37 resultados para W
Resumo:
Heterometallic {3d-4f-5d} aggregates with formula [{LMe2Ni(H2O)Ln(H2O)4.5}2{W(CN)8}2]·15H2O, (LMe2 stands for N,N-2,2-dimethylpropylenedi(3-methoxysalicylideneiminato) Schiff-base ligand) with Ln = Gd, Tb, Dy, have been obtained by reacting bimetallic [LMe2Ni(H2O)2Ln(NO3)3] and Cs3{W(CN)8} in H2O. The hexanuclear complexes are organized in 1-D arrays by means of hydrogen bonds established between the solvent molecules coordinated to Ln and the CN ligands of an octacyanometallate moiety. The X-ray structure was solved for the Tb derivative. Magnetic behavior indicates ferromagnetic {W–Ni} and {Ni–Ln} interactions (JNiW = 18.5 cm-1, JNiGd = 1.85 cm-1) as well as ferromagnetic intermolecular interactions mediated by the H-bonds. Dynamic magnetic susceptibility studies reveal slow magnetic relaxation processes for the Tb and Dy derivatives, suggesting SMM type behavior for these compounds.
Resumo:
We study the possibility of using W pair production and leptonic decay of one of the W's at the ILC with polarized beams as a probe of the Littlest Higgs Model. We consider cross-sections, polarization fractions of the W's, leptonic decay energy and angular distributions, and left-right polarization asymmetry as probes of the model. With parameter values allowed by present experimental constraints detectable effects on these observables at typical ILC energies of 500 GeV and 800 GeV will be present. Beam polarization is further found to enhance the sensitivity.
Resumo:
We describe an investigation of (Ba3MMWO9)-M-II-W-IV oxides for M-II = Ca, Zn, and other divalent metals and M-IV = Ti, Zr. In general, a 1:2-ordered 6H (hexagonal, P6(3)/mmc) perovskite structure is stabilized at high temperatures (1300 degrees C) for all of the (Ba3MTiWO9)-Ti-II oxides investigated. An intermediate phase possessing a partially ordered 1:1 double perovskite (3C) structure with the cation distribution, Ba-2(Zn2/3Ti1/3)(W2/3Ti1/3)O-6, is obtained at 1200 degrees C for Ba3ZnTiWO9. Sr substitution for Ba in the latter stabilizes the cubic 3C structure instead of the 6H structure. A metastable Ba3CaZrWO9 that adopts the 3C (cubic, Fm (3) over barm) structure has also been synthesized by a low-temperature metathesis route. Besides yielding several new perovskite oxides that may be useful as dielectric ceramics, the present investigation provides new insights into the complex interplay of crystal chemistry (tolerance factor) and chemical bonding (anion polarization and d(0)-induced distortion of metal-oxygen octahedra) in the stabilization of 6H versus 3C perovskite structures for the (Ba3MMWO9)-M-II-W-IV series.
Resumo:
We describe an investigation of (Ba3MMWO9)-M-II-W-IV oxides for M-II = Ca, Zn, and other divalent metals and M-IV = Ti, Zr. In general, a 1:2-ordered 6H (hexagonal, P6(3)/mmc) perovskite structure is stabilized at high temperatures (1300 degrees C) for all of the (Ba3MTiWO9)-Ti-II oxides investigated. An intermediate phase possessing a partially ordered 1:1 double perovskite (3C) structure with the cation distribution, Ba-2(Zn2/3Ti1/3)(W2/3Ti1/3)O-6, is obtained at 1200 degrees C for Ba3ZnTiWO9. Sr substitution for Ba in the latter stabilizes the cubic 3C structure instead of the 6H structure. A metastable Ba3CaZrWO9 that adopts the 3C (cubic, Fm (3) over barm) structure has also been synthesized by a low-temperature metathesis route. Besides yielding several new perovskite oxides that may be useful as dielectric ceramics, the present investigation provides new insights into the complex interplay of crystal chemistry (tolerance factor) and chemical bonding (anion polarization and d(0)-induced distortion of metal-oxygen octahedra) in the stabilization of 6H versus 3C perovskite structures for the (Ba3MMWO9)-M-II-W-IV series.
Resumo:
W/Cr codoped Bi4Ti3O12 ceramics, Bi4Ti3-xWxO12+x+0.2 wt%Cr2O3 (BITWC, x=0-0.15), were prepared using a solid-state reaction method. The crystallographic evolution and phase analysis were distinctly determined focusing on the X-ray diffraction peak changes in (020)/(200) and (220)/(1115) diffraction planes, by which the lattice parameters, a, b, and c can be refined. The thermal variations of permittivity, dielectric loss (tan delta), impedance, and electrical conductivity properties were characterized. A decrease in the values of Curie temperature from 675 degrees to 640 degrees C and an increase in the values of the dielectric constant due to an increase of W6+/Cr3+ content were observed. The highest piezoelectric constant, d(33) of 22 pC/N, was achieved with the composition of Bi4Ti2.975W0.025O12.025+0.2 wt% Cr2O3. Also, this composition had a lower electrical conductivity than the other investigated compositions.
