160 resultados para corrosive wear
Resumo:
The relative significance of corrosive and abrasive wear in ore grinding is discussed. Laboratory marked ball wear tests were carried out with magnetic taconite and quartzite under different conditions, namely dry, wet and in the presence of an organic liquid. The effect of different modes of aeration and of pyrrhotite addition on the ball wear using mild steel, high carbon low alloy steel and austenitic stainless steel balls was evaluated. Results indicate that abrasive wear plays a significant role in ore grinding in the absence of sulfides, and rheological properties of the ore slurry influenced such wear. The effect of oxygen on corrosive wear becomes increasingly felt in the presence of a sulfide mineral such as pyrrhotite. Wear characteristics of the three types of ball materials under different grinding conditions are illustrated.
Resumo:
Laboratory results of marked-ball wear tests are used to discuss the relative significance of corrosive and abrasive wear in wet grinding. The electrochemical mechanism was investigated by correlating the corrosive wear with the corrosion current obtained from polarization curves under abrasion. Slurry rheology governs the manner in which ground slurries coat grinding balls, thereby influencing not only the grinding efficiency but also abrasive wear. The effects of percent solids and a grinding aid are illustrated.
Resumo:
Marked-ball grinding tests were carried out under different grinding conditions and environments. Three types of balls were used, namely, cast hyper steel, high chrome cast iron and EN-31 (forged), which cover a wide range of chemical composition, microstructure and media hardness. The effect of pulp density on ball wear and grinding efficiency was also studied. Relative pulp viscosities at different percent solids for the ore slurry were also determined. As the Kudremukh ore contained about 0.2% pyrite, the effect of addition of pyrite on ball wear was studied separately. Results of marked-ball grinding tests indicated that ball wear increased with time and showed a sharp increase for wet grinding over dry grinding. Ball wear under wet grinding conditions was also influenced by the gaseous atmosphere in the mill. At 70% solids, the best results in terms of reduced ball wear coupled with satisfactory grinding efficiency were obtained. The influence of oxygen on the corrosive wear of grinding balls was increasingly felt only if sulphide minerals such as pyrite were also present in the ore. The various ball materials could be arranged in the following order with respect to their overall wear resistance: high chrome cast iron > EN-31 (forged) > cast hyper steel.Possible ball wear mechanisms involved in the grinding of Kudremukh ore are discussed.
Resumo:
Marked ball grinding tests were carried out in the laboratory using high carbon low alloy steel (cast and forged) and high chrome cast iron balls. Relative ball wear as a function of grinding period and milling conditions was evaluated for the different type of ball materials in the grinding of lead-zinc sulphide and phosphate ores. Results indicated that ball wear increased with time and showed a sharp increase for wet grinding over dry grinding. Ball wear under wet grinding conditions was also influenced by the gaseous atmosphere in the mill. The influence of oxygen on the corrosive wear of grinding balls was increasingly felt in case of sulphide ore grinding. The grinding ball materials could be arranged in the following order with respect to their overall wear resistance:
Resumo:
With the progress in modern technological research, novel biomaterials are being largely developed for various biomedical applications. Over the past two decades, most of the research focuses on the development of a new generation of bioceramics as substitutes for hard tissue replacement. In reference to their application in different anatomical locations of a patient, newly developed bioceramic materials can potentially induce a toxic/harmful effect to the host tissues. Therefore, prior to clinical testing, relevant biochemical screening assays are to be performed at the cellular and molecular level, to address the issues of biocompatibility and long term performance of the implants. Along with testing strategies in the bulk material toxicity, a detailed evaluation should also be conducted to determine the toxicity of the wear products of the potential bioceramics. This is important as the bioceramics are intended to be implanted in patients with longer life expectancy and notwithstanding, the material will eventually release finer (mostly nanosized) sized debris particles due to continuous wear at articulating surfaces in the hostile corrosive environment of the human body. The wear particulates generated from a biocompatible bioceramic may act in a different way, inducing early/late aseptic loosening at the implant site, resulting in osteolysis and inflammation. Hence, a study on the chronic effects of the wear particulates, in terms of local and systemic toxicity becomes the major criteria in the toxicity evaluation of implantable bioceramics. In this broad perspective, this article summarizes some of the currently used techniques and knowledge in assessing the in vitro and in vivo cytotoxicity and genotoxicity of bioceramic implant materials. It also addresses the need to conduct a broad evaluation before claiming the biocompatibility and clinical feasibility of any new biomaterial. This review also emphasizes some of the case studies based on the experimental designs that are currently followed and its importance in the context of clinical applications.
