204 resultados para Aligned ZnO Nanorods
Resumo:
We report on the novel flow sensing application of piezoelectric ZnO thin film deposited on Phynox alloy sensing element. Characterization of piezoelectric ZnO films deposited on Phynox (Elgiloy) substrate at different RF powers is discussed. ZnO films deposited at RF power of 100W were found to have fine c-axis orientation, possesses excellent surface morphology with lower rms surface roughness of 1.87 nm and maximum d(31) coefficient value 4.7 pm V-1. The thin cantilever strip of Phynox alloy with ZnO film as a sensing layer for flow sensing has been tested for flow rates ranging from 2 to 18 L min(-1). A detailed theoretical analysis of the experimental set-up showing the relationship between output voltage and force at a particular flow rate has been discussed. The sensitivity of now sensing element is similar to 18 mV/(L min(-1)) and typical response time is of the order of 20 m s. The sensing element is calibrated using in-house developed testing set-up. (C) 2012 Elsevier B.V. All rights reserved.
Resumo:
Here, we report the ZnO/poly(3,4-ethylenedioxythiophene) poly(styrenesulfonate) (PEDOT:PSS) based photodetectors that can response to ultraviolet as well as visible light. The temporal response of the heterostructures for various excitations in the ultraviolet (UV) and visible range are performed. The time constants are found to be excitation-dependent, the response to visible light is better as compared to UV. The reason behind the better response to UV light is the high level of defects present in ZnO as confirmed by the photoluminescence (PL) measurements. This is corroborated by the time resolved fluorescence (TRF) measurements which provides sufficient information behind the slow response time under the UV excitations. The possible explanation being the non-radiative recombinations occurring due to the traps or impurities present in the film which slows down the photoresponse.
Resumo:
In this work, Na0.33V2O5 center dot 1.5H(2)O nanorings/nanorods and Na0.33V2O5 center dot 1.5H(2)O/reduced graphene oxide (RGO) composites have been prepared through a facile hydrothermal route in acidic medium at 200 degrees C for 2 days. The hydrothermally derived products have been characterized by powder X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), Raman spectroscopy, UV-Visible spectroscopy, Thermogravimetric analysis (TGA), Field emission scanning electron microscopy (FESEM), Transmission electron microscopy (TEM) and electrochemical discharge-charge cycling in lithium ion battery. XRD pattern exhibits the layered structure of Na0.33V2O5 center dot 1.5H(2)O and the composite shows the presence of RGO at 2 theta = 25.8 degrees. FTIR spectrum shows that the band at 760 cm(-1) could be assigned to a V-OH2 stretching mode due to coordinated water. Raman spectrum shows that the band at 264 cm(-1) is due to the presence of water molecules between the layers. FESEM/TEM micrographs reveal that the products consist of nanorings of inner diameter 5 mu m and thickness of the ring is found to be 200-300 nm. Addition of exfoliated graphene oxide (EGO) destroys the formation of rings. The reduction of EGO sheets into RGO is also evidenced by the red shift of the absorbance peak from 228 nm to 264 nm. In this composite Na0.33V2O5 center dot 1.5H(2)O nanorods may adhere to the surface of RGO and/or embedded in the RGO nanosheets. As a result, an effective three-dimensional conducting network was formed by bridging RGO nanosheets, which can facilitate electron transport effectively and thus improve the kinetics and rate performance of Na0.33V2O5 center dot 1.5H(2)O nanorings/nanorods. The Na0.33V2O5 center dot 1.5H(2)O/RGO composites exhibited a discharge capacity of 340 mAh g(-1) at a current density of 0.1 mA g(-1) and also an improved cyclic stability. RGO plays a `flexible confinement' function to enwrap Na0.33V2O5 center dot 1.5H(2)O nanorods, which can compensate for the volume change and prevent the detachment and agglomeration of pulverized Na0.33V2O5 center dot 1.5H(2)O, thus extending the cycling life of the electrode. A probable reaction mechanism for the formation of Na0.33V2O5 center dot 1.5H(2)O nanorings is also discussed. (C) 2012 Elsevier B.V. All rights reserved.
