energy were determined. The average electronic polarizability calculated from the refractive index expression. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Soft-chemical oxidation of KTiOPO4-like KM(0.5)(V)Ti(0.5)(III)OPO(4) (M = Nb, Ta) using chlorine in CHCl3 is accompanied by partial deintercalation of potassium, yielding K(0.5)MV(0.5)Ti(0.5)(IV)OPO(4) compounds which are new non-linear optical materials that exhibit efficient second-harmonic generation of 1064 nm radiation, as does KTiOPO4.
Resumo:
This article describes a facile, low-cost, solution-phase approach to the large-scale preparation of Hg1-xCdxTe nanostructures of different shapes such as nanorods, quantum dots, hexagonal cubes of different sizes and different compositions at a growth temperature of 180 degrees C using an air stable Te source by solvothermal technique. The XRD spectrum shows that the crystals are cubic in their basic structure and reveals the variation in lattice constant as a function of composition. The size and morphology of the products were examined by scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The formation of irregular shaped particles and few nano-rods in the present synthesis is attributed to the cetyl trimethylammonium bromide (CTAB). The room temperature FTIR absorption and PL studies for a compositon of x = 0.8 gives a band gap of 1.1 eV and a broad emission in NIR region (0.5-0.9 eV) with all bands attributed to surface defects.
Resumo:
Layered lanthanide sulfate compounds with three different structures have been prepared and characterized. The compounds C10H10N2] La(SO4)(2)]center dot 2H(2)O (I), C10H10N2] La(SO4)(2)(H2O)(2)](2) (Ha), C10H10N2]Pr(SO4)(2)(H2O)(2)](2) (IIb), C10H10N2]Nd-2(SO4)(4)(H2O)(2)](2) (IIIa), C10H10N2]Sm-2(SO4)(4)(H2O)(2)](2) (IIIb), and C10H10N2]Eu-2(SO4)(4)(H2O)(2)] 2 (IIIC) have anionic lanthanide sulfate layers separated by protonated bipyridine molecules. The layers are formed by the connectivity between the lanthanide polyhedra and sulfate tetrahedra. The formation of a two-dimensional La-O-La layer (la), Pr-O-Pr chains (IIb), and a tetramer cluster (IIIa) is noteworthy. The compounds exhibit honeycomb (I), square (IIa, IIb), and honeycomb (IIIa-IIIc) net arrangements, when the connectivity between the lanthanide ions is considered. Optical studies indicate the observation of characteristic metal-centered emission at room temperature. The Nd compound (IIIa) exhibits a two-photon upconversion behavior.