Resumo:
The present work provides an insight into the dry sliding wear behavior of titanium based on synergy between tribo-oxidation and strain rate response. Pin-on-disc tribometer was used to characterize the friction and wear behavior of titanium pin in sliding contact with polycrystalline alumina disk under ambient and vacuum condition. The sliding speed was varied from 0.01 to 1.4 ms(-1), normal load was varied from 15.3 to 76 N and with a sliding distance of 1500 m. It was seen that dry sliding wear behavior of titanium was governed by combination of tribo-oxidation and strain rate response in near surface region of titanium. Strain rate response of titanium was recorded by conducting uni-axial compression tests at constant true strain rate of 100 s(-1) in the temperature range from 298 to 873 K. Coefficient of friction and wear rate were reduced with increased sliding speed from 0.01 to 1.0 ms(-1). This is attributed to the formation of in situ self lubricating oxide film (TiO) and reduction in the intensity of adiabatic shear band cracking in the near surface region. This trend was confirmed by performing series of dry sliding tests under vacuum condition of 2 x 10(-4) Torr. Characterization tools such as optical microscopy, scanning electron microscopy, and X-ray diffractometer provided evidence of such processes. These experimental findings can be applied to enhance the dry sliding wear behavior of titanium with proper choice of operating conditions such as sliding speed, normal load, and environment.
Resumo:
Controversy exists in the published literature as to the effect of silicon content and pressure on the dry sliding wear of Al---Si alloys. The present paper attempts to clarify the question by reporting a statistical analysis of data obtained from factorially designed experiments conducted on a pinon-disc machine in the pressure range 0.105–1.733 MPa and speed range 0.19–0.94 m s−1. Under these conditions it was found that, in the range 4–24 wt.% Si, wear of binary unmodified alloys does not significantly differ between the alloys. However, it is significantly less than that corresponding to an alloy containing no silicon. The effect of pressure on wear rate was found to be linear and monotonie and, over the narrow range of speeds used, the wear rate was found to be unaffected by speed. The coefficient of friction was found to be insensitive to variations in silicon content, pressure and speed.
Resumo:
The effect of corundum particle content on the wear of aluminium was studied. Composites of different corundum contents were tested for their wear characteristics. Hardness and density measurements were made on specimens before and after test. Specimens were examined by scanning electron microscopy in the as-compacted, sintered and worn states. The wear decreased as the oxide content increased, showing an optimum value at a composition range of 25 wt.%–35 wt.% of corundum. The mechanism of reinforcement and its effect on the operative wear mode are discussed.
Resumo:
The effect of corundum particle content on the wear of aluminium was studied. Composites of different corundum contents were tested for their wear characteristics. Hardness and density measurements were made on specimens before and after test. Specimens were examined by scanning electron microscopy in the as-compacted, sintered and worn states. The wear decreased as the oxide content increased, showing an optimum value at a composition range of 25 wt.%–35 wt.% of corundum. The mechanism of reinforcement and its effect on the operative wear mode are discussed.
Resumo:
In the present investigation, the wear behaviour of a creep-resistant AE42 magnesium alloy and its composites reinforced with Saffil short fibres and SiC particles in various combinations is examined in the longitudinal direction i.e., the plane containing random fibre orientation is perpendicular to the steel counter-face. Wear tests are conducted on a pin-on-disc set-up under dry sliding condition having a constant sliding velocity of 0.837 m/s for a constant sliding distance of 2.5 km in the load range of 10-40 N. It is observed that the wear rate increases with increase in load for the alloy and the composites, as expected. Wear rate of the composites is lower than the alloy and the hybrid composites exhibit a lower wear rate than the Saffil short fibres reinforced composite at all the loads. Therefore, the partial replacement of Saffil short fibres by an equal volume fraction of SiC particles not only reduces the cost but also improves the wear resistance of the composite. Microstructural investigation of the surface and subsurface of the worn pin and wear debris is carried out to explain the observed results and to understand the wear mechanisms. It is concluded that the presence of SiC particles in the hybrid composites improves the wear resistance because these particles remain intact and retain their load bearing capacity even at the highest load employed, they promote the formation of iron-rich transfer layer and they also delay the fracture of Saffil short fibres to higher loads. Under the experimental conditions used in the present investigation, the dominant wear mechanism is found to be abrasion for the AE42 alloy and its composites. It is accompanied by severe plastic deformation of surface layers in case of alloy and by the fracture of Saffil short fibres as well as the formation of iron-rich transfer layer in case of composites.
Resumo:
A pin-on-disc test configuration has been used to examine the formation of the strain-hardened projection, or wear lips, especially at the trailing edge of the pin during dry sliding of aluminium alloys against steel discs. The mechanism of formation of such wear lips is studied with the aid of optical and electron microscopes. The plastic deformation of the pin, growth and eventual removal of the wear lip as wear debris are elucidated. The size and shape of the wear lips in pins of different shapes, i.e. square, rectangular, triangular and circular cross-sections, are described.
Resumo:
Some tribological properties of a mica-dispersed Al-4%Cu-1.5%Mg alloy cast by a conventional foundry technique are reported. The effect of mica dispersion on the wear rate and journal bearing performance of the matrix alloy was studied under different pressures and under different interface friction conditions. The dispersion of mica was found (a) to increase the wear rate of the base alloy, (b) to decrease the temperature rise during wear and (c) to improve the ability of the alloy to resist seizure.