Resumo:
Optically clear glasses in the ZnO-Bi2O3-B2O3 (ZBBO) system were fabricated via the conventional melt-quenching technique. Dielectric constant and loss measurements carried out on ZBBO glasses unraveled nearly frequency (1 kHz-10 MHz)-independent dielectric characteristics associated with significantly low loss (D = 0.004). However, weak temperature response was found with temperature coefficient of dielectric constant 18 +/- 4 ppm A degrees C-1 in the 35-250 A degrees C temperature range. The conduction and relaxation phenomena were rationalized using universal AC conductivity power law and modulus formalism respectively. The activation energy for relaxation determined using imaginary parts of modulus peaks was 2.54 eV which was close to that of the DC conduction implying the involvement of similar energy barriers in both the processes. Stretched and power exponents were temperature dependent. The relaxation and conduction in these glasses were attributed to the hoping and migration of Bi3+ cations in their own and different local environment.
Resumo:
Undoped and co-doped (Ag, Co) ZnO powders were synthesized by chemical co-precipitation method without using any capping agent. The X-ray diffraction results indicate that the undoped and co-doped ZnO powders have pure hexagonal structure and are consisting of nanosized single-crystalline particles. The size of the nanoparticles increases with increasing Ag concentration from 1 to 5 mol% as compared to that of undoped ZnO. The presence of substitution dopants of Ag and Co in the ZnO host material was confirmed by the Energy dispersive analysis of X-rays (EDAX). Optical absorption measurements indicate blue shift and red-shift in the absorption band edge upon doping concentration of Ag and blue emission was observed by photoluminescence (PL) studies.
Resumo:
Interaction of CdSe and ZnO nanocrystals with electron-donating tetrathiafulvalene (TTF) and electron-withdrawing tetracyanoethylene (TCNE) has been investigated. Isothermal calorimetry shows CdSe nanocrystals interact more strongly with TCNE than TTF. Interaction of larger CdSe nanocrystals with TCNE causes a red-shift in the band-edge emission because of agglomeration, while the smaller CdSe nanocrystals, exhibiting stronger interaction with TCNE modify the optical gap of the nanocrystal. Luminescence of CdSe gets quenched sharply after addition of both TTF and TCNE. ZnO nanocrystals also exhibit luminescence quenching to lesser extent. Defect-emission of ZnO nanocrystals gets red or blue-shifted after interaction with TTF or TCNE respectively. (C) 2012 Elsevier B. V. All rights reserved.
Resumo:
A combination of chemical and thermal annealing techniques has been employed to synthesize a rarely reported nanocup structure of Mn doped ZnO with good yield. Nanocup structures are obtained by thermally annealing the powder samples consisting of nanosheets, synthesized chemically at room temperature, isochronally in a furnace at 200-500 degrees C temperature range for 2 h. Strong excitonic absorption in the UV and photoluminescence (PL) emission in UV-visible regions are observed in all the samples at room temperature. The sample obtained at 300 degrees C annealing temperature exhibits strong PL emission in the UV due to near-band-edge emission along with very week defect related emissions in the visible regions. The synthesized samples have been found to be exhibiting stable optical properties for 10 months which proved the unique feature of the presented technique of synthesis of nanocup structures. (C) 2012 Elsevier B.V. All rights reserved.
Resumo:
We report on the substrate assisted doping of ZnO nanowires grown by a vapor transport technique. The nanowires were grown non-catalytically on multiwalled carbon nanotubes (MWCNTs) and soda lime glass (SLG). Carbon from MWCNTs and sodium from SLG diffuse into ZnO during the growth and are distributed uniformly and provide doping. An advantage associated with the technique is that no conventional external dopant source is required to obtain doped ZnO nanowires. The diameter, length and hence the aspect ratio can easily be varied by changing the growth conditions. The transport studies on both carbon and sodium doped ZnO support the p-type nature of ZnO. The p-type nature of carbon doped ZnO is stable for at least eight months.
Resumo:
In this study, the dielectric properties of PVA/ZnO nanocomposites films were evaluated. The composites were prepared by a solution casting technique. The dispersion and functionalization of the ZnO nanoparticles in the composite films were characterized by spectroscopic technique. The surface morphology of the PVA/ZnO nanocomposites films were elucidated using AFM. The charge transport properties were evaluated based on the dielectric and impedance spectroscopy techniques. Low ZnO loading composite shows low dielectric value at higher frequency and behaves as a lossless material. The complex impedance spectra suggest the change in conductivity, due to the change in bulk resistance of the materials and less relaxation time. Thus, all PVA/ZnO nanocomposites behave as lossless materials above 10(6) Hz indicating the composites are useful in microwave application. (c) 2012 Elsevier Ltd. All rights reserved.