Resumo:
The phase diagram of the Ni-W-O system at 1200 K was established by metallographic and X-ray identification of the phases present after equilibration at controlled oxygen potentials. The oxygen partial pressures over the samples were fixed by metered streams of CO+CO2 gas mixtures. There was only one ternary oxide, nickel tungstate (NiWO4), in the Ni-W-O system at a total pressure of 1 atm, and this compound decomposed to a mixture of Ni+WO2.72 on lowering the oxygen potential. The Gibbs' free energy of formation of NiWO4 was determined from the measurement of the e.m.f. of the solid oxide galvanic cell, Pt, Ni+NiWO4+WO2.72/CaO-ZrO2/Ni+NiO, Pt and thermodynamic properties of tungsten and nickel oxides available in the literature. For the reaction, NiO(s)+WO3(s)rarrNiWO4(s) DeltaG°=–10500–0.708 T (±250) cal mol–1.
Resumo:
Electron energy loss spectra (EELS) of Cr, Mo and W hexacarbonyls in the vapour phase are reported. Most of the bands observed are similar to those in optical spectra, but the two high energy transitions in the 9·8–11·2 eV region are reported here for the first time. Based on the orbital energies from the ultraviolet photoelectron spectra and the electronic transition energies from EELS and earlier optical studies, the molecular energy level schemes of these molecules are constructed.
Resumo:
An interdiffusion study is conducted on the Co-W system by a diffusion couple technique. The interdiffusion coefficient of the Co(W) solid solution and the Co7W6 mu phase is determined. The activation energy is found to increase with the W content of the Co(W) solid solution. (C) 2010 Elsevier Ltd. All rights reserved.
Resumo:
We consider the possibility of fingerprinting the presence of heavy additional Z' bosons that arise naturally in extensions of the standard model such as E-6 models and left-right symmetric models, through their mixing with the standard model Z boson. By considering a class of observables including total cross sections, energy distributions and angular distributions of decay leptons we find significant deviation from the standard model predictions for these quantities with right-handed electrons and left-handed positrons at root s= 800GeV. The deviations being less pronounced at smaller centre of mass energies as the models are already tightly constrained. Our work suggests that the ILC should have a strong beam polarization physics program particularly with these configurations. On the other hand, a forward backward asymmetry and lepton fraction in the backward direction are more sensitive to new physics with realistic polarization due to interesting interplay with the neutrino t-channel diagram. This process complements the study of fermion pair production processes that have been considered for discrimination between these models.
Resumo:
Three features of avian sex chromosomes - female heterogamety (ZZ male, ZW female), the apparently inactive state of the W chromosome, and dose-dependent expression of Z-linked genes - are examined in regard to their possible relation to sex determination. It is proposed that the W chromosome is facultatively heterochromatic and that the Z and W chromosomes carry one or more homologous sex-determination genes. The absence of dosage compensation in ZZ embryos, and W inactivation in ZW embryos, would then bring about a 2n(ZZ)-n(ZW) inequality in the effective copy number of such genes. The absence of dosage compensation of Z-linked genes in ZZ embryos is viewed as a means by which two copies of Z-W homologous sex determination genes are kept active to meet the requirements of testis determination. W inactivation may promote ovarian development by reducing the effective copy number of these genes from 2n to n. If there is a W-specific gene for femaleness, spread of heterochromatization to this gene in cells forming the right gonadal primordium may explain the latter's normally undifferentiated state; reversal of heterochromatization may similarly explain the development of the right gonad into a testis following left ovariectomy.
Resumo:
Electron microscopy and diffraction studies of ordering in stoichiometric Ni-20%W and off-stoichiometric Ni-15%W alloys have been carried out. The specimens of Ni-20%W were first disordered at 1398 K for 4 h and then quenched rapidly into water. Short range order (SRO) spots were observed at {1 1/2 0}* positions. Two hitherto unknown metastable phases: D-2h(25)-Ni2W and DO22-Ni3W were observed in the diffraction patterns. Long range order (LRO) transformations were studied at 1103 and 1213 K. Kinetics and mechanism of transformations have been identified. Ni-15%W specimens were solution treated at 1523 K for 1 h followed by quenching in water. SRO spots similar to those found in Ni-20%W were observed in this alloy as well. The transition to LRO was studied at 1093 K. Distinct Ni4W precipitates could be observed after 5 h of annealing at this temperature. After 100 h of annealing precipitates were found to grow into faceted shape coherent with the disordered matrix. After prolonged annealing for over 150 h the Ni4W precipitates began to lose coherency by the generation of misfit dislocations. The microstructural observations have been compared for the stoichiometric and off-stoichiometric alloys.