Resumo:
A zinc-nicotinate complex has been prepared by direct reaction of zinc acetate and nicotinic acid in the presence of template tetramethylethylenediamine and is characterized by elemental analysis, FTIR, and TGA/DTA. The Zn complex was a precursor for the synthesis of ZnO nanoparticles. A correlation of the thermal and spectral properties of the precursor complex with its structure has been discussed. Thermolysis under air was studied by thermogravimetry, and the resulting ZnO product was characterized by XRD and TEM, showing compact particles with a diameter of about 1750nm.
Resumo:
In this article, we have reported the controlled synthesis of uniformly grown zinc oxide nanoparticles (ZnO NPs) films by a simple, low-cost, and scalable pulsed spray pyrolysis technique. From the surface analysis it is noticed that the as-deposited films have uniformly dispersed NPs-like morphology. The structural studies reveal that these NPs films have highly crystalline hexagonal crystal structure, which are preferentially orientated along the (001) planes. The size of the NPs varied between 5 and 100 nm, and exhibited good stoichiometric chemical composition. Raman spectroscopic analysis reveals that these ZnO NPs films have pure single phase and hexagonal crystal structure. These unique nanostructured films exhibited a low electrical resistivity (5 Omega cm) and high light transmittance (90 %) in visible region.
Resumo:
We have studied the preparation of zinc oxide nanoparticles loaded in various weight percentages in ortho-chloropolyaniline by in situ polymerization method. The length of the O-chloropolyaniline tube is found to be 200 nm and diameter is about 150 nm wherein the embedded ZnO nanoparticles is of 13 nm as confirmed from scanning electron microscopy as well as transmission electron microscopy characterizations. The presence of the vibration band of the metal oxide and other characteristic bands confirms that the polymer nanocomposites are characterized by their Fourier transmission infrared spectroscopy. The X-ray diffraction pattern of nanocomposites reveals their polycrystalline nature. Electrical property of nanocomposites is a function of the filler as well as the matrix. Cole-Cole plots reveal the presence of well-defined semicircular arcs at high frequencies which are attributed to the bulk resistance of the material. Among all nanocomposites, 30 wt% shows the low relaxation time of 151 s, and hence it has high conductivity.
Resumo:
We report, strong ultraviolet (UV) emission from ZnO nanoparticle thin film obtained by a green synthesis, where the film is formed by the microwave irradiation of the alcohol solution of the precursor. The deposition is carried out in non-aqueous medium without the use of any surfactant, and the film formation is quick (5 min). The film is uniform comprising of mono-disperse nanoparticles having a narrow size distribution (15-22 nm), and that cover over an entire area (625 mm(2)) of the substrate. The growth rate is comparatively high (30-70 nm/min). It is possible to tune the morphology of the films and the UV emission by varying the process parameters. The growth mechanism is discussed precisely and schematic of the growth process is provided.
Comparison of ZnO films deposited on indium tin oxide and soda lime glass under identical conditions
Resumo:
ZnO films have been grown via a vapour phase transport (VPT) on soda lime glass (SLG) and indium-tin oxide (ITO) coated glass. ZnO film on ITO had traces of Zn and C which gives them a dark appearance while that appears yellowish-white on SLG. X-ray photoelectron spectroscopy studies confirm the traces of C in the form of C-O. The photoluminescence studies reveal a prominent green luminescence band for ZnO film on ITO. (C) 2013 Author(s).
Resumo:
Nondegenerate pump probe differential transmission experiments on gold nanorods with varying longitudinal surface plasmon resonance have revealed a new phenomenon where the polarity of the transient transmission signal can be reversibly switched between photo bleaching and photo-induced absorption by controlling probe fluence. Under the usual case where probe fluences are nominal, photo bleaching effect is observed for the nanorods with longitudinal surface plasmon resonance energy smaller than the probe photon energy. The laser-induced melting of the nanorods or change in their shape is ruled out for the observed optical switching effect. A quantitative understanding of the results is attempted by invoking a cascaded two-photon absorption dominant beyond a threshold probe fluence of similar to 75 mu J/cm(2).